Claims
- 1. A process for producing an inorganic fiber superior in stretchability and mechanical strength, which comprises heating a polymetalloxane in solid form at 25.degree. C. to a temperature of 40.degree. to 250.degree. C. to prepare a spinning liquid having a viscosity of 1 to 3000 poises; spinning the spinning liquid to form a precursor fiber; and baking the precursor fiber.
Priority Claims (1)
Number |
Date |
Country |
Kind |
59-72471 |
Apr 1984 |
JPX |
|
Parent Case Info
This application is a continuation of application Ser. No. 789,963, filed Oct. 3, 1985 now abandoned.
US Referenced Citations (3)
Number |
Name |
Date |
Kind |
4101615 |
Horikiri et al. |
Jul 1978 |
|
4515742 |
Yajima et al. |
May 1985 |
|
4535007 |
Cannady |
Aug 1985 |
|
Foreign Referenced Citations (7)
Number |
Date |
Country |
0083839 |
Jul 1983 |
EPX |
49-124336 |
Nov 1974 |
JPX |
50-18726 |
Feb 1975 |
JPX |
50-136424 |
Oct 1975 |
JPX |
51-13768 |
May 1976 |
JPX |
58-91825 |
May 1983 |
JPX |
1457801 |
Dec 1976 |
GBX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
789963 |
Oct 1985 |
|