Claims
- 1. A process for forming a bipolar electrode structure which comprises:
- a) introducing into a nip of a pressure roller assembly a laminate comprised of an electronegative layer; an electrically conductive impermeable intermediate layer of a thickness of 0.5 to 5 mils, a volume resistivity of 0.5 to 100 ohm-cm. and having pressure sensitive adhesive surfaces and an electropositive layer;
- b) passing said laminate through said pressure roller assembly at a pressure of from 20 to 500 psig. to effect adhesion of said electronegative and electropositive layers; and
- c) withdrawing said bipolar electrode structure from said pressure roller assembly.
- 2. The process for forming a bipolar electrode structure as defined in claim 1 wherein said pressure roller assembly is heated to a temperature of from 30.degree. to 180.degree. F.
Parent Case Info
This is a division, application Ser. No. 07/321,896, filed Mar. 10, 1989, now U.S. Pat. No. 4,892,797.
US Referenced Citations (1)
Number |
Name |
Date |
Kind |
4502903 |
Bruder |
Mar 1985 |
|
Foreign Referenced Citations (1)
Number |
Date |
Country |
48-14319 |
May 1973 |
JPX |
Divisions (1)
|
Number |
Date |
Country |
Parent |
321896 |
Mar 1989 |
|