Claims
- 1. In a process of preparing at least approximately equilibrated organopolysiloxane mixtures having silylhalide groups, by redistribution of siloxane and silylhalide groups, wherein mixtures of organohalogensilanes and organopolysiloxanes or mixtures of organopolysiloxanes with terminal silylhalide groups are equilibrated in the presence of an equilibration catalyst, the molecular weight distribution or the distribution of the individual siloxane structures of the mixtures to be treated deviating from the statistical equilibrium, the improvement which comprises that the equilibration treatment is performed in the presence of an equilibration catalyst which is a mixed catalyst comprising
- a. hydrogen halide acid and
- b. peralkylated acid amide,
- the amount of said mixed catalyst being in the range of 0.002 to 0.2 mole per siloxane bond, said mixed catalyst being removed from the system after the equilibration treatment by phase separation.
- 2. The improvement of claim 1, wherein said acid of
- a. is HCl, while said amide of
- b. is dimethylformamide.
- 3. The improvement of claim 1, wherein the equilibration treatment is carried out at a temperature of > 50.degree. to 110.degree. C.
- 4. The improvement of claim 1, wherein the equilibration treatment is carried out under a pressure which is above atmospheric pressure.
- 5. The improvement of claim 1, wherein the equilibration treatment is carried out in a closed reaction vessel at that pressure which is the corollary of the temperature of the reaction mixture.
- 6. The improvement of claim 1, wherein said mixed catalyst essentially consists of dimethylformamide . 2 HCl and said equilibration treatment is performed at about 100.degree. C.
- 7. The improvement of claim 1, wherein said silylhalide groups are SiCl groups.
- 8. The improvement of claim 1, wherein said catalyst additionally contains HFeCl.sub.4 in amounts of 1 ppm to 1 percent by weight, calculated on each siloxane bond in the mixture to be equilibrated.
- 9. The improvement of claim 8, wherein 0.001 to 0.1 percent by weight of HFeCl.sub.4 is used.
- 10. The improvement of claim 1, wherein the equilibration treatment is performed in stage wise manner.
- 11. The improvement of claim 10, wherein the equilibration treatment is initiated with said HFeCl.sub.4 whereafter the equilibration treatment is continued and terminated with said mixed catalyst of (a) and (b) in one or several stages.
- 12. The improvement of claim 1, wherein said mixed catalyst of (a) and (b) is in the form of liquid mixtures or complexes.
- 13. The improvement of claim 1, wherein said mixed catalyst is a room-temperature saturated solution of hydrogen halide acid in dimethylformamide.
Priority Claims (1)
Number |
Date |
Country |
Kind |
2353166 |
Oct 1973 |
DT |
|
Parent Case Info
This is a continuation of application Ser. No. 517,319, filed Oct. 23, 1974, now abandoned.
US Referenced Citations (2)
Continuations (1)
|
Number |
Date |
Country |
Parent |
517319 |
Oct 1974 |
|