The present invention relates to a solid-state battery.
In recent years, demand for batteries as power sources for portable electronic devices such as mobile phones and portable personal computers has increased significantly. In batteries used for such purposes, an electrolyte (electrolytic solution) such as an organic solvent has been used as a medium for moving ions. However, in the battery having the above configuration, there is a risk that the electrolytic solution may leak. Further, the organic solvent and the like used in the electrolytic solution are combustible substances. Therefore, it is desired to improve the safety of the battery.
In order to improve the safety of the battery, research on a solid-state battery using a solid electrolyte as an electrolyte instead of an electrolytic solution is in progress.
The solid-state battery is produced, for example, by forming a positive electrode layer green sheet, a negative electrode layer green sheet, and a solid electrolyte layer green sheet, alternately stacking the positive electrode layer green sheet and the negative electrode layer green sheet with the solid electrolyte green sheet interposed therebetween, further stacking the solid electrolyte layer green sheet on both upper and lower surfaces to form an electrode stacked body, firing the electrode stacked body, chamfering corners of the electrode stacked body by polishing, then forming extraction terminals on the electrode stacked body, and further providing a protective layer on the electrode stacked body, if necessary (e.g., Patent Document 1).
Patent Document 1: Japanese Patent Application Laid-Open No. 2016-1602
However, when chamfering the corners of the electrode stacked body by polishing or the like at the time of production, or when conveying the electrode stacked body, the corners or ridges of the electrode stacked body may be chipped. For example, the present inventors have found that when the corners of the electrode stacked body are chipped, the upper portion and lower portion electrode layers of the electrode stacked body in the vicinity of the corners are exposed on the surface of the electrode stacked body and react with moisture in the air, whereby the battery characteristics may be deteriorated.
On the other hand, it is also possible to prevent the corners and ridges of the electrode stacked body from being chipped at the time of producing or mounting by reviewing the material constituting the electrode stacked body. However, such a method can increase production costs. Consequently, there is a need for a method in which conventional materials can be employed.
Therefore, an object of the present invention is to provide a solid-state battery capable of suppressing deterioration of battery characteristics when corners or ridges of an electrode stacked body are chipped.
In order to solve the above problems, a solid-state battery according to one aspect of the present invention includes an electrode stacked body including a plurality of electrode layers alternately stacked with a solid electrolyte layer interposed therebetween, in which, in a sectional view of the electrode stacked body, at least one of opposed end surfaces of each of the electrode layers is spaced from a respective end surface of the electrode stacked body, and a first clearance from the at least one end surface of an uppermost electrode layer of the plurality of electrode layers to the respective end surface of the electrode stacked body in an upper portion and from the at least one end surface of a lowermost electrode layer of the plurality of electrode layers to the respective end surface of the electrode stacked body in a lower portion in a stacking direction of the electrode stacked body is larger than a second clearance from the at least one end surface of a central electrode layer of the plurality of electrode layers to the respective end surface of the electrode stacked body in a central portion in the stacking direction of the electrode stacked body.
According to the present invention, it is possible to provide a solid-state battery capable of suppressing deterioration of battery characteristics when the corners or ridges of the electrode stacked body are chipped.
Hereinafter, embodiments of the present invention will be described with reference to the drawings or the like.
A solid-state battery according to an embodiment of the present invention includes an electrode stacked body including a plurality of electrode layers alternately stacked with a solid electrolyte layer interposed therebetween, in which, in a sectional view of the electrode stacked body, at least one of opposed end surfaces of each of the electrode layers is spaced from a respective end surface of the electrode stacked body, and a first clearance from the at least one end surface of an uppermost electrode layer of the plurality of electrode layers to the respective end surface of the electrode stacked body in an upper portion and from the at least one end surface of a lowermost electrode layer of the plurality of electrode layers to the respective end surface of the electrode stacked body in a lower portion in a stacking direction of the electrode stacked body is larger than a second clearance from the at least one end surface of a central electrode layer of the plurality of electrode layers to the respective end surface of the electrode stacked body in a central portion in the stacking direction of the electrode stacked body.
