This application is a national entry of PCT/GB2010/051238, Filed on Jul. 28, 2010, which claims priority of Great Britain Application No. 0913297.8, filed on Jul. 31, 2009. The entirety of all of the aforementioned applications is incorporated herein be reference.
The present invention relates to a security document and a method of production thereof and particularly, but not exclusively, to a security document comprising a bank note and a method of production thereof.
Polymer films are increasingly being used as substrates in fields where security, authentication, identification and anti-counterfeiting are important. Polymer-based products in such areas include for example bank notes, important documents (e.g. ID materials such as for example passports and land title, share and educational certificates), films for packaging high-value goods for anti-counterfeiting purposes, and security cards.
Polymer-based secure materials have advantages in terms of security, functionality, durability, cost-effectiveness, cleanliness, processability and environmental considerations. Perhaps the most notable amongst these is the security advantage. Paper-based bank notes, for example, can be relatively easy to copy, and there is lower occurrence of counterfeits in countries with polymer-based bank notes compared to paper-based bank notes. Polymer-based bank notes are also longer-lasting and less-easily torn.
Security materials based on polymer films are amenable to the incorporation of a variety of visible and hidden security features. Since the introduction of the first polymer bank notes approximately 25 years ago, security features have included optically variable devices (OVD), opacification features, printed security features, security threads, embossings, transparent windows and diffraction gratings. Aside from complicated security features there is also the more immediate advantage that the high temperatures used in copying machines will often cause melting or distortion of polymer base-material if counterfeiters attempt simply to copy secure materials (e.g. bank notes) using such machines.
The basic polymer substrate for such bank notes is processed using some, or all, of the following steps to arrive at the finished product:
1. Opacifying—two layers of ink (usually white) are applied to each side of the note, except for a region that is deliberately left clear, i.e. as a transparent window;
2. Sheeting—the substrate is cut into sheets suitable for the printing press;
3. Printing—one or more of traditional offset, intaglio and letterpress printing processes may be used; and
4. Overcoating—notes are coated with a protective varnish.
In-film features such as embossings, etchings, etc. are often incorporated into transparent and/or partially transparent windows in otherwise substantially opaque security documents.
As noted above, an intaglio printing process is a known method of providing printed features on such security documents. A window has become an important feature of security document substrates and is often enhanced by embossing numbers, text or images directly into the bare window. Where a security document comprises an opacified region and a window having such embossings, the embossings can be formed as part of the intaglio process. The heat and pressure of the intaglio process is such that it allows for embossing simultaneously with intaglio printing.
Current processes suffer limitations in that the embossing is often the final process and therefore cannot be integrated with opacification and/or offset printing. Further, in current processes, the embossings are effectively a free fringe benefit of the intaglio process, but security document printers charge the substrate suppliers for this feature as a separate security document feature.
Whilst the above described security documents and methods of production thereof offer features of interest, it is desirable to provide a security document and method of production thereof which offers improved properties, and thus the present invention seeks to provide for a security document and method of production thereof having advantages over known such security documents and methods of production thereof.
The present invention is described further hereinafter, by way of example only, with reference to the accompanying drawings in which:
a illustrates a schematic side elevation of a security document marked with a security feature and having opacifying layers applied thereto in a first embodiment;
b illustrates a schematic perspective view of the security document of
a illustrates a schematic side elevation of a security document marked with a security feature and having opacifying layers applied thereto in an eighth embodiment;
c illustrates a plan view of the security document of
a illustrates a schematic side elevation of a security document marked with a security feature and having opacifying layers applied thereto in a ninth embodiment;
b illustrates a plan view of the security document of
c illustrates a plan view of the security document of
a illustrates a schematic side elevation of a security document marked with a security feature and having opacifying layers applied thereto in a tenth embodiment;
b illustrates a plan view of the security document of
c illustrates a plan view of the security document of
a illustrates a schematic side elevation of a security document marked with a security feature and having opacifying layers applied thereto in an eleventh embodiment;
b illustrates a plan view of the security document of
c illustrates a plan view of the security document of
a illustrates a schematic side elevation of a security document marked with a security feature and having opacifying layers applied thereto in a twelfth embodiment;
b illustrates a plan view of the security document of
c illustrates a plan view of the security document of
d illustrates a bottom view of the security document of
e illustrates a bottom view of the security document of
According to an aspect of the present invention, there is provided a method of producing a security document, comprising: forming a polymer substrate having first and second surfaces; forming a security feature on a region of at least one of said first and second surfaces of said polymer substrate; forming an opacifying layer on at least a portion of at least one of said first and second surfaces of said polymer substrate; printing a design on said opacifying layer; wherein said security feature forming step occurs at least prior to said printing step, wherein said security feature forming step occurs at least prior to said opacifying layer forming step, and wherein said security feature forming step comprises embossing of said security feature in said region of at least one of said first and second surfaces of said polymer substrate and/or etching of said security feature in said region of at least one of said first and second surfaces of said polymer substrate.
