The present invention relates generally to batteries and, more particularly, to batteries having nanostructured surfaces.
Many beneficial devices or structures in myriad applications rely on batteries as a power source. A typical liquid-cell battery, such as battery 101 in
As the above process continues, the active materials of the positive and negative electrodes 104 and 105, respectively, eventually become depleted and the reactions slow down until the battery is no longer capable of supplying electrons. At this point the battery is discharged. It is well known that, even when a liquid-cell battery is not inserted into an electrical circuit, there is often a low-level reaction with the electrodes 104 and 105 that can eventually deplete the material of the electrodes. Thus, a battery can become depleted over a period of time even when it is not in active use in an electrical circuit. This period of time will vary depending on the electrolyte fluid used and the materials of the electrodes.
More recently, batteries having at least one nanostructured surface have been proposed wherein nanostructures are used to separate the electrolyte from the electrode until such a time that the battery is to be used. An example of the use of electrowetting principles applied to batteries is described in copending U.S. patent application Ser. No. 1 01716084 filed Nov. 11, 2003 and entitled “Electrowetting Battery Having Nanostructured Surface,” which is hereby incorporated by reference herein in its entirety. As disclosed in the '084 application, when it is desired that the battery generate a charge, the electrolyte is caused to penetrate the nanostructured surface and to come into contact with the electrode of the battery, thus resulting in the above-discussed flow of electrons around a circuit. Such a penetration of nanostructures is achieved, for example, by applying a voltage to the nanostructures such that the contact angle of the electrolyte relative to the nanostructured surface is decreased. When the contact angle is decreased, the electrolyte penetrates the nanostructures and is brought into contact with the electrode.
The present inventors have realized that it would be advantageous to be able to selectively control the voltage and/or current of a battery and to variably control the operational life of such a battery.
Therefore, the present inventors have invented a battery having an electrode with at least one nanostructured surface. The nanostructured surface is divided into cells and is disposed in a way such that an electrolyte fluid of the battery is prevented from contacting the portion of electrode associated with each cell. When a voltage is applied to the nanostructured surface associated with a particular cell, the electrolyte fluid is caused to penetrate the nanostructured surface of that cell and to contact the electrode, thus activating the portion of the battery associated with that cell. Thus, when the activated battery is inserted into an electrical circuit, electrons will flow along the circuit.
The voltage generated by the battery is controlled by selectively activating only a portion of the cells. Multiple cells can be active simultaneously to produce the desired voltage and/or current. The more cells at are active, the higher the voltage and/or current and the lower the overall life of the battery. The life of the battery can be extended by activating fewer cells simultaneously.
As typically defined a “nanostructure” is a predefined structure having at least one dimension of less than one micrometer and a “microstructure” is a predefined str˜cture having at least one dimension of less than one millimeter. However, although the disclosed embodiments refer to nanostructures and nanostructured surfaces, it is intended by the present inventors, and will be clear to those skilled in the art, that microstructures may be substituted in many cases. Accordingly, the present inventors hereby define nanostructures to include both structures that have at least one dimension of less than one micrometer as well as those structures having at least one dimension less than one millimeter. The term “feature pattern” refers to either a pattern of microstructures or a pattern of nanostructures. Further, the terms “liquid,” “droplet,” and “liquid droplet” are used herein interchangeably. Each of those terms refers to a liquid or a portion of liquid, whether in droplet form or not.
The present inventors have recognized that it is desirable to be able to control the penetration of a given liquid into a given nanostructured or microstructured surface and, thus, control the contact of the liquid with the underlying substrate supporting the nanostructures or microstructures.
The illustrative battery 900 of
In one potential embodiment of a selective and variable current application, battery 900 of
The foregoing embodiment describes a battery where the current generated by the battery is capable of being varied. One skilled in the art will recognize that this is possible when the electrolyte is disposed in an open chamber between the electrodes in a way such that the electrolyte is common among all the cells. The plurality of cells formed on the electrode(s) are electrically connected in parallel and, therefore, the current of the battery can be varied by activating one or more cells. The more cells that are activated, the greater the current generated by the battery.
