The present application is a national stage application of PCT/JP2015/051628 filed Jan. 22, 2015, and claims foreign priority to Japanese Patent Application No. 2014-038240 filed Feb. 28, 2014, the contents of which are incorporated herein in their entirety.
Technical Field
The present invention relates to a sprayed coating forming method of forming a sprayed coating on an inner surface of a cylinder bore.
Related Art
Bore spraying is a method of forming a coating on an inner surface of a cylinder bore of a cylinder block for an automobile or the like by spraying a metal or a ceramic, then smoothing its surface by honing, and thereby forming a sliding surface for a piston ring. The bore spraying is applied as a technique for improving fuel efficiency.
To improve adhesion of such a coating to a base material, a cylinder block is subjected to heating (this heating is called pre-heating) before spraying (see Non Patent Literature 1).
Non Patent Literature 1: Journal of the Japan Institute of Metals, Vol. 71, No. 3 (2007), 354-360
In spraying of droplets of a molten metal material, residual particles, soot, or splattered droplets that fail to adhere to a sprayed surface may be captured in a sprayed coating. To avoid this, the splattered droplets and the like are discharged to the outside of the cylinder block by conducting exhaust ventilation from a lower side of the cylinder block.
However, the inner surface of the cylinder bore, i.e., the spray target surface is cooled by exhaust airflow that flows in and out of the cylinder block, and a pre-heating temperature of the cylinder block drops as a consequence. For this reason, the adhesion of the sprayed coating to the inner surface of the cylinder bore is deteriorated.
One or more embodiments of the present invention provides a sprayed coating forming method which is capable of suppressing a drop in pre-heating temperature of a cylinder block and enhancing adhesion of a sprayed coating to an inner surface of a cylinder bore.
According to a sprayed coating forming method of one or more embodiments of the present invention, a cylinder bore located while leaving a space of at least one cylinder from a cylinder bore first sprayed is sprayed next.
Embodiments of the present invention will be described below in detail with reference to the drawings. In embodiments of the invention, numerous specific details are set forth in order to provide a more thorough understanding of the invention. However, it will be apparent to one of ordinary skill in the art that the invention may be practiced without these specific details. In other instances, well-known features have not been described in detail to avoid obscuring the invention.
The enclosure 3 is formed as a rectangular box having a shape of a hexahedron, for example. However, the shape of the enclosure 3 is not limited to the shape of
Air to be supplied into the enclosure 3 is introduced to the intake duct 4. The air inside the enclosure 3 is discharged from the exhaust ducts 5 to the outside of the enclosure 3. Of droplets of a molten metal material, residual particles, soot, or splattered droplets that fail to adhere to a sprayed surface are discharged from these exhaust ducts 5 together with the air to be discharged.
The air supplied from the intake duct 4 into the enclosure 3 flows as indicated with arrows in
The spray gun 2 is an arc spray gun as shown in
It has been known that adhesion of the sprayed coating 12 to be formed on the inner surface 6a of the cylinder bore 6 depends on a pre-heating temperature for heating the cylinder block 1 prior to the spraying. As shown in
A sequence to form the coatings on the multiple cylinder bores 6A to 6D is important for forming the sprayed coatings 12 by spraying the molten metal droplets 11 onto the inner surfaces 6a of the cylinder bores 6. Here, the cylinder bores 6 formed in the cylinder block 1 for an in-line four-cylinder engine are defined as a first cylinder bore 6A, a second cylinder bore 6B, a third cylinder bore 6C, and a fourth cylinder bore 6D sequentially from one end, for example.
After this cylinder block 1 is disposed in the enclosure 3, the cylinder block 1 is pre-heated by heating means such as a heater. Then, the inside of the enclosure 3 is subjected to exhaust ventilation. Hence, the airflow occurs as illustrated in
In one or more embodiments of the present invention, the order of spraying the multiple cylinder bores 6A to 6D is set as described below, so as to avoid a sudden drop in cylinder block temperature after the pre-heating due to the exhaust ventilation. Specifically, the cylinder bore located while leaving a space of at least one cylinder from the cylinder bore first sprayed is sprayed next.
To be more precise, as shown in
The spray gun 2 is inserted deep into the second cylinder bore 6B from a cylinder head surface side thereof. Simultaneously, the molten metal droplets 11 are sprayed onto the inner surface of the cylinder bore. The sprayed coating 12 is formed by spraying and depositing the metal droplets 11 on the inner surface of the cylinder bore. During the spraying, residual particles, soot, or splattered droplets 11 that fail to adhere to the inner surface of the cylinder bore are discharged to the outside of the enclosure 3 through the exhaust ducts 5 by the exhaust ventilation. Thus, it is possible to avoid deterioration in quality of the sprayed coating 12.