It will be understood from the above discussion of conventional techniques that embossing/etching is currently carried out at least after opacification. By reversing this process, i.e. embossing/etching the films during an earlier stage of the manufacturing process (at least prior to the printing step and the step of forming the opacifying layer), the present invention offers the advantage that it is possible to generate markings/features that are integrated with subsequent printed layers. Thus, any marking/feature can be integrated across two or more layers, thereby increasing the difficulty involved in copying. For instance, in a security document formed by the method of the present invention and which incorporates a window in which is formed a security feature, and where the security feature also extends under an opacification layer, the common method of counterfeiting polymer security documents having a window, i.e. cutting a hole in the counterfeit security document and forming a window using an adhered film patch, would be prevented because the security feature extends under the opacification layer. it will be appreciated that the features of a security document formed according to a method of the present invention will have greater security and appeal as these features can be combined with print layers to produce marks that could only be made during the manufacturing process. Moreover, the opacifying layer will be of variable thickness over the embossing or etching, giving rise to differential visual effects in the opacifying layer.
Conveniently, said security feature forming step occurs during a slitting step of a film from a web, said film forming said polymer substrate.
If required, said region of at least one of said first and second surfaces of said polymer substrate may be in register with said at least a portion of at least one of said first and second surfaces of said polymer substrate having an opacifying layer formed thereon.
Further, said region of at least one of said first and second surfaces of said polymer substrate may be partially overlapped by said at least a portion of at least one of said first and second surfaces of said polymer substrate having an opacifying layer formed thereon.
In particular, said opacifying layer may be formed over the entire first and/or second surface of said polymer substrate.
Additionally, said region of at least one of said first and second surfaces of said polymer substrate may not be overlapped by said at least a portion of at least one of said first and second surfaces of said polymer substrate having an opacifying layer formed thereon.
The security feature forming step comprises embossing of said security feature in said region of at least one of said first and second surfaces of said polymer substrate and/or etching of said security feature in said region of at least one of said first and second surfaces of said polymer substrate. In particular, an ultrasonic embossing method and/or laser etching method are preferable. Ultrasonic embossing is advantageous in that it can be carried out at high speeds. Additionally, an embossing head in such a process is self cleaning, thereby preventing accumulation of debris. The embossing head is also small, energy efficient and can be integrated into a web based process.
The advantages of laser etching are that it can be carried out at high speed, the etching can be single or double sided, it results in little distortion of the film forming the substrate, no tooling is required for different jobs (since patterns can be set using software), and depths within a single pattern can be varied. Laser etching also offers an advantage over ultrasonic embossing in that it can allow for finer patterning than ultrasonic embossing. It does, however, suffer a disadvantage compared with ultrasonic embossing in that, whilst offering a high speed of marking, this is not as fast as is possible with ultrasonic embossing.
Further, the lasers envisaged to be used to carry out laser etching in the present invention (CO2 lasers) are cheap, efficient and reliable. Of course, other laser types may also be used.
