Abstract
The purpose of the present disclosure is to provide a pre-coating processing method and a pre-coating processing system (1) for fiber-reinforced thermoplastic member, which can achieve the coating adherence required in the field of aircraft. In a pre-coating processing method according to the present disclosure, a to-be-coated surface of a fiber-reinforced thermoplastic plastic member (2) is subjected to an activation treatment: in which the to-be-coated surface is activated under a condition such that the surface free energy of the to-be-coated surface immediately after the activation treatment reaches at least 70 mJ/m2; and in which the to-be-coated surface is heated to a temperature at which the modulus of elasticity of the to-be-coated surface becomes lower than that at normal temperature.
Description
Claims
  • 1. A pre-coating processing method for a fiber-reinforced thermoplastic member, the method comprising: performing activation treatment on a coating target surface of the fiber-reinforced thermoplastic member before coating,wherein the activation treatment includes activating the coating target surface under a condition that surface free energy of the coating target surface immediately after the activation treatment is 70 mJ/m2 or higher, andheating the coating target surface to a temperature at which an elastic modulus of the coating target surface is lowered, compared to an elastic modulus at a normal temperature.
  • 2. The pre-coating processing method for a fiber-reinforced thermoplastic member according to claim 1, wherein the temperature is a temperature at which a reduction range of the elastic modulus due to the heating is 5% or larger, compared to 100% of the elastic modulus of the coating target surface at the normal temperature.
  • 3. The pre-coating processing method for a fiber-reinforced thermoplastic member according to claim 1, wherein in the fiber-reinforced thermoplastic member, a reinforcing fiber is a carbon fiber, and a preform is a low melting point polyaryl ether ketone, andduring the heating, the heating is performed on the coating target surface until the temperature of the coating target surface reaches 90° C. or higher.
  • 4. The pre-coating processing method for a fiber-reinforced thermoplastic member according to claim 1, wherein in the activation treatment, a temperature of the coating target surface is measured, andwhen the temperature of the coating target surface does not reach the temperature at which the elastic modulus of the coating target surface is lowered, compared to the elastic modulus at the normal temperature, based on the temperature obtained by the measurement, a condition for activating the coating target surface and a condition for the heating are changed to reach the temperature at which the elastic modulus of the coating target surface is lowered, compared to the elastic modulus at the normal temperature.
  • 5. The pre-coating processing method for a fiber-reinforced thermoplastic member according to claim 4, wherein correlation data in which a temperature measured by a temperature measuring device adopting a contact type and a temperature measured by a temperature measuring device adopting a contactless type are associated with each other is prepared in advance,the activation treatment includes measuring the temperature of the coating target surface by the temperature measuring device adopting the contactless type,correcting the temperature obtained by the temperature measuring device, based on the correlation data, andchanging the condition for activating the coating target surface and the condition for the heating, based on the corrected temperature.
  • 6. A pre-coating processing system which performs surface treatment on a coating target surface of a fiber-reinforced thermoplastic member before coating, the system comprising: an activation device that activates the coating target surface;a heating device that heats the coating target surface;a temperature measuring device that measures a temperature of the coating target surface; anda control device electrically connected to the activation device, the heating device, and the temperature measuring device,wherein the control device includes a feedback controller that outputs a feedback signal for changing settings of the activation device and the heating device to the activation device and the heating device, based on the temperature obtained by the temperature measuring device.
  • 7. The pre-coating processing system according to claim 6, wherein the temperature measuring device adopts a contactless type,the control device includes a correction unit that corrects the temperature obtained by the temperature measuring device adopting the contactless type and outputs a corrected temperature signal to the feedback controller, andthe correction unit corrects the temperature obtained by the temperature measuring device adopting the contactless type, based on correlation data in which a temperature measured by the temperature measuring device adopting a contact type and a temperature measured by the temperature measuring device adopting the contactless type are associated with each other.