The invention relates to a process and a device for producing a shell-like consumable goods from mass containing fat, in particular a bulk fat containing cocoa or chocolate.
Processes and devices for producing shell-like chocolate articles are already known. For example, EP 0 589 820 B1 discloses a process and a device for producing outer shells from masses containing fat, and similar to chocolate, in particular for chocolate articles. At the same time an alveola (a moulded cavity) is filled with tempered chocolate-like mass, which hardens inwards from the aveola out with crystallisation for developing the outer shape of the shell, whereby the alveola has a lower temperature than that of the tempered mass. Immediately after the mass is poured into the alveola a cooling body with a temperature below 0° C. is lowered into the mass and kept in this fully immersed position for a preset period in the mass, so that a preset shell volume between the cooling body and the alveola is specified.
With this particular method of operation there is, however, no guarantee that the mass containing fat filling the alveola is free from air pockets. Such air pockets can be present e.g. in the case of tempered chocolate mass in more or less large and more or less evenly distributed air bubbles in the melted bulk fat. They can e.g. already be contained in the tempered chocolate mass in the storage vessel before filling of the alveola or originate from the environmental air when the alveolae are being filled with chocolate mass.
WO 98/52425 describes a process and a device for producing shell-like chocolate articles.
U.S. Pat. No. 6,135,016 also describes a plant for producing chocolate articles with a vibration section for vibrating shells filled with liquid chocolate.
Furthermore, according to the nature of the mass containing fat to be treated it can also eventuate that the alveola filled with mass is not evenly distributed in the alveola.
Both air pockets in the mass containing fat and uneven distribution of the mass in the alveola can result impairing of the mass in the alveola can result impairing the quality of the shell-like consumable goods formed after the cooling body is lowered into the liquid mass, such as e.g. uneven shell thickness including holes in the shell, uneven shell edge, etc.
The object of the invention is therefore to provide a process and a corresponding device for producing a shell-like consumable goods from a fatty mass, in particular a bulk fat containing cocoa or chocolate, wherein the shortcomings mentioned at the outset are by and large avoided.
This task is achieved according to the present invention in the initially described process of the prior art, after the alveola is filled and before the cooling body is immersed, by the flowable tempered bulk fat being treated for a specific duration of vibration in vibration, characterised in that the exciting vibration frequency has approximately the same value as a resonance frequency of the liquid mass in the alveola.
This task is solved in terms of equipment by in a device of the state of the art vibration means being provided, with which the mass containing fat can be treated in vibration, characterized in that the vibration means can be operated with variable frequency.
Due to the process according to the present invention even before the cooling body is lowered, i.e. before the actual step of cold stamping, the mass is distributed as evenly as possible in the alveola. And at least extensive ventilation of the mass takes place before the actual crystallisation and moulding step.
Vibration of the flowable tempered bulk fat in the alveolae of the mould is preferably generated by vibrating the mold, which then imparts its vibration completely to the substance contained therein. As an alternative or by way of addition, the free-flowing, heated fatty substance can also be made to vibrate in the alveoli by vibrating the air over the alveoli, which then conveys the vibration to the substance in the alveolus via the air.
Depending on the consistency of the substance to be processed, it may be advantageous to have vibration take place during the period of vibration at a frequency that progresses from a minimum frequency at the start of the vibration period to a maximum frequency at the end of the vibration period, or have vibration take place during the period of vibration at a frequency that progresses from a maximum frequency at the start of the vibration period to a minimum frequency at the end of the vibration period. On the other hand, it can also be advantageous to have vibration take place during the period of vibration independently thereof at an amplitude that progresses from a maximum amplitude at the start of the vibration period to a minimum amplitude at the end of the vibration period, or have vibration take place during the period of vibration at an amplitude that progresses from a minimum amplitude at the start of the vibration period to a maximum amplitude at the end of the vibration period.
These measures make it possible to take into account the type of air pockets, e.g., large or small, air bubbles present mainly on the floor of the mold or the surface of the substance, which enables a more efficient smoothing out of the substance and its more efficient evacuation.
