The present invention contains subject matter related to Japanese Patent Application JP 2007-334844 filed in the Japanese Patent Office on Dec. 26, 2007, the entire contents of which are incorporated herein by reference.
1. Field of the Invention
The present invention relates to a reflection property control layer and display device whereby reflection properties can be switched.
2. Description of the Related Art
There are some display devices or the like which subject a screen surface to uniform gloss processing for the sake of improving the texture of an objet within a display image. This utilizes an advantage wherein the surface employs gloss specular reflection, so a substantial white level increases and also a black level decreases due to external light, and consequently a dynamic range is enlarged as compared to antiglare.
However, with regard to large displays, the uniformity of the screen is impaired by external light being projected thereon, and the fatigue of a viewer increases, so the screen surface is not subjected to gloss processing in many cases, and the gloss appearance and three-dimensional appearance of an object within a display image are impaired.
Also, with regard to printer apparatuses, a technique has been proposed wherein a gloss region of a light source or projection of the light source is detected from an input image, and a gloss appearance (glare/antiglare) is represented on an output printing sheet (e.g., see Japanese Unexamined Patent Application Publication No. 2002-51226). With regard to display devices, no technique has been proposed wherein glare/antiglare is dynamically switched according to an input image.
There has been recognized demand for providing a reflection property control layer and display device whereby the gloss appearance and three-dimensional appearance of an object can be improved.
A reflection property control layer according to an embodiment of the present invention is disposed in the front face of a display screen, whereby reflection properties are switched for each predetermined region.
A reflection property control layer according to an embodiment of the present invention is disposed in the front face of a display screen, wherein different reflection properties are disposed uniformly over the entire screen.
A display device according to an embodiment of the present invention includes: a reflection property control layer which is disposed in the front face of a display screen, whereby reflection properties are switched for each predetermined region; and a control unit configured to switch the reflection properties of the reflection property control layer depending on an input image.
Also, a display device according to an embodiment of the present invention includes: a reflection property control layer which is disposed in the front face of a display screen, wherein different reflection properties are disposed uniformly over the entire screen; and a control unit configured to select the reflection properties of the reflection property control layer by having the pixels of the display screen emit light.
According to the above configurations, the reflection properties of the reflection property control layer disposed in the front face of the display screen are changed according to a gloss region of an input image, whereby the gloss appearance and three-dimensional appearance of an object can be improved.
Specific embodiments according to the present invention will be described below in detail with reference to the drawings. A viewer evaluates the gloss appearance of an object displayed on a display depending on specular reflected light intensity (gloss) and image clarity. Weighting between gloss and image clarity is 3:4, so image clarity (sharpness) is somewhat superior, but specular reflected light intensity (gloss) is also an important factor (see FUJI FILM RESEARCH & DEVELOPMENT (No. 51-2006) Development of high image quality ink-jet super-gloss receiver paper Kassai “Photo-finishing Pro”). With the present embodiment, external reflection (generally equal to specular reflected light intensity) in a display is controlled, thereby controlling the gloss appearance of an object.
First Embodiment
Overall Configuration
The gloss processing unit 1 determines whether an image region included in an input image signal is a gloss region or non-gloss region for each object, and outputs a gloss control signal to the transparent thin plate 2 wherein a gloss region is subjected to specular reflection (glare), and a non-gloss region is subjected to diffused reflection (antiglare). Also, the gloss processing unit 1 optimizes the luminance information or the like of an input image signal so as to clarify gloss regions and non-gloss regions.
The transparent thin plate 2 is a transparent reflection property control layer disposed in the front face of the display panel 3, and is sectioned in a fine size, whereby specular reflection and diffused reflection can be switched in increments of sections. Subsequently, external reflection to the front face of the transparent thin plate 2 is controlled in increments of sections, thereby controlling gloss appearance for each object of a display image.
The display panel 3 is equivalent to a liquid crystal panel or plasma panel of a display device for displaying an image.
With this display device, the transparent thin plate 2 makes up an active actuator wherein surface reflection properties are changed for each minute region, the gloss processing unit 1 supplies a gloss control signal to the transparent thin plate 2, and supplies a picture signal of which the luminance is corrected in sync with the gloss control signal to the display panel 3, so gloss appearance and three-dimensional appearance can be improved according to cooperation of both.