The term “solid-state battery” as used herein refers in a broad sense to a battery in which its components (particularly an electrolyte layer) are constituted of solids, and refers in a narrow sense to an “all-solid-state battery” in which its components (particularly all the components) are constituted of solids. The term “solid-state battery” as used herein includes what is called a “secondary battery” capable of repeating charging and discharging, and a “primary battery” capable of discharging only. The “solid-state battery” is preferably the “secondary battery”. The term “secondary battery” is not excessively limited by its name, and can include, for example, “an electricity storage device”.
The term “planar view” used herein refers to a state (top view or bottom view) when an object is viewed from the upper side or the lower side along the thickness direction based on a stacking direction T of the electrode stacked body constituting the solid-state battery. The term “sectional view” used herein refers to a sectional state (sectional view) when viewed from a direction substantially perpendicular to the thickness direction based on the stacking direction T of the electrode stacked body constituting the solid-state battery. The terms “vertical direction” and “horizontal direction” used directly or indirectly herein respectively correspond to the vertical direction and the horizontal direction in the drawings. Unless otherwise specified, the same reference symbols or symbols shall denote the same members and portions or the same semantic contents. In a preferred aspect, it can be considered that a vertical downward direction (i.e., the direction in which gravity acts) corresponds to a “downward direction” and the opposite direction corresponds to an “upward direction”. Further, the term “corner of the electrode stacked body” used herein indicates a portion where three surfaces of the electrode stacked body adjacent to one another intersect, and the term “ridge of the electrode stacked body” indicates a portion where two adjacent surfaces of the electrode stacked body intersect.
(Electrode Stacked Body)
In a conventional solid-state battery in which electrode layers included in an upper portion, a central portion, and a lower portion of an electrode stacked body have an equal clearance, when the corners of the electrode stacked body are chipped, the electrode layers included in the upper portion and the lower portion in the vicinity of the corners are exposed on the surface and react with moisture in the air, as a result of which battery characteristics may be deteriorated. However, in the present invention, the clearance of each of the electrode layers included in the upper portion and the lower portion is larger than the clearance of each of the electrode layers included in the central portion, so that it is possible to increase a distance between a corner R and each of the widthwise end surfaces 1a and 1b of the first electrode layer 1 and a distance between a corner R and each of the widthwise end surfaces 2a and 2b of the first electrode layer 2. Accordingly, when the corners R of the electrode stacked body 100 are chipped, it is possible to prevent the widthwise end surfaces 1a and 1b of the first electrode layer 1 and the widthwise end surfaces 2a and 2b of the first electrode layer 2 from being directly exposed on the surface of the electrode stacked body 100.
On the other hand,
As illustrated in
In addition, the clearances of the two electrode layers: the uppermost layer and the lowermost layer may be larger than the clearances of all the other electrode layers except the uppermost layer and the lowermost layer. A distance between each of the uppermost layer and the lowermost layer closest to the corners of the electrode stacked body and a corner of the electrode stacked body is increased in order to prevent the electrode layers in the upper portion and the lower portion from being exposed on the surface of the electrode stacked body. Further, it is necessary that the clearances of all the other electrode layers except the uppermost layer and the lowermost layer are smaller than the clearances of the uppermost electrode layer and the lowermost electrode layer, and thus the tolerance for the accuracy of the width dimension can be increased. Accordingly, the printing of the electrode becomes easy, the required amount of electrode can be reduced, and the production costs can be reduced.
The electrode stacked body 200 has an upper surface 39 and a bottom surface 40 facing each other in the stacking direction T, and has a pair of widthwise end surfaces 41 and 42 facing each other in the width direction W. Each of the first electrode layers and each of the second electrode layers are alternately stacked with a solid electrolyte layer 35 interposed therebetween. In
Here, the central portion of the electrode stacked body 200 is a region including a virtual central line CL drawn in a direction orthogonal to the stacking direction of the electrode stacked body 200, and the region has a thickness of about ⅓ of a thickness T10 of the electrode stacked body 200 and includes the first electrode layers 28 and 30 in
According to the aspect illustrated in
In the aspects illustrated in
The sizes of the first electrode layer and the second electrode layer are usually determined by the capacity ratio between the positive electrode layer and the negative electrode layer. Therefore, when the clearances of the electrode layers included in the upper portion and the lower portion are made larger than the clearances of the electrode layers included in the central portion, it is preferable to increase the thicknesses of the electrode layers included in the upper portion and the lower portion from the viewpoint of securing the capacity ratio.
