The disclosure relates to seal assemblies for battery cells and more specifically to seal assemblies that are configured to reduce leakage of an electrolyte from inside the battery cell.
Consumer electronic devices have certain power requirements. Generally, consumer electronic devices receive power from a single battery cell (contained within the device itself), or from a portable battery pack that may include one or more battery cells. Alternatively, one or more single use or rechargeable consumer battery cells may be used and replaced in a device as needed. Replaceable and rechargeable consumer battery cells generate electricity through reduction of a cathode and oxidation of an anode. An alkaline electrolyte is often used to facilitate movement of ions from the anode to the cathode.
Alkaline battery cells (including rechargeable alkaline battery cells) are known to be susceptible to the leakage of alkaline electrolytes from a battery seal. See, for example, Hull et al., “Why Alkaline Cells Leak,” J. Electrochem. Soc., 124(3):332-339, (1977) and Davis et al, “Aspects of Alkaline Cell Leakage,” J. Electrochem. Soc., 125(12):1918-123 (1978). Evidence of alkaline electrolyte leakage can be visibly detected because a white powder is deposited around a battery cell seal. Alkaline electrolyte leakage may be attributable to alkaline electrolyte creepage along negatively polarized electrodes. Alkaline electrolyte leakage may be exacerbated by physical factors such as scratches or other physical deformations/imperfections in a seal of a battery cell. Although the powdered alkaline electrolyte is generally safe for human contact, contact should be minimized because respiratory, eye, and skin irritation may occur. Moreover, loss of electrolyte can lead to decline of battery cell performance.
According to one embodiment, a seal assembly for a battery cell includes a grommet having an opening with an inner surface, the opening having a proximal end and a distal end. A nail has a nail head and a stem extending from the nail head. The stem includes a first portion with a larger first stem diameter and a second portion with a smaller second stem diameter and the stem extends through the opening in the grommet. The stem and the grommet form a first interference fit at the distal end of the opening. A trap clearance is formed between the distal end of the opening and the proximal end of the opening. The trap clearance being radially and longitudinally located between the second portion of the nail and the inner surface, and the trap clearance defining a trap for a sealant. A sealant is disposed on the stem and is located at least partially in the trap.
According to another embodiment, a battery cell includes a housing. The housing has a first cover at a first housing end and a second cover at a second housing end. An anode and a cathode are disposed within the housing. A seal assembly is located proximate to the first cover. The seal assembly includes a grommet having an opening and an inner surface. A nail has a nail head and a stem extending from the nail head. The stem includes a first portion with a larger first diameter and a second portion with a smaller second diameter and the stem extends through the opening in the grommet. The stem and the grommet form a first interference fit at a distal end of the opening. A trap clearance is formed between the distal end of the opening and the nail head. The trap clearance being radially and longitudinally located between the second portion of the nail and the inner surface, and the trap clearance defining a trap for a sealant. A sealant is disposed on the stem and the sealant is located at least partially in the trap.
According to another embodiment, a seal assembly for a battery cell includes a grommet having an opening including a distal end, a proximal end, and a bore having an inner surface between the distal end and the proximal end. An internal annular ring is positioned proximate the distal end, the internal annular ring having a ring diameter. The bore has a bore diameter. A headspace is located at the proximal end and the headspace has a headspace diameter. The ring diameter is smaller than the bore diameter and the headspace diameter, and the bore diameter is smaller than the headspace diameter. A nail has a nail head and a stem extending from the nail head. The stem includes a first portion with a first stem diameter and a second portion with a second stem diameter. The first stem diameter is larger than the second stem diameter. The stem extends through the opening in the grommet. The stem and the grommet form a first interference fit between the second portion of the stem and the ring diameter. The stem and the grommet form a trap clearance between the second portion of the stem and the bore diameter, the trap clearance defining a trap for a sealant. A sealant is disposed on the stem and at least partially located in the trap.