As noted above, both ultrasonic embossing and laser etching have distinct advantages. Ultrasonic embossing equipment is cheap and simple; the process is not complex and is robust. However, tooling costs are potentially prohibitive between jobs and laser etching is capable of finer features without distorting the base film. Ultrasonic embossing does have the advantage that the speed of the process is not related to the complexity of the patterns being generated. Whilst laser etching scribes out patterns and does so at very high speeds (>15 m/s), a very complex pattern can be too time-consuming for a moving web as may be required to perform the method of the present invention. Another advantage of such techniques is the ability to control the quantum (e.g. height) of debossment, embossment or etching, as the case may be; greater embossment heights for example giving more evident visual effects in the opacifying layer. Aside from process advantages when compared with other techniques, the concept of putting in-film features into films at an earlier stage in the production process also has a number of design advantages. A number of design based features can be generated that take advantage of this and these are described further below in the specific description.
In the context of the present invention, the term opacifying layer may include at least one of: actual opacifying layers, white or otherwise; and/or offset, screen printed, colored gravure and/or foil patches.
Preferably, said polymer substrate is transparent. Further, said polymer substrate may be formed from a polymer film which is, preferably, a biaxially oriented propylene polymer (BOPP) film.
If required, the security feature may be at least one of: machine readable; and human readable.
According to another aspect of the present invention, there is proved a security document, comprising: a polymer substrate having first and second surfaces; a security feature formed in a region of at least one of said first and second surfaces of said polymer substrate; an opacifying layer formed on at least a portion of at least one of said first and second surfaces of said polymer substrate; a printed design formed on at least a portion of said opacifying layer; wherein said security feature is formed at least prior to said printed design being formed, wherein said security feature is formed at least prior to said opacifying layer being formed, and wherein said security feature is formed by embossing of said security feature in said region of at least one of said first and second surfaces of said polymer substrate and/or etching of said security feature in said region of at least one of said first and second surfaces of said polymer substrate.
In the following description, a number of design based features that are generated as a result of adding in-film features at an earlier stage in the production process are described (i.e. where the in-film features are formed prior to an intaglio printing step). In each case, the marking method to form the in-film security feature (e.g. laser etching and/or ultrasonic embossing) can be performed on one or both sides of the film. Further, whilst variations in opacification layers are only illustrated in one dimension in the figures, they can just as easily be in two dimensions.
The term opacifying layer can apply to an actual white opacifying layer and/or to offset, screen printed, colored gravure or even foil patches. Also, when referring to markings formed in the substrate to form a security feature, these markings may be formed by laser etching and/or ultrasonic embossing, or any other suitable marking method.
In the embodiments described hereinafter, a substrate forming part of a described security document is preferably a biaxially oriented propylene polymer film.
a and 1b illustrate a security document 10 which comprises a substrate 12, having formed on a region of a first surface 14 thereof a plurality of markings 16 arranged to form a security feature of the security document 10. A portion of the first surface 14 also h as an opacifying layer 18 formed thereon. The opacifying layer 18 is formed with a gap 20 therein, and said gap 20 is located above the plurality of markings 16. The substrate 12 has, on a portion of a second surface 22 thereof, an opacifying layer 24 formed thereon, with a gap 26 being formed in said opacifying layer 24. The gap 26 is located under the plurality of markings 16.
The arrangement of the gaps 20, 26 formed in the respective opacifying layers 18, 24 effectively forms a window in the security document. As will be appreciated, this window is aligned with the plurality of markings 16 (see
In
The opacifying layer 24 is formed over the entire second surface 22 of the substrate 12, while the first surface 14 of the substrate 12 is uncoated. The plurality of markings 16 forming the security feature can be thought of as being in a “half-window”. Such an arrangement provides for a form of integrating the plurality of markings 16 with an opacifying layer (i.e. underlying opacifying layer 24).
In this embodiment, the visibility of the plurality of markings 16 will vary according to a viewing angle, because the gloss of the untreated first surface 14 will differ from that of the first surface in the region of the plurality of markings 16. Also, the appearance of the first surface in the region of the plurality of markings 16 will differ depending on if viewed in transmission or reflection, and on the depth and density of the plurality of markings 16.
