1. Field of the Invention
The invention relates to structural joining of advanced superalloy components during fabrication and/or repair. In some embodiments, the invention relates to surface repair of superalloy turbine blades and vanes in steam or gas turbines, by use of splice inserts that are affixed to a new or repaired substrate by projection resistance heat brazing under contact pressure, in a manner that does not significantly reduce mechanical structural or material properties of the joined components.
2. Description of the Prior Art
“Structural” repair of gas turbine or other superalloy components is commonly recognized as replacing damaged material with matching alloy material and achieving properties, such as strength, that are close to the original manufacture component specifications (e.g., seventy percent ultimate tensile strength of the original specification). For example, it is preferable to perform structural repairs on turbine blades that have experienced surface cracks, so that risk of further cracking is reduced, and the blades are restored to original material structural and dimensional specifications.
Structural repair or new fabrication of nickel and cobalt based superalloy material that is used to manufacture turbine components, such as cast turbine blades, is challenging, due to the metallurgic properties of the finished blade material. For example, as shown in
A past attempt to perform traditional “spot” electric resistance welding of superalloys, in a heat resistance joining apparatus, by passing current between compressed electrodes into a pair of abutting superalloy components also caused solidification cracking within the weld zone. Alternative superalloy welding processes, including laser microcladding with chill fixtures, welding in so-called “hot” boxes at elevated temperatures, and inertia friction welding may still lead to post weld heat treatment strain age cracking. Other friction welding processes, such as friction stir welding, can reduce superalloy cracking propensity, but the employed welding apparatus has relatively limited tool life. The same cracking concerns occur during superalloy component fabrication, when separate components constructed of superalloy material are joined by welding processes.
In comparison to structural repair or fabrication, “cosmetic” repair or fabrication of superalloys is recognized as replacing damaged material (or joining two components of newly fabricated material) with unmatching alloy material of lesser structural property specifications, where the localized original structural performance is not needed. For example, cosmetic repair may be used in order to restore the repaired component's original profile geometry. As noted above, it is desirable to perform structural repairs on surface cracks in order to reduce their likelihood of subsequent spreading when the component is returned to service. Conversely, an example of cosmetic repair is for filling surface pits (as opposed to structural cracks) on a turbine blade airfoil in order to restore its original aerodynamic profile, where the blade's localized exterior surface is not critical for structural integrity of the entire blade. Cosmetic repair or fabrication is often achieved by using oxidation resistant weld or braze alloys of lower strength than the blade body superalloy substrate, but having higher ductility and lower application temperature that does not negatively impact the superalloy substrate's material properties.
In the past, electric resistance brazing has been commonly used for cosmetic metal joining of common ferrous and non-ferrous (e.g., copper) alloys. As shown in
Given the shortcomings of superalloy structural repair welding, often the only commercially acceptable solution is to scrap damaged turbine blades that require structural repair, because past experience has shown limited success of such structural repairs. Thus repairs have been limited to those that have in the past been proven to be performed successfully by alternative superalloy welding processes described above, or by cosmetic welding, employing more ductile welding rod filler materials with reduced structural strength.
Thus, a need exists in the art for a method for performing structural joining or repairs on surfaces of superalloy components, such as turbine vanes and blades, so that subcomponents can be joined; or that structural cracks and other surface defects can be repaired.
Another need exists in the art to increase successful rates of structural repairs on surfaces of superalloy components, such as turbine vanes and blades, so that damaged blade scrap rates can be reduced.
Yet another need exists in the art for a method for performing structural joining or repairs on surfaces of superalloy components, such as turbine vanes and blades, with proven, repeatable repair techniques and machinery, that do not require complex welding or post-repair heat treatment procedures.
Accordingly, an object of the invention is to perform structural joining or repairs on surfaces of superalloy components, such as turbine vanes and blades, so components can be joined; or that structural cracks and other surface defects can be repaired.
Another object of the present invention is to increase the likelihood of performing successful structural repair of superalloy components, such as turbine vanes and blades, so that damaged component scrap rates can be reduced.
Yet another object of the present invention is to perform structural fabrication or repair of superalloy components, such as turbine blades or vanes, with proven, repeatable repair techniques and machinery that do not require complex welding or post-repair heat treatment procedures.
