Claims
- 1. A method of suppressing the flow of radon from the ground into a building, the method comprising:(a) obtaining a sheet of multilayer plastic film comprising an inner layer having an oxygen diffusivity of less than about ten cubic centimeters per day and outer layers comprising polyethylene, polypropylene, or ethylene vinyl acetate; and (b) placing the plastic film on or under the lowest floor of the building.
- 2. The method of claim 1 wherein the plastic film is placed on the lowest floor of the building.
- 3. The method of claim 2 wherein the inner layer of the film comprises ethylene vinyl alcohol copolymers, polyvinylidene chloride, nylon, polyethylene terephthalate, or polyvinyl alcohol.
- 4. The method of claim 3 wherein the inner layer of the film comprises ethylene vinyl alcohol copolymers.
- 5. The method of claim 4 wherein the inner layer of the film comprises ethylene vinyl alcohol copolymers having about 20 to 60 mole percent ethylene monomers.
- 6. The method of claim 5 wherein the inner layer of the film has an oxygen diffusivity of less than about five cubic centimeters per day.
- 7. The method of claim 6 wherein adhesive layers are sandwiched between the inner layer and the outer layers.
- 8. The method of claim 7 wherein the multilayer film has a thickness of about 0.5 to 20 mils, and wherein the inner layer of ethylene vinyl alcohol copolymer comprises about 5 to 70 percent of the thickness, the adhesive layers comprise about 5 to 40 percent of the thickness, and the outer layers of polyethylene, polypropylene, or ethylene vinyl acetate comprise about 5 to 80 percent of the thickness.
- 9. A method of suppressing the ingress of radon gas from soil into a building through a floor of the building, the method comprising:(a) providing a first layer comprising an ethylene vinyl comprising a plastic alcohol copolymer having a predetermined percent mole ethylene; (b) providing a second layer wherein the plastic is different than ethylene vinyl alcohol copolymer adjacent the ethylene vinyl alcohol copolymer layer to form a multilayer film; (c) disposing the multilayer film on or under the floor; and (d) covering the multilayer film.
- 10. The method of claim 9 wherein the predetermined percent mole of ethylene vinyl alcohol copolymer ranges between 20 to 60 percent of ethylene.
- 11. The method of claim 10 wherein the second layer comprises an adhesive layer.
- 12. The method of claim 11 wherein the second layer comprises a polyolefin.
- 13. The method of claim 12 wherein the ethylene vinyl alcohol copolymer layer is about 5 to 70 percent of a thickness of the multilayer film.
- 14. The method of claim 13 wherein the adhesive layer is about 5 to 40 percent of a thickness of the multilayer film.
- 15. The method of claim 14 wherein the plastic layer is about 5 to 80 percent of a thickness of the multilayer film.
- 16. The method of claim 9 wherein the disposing step further includes disposing the film adjacent the soil.
- 17. The method of claim 9 wherein the multilayer film has a thickness of between about 0.5 mil and 20 mil.
CROSS-REFERENCE TO RELATED APPLICATION
This application is a continuation-in-part of U.S. patent application Ser. No. 09/691,428, filed Oct. 18, 2000, now abandoned.
US Referenced Citations (2)
Number |
Name |
Date |
Kind |
5137764 |
Doyle et al. |
Aug 1992 |
A |
20020061982 |
Donald et al. |
May 2002 |
A1 |
Foreign Referenced Citations (1)
Number |
Date |
Country |
2 236 127 |
Mar 1991 |
GB |
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
09/691428 |
Oct 2000 |
US |
Child |
10/349900 |
|
US |