According to another embodiment, a battery cell includes a housing having a first cover at a first housing end and a second cover at a second housing end, and an anode and a cathode disposed within the housing. A seal assembly is located proximate the first cover. The seal assembly includes a grommet having an opening including a distal end, a proximal end, and a bore having an inner surface between the distal end and the proximal end. An internal annular ring is positioned proximate the distal end, the internal annular ring having a ring diameter. The bore has a bore diameter. A headspace is located at the proximal end and the headspace has a headspace diameter. The ring diameter is smaller than the bore diameter and the headspace diameter, and the bore diameter is smaller than the headspace diameter. A nail has a nail head and a stem extending from the nail head. The stem includes a first portion with a first stem diameter and a second portion with a second stem diameter. The first stem diameter is larger than the second stem diameter. The stem extends through the opening in the grommet. The stem and the grommet form a first interference fit between the second portion of the stem and the ring diameter. The stem and the grommet form a trap clearance between the second portion of the stem and the bore diameter, the trap clearance defining a trap for a sealant. A sealant is disposed on the stem and at least partially located in the trap.
The foregoing embodiments of a seal assembly or a battery cell may further include any one or more of the following optional features, structures, and/or forms.
In some optional forms, the second portion is distal to the first portion relative to the head.
In other optional forms, the first portion and the second portion are joined by a chamfer.
In other optional forms, the inner surface of the opening includes the bore having the bore diameter, the bore diameter being larger than the second stem diameter and smaller than the first stem diameter, at least some of the second stem diameter is located within the bore diameter, such that no interference fit is present between the second stem diameter and the bore diameter when the nail is assembled in the grommet.
In other optional forms, the trap is formed, in an assembled battery cell, between the bore and the second portion of the stem, the bore diameter being larger than the second stem diameter.
In other optional forms, the bore diameter is between 0.03 mm and 0.05 mm larger than the second stem diameter.
In other optional forms, the grommet opening includes an internal annular ring.
In other optional forms, the internal annular ring has a ring diameter that is smaller than the bore, and the internal annular ring forms the first interference fit with the second portion of the stem.
In other optional forms, the trap is located above the internal annular ring, along a length of the stem.
In other optional forms, the trap has a volume of between 0.35 mm3 and 1.5 mm3.
In other optional forms, the stem includes an annular recess.
In other optional forms, the trap clearance is formed by the annular recess.
In other optional forms, the stem includes a plurality of annular recesses.
In other optional forms, the grommet comprises a polymer, such as polypropylene or nylon.
In other optional forms, the nail comprises a metal, such as brass or bronze.
In other optional forms, the sealant comprises a polymer such as polyamide or a petroleum-based material, such as an asphalt based material.
In other optional forms, a head clearance is formed between the nail head and the grommet and sealant is also disposed in the head clearance.
While the specification concludes with claims particularly pointing out and distinctly claiming the subject matter, which is regarded as forming the present invention, the invention will be better understood from the following description taken in conjunction with the accompanying drawings.
Electrochemical cells, or batteries, may be primary or secondary. Primary batteries are meant to be discharged, e.g., to exhaustion, only once and then discarded. Primary batteries (or disposable batteries) are described, for example, in David Linden, Handbook of Batteries (4th ed. 2011), which is hereby incorporated by reference. Secondary batteries (or rechargeable batteries) are intended to be recharged and used over and over again. Secondary batteries may be discharged and recharged many times, e.g., more than fifty times, a hundred times, or more. Secondary batteries are described, for example, in David Linden, Handbook of Batteries (4th ed. 2011), which again is hereby incorporated by reference. Accordingly, batteries may include various electrochemical couples and electrolyte combinations. The description and examples provided herein apply to both primary and secondary batteries of aqueous, nonaqueous, ionic liquid, and solid state systems. While consumer single use primary alkaline battery cells are the main focus of the accompanying description, the following description may be equally applied to any battery cell, including but not limited to rechargeable alkaline battery cells, such as rechargeable alkaline manganese (RAM) battery cells, as well as any other type of battery cell that includes an electrolyte solution.