In another possible variant of the procedure according to the invention, the exciting vibration frequency has roughly the same value as a resonance frequency of the fluid substance in the alveolus, wherein the exciting vibration frequency preferably passes through several frequency ranges in which a resonance frequency of the fluid substance in the alveolus lies. It is best to allow the exciting vibration frequency to remain at least at one of the resonance frequencies of the fluid substance during its frequency progression for a period measuring a fraction of the overall vibration period.
As an alternative or by way of addition, the exciting vibration frequency can have roughly the same value as a resonance frequency of the alveolus, wherein the exciting vibration frequency can here as well in particular be made to pass through several frequency ranges, in which a resonance frequency of the alveolus lies. During its progression through the frequencies, the exciting vibration frequency is here also best allowed to stay at least at one of the resonance frequencies of the alveolus for a duration representing a fraction of the overall vibration period.
Working with resonance frequencies (natural frequencies) of the mold containing the fluid substance and/or the alveolus or alveoli enables a considerable infusion of mechanical oscillation energy into the fluid substance to be processed, wherein various resonance frequencies of the substance and/or the alveolus can be used in a targeted fashion to “drive out” air blisters or air bubbles of varying size. In particular, various frequencies, in particular resonance frequencies, can be simultaneously used for excitation purposes, wherein the one frequency is introduced into the substance via the air, and the other frequency via the alveolus.
In another preferred variant, the alveolus and cooling element are each rotationally symmetric along a shared axis of symmetry. After the alveolus has been filled and before the cooling element is submerged, each alveolus and the heated, free-flowing fatty substance therein can be made to rotate around the axis of symmetry for a specific period of rotation.
Since the alveolus is filled only slightly with fluid substance before the cooling element is submerged, the free-flowing substance forms a paraboloidal surface during exposure to the centrifugal and gravitational forces inside the alveolus, which is considerably larger than the flat surface of the substance without rotation. This facilitates the evacuation of the fluid substance, primarily owing to the fact that the air bubbles only still have a distinctly shorter path to the surface on the one hand, and that a stronger field of force prevails inside the paraboloidally arranged fluid substance on the other hand, so that the air bubbles are driven out of the substance much faster than without rotation along the lines of force that are curved inside the substance and run perpendicular to the surface of the substance at a constant viscosity of the substance. Use is here made of the fact that the lines of force of the substance forces (gravitational force+centrifugal force) are curved at all locations of the surface perpendicular to the surface and inside the fluid substance, but still run approximately perpendicular to the surface over wide areas in the fluid substance after the paraboloidal equilibrium surface caused by the rotation and gravitation has been reached. At the same time and also advantageously, however, the substance is already pre-distributed to approximate the desired shell form while preparing for the subsequent cold-stamping and crystallization step. This is expedient and desired, since, during the expulsion process and formation of the fluid substance during the actual cold-stamping step, the greater part of the substance contained in the mold only has to traverse shorter paths while flowing into the final mold, which as a whole results in an improved “uniform treatment” of all parts of the substance during cooling, flowing and crystallizing.
In another variant, the alveolus and cooling element are also each rotationally symmetric along a shared axis of symmetry, and, after the alveolus has been filled and before the cooling element is submerged, a stream of air rotationally symmetric relative to the axis of symmetry shared by the alveolus and cooling element is injected into the alveolus via the free-flowing, heated fatty substance contained therein over a specific injection period. Similarly to rotation, this increases the surface, and yields a distribution of the fluid substance approximating the final shell shape, with similar advantages.
The air enveloping the cooling element in the procedure is best continuously dehumidified to prevent the condensation of water vapor on the cooling element. The air enveloping the cooling element in the procedure can additionally be continuously cooled.
The air used for rotationally symmetric injection into the alveolus preferably has the same temperature as the fluid, heated substance in the alveolus. This prevents the surface of the fluid substance from cooling, and crystallization from setting in prematurely before the cooling element is submerged. This also facilitates a “uniform treatment” of all areas of the fluid substance during the cold-stamping step, and hence more uniform products.
The air used in the alveolus for rotationally symmetric insertion is also best continuously dehumidified to minimize the penetration of water into the fluid substance.
It is particularly advantageous for the dew point of the air to always be kept under the surface temperature of the cooling element. As a result, the cooling element always remains dry, and retains its surface that defines the inner shell surface, thereby preventing adulteration of the inner shell surface. Hygiene is also improved, since bacterial growth is inhibited on a cool and dry surface.