These and other objects are achieved in accordance with the present invention embodiments by structurally joining superalloy components, or repairing defects in superalloy material components, such as turbine blades or vanes. In repair embodiments, the surface defect is removed from the component substrate by electric discharge machining or other known metal working process, forming an excavated recess. A repair splice is formed, preferably of a same material with similar mechanical structural properties, having a mating projection with profile conforming to the corresponding recess profile. The repair splice is inserted and captured within the recess so that they abut each other along a contact surface. The splice and substrate are resistance heated under compression pressure until melting of braze alloy occurs along the contact surface, so that they are mutually affixed. A repair alloy braze must be interposed between the splice and recess substrate prior to resistance heating.
The present invention features a joined superalloy component including a superalloy substrate defining a recess having a recess profile; and a mating superalloy splice having a splice projection captured within the substrate recess, with a projection profile conforming with the substrate profile along a contact surface within the recess. The substrate and splice are affixed to each other along the contact surface by the process of electric resistance brazing by interposing brazing alloy between the recess and repair splice along the contact surface. Next the substrate and splice projection are compressed together along the contact surface at a selected pressure. The substrate and splice are contacted with separate conductive electric resistance brazing electrodes. Current is passed through the substrate and splice projection between the electrodes at a selected flow rate and application time period until localized melting of the brazing alloy occurs along the contact surface. Current flow is ceased after the substrate and splice projection are mutually affixed to each other.
The present invention features a method for joining superalloy structures by forming a recess in a superalloy component substrate having a recess profile defined by the remaining substrate; and forming a mating superalloy splice having a splice projection, with a projection profile conforming with the substrate recess profile along a corresponding contact surface. Brazing alloy is interposed between the recess and repair splice along the contact surface. The splice is inserted and captured within the recess, so that the projection and recess are in abutting contact along the contact surface. The substrate and splice projection are compressed together along the contact surface at a selected pressure. The substrate and splice are in contact with separate conductive electric resistance brazing electrodes. Current is passed through the substrate and splice projection between the electrodes at a selected flow rate and application time period until brazing alloy localized melting occurs along the contact surface. Current flow ceases after the substrate and splice projection are mutually affixed to each other.
The present invention also features a method for repairing a superalloy component by removing a damaged portion of superalloy component substrate and forming an excavated recess therein having a recess profile defined by the remaining substrate. A mating superalloy repair splice is formed, having a splice projection, with a projection profile conforming with the substrate recess profile along a corresponding contact surface. Brazing alloy is interposed between the recess and repair splice along the contact surface. The repair splice is inserted and captured within the recess, so that the projection and recess are in abutting contact along the contact surface. The substrate and splice projection are compressed together along the contact surface at a selected pressure with a pair of opposed electric resistance brazing electrodes. Current is passed through the substrate and splice projection between the electrodes at a selected flow rate and application time period until brazing alloy localized melting occurs along the contact surface and they are mutually affixed to each other.
The objects and features of the present invention may be applied jointly or severally in any combination or sub-combination by those skilled in the art.
The teachings of the present invention can be readily understood by considering the following detailed description in conjunction with the accompanying drawings, in which:
To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures.
After considering the following description, those skilled in the art will clearly realize that the teachings of the present invention can be readily utilized for mechanical structural joining/repair of superalloy components. In some embodiments, the teachings of the present invention can be readily utilized for structural repair of superalloy material turbine blades and vanes of the type used in steam or gas turbines, by use of splice inserts, in a manner that does not significantly reduce mechanical structural or material properties of the joined or repaired blade. In the present repair method, the damage is removed, forming an excavated recess. A repair splice is formed of a same material with similar mechanical structural properties, having a mating outer profile conforming to the corresponding recess profile. The repair splice is inserted and captured within the recess, so that the blade body and repair splice are in abutting contact along a contact surface. The splice and abutting substrate are compressed under pressure and locally heated with an electric resistance heating brazing apparatus, until melting of braze alloy occurs along the contact surface, so that they are mutually affixed. The repaired component's overall mechanical structural properties are similar to those of an undamaged component. The repair methods of the present invention do not require complex brazing, welding or heat treatment procedures, and use known electric resistance heating brazing equipment and affixation processes. In addition to performing repairs, the joining methods of the present invention may be used to fabricate superalloy structures by joining subcomponents.
