- 1. A process for producing molecular sieve carbon fibers, comprising the steps of:
- spinning a material selected from the group consisting of oil residue and coal residue to form green fibers having diameters in the range of 5 to 50 .mu.m;
- treating said green fibers in air at a temperature in a range of 250.degree. to 450.degree. C. to introduce oxygen into said green fibers so that an amount of oxygen introduced in said fibers which is in a range of 8 to 28% by weight of the total weight of said fibers after the oxygen is introduced;
- cartionizing said fibers in an inactive atmosphere at a temperature of 500.degree. to 750.degree. C. whereby a component of said material, including oxygen atoms introduced thereto in said treating step is released from said fibers to form a number of micropores opening directly at the surface of said fibers, which micropores have diameters in the range of 0.5 nm and below and substantially no pores larger than 0.5 nm in size.
- 2. The process of claim 1, wherein said material is an oil residue pitch.
- 3. The process of claim 1, wherein said material is coal tar.
Priority Claims (1)
Number |
Date |
Country |
Kind |
59-82818 |
Apr 1984 |
JPX |
|
Parent Case Info
This is a division of application Ser. No. 720,378, filed Apr. 5, 1986, which was abandoned upon the filing hereof.
US Referenced Citations (4)
Foreign Referenced Citations (2)
Number |
Date |
Country |
101024 |
Jun 1982 |
JPX |
199922 |
Oct 1985 |
JPX |
Divisions (1)
|
Number |
Date |
Country |
Parent |
720378 |
Apr 1986 |
|