Claims
- 1. A method for recovering alkali values from underground trona deposits which comprises
- (i) introducing into the region of the trona deposit an aqueous mining solvent having dissolved therein from about 2 to 7% by weight sodium hydroxide;
- (ii) maintaining the solvent in the region for a period sufficient to solubilize at least a portion of the trona as sodium carbonate;
- (iii) withdrawing from the region at least a portion of the resulting mining solution;
- (iv) carbonating at least a portion of the withdrawn mining solution to convert the major portion of the sodium carbonate contained therein into sodium sesquicarbonate and/or sodium bicarbonate;
- (v) crystallizing the sodium sesquicarbonate and/or sodium bicarbonate;
- (vi) separating the crystallized solids from the mining solution mother liquor;
- (vii) calcining the crystallized solids in a direct coal fired calciner to form anhydrous sodium carbonate contaminated with impurities;
- (viii) recrystallizing the contaminated anhydrous sodium carbonate in water to form sodium carbonate-containing crystals while the contaminants remain in the aqueous liquor;
- (ix) separating purified sodium carbonate-containing crystals from the aqueous liquor containing contaminants;
- (x) maintaining an aqueous purge of liquor containing said contaminants;
- (xi) adding sodium hydroxide and water to at least one of said liquors, the amounts of sodium hydroxide and water being adjusted so as to form an aqueous mining solvent containing from about 2 to 7% by weight sodium hydroxide; and
- (xii) reintroducing the resulting aqueous mining solvent into the region of the trona deposit and repeating the cycle of recovery.
- 2. The method of claim 1 wherein the mining solvent contains from 3 to 5.5% sodium hydroxide.
- 3. The method of claim 1 wherein step (viii) is conducted under conditions to form sodium carbonate monohydrate as the sodium carbonate-containing crystals.
- 4. The method of claim 1 wherein step (viii) is conducted at atmospheric pressure and at a temperature between 80.degree. C. and 100.degree. C. to form sodium carbonate monohydrate as the sodium carbonate-containing crystals.
- 5. The method of claim 1 wherein step (viii) is conducted under conditions to form anhydrous sodium carbonate as the sodium carbonate-containing crystals.
- 6. The method of claim 1 wherein step (viii) is conducted under superatmospheric pressure and at a temperature of at least about 110.degree. C. to form anhydrous sodium carbonate as the sodium carbonate-containing crystals.
- 7. The method of claim 1 wherein the separated aqueous liquor in step (ix) serves as the aqueous purge liquor containing the contaminants.
- 8. The method of claim 1 wherein the aqueous liquor in step (viii) serves as the aqueous purge liquor containing the contaminants.
- 9. The method of claim 1 wherein sufficient water is added in step (xi) to compensate substantially for water losses and for the volume of solvent left in the region of the trona deposit.
- 10. The method of claim 1 wherein the sodium hydroxide in step (xi) is added by causticizing the selected liquor or liquors with lime.
- 11. The method of claim 1 wherein in step (xi) at least one of the separated liquors is treated with lime to convert the contained sodium carbonate into sodium hydroxide and calcium carbonate, to provide the required sodium hydroxide, the calcium carbonate is separated from the treated liquor, the recovered calcium carbonate is burned in a kiln to form said lime and carbon dioxide and at least a portion of said carbon dioxide is used as the carbonating agent in step (iv).
- 12. The method of claim 1 wherein the trona deposit is associated with substantial amounts of sodium chloride.
- 13. The method of claim 1 wherein the carbonation of step (iv) is effected by introducing carbon dioxide into the mining solution.
- 14. The method of claim 1 wherein ammonia is introduced in step (v).
- 15. The method of claim 1 wherein ammonia is introduced in step (v), the mother liquor of step (vi) is distilled to recover ammonia and the ammonia is introduced in step (v).
- 16. The method of claims 1, 3 or 4 wherein the purified sodium carbonate-containing crystals are dried to form dense soda ash.
Parent Case Info
This is a continuation-in-part of application Ser. No. 114,020, filed Jan. 21, 1980 and now abandoned.
US Referenced Citations (8)
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
114020 |
Jan 1980 |
|