The seal assemblies according to the disclosure may be included in any type of electrochemical battery cell. For example, the seal assemblies according to the disclosure may be employed in consumer alkaline electrochemical cells of any size and/or shape (including for example, batteries having cylindrical, rectangular, or square shapes or cross-sectional shapes) including, but not limited to, AAAA cells, AAA cells, AA cells, B cells, C cells, D cells, 9 V cells, and the like.
Turning now to
To couple an anode current collector 30 and the first cover 12, which provides a negative terminal in the assembled battery cell 10, in this example, the seal 28 includes a first opening 32 having a wider portion 34 defining a head clearance or space 36, where an end or head 38 of the anode current collector 30 (sometimes referred to as a “nail”) is positioned and electrically coupled to the first cover 12. This space 36 may have a chamfered or angled configuration to accommodate the head 38. In this example, a body 40 of the anode current collector 30 extends through the first opening 32 and into the anode 18. An electrolyte solution is contained within the housing 16.
The seal 28 of
As discussed above, battery cells are susceptible to electrolyte leakage, for example, due to electrolyte creepage, along the body of the anode current collector 30, such that electrolyte can escape from the first opening 32 in the seal 28. Prior attempts to prevent leakage have been made by providing a sealant around the nail in the opening 32, with the result that the sealant is “squeegeed” or wiped up during assembly (by the interference fit with the seal 28) and thus ultimately disposed in the space 36 around the head 38. However, the sealant may not be uniformly provided around the head and thus may not provide a uniform seal and/or may be displaced from the space 36 by electrolyte creepage. Moreover, this existing arrangement is more susceptible to developing leaks due to imperfections that may be introduced during manufacturing.
For example, the distal end of the anode current collector 30 (e.g., the bottom end in
The disclosed seal 28 may be formed by a variety of manufacturing techniques, molding processes. In particular, injection molding and blow molding, which use pins to create voids, are particularly advantageous. Imperfections can be formed during injection or blow molding of the seal 28 that are similar to those described above with respect to the anode current collector because the pins used in injection and blow molding may also have imperfections such as burrs and flashes. Typically, the seal 28 is formed by injection molding and a pin is used during the molding process to create a void forming the first opening 32 of the seal 28. The distal end of such injection molding pins are ground and thus frequently have burrs or flashes as a result, which can also cause the formation of scratches during manufacture. For example, as the pin is withdrawn from the first opening 32 after the molding process is complete, any imperfections in the pin may scratch internal surfaces of the seal 28 as the pin is withdrawn, similar to the anode current collector 32 scratching the internal surfaces as described above with respect to nail insertion into the seal assembly.
When sealant is applied to the anode current collector 30 of
Turning now to
The cathode 120 may comprise any known electrochemically active cathode material including but not limited to manganese oxide, manganese dioxide, electrolytic manganese dioxide (EMD), chemical manganese dioxide (CMD), high power electrolytic manganese dioxide (HP EMD), lambda manganese dioxide, gamma manganese dioxide, beta manganese dioxide, and mixtures thereof. Other electrochemically active cathode materials include, but are not limited to, silver oxide; nickel oxide; nickel oxyhydroxide; copper oxide; copper salts, such as copper iodate; bismuth oxide; high-valence nickel compound; high-valence iron compound; and mixtures thereof. The nickel oxide can include nickel hydroxide, nickel oxyhydroxide, cobalt oxyhydroxide-coated nickel oxyhydroxide, partially delithiated layered nickel oxide, and mixtures thereof. Partially delithiated layered nickel oxides suitable for use as the electrochemically active cathode material are described in U.S. Pat. No. 10,910,647B2, which is hereby incorporated herein by reference. The nickel hydroxide or oxyhydroxide can include beta-nickel oxyhydroxide, gamma-nickel oxyhydroxide, and/or intergrowths of beta-nickel oxyhydroxide and/or gamma-nickel oxyhydroxide. The cobalt oxyhydroxide-coated nickel oxyhydroxide can include cobalt oxyhydroxide-coated beta-nickel oxyhydroxide, cobalt oxyhydroxide-coated gamma-nickel oxyhydroxide, and/or cobalt oxyhydroxide-coated intergrowths of beta-nickel oxyhydroxide and gamma-nickel oxyhydroxide. The high-valence nickel compound may, for example, include tetravalent nickel. The high-valence iron compound may, for example, include hexavalent iron. The electrochemically active cathode material may include a combination of one or more of the foregoing exemplary electrochemically active cathode materials.
