1. Field of the Invention
The present invention relates to a processing system for manufacturing composite cementitious materials as hydraulic blended cements with significantly reduced Portland clinker minerals content. The materials include an increased quantity of supplementary cementitious materials, such as, for example, fly ash, blast furnace slag, fine quartz, granitic quarry fines, and the like, along with highly reactive pozzolans or mineral fillers, such as, for example, fly ash, blast furnace slag, fine quartz, granitic quarry fines, and the like, for direct replacement of a part of the Portland cement in concrete mixtures. Such mixtures are therefore characterized by a significantly improved environmental profile.
2. Description of the Related Art
It is well known that each ton of production of standard Portland cement is accompanied by the release of about one ton of carbon dioxide. About half of that quantity comes from the decarbonation of limestone within the kiln and the other half from energy consumption, primarily within the kiln.
It follows that the only way in which the cement industry can achieve meaningful reductions in carbon dioxide emissions is by reduction of Portland clinker production and an increased use of fillers.
Traditional plants for the production of blended cement include the intergrinding of Portland cement clinker with different types of microfillers, for example, blast furnace slag, fly ash, limestone, and the like, mainly in rotating ball mills. Such methods do not provide more than about 20 to 25% of Portland clinker replacement by fly ash, and approximately 30 to 50% by blast furnace slag, without a significant negative influence on the cement performance, such as a sharp increase of setting time, a very low strength development during the curing period of from 0 to 28 days, and the like. It takes up to 3 times longer, such as 2 to 3 months, to achieve the 28-day strength of traditional Portland cement concretes. At the same time, high volume fly ash (HVFA) cements do have significant benefits in comparison with traditional Portland cements.
The introduction of fly ash or other types of fillers, for example fines from granitic quarries or quartz sand fines, for replacement of Portland cement directly in the concrete mixer in amounts more that 15 to 20% is not efficient, and it could negatively influence the performance of the concrete (reduced strength, etc).
Existing methods of grinding and mechanical activation of such fillers could give some improvement, as described in U.S. Pat. No. 6,630,022, but it appears to be economically ineffective, and it allows replacement of only 20% of Portland cement without experiencing a reduction of the concrete compressive strength.
In International Patent Application No. PCT/SE03/001009 (Publication No. WO 2004/041746 A1) there is described a process for producing a blended cement. The blended cement contains Portland cement that is mixed thoroughly with a microfiller, and possibly a water reducing agent, to a dry cement mixture, along with fine supplementary cementitious materials selected from the materials blast furnace slag, fly ash, quartz, silica, and amorphous silicon dioxide. According to the disclosure in that application, supplementary materials are subjected to a grinding step in a dry state, and the supplementary ground materials are then subjected to grinding together with at least 20% by weight of the total grinding mass of a highly reactive cement mixture in a dry state. A polymer in the form of a powdery water-reducing agent is also added.
A problem in producing such a cement mixture is that in order to obtain the desired result the fineness of the components must be strictly controlled. This is especially true for a plant where the cement mixture is produced in a continuous way.
The present invention is directed to such a continuous production plant.
The present invention thus relates to a processing arrangement for manufacturing composite cementitious materials such as hydraulic blended cements with significantly reduced Portland clinker minerals content. The cementitious materials include an increased amount of supplementary cementitious materials, such as, for example, fly ash, blast furnace slag, fine quartz, granitic quarry fines, and the like, along with highly reactive pozzolans or mineral fillers, such as, for example, fly ash, blast furnace slag, fine quartz, granitic quarry fines, and the like, for direct replacement of Portland cement in concrete. The arrangement includes a silo for Portland cement, a silo for fly ash or other types of supplementary materials, and a silo for cement kiln dust or other types of setting-time-regulating agents, and a storage unit for polymer additives. The arrangement also includes proportioning means, mixing means, grinding devices, and discharge means. A milling unit is provided for pregrinding the supplementary materials and milling unit is provided for pregrinding the Portland cement. The pregrinding unit is followed by a grinding unit for grinding the preground components. The pregrinding unit is adapted to work in an open circuit or in a closed circuit for the material being ground.
