Preform for producing containers with an inner partition from a thermoplastic material

Abstract
A preform (9) made of thermoplastic material and including a body (11) provided with an at least partially longitudinally extending inner partition (10). The preform is used for molding and particularly blow molding or stretch-blow molding a container with a body having opposed portions defining hollow recesses with inwardly-directed convex surfaces, said portions being spaced apart by said inner partition. In a straight cross-sectional view, the body (11) has a non-circular outline with two opposed portions (a, b) separated by a minimum distance (d1) that is smaller than the distances between the other pairs of opposed portions of said outline. The inner partition (10) extends between said two opposed portions (a, b), and said distance (d1) is such that, relative to the periphery of the body (11) of the preform, during molding, the inner partition (10) is transversely stretched at a rate equal to that at which the body (11) is transversely or peripherally stretched.
Description




FIELD OF THE INVENTION




The present invention relates to improvements made to preforms made of thermoplastic, having a body provided with an at least partially longitudinally extended internal partition and intended for the manufacture, by molding, especially by blow molding or by stretch-blow molding, of a container whose body has opposed portions forming hollow recesses with inwardly directed convex surfaces, said recesses being braced by said internal partition.




BACKGROUND OF THE INVENTION




It is known to provide containers, especially bottles, made of a thermoplastic such as polyethylene terephthalate PET, polyethylene naphthalate PEN, or another thermoplastic, with an internal partition. Such a partition may be complete, i.e. it may extend over the entire height of the container, in order to divide the internal volume of the container into two chambers containing two respective liquids which must not be mixed together before being poured. As shown in

FIG. 1

of the appended drawing, the partition


1


may also be partial, i.e. it may extend only over part of the length of the body


2


of the container


3


, in order to retain (bracing) two opposed portions of the body of the container, for example in order to maintain two gripping recesses


4


hollowed out in the body of a container filled with a pressurized liquid, which recesses, even if they were not reinforced, would risk being deformed due to the effect of the pressure of the liquid.




It is known to manufacture such containers from preforms which themselves are provided with a totally or partially longitudinally extended internal partition depending on the type of final container to be obtained. Such a preform


5


with a partially longitudinally extended internal partition


6


, intended for the manufacture of the container in

FIG. 1

, is illustrated in

FIGS. 2 and 3

of the appended drawing, respectively as a side view in

FIG. 2 and

, in the case of

FIG. 3

, in a cross-sectional top view on the line II—II of FIG.


2


. It has a general structure similar to that of a partitionless preform with a neck


7


and a thick-walled body


8


which are conventionally shaped. The internal partition


6


has a thickness appreciably smaller than that of the thick wall of the body.




When this known preform, after it has been heated, is subjected to a stretching or stretch-blowing process in order to obtain a container, the internal partition stretches, as does the wall of the body: the longitudinal stretch ratio of the partition is identical to that undergone by the body (for example, in order to be specific, typically 2.22 to 3.5 for the PET grades currently used on an industrial scale). On the other hand, when the body of the container to be obtained has to have a localized transverse necking—for example distance between the bottom of the gripping recesses


4


of the container of FIG.


1


—, the transverse stretch ratio of the partition is locally very much less than the transverse (or perimetric) stretch ratio of the body of the container: in order to be specific, the transverse or perimetric stretch ratio of the body is generally at least about 4, while the transverse stretch ratio undergone by the partition remains here less than 4.




As a result, there is a disadvantageous difference between the properties of the material of the partition and of the material of the body of the container: since its material has not undergone sufficient transverse elongation, in order to orient the molecular chains in a complementary fashion the partition is subject to deformation when the container is subsequently exposed to severe conditions of use and the partition is no longer capable of effectively ensuring its bracing function.




BRIEF DESCRIPTION OF THE DRAWINGS





FIG. 1

is a drawing of a container having a partition formed therein for maintaining gripping recesses.





FIG. 2

is a drawing of a preform for the container of

FIG. 1

with a partial section view of the longitudinally extended internal partition.





FIG. 3

is a cross-sectional view of the preform shown in

FIG. 2

along the line III-III.





