- 1. An alumina coated phosphor treatment process comprising the following steps:
- step 1--fluidizing a manganese activated zinc silicate phosphor having an alumina protective coating and having a particle size of about 10-12 microns in an isothermal fluidized bed to form a fluidized phosphor powder, the alumina coating having been applied through chemical vapor deposition;
- step 2--heating said fluidized phosphor powder to form an annealed phosphor powder, wherein said heating is carried out at a temperature from about 200.degree. C. to about 850.degree. C. and for a period of time sufficient to preclude adversely affecting said alumina protective coating of said phosphor during subsequent water-based suspension processing and to preclude detrimentally altering said phosphor;
- step 3--cooling said annealed phosphor powder from step 2 to form a cooled annealed phosphor powder; and
- step 4--adding said cooled annealed phosphor powder from step 3 to a water-base suspension.
- 2. An alumina coated phosphor treatment process in accordance with claim 1 wherein said period of time being from about 15 minutes to about 20 hours.
- 3. An alumina coated phosphor treatment process in accordance with claim 1 wherein said temperature in Step 2 being from about 750.degree. C. to about 770.degree. C. and said period of time being from about 1 hour to about 4 hours.
Parent Case Info
This is a continuation-in-part of copending application Ser. No. 07/746,162, filed on Aug. 14, 1991, now abandoned, which is a continuation of application Ser. No. 07/306,129, filed on Feb. 6, 1989, and now abandoned.
US Referenced Citations (4)
Continuations (1)
|
Number |
Date |
Country |
Parent |
306129 |
Feb 1989 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
746162 |
Aug 1991 |
|