Cathode 120 may include a conductive additive, such as carbon particles, and a binder. The carbon particles are included in the cathode 120 to facilitate electron flow through the cathode 120. The carbon particles may be graphite, such as expanded graphite and natural graphite; graphene, single-walled nanotubes, multi-walled nanotubes, carbon fibers; carbon nanofibers; and mixtures thereof. It is preferred that the amount of carbon particles in the cathode is relatively low, e.g., less than about 10%, less than about 7.0%, less than about 4.25%, less than about 3.75%, less than about 3.5%, or even less than about 3.25%, for example from about 2.0% to about 3.25%. The lower carbon level enables inclusion of a higher loading of electrochemically active cathode material within the cathode 120 without increasing the volume of the cathode 120 or reducing the void volume of the finished battery 10 (which must be maintained at or above a certain level to prevent internal pressure from rising too high as gas is generated within the cell). Suitable expanded graphite may be, for example, BNB-90 graphite available from TIMCAL Carbon & Graphite (Bodio, Switzerland).
Examples of binders that may be used in the cathode 120 include polyethylene, polyacrylic acid, or a fluorocarbon resin, such as PVDF or PTFE. An example of a polyethylene binder is sold under the trade name COATHYLENE HA-1681 (available from Hoechst or DuPont). Examples of other cathode additives are described in, for example, U.S. Pat. Nos. 5,698,315, 5,919,598, 5,997,775 and 7,351,499.
Anode 118 comprises at least one electrochemically active anode material, and typically further comprises a gelling agent, and minor amounts of additives, such as gassing inhibitor. The electrochemically active anode material may include zinc; cadmium; iron; metal hydrides, including but not limited to AB5, AB2, and A2B7 metal hydride alloys; and mixtures thereof. Anode 118 typically is provided as a gelled zinc anode.
To close an end 124 after the components of the battery cell 110 are disposed within the housing 116, the first cover 112 is received within a groove 126 of a grommet or seal 128, disposed proximate to a distal end 115 of the housing 116, and a sidewall 129 of the housing 116 is crimped over a peripheral edge of the seal 128. In some examples, the seal 128 is spaced from the cathode 120 to enable the cathode 120 to expand. In some examples, the seal 128 is similarly spaced from the anode 118 to enable the anode 118 to expand. The cover 112 is disposed above the seal 128 to create a space or void X. The void X allows space for gas to vent when pressure builds up inside the housing 116.
To couple an anode current collector 130 and the first cover 112, which provides a negative terminal in the assembled battery cell 110, in this example, the seal 128 includes a first opening 132 having a wider portion 134 defining a head clearance or space 136, where an end or head 138 of the anode current collector 130 (sometimes referred to as a “nail”) is positioned and electrically coupled to the first cover 112. This space 136 may have a chamfered or angled configuration to accommodate the head 138. In this example, a body 140 of the anode current collector 130 extends through the first opening 132 and into the anode 118. An electrolyte solution is contained within the housing 116.
The seal 128 includes a cylindrical portion or boss 133 that surrounds the first opening 132. The boss 133 extends both upward and downward from a planar seal portion or shelf 135 that extends laterally outward from the boss 133. The boss 133 is referred to herein as a long boss. As used herein, “long bosses” are bosses that have cylindrical segments that are provided both above and below the shelf 135.
Turning now to
When assembled, the stem 140 extends through the opening 132 in the seal 128 from the proximal end 151 through the distal end 154 and the nail head 138 seats in the headspace 136 near the proximal end 151. The headspace 136 may be chamfered. As assembled, the stem 140 and the seal 128 form a first interference fit 152 adjacent the distal end 154 of the opening 132 and a second interference fit 157 (
As best illustrated in
The bore 150 includes the bore diameter C. The bore diameter C is larger than the second stem diameter B and smaller than the first stem diameter D.