The structure, operation, and advantages of the present invention will become further apparent upon consideration of the following description, taken in conjunction with the accompanying drawing in which
In
According to a preferred embodiment there is provided a unit 21 for carbon removal from fly ash, which unit is adapted to lower the carbon content in the fly ash to below about 4% by weight. The unit can operate according to any suitable known technique for carbon removal.
As is apparent from the international application referred to above, the quartz in the above example can be any suitable supplementary quartz material.
According to the above, sand, slag, additives in the form of, for example, a water reducing agent, and Portland cement are fed into the present arrangement.
Regarding the quartz, or sand, the sand is first fed from feeding station 1 to drying unit 2, where it is dried. Thereafter it is fed to intermediate silo 5. Slag, or any other suitable additive, is fed from a silo 3 to a conduit merging with a conduit from silo 5 for sand. The mixture of sand and slag is fed to milling unit 6. After the sand and slag have been preground, they are fed to silo 16 and then to silo 10.
Regarding the Portland cement, the cement is fed from silo 8 to silo 10. Additives like water reducing agents are also fed to silo 10, as well as sand and slag that have been preground in milling unit 6. Portland cement is also fed from silo 8 to milling unit 9. From milling unit 9 the cement is fed to silo 15 for preground cement. The materials in silos 10 and 15 are then fed to a rotary mixer 12 and thereafter to silo 17.
From silo 17 the mixture of materials is fed to final milling unit 13. After being milled in milling unit 13 the final material is fed to silo 14.
According to the invention, the arrangement thus includes milling unit 6 for pregrinding the supplementary materials and milling unit 9 for pregrinding the Portland cement, which pregrinding unit is followed by grinding unit 13 for grinding of the preground components.
According to a very important feature of the present invention, the pregrinding milling units 6, 9 are adapted to work as an open circuit or a closed circuit for the material being ground. The closed circuit associated with milling unit 6 includes a conduit 18 from the milling unit to air classifier 19, which is able to sort out and convey large fractions of the material being ground back to mill 6 through a conduit 20.
The closed circuit associated with milling unit 9 includes, in a corresponding way, a conduit 24 from the milling unit to air classifier 22, which is able to sort out and convey large fractions of the material being ground back to mill 9 through a conduit 23.
To both milling units 6, 9 there are connected a cyclone and a dust collector. The material collected there is fed to a respective downstream silo in the main flow.
According to a preferred embodiment of the invention, milling unit 6 for the supplementary material is arranged to pregrind the supplementary material to a fineness of an average particle size of from about 100 to about 300 microns.
According to another preferred embodiment of the invention, milling unit 9 for the Portland cement is arranged to pregrind the Portland cement to a fineness of an average particle size of from about 10 to about 30 microns.
Since only material fractions that are too large will be sorted out in the air classifiers, the circuits will be open when there are no such materials leaving the respective milling units 6, 9.
According to still another preferred embodiment, the arrangement includes a unit 2 for drying the supplementary material and fillers to a moisture content of less than about 0.2% by weight, which unit is located upstream of the milling unit.
Thus, the present invention provides a production plant, or arrangement, in which production of the cement material mentioned in the introductory part of the application can be performed in a continuous way.
Although particular embodiments of the present invention have been illustrated and described, it will be apparent to those skilled in the art that changes and modifications can be made without departing from the spirit of the present invention. Accordingly, it is intended to encompass within the appended claims all such changes and modifications that fall with the scope of the present invention.
Number | Date | Country | Kind |
---|---|---|---|
0401238 | May 2004 | SE | national |
Number | Name | Date | Kind |
---|---|---|---|
4783012 | Blasczyk et al. | Nov 1988 | A |
5110056 | Blasczyk et al. | May 1992 | A |
5804175 | Ronin et al. | Sep 1998 | A |
6241816 | Ronin | Jun 2001 | B1 |
6575390 | Kamikawa et al. | Jun 2003 | B2 |
6630022 | Lessard et al. | Oct 2003 | B2 |
Number | Date | Country |
---|---|---|
WO 2004041746 | May 2001 | WO |
Number | Date | Country | |
---|---|---|---|
20050252421 A1 | Nov 2005 | US |