An arrangement will be described later wherein the transparent thin plate 2 is changed to glare/antiglare dynamically for each region, but for example, there may be employed a method for controlling the transparent thin plate 2 by employing change in a physical state according to voltage (electric field), or a method for controlling the transparent thin plate 2 by employing change in a thermal/chemical state according to electric current.
Thus, the front face of the display screen is changed to glare/antiglare dynamically for each region, the substantial dynamic range of an image is enlarged according to external light, and accordingly, the gloss appearance and three-dimensional appearance of the image (object) can be improved.
Gloss Processing Unit
Next, description will be made regarding the gloss processing unit 1 for extracting a gloss region from an input image. With extraction of a gloss object according to the present embodiment, not only a gloss region but also the entire region of a material projecting a gloss appearance within an object are extracted. For example, a technique disclosed in Japanese Unexamined Patent Application Publication No. 2002-51226 may be employed as technique for extracting a gloss object.
Also, the gloss control unit 4 includes a splitter 41 for splitting the color space of an input image signal, an edge extracting unit 42 for extracting the edge of an object, an external light reflection region detection unit 43 for detecting an external reflection region, an expanded processing unit 44 for expanding the external reflection region to the edge, and a gloss determining unit 45 for determining the gloss of the expanded gloss area.
For example, with regard to the original image shown in (A) in
The respective components of the gloss processing unit 1 will be described below with reference to
The edge detecting unit 421 subjects the V plane to filtering according to a Sobel operator, thereby detecting an edge. Specifically, a Sobel filter shown in the following expression is employed for the first derivation of an input image, thereby estimating an edge.
The binarization unit 422 binarizes the edge image of the V plane by comparing this and a predetermined threshold, and supplies the binarized image of the V plane obtained as a result thereof to the boundary image storage unit 423.
Also, not only the V plane in a biased to lightness but also a great number of components are employed, whereby the edge extraction function can be improved.
That is to say, edge images obtained from the H, S, and V planes are supplied from edge detecting units 421H, 421S, and 421V to the binarization units 422H, 422S, and 422V, respectively. The binarization units 422H, 422S, and 422V binarize the edge images of the H, S, and V planes by comparing these and predetermined thresholds, and supplies binarized images of the H, S, and V planes obtained as a result thereof to an OR processing unit 424.
The OR processing unit 434 calculates logical addition (OR) regarding each pixel of the binarized image of the H, S, and V planes, and generates a boundary image. The generated boundary is stored in the boundary image storage unit 423.
Also, an edge may be extracted from color space such as L*a*b* (Luminance alpha beta), RGB, YUV (Y denotes luminance, U(Cb) denotes a blue difference signal, and V(Cr) denotes a red difference signal.), or the like.
As can be understood from these drawings, a great number of components are employed, whereby the edge extraction function can be improved. For example, with the image of the V plane alone shown in (C) in
The changed portion detecting unit 431 detects a rapid changed portion of a signal from the V plane, i.e., a portion of which the lightness is higher than the surroundings thereof. The high-lightness region detecting unit 432 detects a high-lightness region based on an external threshold (lightness). The external light reflection region crop-out unit 433 crops out a high-lightness region as an external light reflection region. That is to say, the external light reflection region detection unit 43 detects a rapid changed portion of a signal from the V plane, a threshold is externally applied thereto, thereby cropping out a high-lightness region of which the lightness is equal to or higher than the threshold as an external light reflection region to output this to the expanded processing unit 44 of the subsequent stage.
The expanded processing unit 44 performs processing wherein the external light reflection region detected at the external light reflection region detection unit 43 is taken as the center, and the external light reflection region is expanded toward the vicinity thereof up to the edge. Regarding whether or not expansion is performed is determined depending on regarding whether or not a pixel of interest in the vicinity of the external light reflection region has similarity with the external light reflection region. The external light reflection region is thus expanded, whereby the entire region of a material projecting a gloss appearance within an object can be extracted.
The gloss determining unit 45 determines whether or not a gloss object candidate which is the expanded external light reflection region where the external light reflection region having a luminance value equal to or greater than a certain threshold is expended is an object having gloss or an object of which the surface is subjected to irregular reflection.