FIGS. 4 and 5

are cross-sectional views of preforms in accordance with the present invention.





FIGS. 6 and 7

are cross-sectional views of preforms in accordance with the present invention having their respective partitions joined by rounded parts of relatively large radius.











DETAILED DESCRIPTION OF THE INVENTION




The object of the invention is specifically to remedy this drawback and to provide a technical solution which allows, during the blowing or stretch-blowing process, a transverse elongation ratio substantially identical for the body of the preform and for the internal partition so that the constituent materials of each of them have appreciably similar physical and mechanical properties and behave in a homogeneous fashion.




To these ends, and with reference to

FIGS. 4 and 5

of the appended drawing illustrating, respectively, in a cross-sectional top view and on an appreciably greater scale than that in

FIG. 3

, two possible embodiments of a preform according to the invention which are given by way of non-limiting examples, a preform


9


as indicated in the preamble is essentially characterized, being designed in accordance with the invention, in that its body


11


has, in cross section, a noncircular outline with two opposed portions a and b separated from each other by a minimum distance d


1


which is less than the distances separating the other pairwise opposed portions of said outline, in that the internal partition


10


extends between said two opposed portions a, b separated by a minimum distance d


1


and in that said minimum distance d


1


is chosen, with respect to the perimeter of the body


11


of the preform, such that, during molding, the internal partition


10


undergoes a transverse stretch ratio which has approximately the same value as the transverse (or perimetric) stretch ratio undergone by the body.




Moreover, because of the fact that the correct execution of the blow-molding or stretch-blow molding process virtually excludes the use of preforms having a body of geometrically too complex shape, a preform


9


will advantageously be used whose body


11


has a maximum transverse dimension d


3


, regarded as being parallel to the internal partition


10


, which is appreciably less than its maximum transverse dimension d


2


, regarded as being approximately perpendicular to the internal partition


10


, the ratio of said transverse dimensions d


3


and d


2


then being such that, during molding, the internal partition


10


undergoes a transverse stretch ratio which is approximately identical to the transverse stretch ratio undergone by the body.




Although other arrangements may in principle be envisaged, it is, however, simpler and, for most practical applications, sufficient for the partition


10


to extend centrally in a plane of symmetry of the body


11


.




It is desirable for the use of preforms according to the invention to involve only minimal adaptations of plants for manufacturing containers in order to obtain final containers of given shapes and properties (dimensions, thickness of the walls, thermal resistance, etc.). However, the various ways of implementing the manufacturing process and said properties of the final containers are dependent on the properties of the starting preform, and in particular on the geometrical dimensions of its body (perimeter, wall thickness, etc.). Thus, a minimal modification of the manufacturing conditions and of the manufacturing plants in order to achieve a given container means that the preform according to the invention preserves the fundamental properties of the prior preforms for the use of which the current manufacturing plants are designed. The same applies in particular to the perimeter of the body.




It is therefore desirable in practice, whatever the geometrical shape given to the body of the preform, for the perimeter of the cross section of said body


11


, at least in that part of the latter which is provided with an internal partition, to maintain a value approximately similar to that of the perimeter of the cylindrical body of revolution


8


of the conventional preform, while the internal partition


10


is, in accordance with the abovementioned arrangements of the invention, narrower than the partition


6


of the prior preforms.




Having established this, the body


11


of the preform


9


designed according to the invention may be given any shape complying with this basic condition. In particular, the body may be cylindrical, especially with a cross section of oval or elliptical shape, as shown in

FIG. 4

; the two aforementioned portions a and b are then the parts of largest radius of curvature and the internal partition


10


extends along the minor axis of the oval or of the ellipse, the aforementioned distances d


1


and d


3


then being identical. It is also possible to provide, as shown in

FIG. 5

, a body having a bilobate outline, the partition


10


extending between the two lobes


12


; here, the aforementioned portions a and b are angular parts joining the two lobes together.




In order to facilitate the stretching process and to reinforce the container, it is desirable for the partition


10


to be joined to the wall of the preform by rounded parts of relatively large radius, as shown in

FIGS. 6 and 7

which correspond respectively to

FIGS. 4 and 5

.