The opacifying layer 18 is formed over the entire first surface 14 of the substrate 12, while the second surface of the substrate 22 is uncoated. The plurality of markings 16 forming the security feature can be thought of as being in a “reverse half-window”. Such an arrangement provides for a simple form of integrating the plurality of markings 16 with an opacifying layer (i.e. overlying opacifying layer 18). In this embodiment, the printing of an opacifying layer 18 into the plurality of markings 16 produces a different result to that achieved in the previously described embodiments. The visual impact of the appearance of the security feature formed from the plurality of markings 16 is reduced compared with the previously described embodiments resulting in a more subtle marking system.
In
A first opacifying layer 18 is formed over the entire first surface 14 of the substrate 12, and a second opacifying layer 24 is fainted on the entire second surface 22 of the substrate 12. The plurality of markings 16 forming the security feature can be thought of as being hidden markings, i.e. the plurality of markings 16 are hidden by the two opacifying layers 18, 24 and are visible only in transmission.
A portion of the first surface 14 has a first opacifying layer 18 formed thereon. The first opacifying layer 18 is formed with two gaps 20a, 20b therein, thereby separating the first opacifying layer 18 into three regions 18a, 18b, 18c. The substrate 12 has, on a portion of a second surface 22 thereof, a second opacifying layer 24 formed thereon, with two gaps 26a, 26b being formed in said second opacifying layer 24. These gaps 26a, 26b separate the second opacifying layer 24 into three regions 24a, 24b, 24c.
A first region 18a of the first opacifying layer 18 is formed so as to be located substantially directly opposite a first region 24a of the second opacifying layer 24. Similarly, a second region 18b of the first opacifying layer 18 is formed so as to be located substantially directly opposite a second region 24b of the second opacifying layer 24, and a third region 18c of the first opacifying layer 18 is formed so as to be located substantially directly opposite a third region 24c of the second opacifying layer 24.
The plurality of markings 16 are formed in the region of substrate 12 which lies between the second region 18b of the first opacifying layer 18 and the second region 24b of the second opacifying layer 24.
Further, first gap 20a formed between first and second regions 18a, 18b of the first opacifying layer 18 is located substantially directly opposite first gap 26a foinied between first and second regions 24a, 24b of the second opacifying layer 24. Similarly second gap 20b formed between second and third regions 18b, 18c of the first opacifying layer 18 is located substantially directly opposite second gap 26b formed between second and third regions 24b, 24c of the second opacifying layer 24.
The arrangement of the pairs of gaps 20a, 26a and 20b, 26b of the respective first and second opacifying layers 18, 24 forms two windows in the security document. As will be appreciated, an “island of opacification” is formed by second region 18b of the first opacifying layer 18 and the second region 24b of the second opacifying layer 24, and it is with this “island of opacification” that the plurality of markings 16 are aligned, i.e. the plurality of markings 16 are hidden in this “island of opacification”.
In
A portion of the first surface 14 has a first opacifying layer 18 formed thereon. The first opacifying layer 18 is formed with a gap 20 therein, thereby separating the first opacifying layer 18 into two separate regions 18a, 18b. The gap 20 extends over a part of the first surface 14 of the substrate 12 including a region thereof where the plurality of markings 16 is located.
The substrate 12 has, on a portion of a second surface 22 thereof, a second opacifying layer 24 formed thereon, with two gaps 26a, 26b being formed in said second opacifying layer 24. These gaps 26a, 26b separate the second opacifying layer 24 into three separate regions 24a, 24b, 24c.
A first region 18a of the first opacifying layer 18 is formed so as to be located substantially directly opposite a first region 24a of the second opacifying layer 24. Similarly, a second region 18b of the first opacifying layer 18 is formed so as to be located substantially directly opposite a third region 24c of the second opacifying layer 24.
The plurality of markings 16 are formed in the region of substrate 12 which lies over a second region 24b of the second opacifying layer 24.