When the second cylinder bore 6B is sprayed, the first cylinder bore 6A and the third cylinder bore 6C, which are the cylinder bores located on two sides, are heated by the heat in the spraying. In
Next, the fourth cylinder bore 6D located while leaving a space of one cylinder from the second cylinder bore 6B is sprayed. Hence, the adjacent third cylinder bore 6C is heated by the heat in the spraying. Subsequently, the first cylinder bore 6A located while leaving a space of two cylinders from the fourth cylinder bore 6D is sprayed. When the first cylinder bore 6A is sprayed, the first cylinder bore 6A is in the heated state by the heat input in the earlier spraying on the second cylinder bore 6B. Thus, a drop in in-bore temperature of the first cylinder bore 6A is suppressed.
And finally, the third cylinder bore 6C located while leaving a space of one cylinder from the first cylinder bore 6A is sprayed. When the third cylinder bore 6C is sprayed, the third cylinder bore 6C is in the heated state by the heat input in the spraying on the fourth cylinder bore 6D and the heat input in the spraying on the second cylinder bore 6B. Thus, a drop in in-bore temperature of the third cylinder bore 6C is suppressed.
By performing the spraying on the cylinder bores 6A to 6D in the above-described order, it is possible to avoid a drop in temperature of the cylinder block after the pre-heating due to the exhaust ventilation, and to enhance the adhesion of the sprayed coatings 12 formed on all the cylinder bores 6A to 6D.
According to a sprayed coating forming method according to one or more embodiments of the present invention, the cylinder bore located while leaving the space of at least one cylinder from the cylinder bore first sprayed is sprayed. Thus, the cylinder bores located on two sides of the cylinder bore first sprayed are heated by the heat of the first spraying. For this reason, by determining the cylinder located while leaving the space of at least one cylinder to be sprayed next, it is possible to suppress the drop in pre-heating temperature as compared to the case of spraying the cylinder bores sequentially from one end. Accordingly, it may be possible to enhance the adhesion of the sprayed coatings 12 formed on the inner surfaces of the cylinder bores 6.
Meanwhile, according to a sprayed coating forming method according to one or more embodiments of the present invention, the second cylinder bore 6B of the in-line four-cylinder engine is first sprayed, and then the fourth cylinder bore 6D, the first cylinder bore 6A, and the third cylinder bore 6C thereof are sprayed in this order. Thus, the pre-heating temperature of the cylinder block 1 that would otherwise gradually drop over time can be recovered by the heat input in the spraying on each cylinder bore. Thus, it is possible to suppress a sudden drop in temperature of the in-bore temperature of each of the cylinder bores 6A to 6D.
Moreover, according to a sprayed coating forming method according to one or more embodiments of the present invention, residual particles, soot, or splattered droplets that fail to adhere to the inner surfaces of the cylinder bores are discharged to the outside of the enclosure, which houses the cylinder block, by conducting the exhaust ventilation in the spraying. Thus, it is possible to suppress deterioration in quality of the sprayed coatings 12 and to control the coating thickness at the same time.
Furthermore, according to a sprayed coating forming method according to one or more embodiments of the present invention, the air supplied into the enclosure to house the cylinder block flows around the cylinder block and also flows inside the cylinder bores formed in the cylinder block. As a consequence, it is possible to prevent residual particles and the like, which may scatter in the spraying, from adhering to the sprayed coatings.
Although embodiments of the present invention are described above, the present invention is not limited only to the above-described embodiments. For example, while the order of spraying is determined in the order of the second cylinder bore 6B, the fourth cylinder bore 6D, the first cylinder bore 6A, and the third cylinder bore 6C, the order is not limited only to the foregoing. Meanwhile, in the above-described embodiments, the sprayed coatings 12 are formed in the in-line four-cylinder engine. However, the sprayed coating forming method according to one or more embodiments of the present invention is also applicable to an in-line six-cylinder engine and a V-type engine. In the meantime, the exhaust ventilation may also be conducted from a head block attaching surface side of the cylinder bores 6.
While the invention has been described with respect to a limited number of embodiments, those skilled in the art, having benefit of this disclosure, will appreciate that other embodiments can be devised which do not depart from the scope of the invention as disclosed herein. Accordingly, the scope of the invention should be limited only by the attached claims.
Number | Date | Country | Kind |
---|---|---|---|
2014-038240 | Feb 2014 | JP | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/JP2015/051628 | 1/22/2015 | WO | 00 |