In addition, both widthwise end surfaces of the first electrode layer and the second electrode layer preferably have a tapered shape in which the thicknesses decrease toward the widthwise end surfaces of the electrode stacked body, the widthwise end surfaces facing each other, in the sectional view in the width direction of the electrode stacked body. The widthwise end surfaces are formed into a tapered shape, so that it is possible to further increase a distance between a corner of the electrode stacked body and each of both widthwise end surfaces of the first electrode layer or the second electrode layer. Accordingly, when the corners of the electrode stacked body are chipped, it is possible to prevent the first electrode layer and the second electrode layer from being exposed on the surface of the electrode stacked body.
The solid-state battery of the present invention may have any shape in a plan view, and usually has a rectangular shape. The rectangular shape includes squares and rectangles.
(Positive Electrode Layer and Negative Electrode Layer)
The positive electrode layer is made of a sintered body of positive electrode active material particles. The positive electrode active material particles may be constituted of a sintered body containing positive electrode active material particles, electron conductive material particles, and solid electrolyte particles contained in the solid electrolyte layer.
The negative electrode layer is made of a sintered body of negative electrode active material particles. The negative electrode active material particles may be constituted of a sintered body containing positive electrode active material particles, electron conductive material particles, and solid electrolyte particles contained in the solid electrolyte layer 3.
The positive electrode active material contained in the positive electrode layer and the negative electrode active material contained in the negative electrode layer are substances involved in exchange of electrons in the solid-state battery, and ions contained in a solid electrolyte material constituting the solid electrolyte layer move (being conducted) between the positive electrode and the negative electrode and exchange electrons, thereby performing charging and discharging. It is preferable that the positive and negative electrode layers are particularly layers capable of occluding and releasing lithium ions. That is, the solid-state battery according to the present invention is preferably a solid-state secondary battery in which lithium ions move between the positive electrode and the negative electrode through the solid electrolyte layer to charge and discharge the battery.
The positive electrode active material contained in the positive electrode layer is not particularly limited, and examples thereof include at least one selected from the group consisting of a lithium-containing phosphoric acid compound having a NASICON-type structure, a lithium-containing phosphate compound having an olivine-type structure, a lithium-containing layered oxide, a lithium-containing oxide having a spinel-type structure, and the like. One example of the lithium-containing phosphate compound having a NASICON-type structure includes Li3V2(PO4)3. One example of the lithium-containing phosphate compound having an olivine-type structure includes Li3Fe2(PO4)3 and LiMnPO4. One example of the lithium-containing layered oxide includes LiCoO2 and LiCo1/3Ni1/3Mn1/3O2. One example of the lithium-containing oxide having a spinel-type structure includes LiMn2O4 and LiNi0.5Mn1.5O4.
The negative electrode active material contained in the negative electrode layer is not particularly limited, and examples thereof include at least one selected from the group consisting of an oxide containing at least one element selected from the group consisting of Ti, Si, Sn, Cr, Fe, Nb, and Mo, a graphite-lithium compound, a lithium alloy, a lithium-containing phosphate compound having a NASICON-type structure, a lithium-containing phosphate compound having an olivine-type structure, a lithium-containing oxide having a spinel-type structure, and the like. One example of the lithium alloy includes Li—Al. One example of the lithium-containing phosphate compound having a NASICON-type structure includes Li3V2(PO4)3. One example of the lithium-containing phosphate compound having an olivine-type structure includes Li3Fe2(PO4)3. One example of the lithium-containing oxide having a spinel-type structure includes Li4Ti5O12.
The electron conductive material contained in the positive electrode layer and the negative electrode layer is not particularly limited, and examples thereof include metal materials such as silver, palladium, gold, platinum, aluminum, copper, or nickel; and carbon materials. Particularly, carbon is preferable because carbon does not easily react with the positive electrode active material, the negative electrode active material, and the solid electrolyte material, and is effective in reducing internal resistance of the solid-state battery.
The solid electrolyte material contained in the positive electrode layer and the negative electrode layer may be selected from, for example, materials similar to solid electrolyte materials that can be contained in the solid electrolyte layer to be described later.