The arrangement of the pairs of gaps 26a, 26b formed in the second opacifying layer 24 in relation to the gap 20 formed in the first opacifying layer 18 and the plurality of markings 16 results in a “half-window island of opacification”, i.e. the plurality of markings 16 forming the security feature can be thought of as being located within this “half-window island of opacification”. Such an arrangement provides for a form of integrating the plurality of markings 16 with an opacifying layer (i.e. underlying opacifying layer 24).
In this embodiment, the visibility of the plurality of markings 16 will vary according to a viewing angle, because the gloss of the untreated first surface 14 (i.e. in the region formed by gap 20) will differ from that of the first surface in the region of the plurality of markings 16 and where the first opacifying layer 18 is formed. Also, the appearance of the first surface 14 in the region of the plurality of markings 16 will differ depending on if viewed in transmission or reflection, and on the depth and density of the plurality of markings 16.
In this figure, there is illustrated a security document 10 in which opacifying layers are applied to both surfaces of substrate 12 and which include window regions. The features illustrated in
A portion of the first surface 14 has a first opacifying layer 18 formed thereon. The first opacifying layer 18 is formed with two gaps 20a, 20b therein, thereby separating the first opacifying layer 18 into three regions 18a, 18b, 18c.
The substrate 12 has, on a portion of a second surface 22 thereof, a second opacifying layer 24 formed thereon, with a gap 26 being formed in said second opacifying layer 24. This gap 26 separates the second opacifying layer 24 into two regions 24a, 24b.
A first region 18a of the first opacifying layer 18 is formed so as to be located substantially directly opposite a first region 24a of the second opacifying layer 24. Similarly, a third region 18c of the first opacifying layer 18 is formed so as to be located substantially directly opposite a second region 24b of the second opacifying layer 24.
The plurality of markings 16 are formed in the region of substrate 12 which lies under a second region 18b of the first opacifying layer 18.
The arrangement of the pairs of gaps 20a, 20b formed in the first opacifying layer 18 in relation to the gap 26 formed in the second opacifying layer 24 and the plurality of markings 16 results in a “reverse half-window island of opacification”, i.e. the plurality of markings 16 forming the security feature can be thought of as being located within this “reverse half-window island of opacification”. Such an arrangement provides for a form of integrating the plurality of markings 16 with an opacifying layer (i.e. overlying opacifying layer 18). in this embodiment, the opacifying layer 18 is printed into the plurality of markings 16 and, as a result, the visual impact of the appearance of the security feature formed from the plurality of markings 16 is reduced compared with the some of the previously described embodiments, thereby resulting in a more subtle marking system.
a illustrates a security document 10 which comprises a substrate 12, having formed on a region of a first surface 14 thereof a plurality of markings 16 arranged to form a security feature of the security document 10. A portion of the first surface 14 also has a first opacifying layer 18 formed thereon. The opacifying layer 18 is foamed with a gap 20 therein, which effectively separates said first opacifying layer 18 into first and second regions 18a, 18b. The gap 20 is located above at least one of the plurality of markings 16. The substrate 12 has fon ied on an entire second surface 22 thereof a second opacifying layer 24.
The arrangement of the gap 20 formed in the first opacifying layer 18 in relation to the plurality of markings 16 such that at least one of the plurality of markings 16 is uncovered, whilst the remainder are overlapped by a portion of the first opacifying layer 18, results in a “half-window/half-hidden” arrangement. Thus, by covering a portion of the plurality of markings 16 with an opacifying layer, and the remaining at least one of the plurality of markings 16 being in a half-window, an effect is achieved whereby the visibility of a section of the plurality of markings 16 (i.e. the uncovered part) will vary with viewing angle due to gloss differences as described above in relation to the embodiments illustrated in
b and 8c illustrate the security document 10 of
The substrate 12 also has formed on a portion of the second surface 22 thereof a second opacifying layer 24. The second opacifying layer 24 is also formed with a gap 26 therein which effectively separates said second opacifying layer 24 into first and second regions 24a, 24b. The gap 26 is located under at least one of the plurality of markings 16, and substantially directly opposite gap 20.