Present Invention Mechanical Structural Joining/Repair
In the repair method of the present invention cracked regions 42 of the component substrate 40 are excavated by electric discharge machining (EDM) or other known metal removal processes, leaving a recess 44 in the uncracked substrate, as shown in
In known repair or fabrication methods, recess 44 would have been filled by heat application of softer filler material (cosmetic repair) or by filler material of similar hardness. As previously discussed, other welding techniques applying superalloy filler generally induce undesirable cracks in the superalloy component during welding or during subsequent post-welding heat treatment.
The present invention differs from prior known replacement of superalloy material in cracks or formed recesses by inserting a repair splice 50, preferably constructed of the same superalloy material with similar material properties as the repaired component, as shown in
A bonding filler braze alloy 60 must be interposed between the mating recess 44 and projection 52 to aid their respective joining during subsequent resistance heating processes. Filler alloy is chosen for compatibility with the chosen resistance heating bonding/joining process. For example, brazing filler alloy, having a lower melting temperature than the superalloy substrate 40 and repair splice 50, is chosen for brazing processes. Welding filler alloys likely will have higher melting temperatures. While powdered bonding filler 60 is shown schematically in
Referring to
Similarly, a continuous seam weld longer than the electrode 22′, 24′ surface area can be formed by using longer, linear electrodes, rolling wheel electrode(s), a plurality of proximal electrodes oriented in an array or moving the electrodes serially relative to the superalloy substrates 40, 50. Similarly, multiple recesses 44 and projecting portions 52 may be formed in superalloy components 40, 50 and subsequently joined by resistance heating tools sequentially and/or simultaneously.
In performing the joining processes of the present invention, sufficient pressure and electric current are selectively applied to cause localized melting and affixation of the projecting portion 52 and recess 44 along the contact surface 62, but not excessive heat or pressure that will significantly alter material properties of the component substrate 40 or the splice 50 at any significant distance from the contact surface. Accordingly, localized heating is stopped when desired braze melting and affixation is achieved. Localized melting properties along the contact surface 62 are affected by the recess 44/projection 52 profile depth d and width W, as those dimensions (along with length) impact applied pressure per unit area and heat transfer flux. It is desirable to construct the contact surface profile so that its depth d is smaller than its width W, and with angled side walls, so that excess melted braze material is extruded from the contact surface 62 juncture, as shown in
After desired braze melting along the contact surface 62 is achieved, resistance heating ceases and the now mutually affixed component substrate 40 and repair splice 50 are allowed to cool for subsequent removal from the resistance heating apparatus 20′. The repair splice 50 and extruded braze material along the contact surface 62 are conformed to the surrounding surface profile, restoring the repaired component 40 to its original condition, shown in
The localized affixation along the contact surface 62 does not significantly negatively impact structural material properties of the repaired component substrate 40 and the splice 50. Limited post repair heat treatment (if any is required) minimizes—if not totally eliminates—subsequent risk of repaired component strain age cracking. Thus, time and expense of superalloy component fabrication or repair may be undertaken with the repair methods of the present invention, without undue risk of repair failure. In the power generation field, surface cracked turbine blades may be repaired without the need to scrap and replace them with new blades.
Different known resistance heating methods may be employed to join the mating superalloy components. Suitable resistance heating methods include resistance brazing, resistance braze diffusion bonding, and resistance transient liquid phase bonding. Resistance heating joining/bonding may be carried out in ambient air, or alternatively in isolated vacuum, inert gas or active gas environments. As noted above, the resistance heating joining/bonding may be performed with filler alloy, flux and/or activator compositions that are compatible with the selected heating process. In any of the selected resistance heating methods the overall objective is to achieve localized bonding between the superalloy subcomponents along the contact surface 62 and ceasing additional heat input, without significantly impacting the superalloy material properties within the generalized substrate of either subcomponent. Unlike known welding techniques that tend to liquefy the respective superalloy substrates (and thus negatively alter material properties making them susceptible to subsequent cracking), the resistance heating application in the present invention avoids gross changes in the superalloy substrates—especially eliminating residual stresses associated with shrinkage typical during weld solidification.
When practicing the present invention, superalloy components can be joined or repaired with known proven equipment. Damaged superalloy component material can be removed and repair splices fabricated by electric discharge machining or other known metal cutting techniques. Known electric resistance heating brazing machinery and techniques may be employed to affix repair splices to their mating recesses. The splice-repaired superalloy component external surface profile can be restored to original profile specifications by grinding or cutting the repair splice and surrounding contact surface to match the repaired component's local profile.