Irregular reflection of light on an object surface has wavelength dependence, so an ultraviolet ray having a long wavelength is most subjected to irregular reflection, and is also most suitable for reading irregularities on the surface. The wavelength dependence of irregular reflection affects visible light regions of blue, green and red, so in a case wherein the fineness of irregularities on the flat portion of the R plane completely differs from that of the B plane, there is an extremely high possibility that the cause thereof is that the material of the flat portion is a material causing irregular reflection.
Therefore, only the R and B planes are employed to narrow down the irregularities of the flat portion to two-dimensional features, and are subjected to class classification at the class classification units 452R and 452B, and in a case wherein the degree of irregularity greatly differs between the R and B planes, i.e., in a case wherein the irregularities of the B plane are apparently finer than those of the R plane, there is irregular reflection, so the gloss determination unit 453 determines that there is no gloss, but in a case wherein the degree of irregularity somewhat differs between the R and B planes, determines that there is not irregular reference but gloss. The gloss region thus determined is output to the transparent thin plate 2 as a gloss control signal.
(A) in
(A) in
Thus, the reflection intensities of the R and B planes are classified according to the degree of irregularity thereof, gloss or non-gloss is determined, whereby texture regarding whether the material to be employed is a material causing specular reflection or irregular reflection can be controlled. Particularly, blue has a shorter wavelength as compared to red and green, so irregular reflection is readily represented, whereby determination can be made regarding whether the material to be employed is a material causing specular reflection or irregular reflection by detecting the degree of irregularity of the contour map of the B plane.
Now, description will be back to
A gloss region is extracted as described above, whereby a gloss region suitable for expressing the texture of a material can be extracted. Also, surface reflection (glare/antiglare) can be controlled for each object of an input image, and the gloss appearance of an object can be improved greatly by utilizing external light. Also, the gloss appearance of an object can be expressed finely, and accordingly, the three-dimensional appearance of a gloss substance can be reproduced in a more realistic manner.
Note that such image processing can also be applied to a printer apparatus. For example, determination is made for each object whether the surface reflection is specular reflection or diffused reflection, ink of which the particle size differs is employed according to the determination result, whereby the texture of a material can be expressed on paper. Also, such image processing can also be realized by causing a CPU (Central Processing Unit) to execute a computer program. In this case, the computer program may also be provided by being recorded in a recording medium, and alternatively, may also be provided by being transmitted through the Internet or other transmission media.
Transparent Thin Plate
Next, a specific example of the transparent thin plate 2 will be described. The transparent thin plate 2, which is disposed in the front face of the display device, has a function wherein the transparent thin plate 2 is sectioned in a fine size in a two-dimensional array, whereby switching can be made whether the surface reflection is specular reflection (glare) or diffused reflection (antiglare), in increments of sections, and controls the gloss appearance of a display image of the display device by controlling external light reflection on an audiovisual environment. Specifically, the surface roughness of the transparent thin plate 2 is changed for a predetermined region. Now, the transparent thin plate 2 is preferably a transmissive type having an aperture ratio of 75% or more. Also, a type capable of active control specular reflection and irregular reflection for each pixel (minute region) is desirable, and further a type capable of high-speed response of 8 ms or less is desirable.
Also, arithmetic mean roughness Ra of irregularities of the antiglare surface of the transparent thin plate 2 is preferably 0.05 to 0.25 μm. According to the arithmetic mean roughness Ra within this range, intended irregular reflection can be obtained. Note that the arithmetic mean roughness Ra of the irregularities represents, as shown in the following expression, a value obtained by extracting a portion from a roughness curve in the direction of the mean line thereof by reference length l, totaling the absolute value of deviation from the mean line of this extracted portion to a measured curve, and averaging this.
Also, the mean interval Sm of irregularities of the antiglare surface of the transparent thin plate 2 is preferably around 30 through 60 μm. According to the mean interval Sm within this range, deterioration in resolution, and harshening of the surface, due to interference with a pixel can be prevented. Note that the mean interval of irregularities represents, as shown in the following expression, a mean value in millimeter (mm) obtained by extracting a portion from a roughness curve in the direction of the mean line thereof by reference length t, obtaining the sum of the length of the mean lint corresponding to one peak and one trough adjacent thereto, and averaging this.