In the same way as for the prior preforms, the internal partition may have a total or partial longitudinal extent with respect to the body of the preform. In the case of a partial partition, provision may optionally be made for the particular shape given to the body


11


of the preform according to the invention to extend longitudinally only in correspondence with the partition and, in the case of the rest of its longitudinal extent, for the body to be a cylinder of revolution, as in the case of a conventional preform.




By virtue of the arrangements adopted in accordance with the invention, an improved preform is produced which is capable of leading to a final container having an internal partition which has uniform properties and which is capable of withstanding, during use, thermal and/or mechanical stresses without thereby resulting in appreciable deformation of the overall body, including deformation of the portions of the latter which previously were subject to being deformed due to the effect of the pressure of a pressurized filling liquid and which are now correctly retained by the correctly stretched partition which appropriately fulfills its bracing function.




As goes without saying and as has already resulted from the foregoing, the invention is in no way limited to those of its modes of application and of its embodiments which have been more particularly envisaged; on the contrary, it encompasses all variants thereof.



Claims
  • 1. A thermoplastic preform, having a body provided with an at least partially longitudinally extended internal partition and intended for the manufacture, by molding, of a container whose body has opposed portions forming hollow recesses with inwardly-directed concave surfaces, said recesses being braced by said internal partition,wherein the body of the preform has, in cross section, an outline of noncircular shape with two opposed portions (a, b) separated from each other by a minimum distance (d1) less than the distances separating the other pairwise opposed portions of said outline, wherein the internal partition extends between said two opposed portions (a, b) separated by a minimum distance (d1), and wherein said minimum distance (d1) is chosen, with respect to the perimeter of the body of the preform, so that, during molding, the internal partition undergoes a transverse stretch ratio which has approximately the same value as the transverse or perimetric stretch ratio undergone by the body.
  • 2. Preform according to claim 1, wherein the body has a maximum transverse dimension (d3), regarded as being parallel to the internal partition, which is appreciably less than the maximum transverse dimension (d2), regarded as being approximately perpendicular to the internal partition, the ratio of said transverse dimensions (d3, d2) being such that, during molding, the internal partition undergoes a transverse stretch ratio which is approximately identical to the transverse stretch ratio undergone by the body.
  • 3. Preform according to claim 1, wherein the internal partition extends centrally in a plane of symmetry of the body.
  • 4. Preform according to claim 1, wherein at least in its part in correspondence with the internal partition, the body has a cylindrical contour.
  • 5. Preform according to claim 3, wherein the cross section of the body is approximately oval or elliptical, with the internal partition extending approximately along the minor axis of the oval or of the ellipse.
  • 6. Preform according to claim 1, wherein the body has a bilobate outline, the internal partition extending between the two lobes.
  • 7. Preform according to claim 1, wherein the internal partition extends over the entire length of the body.
  • 8. Preform according to claim 1, wherein the internal partition extends only over part of the length of the body, and in its part not provided with an internal partition, the body is a cylinder of revolution.
  • 9. Preform according to claim 1, wherein said molding is blow molding.
  • 10. Preform according to claim 1, wherein said molding is stretch-blow molding.
Priority Claims (1)
Number Date Country Kind
95 14707 Dec 1996 FR
PCT Information
Filing Document Filing Date Country Kind 102e Date 371c Date
PCT/FR96/01982 WO 00 11/4/1998 11/4/1998
Publishing Document Publishing Date Country Kind
WO97/21533 6/19/1997 WO A
US Referenced Citations (9)
Number Name Date Kind
3052368 Atkins et al. Sep 1962
5232108 Nakamura Aug 1993
5269441 O'Meara Dec 1993
5482170 Semersky et al. Jan 1996
5529195 Valyi Jun 1996
5579937 Valyi Dec 1996
5788794 Valyi Aug 1998
5837170 Valyi Nov 1998
5849241 Connan Dec 1998
Foreign Referenced Citations (2)
Number Date Country
531 536 Mar 1993 EP