Claims
- 1. A catalytic process for the oxidation of n-butane to maleic anhydride wherein n-butane is contacted with a catalytic amount of vanadium phosphorus oxide catalyst having an atomic ratio of phosphorus to vanadium in the range of about 0.5 to about 5 regenerated according to the following process comprising:
- (A) contacting said catalyst at a temperature in the range of from about 300.degree. C. to about 550.degree. C. with an effective amount of a material selected from the group consisting of:
- (1) molecular chlorine of fluorine or mixtures thereof;
- (2) carbon halides of fluorine, chlorine, bromine or iodine being in the vapor state above about 250.degree. C. at atmospheric pressure represented by the following formula:
- C(X).sub.n
- where each X is a selected halide and n is an integer from 1 to 4, any remaining radicals being hydrogen or mixtures thereof;
- (3) organic halides of fluorine, chlorine, bromine or iodine being in the vapor state above about 250.degree. F. at atmospheric pressure represented by the formula;
- R(X.sub.1).sub.m
- where R is alkane, alkene or alkyne of straight or branched structure having at least two carbon atoms and X.sub.1 is independently a primary, secondary or tertiary halide and m is an integer of from about 1 to about 20 consistent with the number of carbon atoms of said structure or mixtures;
- (4) hydrogen halides or mixturs thereof at regeneration conditions including a temperature in the range of from about 300.degree. C. to about 550.degree. C.; and
- (B) contacting the catalyst with an effective amount of an alkyl ester of other orthophosphoric acid and water.
- 2. The process of claim 1 wherein the catalyst is regenerated by contacting it during the oxidation with water and the phosphorus compound, wherein the amount of water added is about 1,000 parts per million to about 40,000 parts per million by weight of the reaction feedstock.
- 3. A catalytic process for the oxidation of n-butane to maleic anhydride wherein n-butane is contacted with a catalytic amount of vanadium-phosphorus-oxide-cometal catalyst having an atomic ratio of phosphorus to vanadium in the range of about 0.5 to about 5 comprising:
- (A) contacting said catalysft at a temperature in the range of from about 300.degree. C. to about 550.degree. C. with an effective amount of a material selected from the group consisting of:
- (1) molecular chlorine or fluorine or mixtures thereof;
- (2) carbon halides of fluorine, chlorine, bromine or iodine being in the vapor state above about 250.degree. C. at atmospheric pressure represented by the following formula:
- C(X).sub.n
- where each X is a selected halide and n is an integer from 1 to 4, any remaining radicals being hydrogen or mixtures thereof;
- (3) organic halides of fluorine, chlorine, bromine or iodine being in the vapor state above about 250.degree. C. at atomospheric pressure represented by the formula:
- R(X.sub.1).sub.m
- where R is alkane, alkene or alkyne of straight or branched structure having at least two carbon atoms and X.sub.1 is independently a primary, secondary or tertiary halide and m is an interger of from about 1 to about 20 consistent with the number of carbon atoms of said structure or mixtures;
- (4) hydrogen halides or mixtures thereof at regeneration conditions including a temperature in the range of from about 300.degree. C. to about 550.degree. C.; and
- (B) contacting the catalyst with an effective amount of an alkyl ester of orthophosphoric acid and water.
- 4. The process of claim 3 wherein the cometal is selected form the group of zinc and molybdenum.
- 5. The process of claim 4 wherein the catalyst is regenerated according to claim 2.
- 6. The process of claim 1 wherein the oxidation is conducted at a temperature of about 700.degree. F. to about 900.degree. F.
- 7. The process of claim 3 wherein the oxidation is conducted at a temperature of about 700.degree. F. to about 900.degree. F.
- 8. The process of claim 4 wherein the oxidation is conducted at a temperature of about 700.degree. F. to about 900.degree. F.
- 9. The process of claim 3 wherein the cometal is selected from the group of zinc, bismuth, copper, molybdenum, lithium, tungsten, chromium, uranium, niobium, zirconium, tin, cobalt, iron, nickel, antimony, titanium, or mixtures thereof.
- 10. The process of claim 9 wherein the oxidation is conducted at a temperature of about 700.degree. F. to about 900.degree. F.
Parent Case Info
This is a division of application Ser. No. 150,223, filed Jan. 29, 1988 now U.S. Pat. No. 4,861,738.
US Referenced Citations (4)
Number |
Name |
Date |
Kind |
4020174 |
Partenheimer |
Apr 1977 |
|
4089807 |
Partenheimer |
May 1978 |
|
4094816 |
Partenheimer |
Jun 1978 |
|
4780548 |
Edwards et al. |
Oct 1988 |
|
Divisions (1)
|
Number |
Date |
Country |
Parent |
150223 |
Jan 1988 |
|