Claims
- 1. A method for suppressing hard bubbles in a magnetic bubble device comprising an epitaxial magnetic garnet film deposited on a nonmagnetic garnet substrate, said substrate containing ions selected from the group consisting of aluminum ions and gallium ions and said ions having a concentration in the substrate substantially greater than in the film CHARACTERIZED IN THAT said magnetic bubble device is annealed at a temperature in the range of from 1000.degree. C. to 1200.degree. C. and with at least a portion of said film exposed to an inert atmosphere whereby the magnetic moment is significantly altered in a layer of said portion of said film adjacent to said substrate.
- 2. Method of claim 1 in which said inert atmosphere consists essentially of nitrogen,
- 3. Method of claim 1 in which said magnetic film is of composition YGdTmGa.sub.0.7 Fe.sub.4.3 O.sub.12.
- 4. Method of claim 1 in which said device is annealed for a time in the range of from one to twenty-four hours.
- 5. Method of claim 1 in which said magnetic garnet film has a thickness in the range of from 1-20 micrometers.
- 6. Method of claim 1 in which said substrate is a rare earth garnet.
- 7. Method of claim 1 in which said magnetic film is of composition Y.sub.1.93 Sm.sub.0.11 Ca.sub.0.96 Ge.sub.0.96 Fe.sub.4.04 O.sub.12.
Parent Case Info
This application is a continuation of application Ser. No. 558,142 filed Mar. 13, 1975 and now abandoned.
US Referenced Citations (1)
Number |
Name |
Date |
Kind |
3759745 |
Dixon et al. |
Sep 1973 |
|
Continuations (1)
|
Number |
Date |
Country |
Parent |
558142 |
Mar 1975 |
|