The trap 164 is formed between the bore 150 and the second portion 174 of the stem 140. The trap 164 is bounded radially on an inner side by the outer surface of the second portion 174 and is bounded radially on an outer side by the inner surface of the bore 150. The trap 164 in the illustrated example forms an annular-shaped space.
In the illustrated example, the seal opening 132 includes an internal annular ring 180, having a ring diameter A, which protrudes from the inner surface of the bore 150 proximate to the distal end 154 of the seal 128. The ring diameter A is smaller than the bore diameter C. As described above, the stem 140 and the seal 128 form a first interference fit 152 adjacent the distal end 154 of the opening 132 between the second stem diameter B and the ring diameter A. In other words, the internal annular ring 180 forms the first interference fit 152 with the second portion 174 of the stem 140 when the stem 140 is fully inserted into the seal 128, as illustrated in
The trap 164 is located longitudinally along the stem 140 above the internal annular ring 180. In the example illustrated in
In the illustrated example, the bore diameter C is between 0.03 mm and 0.05 mm larger than the second stem diameter B. In other examples, the following dimension ratios advantageously can produce an efficient sealant trap clearance as described herein:
Length E of the first portion of the stem 172: diameter D of the first portion 172 of the stem 140 being between about 1.1 and about 3.0, for example between about 1.1 and about 1.2;
Diameter D of the first portion 172 of the stem 140: diameter B of the second portion 174 of the stem 140 being between about 1.1 and about 3.0, for example between about 1.1 and about 2.0;
Internal ring diameter A of the Internal annular ring 180: diameter B of the second portion 174 of the stem 140 being less than 1.0; and
Length F of the bore 150: length E of the first portion 172 of the stem 140 being between about 1.1 and about 2.0, for example between about 1.1 and about 1.5.
In the illustrated example, the trap 164 has a volume of between about 0.35 mm3 and about 1.5 mm3. In other examples, the trap 164 may be configured to have other volumes, for example, depending upon the viscosity of the sealant 170 and/or the size of the battery cell.
The seal 128 according to the disclosure advantageously reduces or eliminates leakage of electrolyte from inside the battery cell by trapping and locating sealant in a clearance between two interferences, thereby positioning the sealant in a location where it can more effectively provide a barrier to electrolyte creepage because the sealing effect of the sealant is further reinforced by an interference fit between the nail 130 and the seal 128 further along the nail 130 axis towards the proximal end 151 of the seal 128. Moreover, the seal 128 according to the disclosure further reduces electrolyte leakage by reducing or compensating for manufacturing defects. More specifically, as described above, the nail 130 may have imperfections, for example, at a distal end (which is located in the second portion 174 of the stem 140 having the second stem diameter B). During assembly, these imperfections are separated from the first inner surface portion 178 of the opening 132 because the second stem diameter B is smaller than the bore diameter C. As a result, no damage is caused to the first inner surface portion 178 of the opening 132 from the nail 130 during assembly. Any damage that could be caused to the seal 128 by the nail 130 during assembly would be confined to the annular ring 180, where an interference fit exists. However, sealant is purposefully and advantageously positioned above the annular ring 180 in the trap 164, as a result of the sealant being disposed on the second portion 174 of the stem 140 and by being wiped by the annular ring 180 during assembly, and thereby can prevent or reduce any electrolyte creepage (including along any damaged areas of the annular ring 180 as a result of nail 130 insertion), particularly because of the reinforcement of the seal provided by the purposefully positioned sealant 170 by the interference fit between the first portion 172 of the stem 140 and the bore 150.
Furthermore, as best illustrated in
In alternate embodiments, a plurality of sealant traps 164a, 164b may be formed, for example as illustrated in
The plurality of sealant traps 164a, 164b form a staged seal that provides enhanced sealing and increased prevention of electrolyte creepage. The nail 130 includes a first portion 172 with a first diameter H, a second portion 174 with a second diameter I, and a third portion 173 with a third diameter J. The first diameter H is larger than both the second diameter I and the third diameter J, and the second diameter I is larger than the third diameter J.