The present inventors have realized that, in addition to variably controlling the current produced by the battery, it may be desirable to also variably control the voltage of a battery. One skilled in the art will recognize that varying the number of cells connected in series could achieve such a variable control of voltage. Thus, in order to achieve such a series connection, the present inventors have invented a battery wherein, instead of disposing the electrolyte in an open chamber, the area below each cell between electrodes 901 and 907 is separated from the other cells. Thus, multiple individually electrically isolated compartments are associated with each of the cells on electrode 901 so that, when the number of activated cells is varied, the voltage of the battery is correspondingly varied. Accordingly, in this case, activating more cells leads to a higher voltage produced by the battery. One skilled in the art will fully appreciate that, by implementing the appropriate standard electronic circuitry in, for example, the battery control circuit, the battery can be dynamically switched between a series and a parallel connection, thus selectively permitting variable control of the circuit or the voltage of the battery. In many applications, it may be desirable to activate only a portion of cells, such as cells 903, in normal operations and then, in cases where emergency power is require or when any other unusual demand is realized, to active additional cells as needed. In normal operations, the current/voltage supplied to the circuit can be maintained by progressively activating new cells when old cells become depleted. For example, cells 902 represent those cells that have already been depleted and, as discussed, cells 903 represent those cells that are currently active. Cells 904 represent those cells that have not been activated. In this illustrative example, one possible progression of cells is that, as the individual cells in column 914 are depleted, cells in column 915 are progressively activated in direction 908, followed by activation of the cells in column 916, followed by column 917 and then column 918 until the final cell 905 is activated. One skilled in the art will recognize that many paths or selection methods for selecting cells to be activated may be used to achieve a desired voltage/current level and/or battery life, including random activation. The principles of the present invention are contemplated to include any and all such methods. One skilled in the art will also recognize that, in addition to dividing electrode 901 into cells, electrode 907 could likewise be divided into cells. If those divided cells of electrode 907 are nanostructured as discussed above, one or more cells in electrode 907 may be selectively activated at the same time a corresponding cell on electrode 901 is activated, thus providing a discrete flow of ions between one particular cell on electrode 901 and one particular cell on electrode 907. Alternatively, the electrolyte may be permitted to contact the entire area of one of electrodes 901 and 907, but may only be permitted to contact selected activated cells on the other electrode. One skilled in the art will recognize, in light of the teachings herein, that many such arrangements are possible and that such arrangements are fully contemplated by the principles of the present invention.
The foregoing merely illustrates the principles of the invention. It will thus be appreciated that those skilled in the art will be able to devise various arrangements which, although not explicitly described or shown herein, embody the principles of the invention and are within its spirit and scope. For example, one skilled in the art, in light of the descriptions of the various embodiments herein, will recognize that the principles of the present invention may be utilized in widely disparate fields and applications. For example, while the embodiment disclosed herein is a battery having nanostructured surfaces, one skilled in the art will appreciate that such nanostructured surfaces may be used for other uses, such as in use as a thermostat. In such a case, the characteristics of the pattern of nanostructures and the liquid in contact with the nanostructures can be chosen in a way such that, upon a temperature increase of known amount, the liquid will penetrate the surface, thus achieving a desired result. One skilled in the art will be able to devise many similar uses of the underlying principles associated with the present invention, all of which are intended to be encompassed herein. All examples and conditional language recited herein are intended expressly to be only for pedagogical purposes to aid the reader in understanding the principles of the invention and are to be construed as being without limitation to such specifically recited examples and conditions. Moreover, all statements herein reciting aspects and embodiments of the invention, as well as specific examples thereof, are intended to encompass functional equivalents thereof.
This application is a Divisional application which claims the benefit of U.S. application Ser. No. 10/803,565, to Marc Scott Hodes, et al. filed on Mar. 18, 2004, entitled “RESERVE CELL ARRAY NANOSTRUCTURED BATTERY,” currently allowed, which is a continuation-in-part of U.S. application Ser. No. 10/716,084 filed on Nov. 18, 2003 now U.S. Pat. No. 7,227,235 to Timofei Nikita Kroupenkine, et al., entitled “ELECTROWETTING BATTERY HAVING A NANOSTRUCTURED ELECTRODE SURFACE,” commonly assigned with the present invention which issued as U.S. Pat. No. 7,227,235 B2 on Jun. 5, 2007. This application claims subject matter that is described in co-pending United States patent application entitled “Nanostructured Battery Having End-Of-Life Cells”, Ser. No. 10/803,576, filed on Mar. 18, 2004 and Issued as U.S. Pat. No. 7,618,746 on Nov. 17, 2009 and co-pending U.S. patent application Ser. No. 10/803,641 filed on Mar. 18, 2004, entitled “Reversibly-Activated Nanostructured Battery,” published as United States Patent Publication 2005/0208370 dated Sep. 22, 2005.
Number | Name | Date | Kind |
---|---|---|---|
6185961 | Tonucci et al. | Feb 2001 | B1 |
7005593 | Gasparyan et al. | Feb 2006 | B2 |
7048889 | Arney et al. | May 2006 | B2 |
7156032 | Kornblit et al. | Jan 2007 | B2 |
7227235 | Kroupenkine et al. | Jun 2007 | B2 |
7618746 | Kroupenkine et al. | Nov 2009 | B2 |
7678495 | Kolodner et al. | Mar 2010 | B2 |
20040191127 | Kornblit et al. | Sep 2004 | A1 |
20050039661 | Kornblit et al. | Feb 2005 | A1 |
20050069458 | Hodes et al. | Mar 2005 | A1 |
20050106459 | Kroupenkine et al. | May 2005 | A1 |
20050203613 | Arney et al. | Sep 2005 | A1 |
20050208370 | Hodes et al. | Sep 2005 | A1 |
20050211505 | Kroupenkine et al. | Sep 2005 | A1 |
20050217984 | Gasparyan et al. | Oct 2005 | A1 |
20060040375 | Arney et al. | Feb 2006 | A1 |
Number | Date | Country | |
---|---|---|---|
20100247982 A1 | Sep 2010 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 10803565 | Mar 2004 | US |
Child | 12813792 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 10716084 | Nov 2003 | US |
Child | 10803565 | US |