Claims
- 1. A method of selectively extracting alkylated mono-aromatic hydrocarbons in a lubricating oil feedstock containing at least about 40 wt. % aromatics by solvent extraction which comprises:(a) contacting the feedstock with a solvent under solvent extraction conditions, the solvent comprising at least one of N-methyl-2-pyrrolidone, furfural and phenol and water wherein said solvent extraction conditions include the amount of water in the solvent, solvent treat rate and temperature; (b) adjusting at least one of the amount of water in the solvent, solvent treat rate and temperature such that paraffinic hydrocarbons and alkylated mono-aromatic hydrocarbons are concentrated in a raffinate phase; (c) separating extracted feedstock into a raffinate rich in paraffinic hydrocarbons and alkylated mono-aromatic hydrocarbons and an extract rich in aromatic hydrocarbons including 2+ multi-ring aromatic hydrocarbons; (d) removing solvent from the raffinate to produce a stripped raffinate; (e) hydrofining the stripped raffinate under hydrofining conditions including a temperature of 150 to 450° C., hydrogen pressure of atmospheric to 10,000 psig; and liquid hourly space velocity of 0.1 to 10, (f) solvent dewaxing the hydrofined raffinate under solvent dewaxing conditions to produce a dewaxed hydrofined raffinate; and (g) measuring the VI of the dewaxed hydrofined raffinate and adjusting, if necessary, at least one of the amount of water in the solvent, solvent treat rate and temperature in step (a) to provide a dewaxed hydrofined raffinate having a VI of from about 86 to about 97.
- 2. The method of claim 1 where in solvent is N-methyl-2-pyrrolidone.
- 3. The method of claim 2 wherein the viscosity index is from about 88 to about 92.
- 4. The method of claim 1 wherein hydrofining utilizes a catalyst comprising at least one Group VIB or Group VIII metal.
- 5. The method of claim 4 wherein the catalyst is selected from at least one of cobalt, nickel, molybdenum and tungsten.
- 6. The method of claim 4 wherein hydrofining utilizes reaction conditions of 0.1 to 10 LHSV, temperature of 150 to 450° C. and hydrogen pressure of atmospheric to 10,000 psig.
- 7. The method of claim 1 wherein the amount of water is from about 0.5 to 10 LV %.
- 8. The method of claim 7 wherein the amount of water is from about 3 to 7 LV %.
- 9. The method of claim 1 wherein the feedstock contains at least about 50 wt. % aromatics.
- 10. The method of claim 1 wherein the alkylated mono-aromatic contains at least one long chain alkyl group.
- 11. The method of claim 1 wherein the solvent treat rate is 50-500 LV %, based on amount of feedstock.
- 12. The method of claim 1 wherein dewaxed hydrofined raffinate contains at least about 1.5 wt % more alkylated mono-aromatic hydrocarbons than contained in the feedstock.
Parent Case Info
This application claims the benefit of provisional application 60/145,395, filed Jul. 23, 1999.
US Referenced Citations (14)
Provisional Applications (1)
|
Number |
Date |
Country |
|
60/145395 |
Jul 1999 |
US |