As illustrated, the first sealant trap 164a is formed longitudinally between a first chamfer 176a and the first annular ring 180a, and laterally between the second portion 174 of the nail 130 and a first inner surface portion 178a. The second sealant trap 164b is formed longitudinally between the second chamfer 176b and the second annular ring 180b, and laterally between the third portion 173 of the nail 130 and a second inner surface portion 178b.
In other embodiments, more than two sealant traps may be formed by adding additional annular rings 180 and staging portions of the nail 130 having different diameters.
Turning now to
The stem 240 includes a first portion 272 with a first stem diameter and a second portion 274 with a second stem diameter. The second stem diameter is smaller than the first stem diameter. The second portion 274 is distal to the first portion 272 relative to the nail head 238. The first portion 272 and the second portion 274 are joined by a chamfer 276, but a more “abrupt” stepped transition between the first portion 272 and the second portion 274 may also be used, provided that the second portion 274 has a smaller diameter than the first portion 272 as previously described.
The bore 250 diameter is larger than the second stem diameter and smaller than the first stem diameter.
The trap 264 is formed between the bore 250 and the second portion 274 of the stem 240. The trap 264 is bounded radially on an inner side by the outer surface of the second portion 274 of the stem 240 and is bounded radially on an outer side by an inner surface 278 of the bore 250. The trap 264 in the illustrated example is provided in part by an annular-shaped recess 290 formed in the nail 230. In the illustrated example, the bore diameter is between 0.03 mm and 0.05 mm larger than the second stem diameter.
The embodiment illustrated in
In alternate embodiments, the stem 240 may include a plurality of annular recesses 290.
Battery cells having the trapped sealant seal assemblies described above, with respect to
The leakage test conducted on the battery cells included flushing the space between the seal or grommet and the top cover (labeled as void X in
Two different boss lengths and two different sealants were included in the test cells. The two boss lengths were long and short bosses and the two different sealants were polyamide and asphalt. The AA COPPERTOP® control cells comprised short bosses with the selected sealant in a wiped configuration as described above where the sealant is placed on the nail and it is “wiped” up the nail as the nail is inserted into the seal such that the sealant is placed proximate to the nail head after nail insertion. The second control cell group included a long boss with the selected sealant in a wiped configuration, again with the sealant being placed proximate to the nail head after nail insertion. The trapped sealant cells according to the invention included a seal assembly having the sealant trap discussed above, with respect to
The results of the testing are summarized in Tables 1 and 2 below.
The tabular results above are illustrated in graphical form in
While some improvement over the control cells was expected with the trapped sealant configuration, the magnitude of improvement that was achieved was unexpected and surprising, particularly for the trapped polyamide long boss design.
A trapped short boss configuration was not tested because the short boss configuration does not provide adequate space to practically implement the trapped sealant. In other words, a short boss seal does not have enough space within the inner bore to incorporate a seal trap with enough volume to make the trapped sealant effective.
In any of the foregoing embodiments, the seal or grommet may comprise a polymer, particularly one or more thermoplastic polymers such as polypropylene or nylon. Nylon 66 and nylon 612 are two specific representative materials that may be used alone or in combination.
In any embodiment, the nail may comprise a conductive metal, for example, brass or bronze (including silicon bronze). Brass alloys having a copper content greater than about 50% by weight, for example, 60 wt. % or 70 wt. % and a zinc content greater than 20 wt. %, for example, 30 wt. % or 40 wt. % may be used.