With the transparent thin plate 2, a transparent substrate 211, lower transparent electrode 212, transparent spacer 213, upper transparent electrode 214, and transparent film 215 are layered in this order.
The transparent substrate 211 is formed of a glass substrate and so forth. The lower transparent electrode 212 is made up of ITO (indium tin oxide) and so forth, divided into multiples corresponding to pixels, which can be independently controlled. The transparent spacer 213 is made up of a silicon oxide film, formed in a grating form corresponding to pixels, and an air layer is formed within each grating. The transparent film 215 is a membrane having flexibility such as SiN, SiC, diamond, transparent polymer, or the like, and switches a state including an air layer, and a state including no air layer depending on a state wherein voltage is ON, and a state wherein voltage is OFF, whereby surface roughness can be changed.
With regard to a fabrication method of the transparent thin plate 2, first, for example, In—Zn—O metal serving as the lower transparent electrode 212 is subjected to vacuum deposition on the transparent substrate 211. For example, a silicon oxide film which is an insulating film is formed thereupon by sputtering. Further, the transparent spacer 213 for forming an air layer is formed thereupon by spin coating, and pattering is performed in accordance with a pixel size. The upper electrode 214 is film-formed, for example, on a polyethylene naphthalate (PEN) film which is a polymer membrane by vacuum deposition, and is finally bonded with the lower substrate.
Thus, applying the MEMS technology to the transparent thin plates 2 enables high-speed response (1 μs) of several thousands times of liquid crystal to be realized, and the surface reflection (glare/antiglare) can be controlled for each object of an input image.
With this transparent thin plate 2, a transparent electroconductive plate 221, and raised hairs 222 are layered in this order. The transparent electroconductive plate 221 is made up of ITO and so forth, divided into multiples corresponding to pixels, which can be independently controlled. The raised hairs 222 are made up of transparent polymer such as polyester or the like, and are charged with positive charge or negative charge.
Thus, the raised hairs charged positively or negatively are operated by electric field, whereby the surface reflection can be controlled. Note that the raised hairs may be operated by inverting the polarity of a power supply.
Transparent polymer which changes to fluid (gel) or solid (sol) reversibly may be employed as the transparent substance 231. Examples of such polymer include a hydrophobized polyethylene glycol. The heating element 232 is divided into multiples corresponding to pixels, which can be controlled independently. For example, an element of which the resistance value of ITO has been adjusted may be employed as the heating element 232. The cooling element 233 is made up of, for example, a peltiert element or the like, divided into multiples corresponding to pixels, which can be controlled independently. Note that in a case wherein it is difficult to dispose a cooling element for each minute region, an arrangement may be made wherein cooling elements are disposed on the entire face of the screen, and then these are cooled during a non-display period (vertical blanking period).
Thus, a substance of which the state is changed by change in temperature is employed, whereby the surface reflection can be controlled. Such a device may be employed for a large electronic advertisement plate which does not depend on response speed, or the like.
Also, with the above-mentioned first through third specific examples, the surface state of the transparent thin plate 2 is changed physically, so it is desirable to provide a protection net 21 on the transparent thin plate 2 such as shown in
As described above, the transparent thin plate 2 controls glare/antiglare regarding an extremely fine region on the screen of the display device, whereby expression of presence/absence of a gloss appearance can be improved as compared to the related art. Also, the transparent thin plate 2 has to be added to the surface of the display device, and also may be added thereto lately, and accordingly, a range of application products is very wide regardless of the types of display device.
Second Embodiment
The display device according to the second embodiment includes a gloss processing unit 1 for detecting an image gloss region from an input image signal, outputting a gloss control signal to the transparent thin plate 2 based on the detection result, and outputting an output image signal, a transparent thin plate 6 of which the reflection properties are fixed for each predetermined region, which is provided in the front face of the display panel 3, a region selection unit 7 for selecting a predetermined region where the reflection properties are fixed based on the gloss control signal, and a display panel 3 for having the pixel of the selected reflection properties emit light, and displaying an image.
