Claims
- 1. A process for measuring an electrochemical activity of a slag layer (2) lying on a steel melt (3), using an electrochemical sensor which has a measuring cell (5) and a counter electrode (4), comprising immersing the measuring cell (5) and the counter electrode (4) in the steel melt (3), such that the measuring cell (5) and the counter electrode (4) are protected from contact with the slag layer (2), bringing the measuring cell (5) and counter electrode (4) into contact with the steel melt (3) to heat the measuring cell (5) and the counter electrode (4), and pulling the measuring cell (5) up into the slag layer (2) for carrying out the measurement, such that the counter electrode (4) is located in the steel melt (3) during the measurement.
- 2. The process according to claim 1, wherein the measuring cell (5) and the counter electrode (4) are arranged on a support, and the counter electrode (4) is simultaneously pulled up with the measuring cell (5).
- 3. The process according to claim 1, wherein prior to pulling up the measuring cell (5) from the melt, the oxygen activity of the melt is determined.
- 4. The process according to claim 1, wherein the measurement takes place during the pulling up movement of the measuring cell (5) and the counter electrode (4).
- 5. The process according to claim 1, wherein during the measurement the temperature of the steel melt (3) and/or the slag layer (2) is determined.
Priority Claims (1)
Number |
Date |
Country |
Kind |
196 52 596 |
Dec 1996 |
DEX |
|
CROSS-REFERENCE TO RELATED APPLICATION
This application is a continuation of PCT/EP97/06920, filed Dec. 11, 1997, the disclosure of which is incorporated herein by reference.
US Referenced Citations (7)
Foreign Referenced Citations (2)
Number |
Date |
Country |
0 330 264 A1 |
Aug 1989 |
EPX |
0 450 090 |
Oct 1991 |
EPX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
PCTEP9706920 |
Dec 1997 |
|