The sealant may be any known sealant capable of adhering the grommet to the nail. Thus, in the illustrated embodiments, the sealant may comprise a polyamide sealant, a resin, a polyvinyl acetate sealant, a petroleum-based material such as an asphalt sealant, a polybutene sealant, a polyisobutylene sealant, a polyethylene wax sealant, an epoxy sealant, a silicone sealant, an acrylic sealant, a polysulfide sealant, a polyurethane sealant, and mixtures thereof. In the illustrated embodiments, the grommet comprises a polymer and the nail comprises a metal. In one refinement, a relatively hydrophilic sealant comprising a water-swellable polymer may be used to provide the sealant, for example, a water-swellable acrylate polymer including particles of superabsorbents such as SikaSwell® sealants (Sika AG, Switzerland). Solvents that may be advantageously employed to formulate the sealant for application to the nails include but are not limited to xylene, isopropanol, toluene, and mixtures thereof. In other embodiments, the formulated sealant may comprise a viscosity between about 165 cps and about 1600 cps, with a solids content between about 40% and about 80%. Moreover, in other embodiments, the sealant may advantageously comprise an anaerobic sealant because exposure of the sealant to oxygen is effectively eliminated when the seal assembly is fully assembled such that the sealant trap is formed between the interference fits above and below the trap. Because the sealant can be in the uncured state initially after the nail is inserted into the grommet, the sealant may have sufficient time in the liquid phase to fully fill the trap and to fill any defects, including the manufacturing defects mentioned above, present in the seal and even in the nail, before curing.
The disclosed seal assemblies advantageously trap sealant in the sealant trap, thereby minimizing exposure of the assembled battery cell to oxygen and preventing the electrolyte from migrating to the top of the nail and escaping from the seal assembly. Furthermore, the sealant is effectively disposed in the sealant trap, because of the interference fit between the nail stem and the seal at a distal end of the seal opening, and the relatively larger internal diameter of the first inner portion of the opening relative to the second more narrow inner portion of the opening (e.g., provided by the internal annular ring). The internal annular ring(s) wipes the remaining sealant from the stem as the stem is inserted into the seal and precisely positions the sealant in the sealant trap. Because the sealant is deposited on the nail stem in liquid form prior to seal assembly, the sealant flows uniformly into the sealant trap, due to the wiping of the internal annular ring, to provide a substantially uniform 360-degree seal between the nail and the grommet in a consistent, and controlled reproducible fashion. The sealant in the sealant trap combines with the interference fits above and below the sealant trap to effectively form a seal assembly having three distinct sealing surfaces that prevents or greatly reduces the amount of electrolyte leakage. When sealant is also disposed in the head clearance, four distinct sealing surfaces are formed (the fourth sealing surface being formed by the sealant in the head clearance). In embodiments having more than one sealant trap (e.g., the embodiment illustrated in
The dimensions and values disclosed herein are not to be understood as being strictly limited to the exact numerical values recited. Instead, unless otherwise specified, each such dimension is intended to mean both the recited value and a functionally equivalent range surrounding that value. For example, a dimension disclosed as “40 mm” is intended to mean “about 40 mm.” Moreover, any dimension disclosed in one embodiment is equally applicable in other embodiments. Where an “interference” fit is described above, alternative embodiments could have a very small clearance if a more viscous sealant is used. For example, as viscosity of the sealant increases, the ratio of the diameter A of the annular ring 180 to the diameter B of the second portion 174 of the nail 130 may exceed values greater than 1.0. In such examples, the diameter A being larger than diameter B may facilitate exhausting of gas in the opening 132 during assembly by allowing gas to escape through the very small gap between diameter A and diameter B as the nail 130 is inserted into the seal 128, while the viscous sealant then seals that gap when the sealant contacts the annular ring 180.
Every document cited herein, including any cross referenced or related patent or application and any patent application or patent to which this application claims priority or benefit thereof, is hereby incorporated herein by reference in its entirety unless expressly excluded or otherwise limited. The citation of any document is not an admission that it is prior art with respect to any invention disclosed or claimed herein or that it alone, or in any combination with any other reference or references, teaches, suggests or discloses any such invention. Further, to the extent that any meaning or definition of a term in this document conflicts with any meaning or definition of the same term in a document incorporated by reference, the meaning or definition assigned to that term in this document shall govern.
While particular embodiments of the present invention have been illustrated and described, it would be obvious to those skilled in the art that various other changes and modifications can be made without departing from the spirit and scope of the invention. It is therefore intended to cover in the appended claims all such changes and modifications that are within the scope of this invention.
Number | Date | Country | |
---|---|---|---|
63029273 | May 2020 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 17327091 | May 2021 | US |
Child | 18507821 | US |