U.S. Pat. No. 6,656,391 discloses a process for preparing a castable powder of uranium dioxide (UO2) for the use in the manufacture of MOX fuels. The process includes spray drying of a flowable UO2 powder obtained by dry process conversion of uranium hexafluoride (UF6).
U.S. Pat. No. 6,352,677 discloses a process to produce commercial grade anhydrous hydrogen fluoride (AHF) and UO2 from the defluorination of UF6.
U.S. Pat. No. 5,346,684 discloses a method for recovering an anhydrous hydrogen fluoride from depleted UF6.
U.S. Pat. No. 4,830,841 discloses a UF6 to UO2 dry conversion reactor. Such a conversion is currently done in a single segment reactor with a gas-phase reaction section and a defluorination/agglomeration section which are fixed for running up to the enrichment level required in commercial light water reactors to produce a controlled nuclear reaction, i.e. up to a maximum enrichment of 5% U-235. The upper portion of the reactor separates the solid from the gas phase using sintered metal filters. The UO2F2 is defluorinated and the UO2 is agglomerated in the lower portion of the reactor using a fluidized bed. Both the fixed fluidized bed and gas-phase reaction sections geometries do not allow for timely or cost effective changes to capacity or U-235 enrichment, or ease of maintenance.
Current dry conversion reactors are usually made of material typically used in high temperature applications such as nickel-chromium based superalloys, e.g. Inconel®625, or of material resistant to corrosion such as nickel-copper based alloys, e.g. Monel®, but reactor modifications and maintenance cannot be done on the dry conversion reactors without welding on aged and thermal-cycled materials. Reactors cannot be quickly upgraded in the fluidized bed section except by welding new metal to modify the geometry. Welding on old materials such as Inconel® 625 or Monel® can cause problems with cracking at the welds between the aged and thermal-cycled reactor metal and the new sections. Unless the whole reactor is heat treated, cracking can occur at the weld seams since the aged thermal-cycled metal is dissimilar to the new metal which is more amorphous. Cracking will occur in a short time, typically soon after installation at the restart of operation. Any changes to a gas-phase reactor or a fluidized bed section of an existing reactor design, up to and including a full reactor replacement, are very expensive. Furthermore, although the entire reactor itself can undergo heat treatment, this is very costly and time consuming.
In addition, current reactors are limited to a fixed capacity and enrichment capability with respect to the gas-phase reaction section and the fluidized bed section. They cannot tolerate feeds greater than 5% enrichment without being replaced. These reactors cannot be upgraded unless the fluidized bed section or the gas-phase reaction section are cut out and new geometry sections are welded on, and these can fail from cracking at weld seams.
Current dry conversion reactors are welded in a single piece and therefore cannot be easily modified for changes related to capacity, enrichment, modification or other desired changes. An object of the invention is to provide a method and apparatus to modify a dry conversion reactor, such as the fluidized bed or other reactor sections in a simple and cost effective manner.
The present invention provides a dry conversion reactor for converting uranium hexafluoride to uranium dioxide, the dry conversion reactor comprising a gas-phase reaction segment; and a fluidized bed segment, wherein at least one of the gas-phase reaction segment and the fluidized bed segment is a replaceable segment.
The present invention also provides a method for operating a dry conversion reactor utilizing a uranium hexafluoride to uranium dioxide conversion process, the method comprising replacing at least one replaceable conversion reactor segment.
The present invention of installing pre-designed segments is applicable to a wide range of configurations including other reactor sections such as the fluidized bed plenum connecting to the powder outlet, or the off-gas plenum segment connecting to the off-gas outlet.
One embodiment of the present invention is shown with respect to the drawings in which:
a shows exemplary capacity modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a front view of a lower capacity reactor;
b shows exemplary capacity modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a side view of the lower capacity reactor shown in
c shows exemplary capacity modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a front view of a higher capacity reactor;
d shows exemplary capacity modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a side view of the higher capacity reactor shown in
a shows exemplary enrichment modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a front view of a reactor designed for a lower enrichment;
b shows exemplary enrichment modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a side view of the reactor designed for the lower enrichment shown in
c shows exemplary enrichment modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a front view of a reactor designed for a higher enrichment;
d shows exemplary enrichment modifications using replaceable segments on the dry conversion reactor for a rectangular cross section geometry in a side view of the reactor designed for the higher enrichment shown in
a shows exemplary enrichment modifications using replaceable segments on the dry conversion reactor for a cylindrical geometry with a front view of a reactor designed for a lower enrichment; and
b shows exemplary enrichment modifications using replaceable segments on the dry conversion reactor for a cylindrical geometry with a front view of a reactor designed for a higher enrichment.
