Claims
- 1. A process for preparing a thallium-containing superconductive composition, comprising the steps of:
- (a) providing a mixture of an inorganic salt and a precursor powder composition, wherein said precursor powder composition has a stoichiometry corresponding to a formula selected from the group consisting of A.sub.2 B.sub.2 CuO.sub.6, and A.sub.2 B.sub.2 CaCuO.sub.8, and wherein:
- 1. A is thallium,
- 2. B is barium,
- 3. substantially all of the particles of said precursor powder composition are smaller than about 100 microns, and
- 4. said mixture is comprised of from about 30 to about 80 weight percent of said inorganic salt;
- (b) charging said mixture of said inorganic salt and said precursor powder composition to a closed container;
- (c) thereafter, while said mixture is within said closed container, raising the temperature of said mixture from ambient temperature to an elevated temperature of from about 800 to about 950 degrees Celsius at a rate of from about 100 to about 900 degrees Celsius per hour;
- (d) thereafter, while said mixture is within said closed container, subjecting said mixture to said elevated temperature of from about 800 to about 950 degrees Celsius for from about 1 to about 12 hours;
- (e) thereafter, cooling said mixture within said closed container from said elevated temperature to a temperature of 600 degrees Celsius at a rate of at least 300 degrees Celsius per hour, whereby said thallium-containing superconductive composition is produced.
- 2. The process as recited in claim 1, wherein said inorganic salt is a potassium salt selected from the group consisting of potassium chloride, potassium bromide, potassium iodide, and mixtures thereof.
- 3. The process as recited in claim 1, wherein said powder mixture is comprised of barium peroxide.
- 4. The process as recited in claim 1, wherein mixture is comprised of from about 45 to about 55 weight percent of said inorganic potassium salt.
- 5. The process as recited in claim 1, wherein said closed container is a closed crucible.
- 6. The process as recited in claim 1, wherein, while said mixture is within said closed container, the temperature of said mixture is raised from ambient temperature to an elevated temperature of from about 800 to about 900 degrees Celsius at a rate of from about 300 to about 900 degrees Celsius per hour.
- 7. The process as recited in claim 1 wherein, after said mixture has been cooled within said closed container, it is washed with solvent until substantially all of said inorganic salt has been leached from said powder composition.
- 8. The process as recited in claim 7, wherein said solvent is water.
- 9. The process as recited in claim 7 wherein, after said mixture has been washed with said solvent, it is dried until it contains less than about 0.1 weight percent of moisture.
CROSS REFERENCE TO RELATED PATENT APPLICATION
This application is a continuation-in-part of patent application Ser. No. 07/684,309, filed on Apr. 12, 1991, now U.S. Pat. No. 5,270,293.
US Referenced Citations (4)
Foreign Referenced Citations (3)
Number |
Date |
Country |
2055283 |
Feb 1990 |
JPX |
0097422 |
Apr 1990 |
JPX |
4037607 |
Feb 1992 |
JPX |
Non-Patent Literature Citations (2)
Entry |
Inoue "Superconductive transition of 120K in a Tl-Bi-Sr-Ca-Cu-O", Jap Jnl Appl Phys. vol. 28(7) Jul. 1987 pp. L1167-L1170. |
Katsui "Crystal growht of superconducting Bi-Sr-Ca-Co-O . . . " Jap Jnl Appl Phys. vol. 27(5) May 1988 pp. L844-L845. |
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
684309 |