Claims
- 1. The method of applying a thin narrow width annular coating to a portion of the outer peripheral surface of a can body member comprising:
- rotatably moving the can body member along a path of movement across an elongated rotating coating applicator roller member having a rotational axis extending parallel to the path of movement and transversely to the rotational axis of the can body member; and
- engaging a narrow width portion of the periphery of the lower side wall portion of the can body member with a narrow width elongated portion of the periphery of the coating application roller during substantially only one revolution of the can body member during the movement thereof across the rotating coating application roller.
- 2. The invention as defined in claim 1 and further comprising:
- simultaneously rotatably moving a plurality of can body members along the path of movement in closely spaced relationship;
- causing simultaneous engagement of a plurality of can body members with the rotating coating application roller during the movement thereacross; and
- simultaneously coating peripheral portions of each can body member in engagement with the coating application roller means during movement thereacross.
- 3. The invention as defined in claim 2 and further comprising:
- maintaining uniform rotational speed and speed of movement and spacing of the can body members along the rotating coating application roller.
- 4. The invention as defined in claim 3 and further comprising:
- maintaining uniform constant rotational speed of the coating application roller.
- 5. The invention as defined in claim 4 and further comprising:
- preheating the can body members prior to movement across the coating application roller to a temperature suitable for promoting the application and curing of the coating material used.
- 6. The invention as defined in claim 5 and further comprising preheating the coating material and maintaining it in a fluid state during its application to the can body members.
- 7. The invention as defined in claim 6 and further comprising:
- selecting a coating material that is fluid at temperatures between about 205.degree. F. and 215.degree. F.;
- preheating the can body members to a temperature between approximately 110.degree. F. and 120.degree. F.; and
- maintaining the temperature of the coating material at between approximately 205.degree. F. and 215.degree. F. during the coating of the can body members.
- 8. The invention as defined in claim 7 wherein the coating material selected is capable of being cured by heat or ultraviolet light to a clear abrasion resistant coating, the invention further comprising:
- immediately transferring the coated can body members to a coating curing apparatus after application of the coating; and
- immediately curing the coating after transfer from the coating application roller member.
Parent Case Info
This is a division of application Ser. No. 891,309 filed Mar. 29, 1978.
US Referenced Citations (11)
Divisions (1)
|
Number |
Date |
Country |
| Parent |
891309 |
Mar 1978 |
|