The positive electrode layer and the negative electrode layer may each independently contain a sintering additive. The sintering additive is not particularly limited, and may be, for example, at least one selected from the group consisting of lithium oxide, sodium oxide, potassium oxide, boron oxide, silicon oxide, bismuth oxide, and phosphorus oxide.
The thicknesses of the positive electrode layer and the negative electrode layer are not particularly limited, and may each be, for example, 2 μm or more and 50 μm or less, particularly 5 μm or more and 30 μm or less, independently of each other.
(Solid Electrolyte Layer)
The solid electrolyte layer is made of a sintered body of solid electrolyte particles. The material of the solid electrolyte particles (i.e., a solid electrolyte material) is not particularly limited as long as it can provide ions that can move between the positive electrode layer and the negative electrode layer. Examples of the solid electrolyte material include a lithium-containing phosphate compound having a NASICON structure, an oxide having a perovskite structure, and an oxide having a garnet-type or garnet-like structure. Examples of the lithium-containing phosphate compound having a NASICON structure include LixMy(PO4)3 (1≤x≤2, 1≤y≤2, M is at least one selected from the group consisting of Ti, Ge, Al, Ga, and Zr). One example of the lithium-containing phosphate compound having a NASICON structure includes Li1.2Al0.2Ti1.8(PO4)3. One example of the oxide having a perovskite structure includes La0.55Li0.35TiO3. One example of the oxide having a garnet-type or garnet-like structure includes Li7La3Zr2O12.
The solid electrolyte layer may contain a sintering additive. The sintering additive contained in the solid electrolyte layer may be selected from, for example, materials similar to sintering additives that can be contained in the positive electrode layer and the negative electrode layer.
The thickness of the solid electrolyte layer is not particularly limited, and may be, for example, 1 μm or more and 15 μm or less, particularly 1 μm or more and 5 μm or less.
(Insulating Layer)
As illustrated in
Hereinafter, a method of producing the solid-state battery of the present invention will be described.
The solid-state battery of the present invention can be produced by a printing method such as a screen printing method, a green sheet method using a green sheet, or a composite method thereof. Hereinafter, the case where the printing method is employed will be described in detail, but the method is not limited to this method.
The method of producing the solid-state battery according to the present invention includes at least: a step of forming an unfired electrode stacked body by a printing method, and a step of firing the unfired electrode stacked body.
(Step of Forming Unfired Electrode Stacked Body)
In this step, an unfired electrode stacked body having a predetermined structure is formed on a substrate by a printing method using several types of pastes such as a positive electrode layer paste, a negative electrode layer paste, a solid electrolyte layer paste, and an insulating layer paste as ink.
The paste can be produced by wet-mixing a predetermined constituent material for each layer, selected from the group consisting of a positive electrode active material, a negative electrode active material, an electron conductive material, a solid electrolyte material, an insulating substance, and a sintering additive, with an organic vehicle obtained by dissolving an organic material in a solvent. For example, the positive electrode layer paste contains a positive electrode active material, an electron conductive material, a solid electrolyte material, an organic material, and a solvent. The negative electrode layer paste contains a negative electrode active material, an electron conductive material, a solid electrolyte material, an organic material, and a solvent. The solid electrolyte layer paste contains a solid electrolyte material, a sintering additive, an organic material, and a solvent. The insulating layer paste contains a solid electrolyte material or an insulating substance, an organic material, and a solvent.
The organic material contained in the paste is not particularly limited, and a polymer compound such as a polyvinyl acetal resin, a cellulose resin, a polyacrylic resin, a polyurethane resin, a polyvinyl acetate resin, or a polyvinyl alcohol resin may be used. The solvent is not particularly limited as long as the organic material can be dissolved, and for example, toluene, ethanol, and the like may be used.
In the wet mixing, a medium may be used, and specifically, a ball mill method, a viscomill method, or the like may be used. On the other hand, a wet mixing method that does not use a medium may be used, and a sand mill method, a high-pressure homogenizer method, a kneader dispersion method, or the like may be used.
The substrate is not particularly limited as long as it can support the unfired electrode stacked body, and for example, a polymer material such as polyethylene terephthalate may be used. Note that when the unfired electrode stacked body is subjected to a firing step while being held on the substrate, the substrate used is one having heat resistance to firing temperature.
