Claims
- 1. A secured document comprising a composition capable of anti-Stokes fluorescence comprising(a) a gadolinium oxysulfide selected from the group consisting of (1) a composition of the formula (Gd(1-x-y)YbxTmy)2O2S; and (2) a composition of the formula (Gd(1-x-y)2O2S:YbxTmy, wherein x and y are numbers greater than 0, wherein the wavelength of the emitted electromagnetic radiation is shorter than the wavelength of the absorbed electromagnetic radiation, and wherein the concentrations of Yb and Tm are adjusted to achieve concentration quenching of anti-Stokes luminescence.
- 2. The secured document of claim 1, wherein the composition has the formula(Gd(1-x-y))2O2S:YbxTmy, wherein x is 0.05≦x≦0.80 and y is 0.0001≦y≦0.10.
- 3. The secured document of claim 2, wherein x is 0.20≦x≦0.60 and y is 0.0001≦y≦0.05, and the composition provides a read-out speed of between about 3 and about 6 m/s.
- 4. The secured document of claim 1, wherein said composition is incorporated into an authentication element comprising a pigment.
- 5. The secured document of claim 4, wherein the authentication element has a particle size less than 5 μm.
- 6. The secured document of claim 5, wherein the authentication element has a particle size less than 3 μm.
- 7. The secured document of claim 6, wherein the authentication element has a particle size less than 2 μm.
- 8. The secured document of claim 4, wherein the authentication element is applied to the secured document by a method selected from the group consisting of offset printing, half-tone intaglio printing, die stamping gravure printing, and digital printing.
- 9. The secured document of claim 4, wherein the authentication element further comprises a printing ink or pigment and a degree of filling is within the range of 1 to 30 percent by weight.
- 10. The secured document of claim 9, wherein the degree of filling is in the range of 1 to 20 percent by weight.
- 11. The secured document of claim 9, wherein the degree of filling is in the range of 5 to 10 percent by weight.
- 12. The secured document of claim 4, wherein the authentication element is applied to the document by a method selected from the group consisting of brushing, coating, and surface-coating.
- 13. The secured document of claim 4, wherein the authentication element further comprises an adhesive element.
- 14. The secured document of claim 1, further comprising a matrix composition comprising yttrium, lanthanum, and thulium.
- 15. The secured document of claim 1, further comprising a matrix composition comprising yttrium, lanthanum, or thulium.
Priority Claims (1)
Number |
Date |
Country |
Kind |
101 13 266 |
Mar 2001 |
DE |
|
CROSS-REFERENCE TO RELATED APPLICATIONS
Reference is made to German patent application numbers 101 13 267.0 and 101 13 268.9, which were filed on Mar. 16, 2001. Reference is also made to U.S. application Ser. Nos. 10/101,524 and 10/099,472 (Attorney Docket Nos. 4077/0K319 and 4077/0K315), filed Mar. 18, 2002 and Mar. 15, 2002 respectively. These applications are incorporated herein by reference.
US Referenced Citations (9)
Number |
Name |
Date |
Kind |
5560867 |
Grabmaier et al. |
Oct 1996 |
A |
5609793 |
Yokota et al. |
Mar 1997 |
A |
5844361 |
Petersen et al. |
Dec 1998 |
A |
5944927 |
Seifert |
Aug 1999 |
A |
6137216 |
Yang |
Oct 2000 |
A |
6139065 |
Washburn et al. |
Oct 2000 |
A |
6210777 |
Vermeulen et al. |
Apr 2001 |
B1 |
6255948 |
Wolpert et al. |
Jul 2001 |
B1 |
6506476 |
Kaule et al. |
Jan 2003 |
B1 |
Foreign Referenced Citations (1)
Number |
Date |
Country |
WO 9839392 |
Nov 1998 |
DE |