1. Technical Field
This invention relates to treating clean surfaces with well water containing an agent to inhibit the formation of rust and to cleaning off rust stains from surfaces that have been treated with water containing iron ions, such as the porous surfaces of plants and concrete which have been sprayed with water drawn from a well.
2. Description of the Prior Art
In the prior art it was known to clean off rust stains from the porous surfaces of plants and concrete that have been treated with water containing iron ions, such as surfaces which have been sprayed with water drawn from a well. The most common cleaners contain oxalic acid. This acid containing product is applied after the spraying has ceased. Once applied, this acid had to be treated with water the remove it; after it had cleaned off the rust.
Rust inhibitors containing other substances were then mixed with the incoming well water being sprayed in the next cycle, to prevent further rust formulation.
We have found that current products are not effective over the long run in preventing rust stain reoccurrence.
Our invention comprises several products and processes for preventing the occurrence of rust stains resulting from well water irrigation systems and for cleaning off rust stains resulting from well water irrigation systems.
In one embodiment, we mix ammonium sulfate with well water to form a solution. Then we mix this resulting solution with incoming well water and then treat the surfaces with this mixture of well water to prevent rust formation.
In another embodiment, we mix ammonium bisulfate with water and treat surfaces containing rust stains with this dilute ammonium bisulfate for removal of rust stains. Then we mix ammonium sulfate with the incoming well water being sprayed in the next cycle, to prevent rust formation.
In the preferred embodiment, mix ammonium sulfate with well water to form a solution. Then add this resulting solution to the well water being sprayed out in an irrigation system to prevent rust formation on the porous surfaces of plants and concrete being sprayed. This solution can be prepared using one teaspoon of ammonium sulfate to one gallon of water.
Note that if the water is neutral and has low dissolved solids in it, it would take very little ammonium sulfate to make the water slightly acidic and prevent rust formation.
In another embodiment, mix ammonium bisulfate with water to form a dilute solution. Then treat surfaces containing rust stains with this dilute solution of ammonium bisulfate for removal of rust stains. Then mix a solution of ammonium sulfate with the incoming well water being sprayed in the next cycle (as described above in connection with the preferred embodiment), on the surfaces that had been treated and thus prevent rust formation.
One method of making ammonium bisulfate is to mix 1.5 gal of battery acid (H2SO4) with 7.5 pounds of ammonium sulfate. The resulting solution can then be diluted with an equal amount of water.
This may then be diluted by half again with water.
Apply this resulting solution to stained areas to remove the rust stains.
In alternate embodiments, this solution may be further diluted with water and then applied to stained areas until the diluted solution is no longer effective in removing rust stains. By this trial and error method, the most cost effective rust removal solution may be determined.
Once the rust has been removed, and before the surfaces are dry, treat the surfaces again with an ammonium sulfate solution (as described above in connection with the preferred embodiment) prevent rust formation.
One way to effect this second treatment is to add this second solution to the last ten percent of the initial spraying cycle in an irrigation system spraying well water. This may be accomplished by providing a duplicate parallel timer controlled well pump activation system; set to recycle the irrigation at ten percent of the times used in the irrigation cycle. This duplicate system should include a container for the solution to be added and a means of withdrawing the solution and introducing it into well water being sprayed.
Testing in the actual environment should be done to show the frequency of application needed to prevent rust re-occurrence.
Number | Name | Date | Kind |
---|---|---|---|
1988823 | Winning et al. | Jan 1935 | A |
2101197 | Rice | Dec 1937 | A |
2360509 | Morgan et al. | Oct 1944 | A |
2585616 | Barnes | Feb 1952 | A |
2694657 | Brundin | Nov 1954 | A |
3804757 | Ruschenburg | Apr 1974 | A |
4578243 | Quinlan | Mar 1986 | A |
4828743 | Rahfield et al. | May 1989 | A |
5685993 | Liu | Nov 1997 | A |
5700377 | Cox | Dec 1997 | A |
6361613 | Lee | Mar 2002 | B2 |
6524397 | Sakurai et al. | Feb 2003 | B2 |
6528468 | Matsukawa et al. | Mar 2003 | B2 |
20040082489 | Gernon et al. | Apr 2004 | A1 |
20070023359 | Grott | Feb 2007 | A1 |