Claims
- 1. A method of molding a sabot segment using a sabot segment molding apparatus, comprising the steps of:
- arranging a plurality of plies of a carbon fiber material to form wedge-shaped members having a narrow edge and an opposed wide edge;
- stacking said wedge-shaped members contiguously in an elongated arcuate channel with a central axis and a predetermined diameter, with said wider edges adjacent the inner circumference of the channel, so that said narrow edges of the contiguous wedges are disposed to form an arcuate portion at a distance apart from said central axis;
- positioning a hinged wing assembly with a hinge pin coaxially aligned with said central axis, and a pair of planar substantially rectangular wing members abutting the uppermost stacked wedge-shaped members;
- supporting said hinge pin at opposing ends of the arcuate channel;
- applying a predetermined urging force on said wing members, urging said wing members to pivot about said hinge pin toward one another and compressing the stack of wedge-shaped members with a predetermined pressure;
- applying a predetermined temperature to the compressed stack of wedge-shaped members; and
- maintaining said pressure and temperature for a predetermined period of time.
- 2. The method of claim 1, wherein the step of arranging includes arranging plies of a carbon fiber epoxy impregnated tape material.
- 3. The method of claim 1, wherein the step of arranging includes arranging plies of a thermoplastic resin material.
- 4. The method of claim 1, wherein the step of stacking includes positioning wedge-shaped members to have an inner arcuate surface having a radius at least equal to the predetermined radius of the hinge pin.
- 5. The method of claim 1, wherein the step of compressing forms a sabot segment having an arcuate section of up to 120.degree..
- 6. The method of claim 1, wherein the step of heating includes heating the stack with a predetermined temperature of at least 350.degree. F.
- 7. The method of claim 1, wherein the step of compressing includes compressing the stack with a predetermined pressure of at least 600 psi.
- 8. The method of claim 1, wherein the step of compressing includes compressing the stack for a predetermined period of time of at least two hours.
Parent Case Info
This is a division of application Ser. No. 07/336,445, filed Mar. 10, 1989.
US Referenced Citations (7)
Divisions (1)
|
Number |
Date |
Country |
Parent |
336445 |
Mar 1989 |
|