Claims
- 1. Process for pretreating strips and foils of aluminum or aluminum alloys prior to lacquering, coating with adhesive or laminating with plastic, which comprises: providing an aluminum or aluminum alloy material in the form of strip or foil having a workface; providing a silicate-free non-toxic, non-hazardous aqueous electrolyte having a pH of 4.2 to 12.5 and consisting essentially of 0.01-10 weight percent of an organic compound that forms a complex with aluminum and contains at least one amino group with at least one carboxyl group attached to its nitrogen atom; heating said electrolyte to a temperature of from 25.degree. to 95.degree. C.; passing said material through said electrolyte; and supplying an alternating current of 10 to 500 coulomb/dm.sup.2 to the workface while said material is passing through said electrolyte, and coating said material to provide improved adhesive qualities.
- 2. Process according to claim 1 wherein said carboxyl group is selected from the group consisting of --COOH, --CH.sub.2 COOH and --CH.sub.2 CH.sub.2 COOH.
- 3. Process according to claim 1 wherein said organic compound that forms a complex is a complexing organic salt selected from the group consisting of salts of nitrilo-triacetic acid and salts of ethylene-diamino-tetra-acetic acid.
- 4. Process according to claim 3 wherein the cations in said organic salts are alkali metal ions.
- 5. Process according to claim 3 wherein the concentration of the complexing organic salt added to the electrolyte is 0.1-5 weight percent.
- 6. Process according to claim 1 wherein further additions are made to the electrolyte in order to stabilize it, its pH value and the oxidizing power of the bath, the said additions being selected from the group consisting of sodium hydroxide, potassium hydroxide, sodium carbonate and potassium carbonate.
- 7. Process according to claim 1 wherein the pH is adjusted to 9.5-12.
- 8. Process according to claim 1 wherein said current is 25-100 coulombs per dm.sup.2.
- 9. Process according to claim 1 wherein a current density of 3-100A/dm.sup.2 is employed.
- 10. Process according to claim 1 wherein a throughput time is employed in the region of the electrodes of 0.5-10 seconds.
- 11. Process according to claim 1 wherein a three phase current is employed using three electrodes.
- 12. Process according to claim 11 wherein a middle one of said electrodes is supplied with rectified current.
- 13. Process for pretreating strips and foils of aluminum or aluminum alloys prior to lacquering, coating with adhesive or laminating with plastic, which comprises: providing an aluminum or aluminum alloy material in the form of strip or foil having a workface; providing a silicate-free non-toxic, non-hazardous aqueous electrolyte having a pH of 4.2 to 12.5 and comprising 0.01-10 weight percent of an organic compound that forms a complex with aluminum and contains at least one amino group with at least one carboxyl group attached to its nitrogen atom; heating said electrolyte to a temperature of from 25.degree. to 95.degree. C.; passing said material through said electrolyte; and supplying an alternating current of 10 to 500 coulomb/dm.sup.2 to the workface while said material is passing through said electrolyte, and coating said material to provide improved adhesive qualities, wherein said organic compound that forms a complex is a complexing organic salt selected from the group consisting of nitrilo-triacetic acid and ethylene-diamino-tetra-acetic acid and wherein the cations in said organic salts are ammonium ions.
- 14. Process for pretreating strips and foils of aluminum or aluminum alloys prior to lacquering, coating with adhesive or laminating with plastic, which comprises: providing an aluminum or aluminum alloy material in the form of strip or foil having a workface; providing a silicate-free aqueous electrolyte having a pH of 4.2 to 12.5 and comprising 0.-1-10 weight percent of an organic compound that forms a complex with aluminum and contains at least one amino group with at least one carboxyl group attached to its nitrogen atom; heating said electrolyte to a temperature of from 25.degree. to 95.degree. C.; passing said material through said electrolyte; and supplying an alternating current of 10 to 500 coulomb/dm.sup.2 to the workface while said material is passing through said electrolyte, and coating said material to provide improved adhesive qualities, wherein a polysaccharide is added to the electrolyte in an amount effective to stabilize the electrolyte selected from the group consisting of dextran and starch.
- 15. Process for pretreating strips and foils of aluminum or aluminum alloys prior to lacquering, coating with adhesive or laminating with plastic, which comprises: providing an aluminum or aluminum alloy material in the form of strip or foil having a workface; providing a silicate-free aqueous electrolyte having a pH of 4.2 to 12.5 and comprising 0.01-10 weight percent of an organic compound that forms a complex with aluminum and contains at least one amino group with at least one carboxyl group attached to its nitrogen atom; heating said electrolyte to a temperature of from 60.degree. to 70.degree. C.; passing said material through said electrolyte; and supplying an alternating current of 10 to 500 coulomb/dm.sup.2 to the workface while said material is passing through said electrolyte, and coating said material to provide improved adhesive qualities.
CROSS-REFERENCE TO RELATED APPLICATIONS
This is a Continuation-In-Part of U.S. patent application Ser. No. 792,275, Filed Oct. 28, 1985, which in turn is a Continuation of U.S. patent application Ser. No. 711,598, Filed Mar. 13, 1985 and both now abandoned.
US Referenced Citations (5)
Foreign Referenced Citations (4)
Number |
Date |
Country |
41803 |
Dec 1971 |
JPX |
8787 |
Apr 1975 |
JPX |
411164 |
May 1974 |
SUX |
451801 |
Mar 1975 |
SUX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
711598 |
Mar 1985 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
792275 |
Oct 1985 |
|