While the structural joining of superalloy components exemplary embodiments herein have been primarily described with reference to superalloy component repair, the same methods may be used to fabricate superalloy structures by joining subcomponents. For example, a projection on one superalloy subcomponent may be affixed to a recess on another superalloy subcomponent.
Although various embodiments which incorporate the teachings of the present invention have been shown and described in detail herein, those skilled in the art can readily devise many other varied embodiments that still incorporate these teachings.
This application claims the benefit of U.S. provisional patent application entitled “Projection Resistance Brazing of Superalloys for Repair of Service-Degraded Components”, filed Nov. 7, 2011, and assigned Ser. No. 61/556391, which is incorporated by reference herein.
Number | Name | Date | Kind |
---|---|---|---|
1592609 | Mattice | Jul 1926 | A |
2629803 | Bondley | Feb 1953 | A |
3119632 | Skinner | Jan 1964 | A |
3487530 | Ely | Jan 1970 | A |
4912295 | Arimochi et al. | Mar 1990 | A |
4924054 | Marcie et al. | May 1990 | A |
5033334 | Phaal et al. | Jul 1991 | A |
5479704 | Richter et al. | Jan 1996 | A |
5609776 | Li | Mar 1997 | A |
5961853 | Thornton | Oct 1999 | A |
6210635 | Jackson et al. | Apr 2001 | B1 |
6213379 | Takeshita et al. | Apr 2001 | B1 |
6327766 | Cardente | Dec 2001 | B1 |
6413650 | Dupree et al. | Jul 2002 | B1 |
6908288 | Jackson et al. | Jun 2005 | B2 |
6994920 | Trewiler | Feb 2006 | B2 |
7156280 | Jiang et al. | Jan 2007 | B1 |
8158903 | Meier | Apr 2012 | B2 |
8398374 | Roberts et al. | Mar 2013 | B2 |
20020139794 | Budinger | Oct 2002 | A1 |
20040134887 | Murphy | Jul 2004 | A1 |
20050092717 | Trewiler | May 2005 | A1 |
20070346760 | Zhang et al. | Feb 2007 | |
20080237306 | Sathian | Oct 2008 | A1 |
20090026182 | Hu et al. | Jan 2009 | A1 |
20090140030 | Amancherla et al. | Jun 2009 | A1 |
20090266870 | Yousefiani et al. | Oct 2009 | A1 |
20101358120 | Cairo et al. | Jun 2010 | |
20110031223 | Belanger | Feb 2011 | A1 |
20110062219 | Bezaire et al. | Mar 2011 | A1 |
20110168679 | Qi et al. | Jul 2011 | A1 |
20110233293 | Kral et al. | Sep 2011 | A1 |
20120063894 | Chen et al. | Mar 2012 | A1 |
20120205014 | Bruck et al. | Aug 2012 | A1 |
20130081269 | Trapp et al. | Apr 2013 | A1 |
20130115091 | Bruck et al. | May 2013 | A1 |
20130115480 | Bruck et al. | May 2013 | A1 |
20130260178 | Sansom et al. | Oct 2013 | A1 |
20130263434 | Gugel | Oct 2013 | A1 |
20140044984 | Bruck | Feb 2014 | A1 |
Number | Date | Country |
---|---|---|
4411680 | Aug 1995 | DE |
4447403 | Jan 1996 | DE |
0191300 | Aug 1986 | EP |
1527839 | May 2005 | EP |
2369131 | Sep 2011 | EP |
2492044 | Aug 2012 | EP |
2619331 | Aug 1988 | FR |
1368846 | Oct 1974 | GB |
356021736 | Feb 1981 | JP |
62199260 | Sep 1987 | JP |
Entry |
---|
U.S. Appl. No. 13/352,468, filed Jan. 18, 2012, entitled Projection Resistance Welding of Superalloys, Under Final Rejection. |
U.S. Appl. No. 13/561,174, filed Jul. 30, 2012, entitled Method for Resistance Braze Repair, Under Non-final Rejection. |
U.S. Appl. No. 13/571,754, filed Aug. 10, 2012, entitled Stud Welding Repair of Superalloy Components, Application Allowed. |
Translation of DE 4411680 (EP0676259). |
Machine translation of European Patent document No. 191,300, published Apr. 2015. |
Number | Date | Country | |
---|---|---|---|
20130115477 A1 | May 2013 | US |
Number | Date | Country | |
---|---|---|---|
61556391 | Nov 2011 | US |