Claims
- 1. A process for waterproofing leathers, furs, and other fibrous materials, comprising
- contacting a fibrous material in a float at a pH of 3.5 to 5 with a dispersing or stabilizing auxiliary agent comprising an alkoxy-containing copolymer having a molecular weight of 500 to 100,000 consisting of the following monomer units
- (.alpha.) 1-99% -wt. of water soluble, ethylenically unsaturated, acid group-containing monomers and/or unsaturated dicarboxylic acid anhydrides and/or their salts,
- (.beta.) 1-50% -wt. of ethylenically unsaturated, mono- or polyalkoxylated monomers, and
- (.gamma.) 0-60% -wt. of additional monomers copolymerizable with (.alpha.) and (.beta.), with the proviso that the weight percentage of (.alpha.), (.beta.), and (.gamma.) make up to 100%, where the alkoxy-containing copolymer consists of elements selected from C, H, O, N and S; and
- contacting the fibrous material in the float with a water repellent.
- 2. The process according to claim 1, wherein the dispersing or stabilizing auxiliary agent further comprises sulfochlorinated paraffins or chloroparaffins.
- 3. The process according to claim 1, wherein the dispersing or stabilizing auxiliary agent is mixed with the water repellent and used together.
- 4. The process according to claim 1, wherein the dispersing or stabilizing auxiliary agent is used in a neutralization/retannage step.
- 5. The process according to claim 1, wherein a major portion of the water repellent is used during a neutralization/retannage step.
- 6. The process according to claim 1, wherein the dispersing or stabilizing auxiliary agent is contacted with the fibrous material at a pH from 4.0 to 5.0.
- 7. The process according to claim 1, wherein the dispersing or stabilizing auxiliary agent is contacted with the fibrous material at a pH from 4.3 to 4.7.
- 8. The process according to claim 1, wherein the dispersing or stabilizing auxiliary agent is used in an amount of 2 to 10% -wt. relative to a shaved weight of the fibrous material.
- 9. The water-proofed fibrous material obtained by the process of claim 1.
- 10. The water-proofed fibrous material of claim 9, which is a leather or a fur.
- 11. A process for waterproofing leathers, furs, and other fibrous materials, comprising
- contacting a fibrous material at a pH of 3.5 to 5 with a dispersing or stabilizing auxiliary agent comprising an alkoxy-containing copolymer having a molecular weight of 500 to 100,000 consisting of the following monomer units
- (.alpha.) 1-99% -wt. of water soluble, ethylenically unsaturated, acid group-containing monomers and/or unsaturated dicarboxylic acid anhydrides and/or their salts,
- (.beta.) 1-50% -wt. of ethylenically unsaturated, mono- or polyalkoxylated monomers, and
- (.gamma.) 0-60% -wt. of additional monomers copolymerizable with (.alpha.) and (.beta.), with the proviso that the weight percentage of (.alpha.), (.beta.), and (.gamma.) make up to 100%, where the alkoxy-containing copolymer consists of elements selected from C, H, O, N and S; and
- contacting the fibrous material with a water repellent, wherein
- the dispersing or stabilizing auxiliary agent is mixed with the water repellent and used together.
- 12. The process according to claim 11, wherein the dispersing or stabilizing auxiliary agent further comprises sulfochiorinated paraffins or chloroparaffins.
- 13. The process according to claim 11, wherein the dispersing or stabilizing auxiliary agent is used in a neutralization/retannage step.
- 14. The process according to claim 11, wherein a major portion of the water repellent is used during a neutralization/retannage step.
- 15. The process according to claim 11, wherein the dispersing or stabilizing auxiliary agent is contacted with the fibrous material at a pH from 4.0 to 5.0.
- 16. The process according to claim 11, wherein the dispersing or stabilizing auxiliary agent is contacted with the fibrous material at a pH from 4.3 to 4.7.
- 17. The process according to claim 11, wherein the dispersing or stabilizing auxiliary agent is used in an amount of 2 to 10% -wt. relative to a shaved weight of the fibrous material.
- 18. A water-proofed fibrous material obtained by the process of claim 11.
- 19. The water-proofed fibrous material of claim 18 which is a leather or a fur.
- 20. A process for waterp roofing leathers, furs, and other fibrous materials, comprising
- contacting a fibrous material in a float at a pH of 3.5 to 5 with a dispersing or stabilizing auxiliary agent comprising an alkoxy-containing copolymer having a molecular weight of 500 to 100,000 consisting of the following monomer units
- (.alpha.) 1-99% -wt. of water soluble, ethylenically unsaturated, acid group-containing monomers and/or unsaturated dicarboxylic acid anhydrides, the acid group-containing monomers and dicarboxylic acid anhydrides being selected from the group consisting of acrylic acid, (meth)acrylic acid, (meth)allyl sulfonic acid, vinylacetic acid, 2-acrylamido-2-methyl-propane sulfonic acid, vinylsulfonic acid, styrysulfonic acid, maleic acid, maleic anhydride, flmaric acid, itaconic acid, and the semiesters and semi,des of maleic acid, fimaric acid and itaconic acid,
- (.beta.) 1-50% -wt. of ethylenically unsaturated, mono- or polyalkoxylated monomers selected from the group consisting of methoxypolyethylene glycol (meth)acrylate, nonylphenol polyglycol (meth)acrylate, ethylene and/or propylene oxide-adducts of (meth)allyl alcohol, (meth)allyl amine, and hydroxyethyl (meth)acrylate, and reaction products of at least one of ethylene glycol, isopropyl glycol, butyl glycol, nonylphenol and isotridecanol with ethylene or propylene oxide, and
- (.gamma.) 0-60% -wt. of additional monomers copolymerizable with (.alpha.) and (.beta.) selected from the group consisting of (meth)acrylamide, dimethylaminopropyl (meth)acrylamide, (meth)acrylonitrile, hydroxyethyl (meth)acrylate, N-vinylpyrrolidone, N-vinyl imidazole, N-vinyl acetamide, vinyl acetate, vinyl propionate, versatic acid vinyl ester, and styrene, with the proviso that the weight percentage of (.alpha.), (.beta.), and (.gamma.) make up to 100%; and
- contacting the fibrous material in the float with a water repellent.
Priority Claims (1)
Number |
Date |
Country |
Kind |
195 16 961 |
May 1995 |
DEX |
|
TITLE OF THE INVENTION
This application is a 371 of PCT/EP/96/01851 filed May 3, 1996.
PCT Information
Filing Document |
Filing Date |
Country |
Kind |
102e Date |
371c Date |
PCT/EP96/01851 |
5/3/1996 |
|
|
11/12/1997 |
11/12/1997 |
Publishing Document |
Publishing Date |
Country |
Kind |
WO96/35815 |
11/14/1996 |
|
|
US Referenced Citations (2)
Number |
Name |
Date |
Kind |
5124181 |
Schaffer et al. |
Jun 1992 |
|
5433753 |
Dahmen et al. |
Jul 1995 |
|
Foreign Referenced Citations (1)
Number |
Date |
Country |
4948993 |
Mar 1994 |
AUX |
Non-Patent Literature Citations (1)
Entry |
Ullmann's Encylopedia of Industrial Chemistry, fifth edition, vol. A 15, pp. 274-277 (month unknown), 1990. |