At the time of printing, print layers are sequentially stacked with predetermined thicknesses and pattern shapes, and an unfired electrode stacked body corresponding to a predetermined solid-state battery structure is formed on the substrate, and then a drying treatment (i.e., a solvent evaporation treatment) is performed. In the present invention, the print layer is formed such that the clearances of the electrode layers included in the upper portion and the lower portion in the stacking direction of the electrode stacked body are larger than the clearances of the electrode layers included in the central portion in the stacking direction of the electrode stacked body.
After forming the unfired electrode stacked body, the unfired electrode stacked body may be peeled off from the substrate and subjected to a firing step, or the unfired electrode stacked body may be subjected to a firing step while being held on the substrate.
(Firing Step)
The unfired electrode stacked body is subjected to firing. The firing is carried out by removing the organic material in a nitrogen gas atmosphere containing oxygen gas, for example, at 500° C., and then heating in a nitrogen gas atmosphere, for example, at 550° C. to 1000° C. The firing may be usually performed while pressurizing the unfired electrode stacked body in the stacking direction L (the stacking direction L and the direction M perpendicular to the stacking direction L in some cases). The pressing force is not particularly limited, and may be, for example, 1 kg/cm2 or more and 1000 kg/cm2 or less, particularly 5 kg/cm2 or more and 500 kg/cm2 or less.
Further, a solid-state battery is completed by providing extraction terminals and, if necessary, a protective layer on the fired electrode stacked body.
The solid-state battery according to the present invention may be used in various fields in which electricity storage is expected. The solid-state battery according to the present invention can be used, although merely examples, for electric, information, communication fields where mobile devices are used (e.g., fields of mobile devices such as mobile phones, smart phones, smart watches, laptop computers and digital cameras, activity meters, arm computers, electronic paper, wireless earbuds, and wearable devices), home and small industrial applications (e.g., fields of power tools, golf carts, and domestic, nursing, and industrial robots), large industrial applications (e.g., fields of forklifts, elevators, gantry cranes), transportation system fields (e.g., fields of electric vehicles such as hybrid cars, electric cars, buses, trains, power assisted bicycles, and electric motorcycles), power system applications (e.g., fields of various power generations, road conditioners, smart grids, general household power storage systems, and the like), medical applications (medical equipment fields such as earphone hearing aids), pharmaceutical applications (fields such as dose management systems), and IoT fields, space and deep sea applications (e.g., fields of space probes, submersible research vehicles, and the like), and the like.
1, 2, 4, 6: First electrode layer
1
a, 1b: Widthwise end surface of uppermost layer
2
a, 2b: Widthwise end surface of lowermost layer
4
a, 4b: Widthwise end surface of central portion
6
a, 6b: Widthwise end surface of central portion
3, 5, 7: Second electrode layer
8: Solid electrolyte layer
9: Upper insulating layer
10: Lower insulating layer
11: Intermediate insulating layer
12: Upper surface of electrode stacked body
13: Bottom surface of electrode stacked body
14, 15: Lengthwise end surface of electrode stacked body
16, 17: Widthwise end surface of electrode stacked body
21, 22, 24: First electrode layer
21
a, 21b: Widthwise end surface of uppermost layer
22
a, 22b: Widthwise end surface of lowermost layer
26, 28, 30: First electrode layer
32, 34: First electrode layer
35: Solid electrolyte layer
36: Upper insulating layer
37: Lower insulating layer
38: Intermediate insulating layer
39: Upper surface of electrode stacked body
40: Bottom surface of electrode stacked body
41, 42: Widthwise end surface of electrode stacked body
100, 200: Electrode stacked body
Number | Date | Country | Kind |
---|---|---|---|
2019-152618 | Aug 2019 | JP | national |
The present application is a continuation of International application No. PCT/JP2020/023731, filed Jun. 17, 2020, which claims priority to Japanese Patent Application No. 2019-152618, filed Aug. 23, 2019, the entire contents of each of which are incorporated herein by reference.
Number | Date | Country | |
---|---|---|---|
Parent | PCT/JP2020/023731 | Jun 2020 | US |
Child | 17652020 | US |