This invention relates to mounting processes for optical components in an optical assembly.
Mounting of optical components can be accomplished by various methods. See, e.g., “Opto-mechanical Systems Design” by Paul R. Yoder, Jr., Marcel Dekker, Inc. 1986. Of these methods, bonding of optical components can usually be done faster and cheaper than traditional mechanical clamping. Structural adhesives most frequently used are two-part epoxies, urethanes, and room-temperature-vulcanizing (RTV) elastomers such as silicone. Adhesives emit (i.e., outgas) volatile ingredients during curing or when exposed to vacuum or elevated temperatures. These emitted ingredients may then condense as contaminating films on nearby surfaces, such as optics, opto-mechanical assemblies, or items under process. See, e.g., “Design and Mounting of Prisms and Small Mirrors in Optical Instruments” by Paul R. Yoder, Jr., SPIE Optical Engineering Press, 1998.
Thus, what is needed is a method to reduce undesirable outgassing in optical assemblies.
In one embodiment of the invention, a method to reduce undesirable outgassing includes bonding at least two optical components with a bonding material and encapsulating the bonding material with a capping material. The capping material inhibits the outgassing of species that would otherwise be emitted from the bonding material to the surrounding. In one embodiment, the bonding material is silicone. In one embodiment, the capping material is epoxy.
In action 102, an optical component 202 (
In one embodiment, bonding material 206 is silicone such as Dow Corning® 93-500 Space Grade Encapsulant. For silicone, the outgassing species 208 includes silicones, hydrocarbons, nitrogen, oxygen, and water. For other bonding materials, undesirable outgassing species can include amines, phthalates, epoxy monomers, and photo-polymerization initiators. In other embodiments, bonding material 206 can be a flexible epoxy, such as Cemedine EP001.
In action 104, the exposed periphery of bonding material 206 is encapsulated by a capping material 302 (FIG. 3). Capping material 302 can be any material that substantially inhibits the outgassing of species 208 to an acceptable level for a particular application. Capping material 302 may inhibit the outgassing of species 208 in various ways, including sealing or trapping of species 208. Capping material 302 may emit an acceptable level of outgassing species 304 (
In one embodiment, capping material 302 is epoxy such as Loctite® Hysol® 0151 or Hysol® EA9313. For epoxy, the outgassing species 304 includes amines, phthalates, epoxy monomers, and photo-polymerization initiators. The resin and the curing agent of the epoxy can be premixed and frozen to ensure consistency of the epoxy as described in U.S. patent application Ser. No. 09/603,107, filed on Jun. 22, 2000, which is incorporated by reference in its entirety. Alternatively, the resin and the curing agent of the epoxy can be mixed at room temperature during the mounting process. In other embodiments, capping material 302 can be polyurethane, metal, or a hydrocarbon polymer coating such as Parylene or Pyralin.
Various other adaptations and combinations of features of the embodiments disclosed are within the scope of the invention. Although optical assemblies are specifically mentioned, the above method can be applied to any assembly to reduce undesirable outgassing species. Numerous embodiments are encompassed by the following claims.
Number | Name | Date | Kind |
---|---|---|---|
4950344 | Glover et al. | Aug 1990 | A |
6204906 | Tannas, Jr. | Mar 2001 | B1 |
Number | Date | Country | |
---|---|---|---|
20040046008 A1 | Mar 2004 | US |