In vibrating screens used for fractionation of for example crushed stones and gravel into fractions of stones with different sizes, screening media are used having screening holes for allowing stones smaller than the screening holes to pass through the holes.
The screening media is normally provided in the form of panels or mats. This description is concentrated to panels to simplify the description, but it is to be understood to apply also for screening mats.
In WO 2012/029072 a screen panel is shown having ribs with protrusions. The apertures forming the screening areas are essentially square in form. The protrusions go almost all the way between the ribs. The distance formed between the protrusions and the adjacent rib is to make the seal panels more resilient, whereby the ribs may yield a bit. This should in theory reduce the risk of clogging.
For screening media in the mining industry one always seeks high capacity, long life and minimal maintenance requirement. The normally used square or slotted apertures of screening media leads to risk for blinding and not enough open area.
The capacity of a vibrating screen is influenced by a number of factors. One way to increase the capacity is to increase the ratio of open space in the screening media. Regarding the screening media it is also important that it lets the stones through which it is designed to be let through and that it does not clog easily. The screening media should also be durable.
The screening media of the present invention forms a screening area that could be said being formed of a number of rectangular areas placed mutually perpendicular to each other and coinciding at the ends.
Screening media with the apertures of the present invention have more open area, compared to normal screening media of the prior art, which means higher capacity and reduced risk of blinding. By letting the apertures of the screening media have slots directed both along and traverse to the direction of movement for the material to be screened, particles of different shapes are more readily screened.
In some embodiments of the present invention raised bars are used, to facilitate for fine material to be fed down into the screen openings. The raised bars are directed in the direction of movement for the material to be screened.
With the unique aperture design of the present invention there will be an increased open area, compared to what is normal in screening media today. The risk for migrating and blinding is reduced and all material is guided towards the apertures.
Further objects and advantages of the present invention will be obvious to a person skilled in the art, when reading the detailed description below of embodiments of the present invention.
The invention will be described further below by way of examples and with reference to the enclosed drawings. In the drawings:
In
In the first embodiment shown in
The pins 3 will have some flexibility in that they have a free outer end. This will reduce the risk of plugging, as the pins 3 may yield to some extent.
In the area between two ribs 2, each pin 3 from one of the ribs 2 is placed in the middle between two pins 3 from the other rib 2. In said area between two ribs 2 pins 3 from alternating ribs 2 are placed with even spacing. The pins 3 do not project all the way to the adjacent rib 2, but stops at a distance from the adjacent rib 2. However, the pins 3 of adjacent ribs 2 project a distance past each other.
In the second embodiment shown in
The third embodiment of a screening panel 7, shown in
In
By means of the design of the ribs 2, 5, 10 and the pins 3, 6, apertures are formed between the ribs 2, 5, 10 and the pins 3, 6 in each screening panel 1, 4, 7, 9. As stated above the apertures have the same shape irrespectively of which screening panel 1, 4, 7, 9 it is referred to. For the discussion of the shape of the apertures we now refer to
The size of the rectangular screening areas 12, 13, 14 is amended depending on the size of the fraction to be screened. Independently of the size of the rectangular screening areas 12, 13, 14 they are always of the same mutual size. Thus, the above stated distances a, b, c may vary but are always mutually the same. In practice it is the size of the pins 3 that is amended if the size of the fraction to be screened is to be altered. The width of the ribs 2 do not need to be amended even if the size of the pins 3 is altered, but in some cases also the width of the ribs 2 is altered.
As indicated in
The screening panels 1, 4, 7, 9 of the present invention are preferably produced by injection moulding.
By means of the pattern of the open areas of the screening media of the present invention the open area has both longitudinal and transversal directions, as seen in the direction of movement for the material to be screened. Often screening media have only square or rectangular screening areas. Transversal screening areas counteract blinding or plugging and longitudinal screening areas are beneficial for screening flaking material.
A person skilled in the art realizes that features of the different embodiments may be combined in other ways than in the embodiments shown in the FIGS.
| Number | Date | Country | Kind |
|---|---|---|---|
| 13165267.9 | Apr 2013 | EP | regional |
| Filing Document | Filing Date | Country | Kind |
|---|---|---|---|
| PCT/EP2014/054558 | 3/10/2014 | WO | 00 |