The gloss processing unit 1 is the same as that in the first embodiment, which determines whether or not the region to be processed is a gloss region or non-gloss region for each object from an input image signal, and outputs a gloss control signal which subjects a gloss region to specular reflection (glare), and subjects a non-gloss region to diffused reflection (antiglare) to the region selection unit 7. Also, the gloss processing unit 1 optimizes the luminance information and so forth of an input image signal such that gloss regions and non-gloss regions are clarified.
The region selection unit 7 outputs an output image signal to the display panel 3 such that at least ones of glare regions and antiglare regions on the transparent thin plate 6 based on the gloss control signal. Also, the region selection unit 7 stores the correlation between the position of glare/antiglare in increments of minute sections of the transparent thin plate 6, and the pixel position (x, y) of the display panel 3 in ROM or the like.
With the transparent thin plate 6, as shown in
Thus, the glare (or antiglare) thin plate is subjected to minute drilling processing, whereby a glare/antiglare region can be readily classified. Note that in the case of this drilling method, there is a possibility that the cross-section of the hole a refracts light, so it is desirable to shield light at the cross-section of the hole a.
Also, arithmetic mean roughness Ra of irregularities of the antiglare surface of the transparent thin plate 6 is preferably 0.05 through 0.25 μm. According to the arithmetic mean roughness Ra within this range, intended irregular reflection can be obtained. Note that the arithmetic mean roughness Ra of the irregularities represents, as shown in the above-mentioned Expression (1), a value obtained by extracting a portion from a roughness curve in the direction of the mean line thereof by reference length l, totaling the absolute value of deviation from the mean line of this extracted portion to a measured curve, and averaging this.
Also, the mean interval Sm of irregularities of the antiglare surface of the transparent thin plate 6 is preferably around 30 through 60 μm. According to the mean interval Sm within this range, deterioration in resolution, and harshening of the surface, due to interference with a pixel can be prevented. Note that the mean interval of irregularities represents, as shown in the above-mentioned Expression (2), a mean value in millimeter (mm) obtained by extracting a portion from a roughness curve in the direction of the mean line thereof by reference length l, obtaining the sum of the length of the mean lint corresponding to one peak and one trough adjacent thereto, and averaging this.
Also, it is desirable that the glare/antiglare regions of the transparent thin plate 6 are disposed uniformly over the entire screen. For example, it is desirable that the respective regions are disposed in a checkered pattern, polka-dot pattern, grating pattern, striped pattern, or the like. In particular, glare/antiglare regions are disposed in a checkered pattern for each of the pixels, whereby resolution can be improved.
Such transparent thin plate 6 may be fabricated, for example, by masking a glare surface in a checkered pattern, applying an antiglare material thereto, and removing the masking. Examples of the antiglare material include LUCIFRAL (registered trademark) NAG (manufactured by NIPPON PAINT Co. Ltd.).
For example, as shown in
Thus, only a pixel of the lower portion of a glare region is selected and had to emit light regarding a gloss object, and only a pixel of the lower portion of an antiglare region is selected and had to emit light regarding a non-gloss object, whereby the gloss appearance and three-dimensional appearance of an image (object) can be enhanced.
It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and alterations may occur depending on design requirements and other factors insofar as they are within the scope of the appended claims or the equivalents thereof.
Number | Date | Country | Kind |
---|---|---|---|
2007-334844 | Dec 2007 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
5019536 | Taylor, Jr. | May 1991 | A |
6563553 | Faris | May 2003 | B1 |
6950615 | Jung et al. | Sep 2005 | B2 |
20020094220 | Bartscher et al. | Jul 2002 | A1 |
20020180953 | De Jung et al. | Dec 2002 | A1 |
20050099666 | Kodama et al. | May 2005 | A1 |
20050157224 | Kanbe et al. | Jul 2005 | A1 |
20060181588 | Kusunoki | Aug 2006 | A1 |
20060203154 | Uchida | Sep 2006 | A1 |
20090133922 | Okazaki et al. | May 2009 | A1 |
Number | Date | Country |
---|---|---|
2002-51226 | Feb 2002 | JP |
2004-279669 | Oct 2004 | JP |
WO 2005034067 | Apr 2005 | WO |
Number | Date | Country | |
---|---|---|---|
20090179910 A1 | Jul 2009 | US |