U.S. Pat. No. 4,830,841, incorporated by reference herein, is improved to allow for higher capacity, higher % U-235 enrichments, ease of modification, ease of maintenance and other such improvements while maintaining a high total operating efficiency with minimal process downtime.
The present invention provides a method and apparatus for increasing the capacity of the reactor fluidized bed and modifying the uranium enrichment of existing conversion reactors to 5% U-235 or higher enrichments. This may be done using for instance a slab or cylindrical geometry for nuclear criticality safety. For the purposes of this invention the term slab is used to define a geometry that has a rectangular cross section, the maximum width of the rectangular cross section being determined by criticality safety considerations.
The present invention improves the reactor operations of U.S. Pat. No. 4,830,341 by detailing how the capacity and allowable feed of % U-235 enrichment to the gas-phase reaction section and fluidized bed section can be modified using replaceable segments. Such replaceable segments may include flanged replaceable segments in a variety of configurations.
a to 1d,
As shown in
As shown in
The maximum fluidized bed width, determined by criticality safety calculations for a specific maximum enrichment, would represent the inside width of the replaceable fluidized bed segment.
As shown in
The segments can be designed to quickly change a configuration to the needed capacity, residence time, maintenance or replacement work, criticality safety parameters, or other work requiring quick segment changes.
In addition to capacity and enrichment changes, larger fluidized beds are a process improvement that allow for better defluorination and additional densification, if needed. The replaceable reactor segments may be used to quickly increase or decrease capacity in either gas phase reaction or defluorination/agglomeration fluidized bed sections of the reactor. This provides a way of quickly providing the appropriate increase to fluidized bed volume, and lead to high quality powder for making active (ceramically) and sinterable powder using the methodology discussed in U.S. Pat. No. 4,830,841.
Reactor 1 is built to pressure vessel code. The use of segments improves the current conditions. Repairs to existing reactors, per U.S. Pat. No. 4,830,841, may be done by quickly replacing segments. When segmented sections of the reactor can be more easily modified or repaired, spare segments may be kept on hand to ensure higher production efficiency and minimal downtime. Segments are also much easier to heat treat to restore the metal to its original properties than an entire reactor.
Modification or repair of an old segment can be done, such as welding on a new pipe flange, and the segment can be heat treated in a cost effective way of restoring the metallic properties for reuse. This would include removing the old segment, replacing the defective part or implementing the new changes, for instance by welding, heat treating, reinstalling, etc. Alternatively a spare replacement segment having all of the necessary modifications made to it may be substituted in the place of the old segment which would then be repaired or modified by welding and heat treatment.
The connections between the replaceable segments could use a tubular gasket made of Inconel® or Monel®, coated with silver, for sealing, compressed by nuts and bolts on the flange. Other materials and coatings may also be used. Nozzles, or pipes, with flanges connected to the replaceable segments may be connected with ring joints using copper, nickel or other ring material. HF or uranium leaks from the reactor can be quickly stopped by replacing the damaged or cracked segment or gasket.
Staybolts, rods or internal structural supports, which provide rigidity to the reactor, can also be mechanically sealed with flanged fittings so as to eliminate the need to weld old-new materials.
In the preceding specification, the invention has been described with reference to specific exemplary embodiments and examples thereof. It will, however, be evident that various modifications and changes may be made thereto without departing from the broader spirit and scope of the invention as set forth in the claims that follow. The specification and drawings are accordingly to be regarded in an illustrative manner rather than a restrictive sense.
Priority to U.S. Provisional Patent Application Ser. No. 61/281,172 filed Nov. 12, 2009, is claimed, the entire disclosure of which is hereby incorporated by reference. This invention relates to the dry conversion process of uranium hexafluoride to uranium dioxide.
Number | Date | Country | |
---|---|---|---|
61281172 | Nov 2009 | US |