A first region 18a of the first opacifying layer 18 is formed so as to be located substantially directly opposite a first region 24a of the second opacifying layer 24. Similarly, a second region 18b of the first opacifying layer 18 is formed so as to be located substantially directly opposite a second region 24b of the second opacifying layer 24.
The arrangement of the gaps 20, 26 formed in the respective first and second opacifying layers 18, 24 effectively forms a window in the security document. As will be appreciated, at least one of the plurality of markings 16 is aligned with the window, with the remainder of the plurality of markings 16 being concealed between second region 18b of the first opacifying layer 18 and second region 24b of the second opacifying layer 24. Thus, the security feature formed from said plurality of markings 16 effectively crosses from the window to a fully concealed region.
Therefore, by covering a portion of the plurality of markings 16 with an opacifying layer, and with the remaining at least one of the plurality of markings 16 being in a window, an effect is achieved whereby the visibility of a section of the plurality of markings 16 (i.e. the uncovered part) will vary with viewing angle due to gloss differences as described above in relation to the embodiments illustrated in
b and 9c illustrate the security document 10 of
However, the windows located in the first and second opacifying layers 18, 24 need not be symmetrical. As illustrated in
As will be appreciated, the level of visibility of the hidden portion of the security feature differs from that of the embodiment described in relation to
b and 10c illustrate the security document 10 of
The embodiment illustrated in
As will be appreciated, the level of visibility of the various regions of the plurality of markings (with the second and third regions forming partially hidden and hidden portions respectively of the security feature) will differ due to the fact that there are no opacifying layers above/below the first region 28, there is only an opacifying layer above the second region 30, and there are opacifying layers both above and below the third region 32.
b and 11c illustrate the security document 10 of
The embodiment illustrated in
Gap 20 is formed above both first and second regions 28, 30 of the plurality of markings 16 (with a third region 32 of the plurality of markings having second opacifying region 18b of first opacifying layer 18 located thereover). Gap 26 in the second opacifying layer 24 is located under the first region 28 of said plurality of markings 16. Second opacifying region 24b of second opacifying layer 24 extends under both the second and third regions 30, 32 of said plurality of markings 16.
As will be appreciated, the level of visibility of the various regions of the plurality of markings (with the second and third regions forming partially hidden and hidden portions respectively of the security feature) will differ due to the fact that there are no opacifying layers above/below the first region 28, there is only an opacifying layer below the second region 30, and there are opacifying layers both above and below the third region 32.
b and 12c illustrate top views of the security document 10 of
d and 12e illustrate bottom views of the security document 10 of
The proportions of the security feature that will be visible when the security document 10 is viewed in reflection will differ depending on the side of the note being observed (as will be appreciated from a comparison of
In
In this arrangement, the proportion of the security feature which is visible on one side of the security document differs from the proportion which is visible on the other side. A whole security feature could be viewed in part from an opposing side, e.g. as a way of revealing a hidden pattern in the security feature or combining the sub-pattern in the security feature with a print design that differs from the full security feature pattern.
In this arrangement, a security feature can be partly obscured on one side of the security document by way of an opacified “island”, i.e. second region 18b of the first opacifying layer 18 formed over the second region 30 of the plurality of markings 16. This could be used, as a way of differentiating both sides of the security document, or to integrate a variable appearance into a double-sided design (for example, as described in relation to
This arrangement modifies that illustrated in
As will be appreciated, etching/embossing and opacifying/printing the film results in a change in the transmissive properties of the film. By combining a watermark feature with the above described arrangements, the properties of the watermark feature could be enhanced. The security feature disclosed above may be not only readable by a human, but also may be readable by a machine. Such a feature would have applications in, for example, high speed central sorters which capture images in both reflection and transmission. A security feature as disclosed above would be readable by such high speed central sorters.
Number | Date | Country | Kind |
---|---|---|---|
0913297.8 | Jul 2009 | GB | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/GB2010/051238 | 7/28/2010 | WO | 00 | 4/4/2012 |