The surface of the cooling element is ideally kept at a temperature of less than −10° C.
In a particularly preferred variant of the device according to the invention, the vibrating means is suitably coupled with the alveolus in such a way that the vibrations can be conveyed to the mold (structure-borne noise principle).
In another preferred variant, the vibrating means is suitably coupled with the air over the alveolus in such a way that the vibrations can be conveyed to the air (airborne sound principle).
The vibrating means is best operated at a variable frequency and/or variable amplitude.
In another preferred variant, the mold and cooling element are each rotationally symmetric along a shared axis of symmetry, and the alveolus can be rotated around the axis of symmetry.
In another preferred variant, the alveolus and cooling element are also each rotationally symmetric along a shared axis of symmetry, with a pressure source being provided that can inject a stream of air rotationally symmetric relative to the axis of symmetry shared by the alveolus and cooling element into the alveolus, wherein the device best has an air dehumidifier and/or air heater.
It is particularly advantageous for the cooling element to have a thermal conductivity of over 200 W/mK. This enables a rapid cooling of the fat-containing substance with especially fine crystals.
Additional advantages, features and possible applications of the invention are described in the following description with reference to the accompanying drawings:
The fat-containing chocolate substance is heated in a temperature range of approx. 28 to 34° C. at the heating station 1. Stable triglyceride crystals of cocoa butter lie within this temperature range. They are used as crystal nuclei during the subsequent cooling and solidification of the chocolate substance. The heated chocolate substance is routed in metered quantities via the metering station 2 to the molds to be filled, which were transported in by the transporting device 5.
The molds whose alveoli have been filled with fluid chocolate substance are then transported on by the transporting device 5 to the shaking station 3, in which the alveoli or molds filled with the chocolate substance are vibrated for a specific time to bring about a uniform distribution of the still fluid chocolate substance in the alveoli and evacuate the fluid chocolate substance. As soon as the shaking or vibrating step has been completed at the shaking station 3, the alveoli filled with the still fluid chocolate substance are transported on by the transporting device 5 to the cold-stamping station 4.
At the cold-stamping station 4, an intensely cooled stamp made out of a readily thermally conductive material is submerged in the alveoli filled with fluid chocolate substance at a temperature of below −10°, into the still fluid chocolate substance containing triglyceride crystal nuclei, which then becomes distributed in the shell-shaped mold defined by the alveolus and cold stamp submerged into the alveolus, and shortly thereafter solidifies into the desired chocolate sleeve, whereupon the stamp is again lifted, and the solidified chocolate shells are removed from the alveoli.
Number | Date | Country | Kind |
---|---|---|---|
101 22 548 | May 2001 | DE | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/DE02/00806 | 3/6/2002 | WO | 00 | 12/17/2003 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO02/089595 | 11/14/2002 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
3447587 | Bodine, Jr. | Jun 1969 | A |
3666388 | Oberwelland | May 1972 | A |
3798337 | Abalo | Mar 1974 | A |
4421773 | Akutagawa | Dec 1983 | A |
4478858 | Baird et al. | Oct 1984 | A |
5034240 | Tanaka et al. | Jul 1991 | A |
5409722 | Binley | Apr 1995 | A |
5492708 | Hemmerich | Feb 1996 | A |
5635230 | Aasted | Jun 1997 | A |
5705217 | Aasted | Jan 1998 | A |
5795613 | Scharfmann et al. | Aug 1998 | A |
6135016 | Bindler | Oct 2000 | A |
6268006 | Knobel | Jul 2001 | B1 |
6497568 | Aasted | Dec 2002 | B1 |
6641386 | Aasted | Nov 2003 | B2 |
Number | Date | Country |
---|---|---|
11 13 865 | Sep 1961 | DE |
11 45 467 | Mar 1963 | DE |
37 34 626 | Oct 1988 | DE |
4241610 | Jun 1994 | DE |
0914774 | May 1999 | DK |
0914775 | May 1999 | DK |
0 589 820 | Mar 1994 | EP |
05030912 | Feb 1993 | JP |
9852425 | Nov 1998 | WO |
WO-9852425 | Nov 1998 | WO |
9934685 | Jul 1999 | WO |
Number | Date | Country | |
---|---|---|---|
20040137113 A1 | Jul 2004 | US |