Claims
- 1. A method for the preparation of a sulfurized composition which comprises the steps of reacting at about 50.degree.-300.degree. C., under superatmospheric pressure and in the absence of catalysts, sulfur and hydrogen sulfide with at least one olefinic compound containing 3 to about 30 carbon atoms to form a sulfurized mixture; about 1.2-3.0 gram-atoms of sulfur and about 0.1-1.5 moles of hydrogen sulfide being used per mole of olefinic compound; and removing from said sulfurized mixture substantially all low boiling materials including unreacted olefin, mercaptan and monosulfide.
- 2. The method according to claim 1 wherein the reaction temperature is about 100.degree.-200.degree. C.
- 3. The method according to claim 2 wherein about 1.2-2.0 gram-atoms of sulfur and about 0.2-1.25 moles of hydrogen sulfide are used per mole of the olefinic compound.
- 4. The method according to claim 3 wherein about 0.4-0.8 mole of hydrogen sulfide is used per mole of the olefinic compound.
- 5. The method according to claim 4 wherein the olefinic compound is an olefinic hydrocarbon containing from 3 to about 16 carbon atoms.
- 6. The method according to claim 5 wherein at least one of the olefinic compounds has one or two carbon-to-carbon double bonds.
- 7. The method according to claim 6 wherein the olefin is a monoolefin selected from propane, isobutene and dimers, trimers and tetramers thereof.
- 8. The method according to claim 7 wherein the olefin is isobutene or diisobutene.
- 9. The method for the preparation of a sulfurized composition which comprises the steps of reacting at about 50.degree.-300.degree. C., under superatmospheric pressure and in the absence of catalysts, sulfur and hydrogen sulfide with at least one terminal aliphatic monoolefin containing less than 9 carbon atoms to form a sulfurized mixture, about 1.2-2.0 gram-atoms of sulfur and about 0.1-1.5 moles of hydrogen sulfide being used per mole of monoolefin; and removing from said sulfurized mixture substantially all low boiling materials including unreacted monoolefin, mercaptan and monosulfide.
- 10. The method according to claim 9 wherein the reaction temperature is about 100.degree.-200.degree. C. and about 0.2-1.0 mole of hydrogen sulfide is used per mole of monoolefin.
- 11. The method according to claim 10 wherein the monoolefin is isobutene.
- 12. The method according to claim 10 wherein about 1.2-1.5 gram-atoms of sulfur and about 0.4-0.8 mole of hydrogen sulfide are used per mole of the monoolefin.
- 13. The method according to claim 1 which includes the step of treating the product after removal of low boiling materials with an alkali metal sulfide to reduce active sulfur.
- 14. The method according to claim 13 wherein the olefinic compound is a monoolefinic hydrocarbon containing from 3 to about 16 carbon atoms.
- 15. The method according to claim 14 wherein the olefin is at least one of propene, isobutene and dimers, trimers and tetramers thereof.
- 16. The method according to claim 15 wherein the olefin is isobutene or diisobutene.
- 17. The method according to claim 9 which includes the step of treating the product after removal of low boiling materials with an alkali metal sulfide to reduce active sulfur.
- 18. The method according to claim 17 wherein the olefin is isobutene.
- 19. The sulfurized composition prepared by the method of claim 1.
- 20. The sulfurized composition prepared by the method of claim 3.
- 21. The sulfurized composition prepared by the method of claim 5.
- 22. The sulfurized composition prepared by the method of claim 7.
- 23. The sulfurized composition prepared by the method of claim 8.
- 24. The sulfurized composition prepared by the method of claim 9.
- 25. The sulfurized composition prepared by the method of claim 11.
- 26. An additive concentrate comprising a substantially inert, normally liquid diluent and about 20-90% by weight of the sulfurized composition of claim 19.
- 27. An additive concentrate comprising a substantially inert, normally liquid diluent and about 20-90% by weight of the sulfurized composition of claim 20.
- 28. An additive concentrate comprising a substantially inert, normally liquid diluent and about 20-90% by weight of the sulfurized composition of claim 21.
- 29. An additive concentrate comprising a substantially inert, normally liquid diluent and about 20-90% by weight of the sulfurized composition of claim 22.
- 30. An additive concentrate comprising a substantially inert, normally liquid diluent and about 20-90% by weight of the sulfurized composition of claim 23.
- 31. An additive concentrate comprising a substantially inert, normally liquid diluent and about 20-90% by weight of the sulfurized composition of claim 24.
- 32. An additive concentrate comprising a substantially inert, normally liquid diluent and about 20-90% by weight of the sulfurized composition of claim 25.
- 33. A lubricating composition comprising a major proportion of lubricating oil and a minor proportion, sufficient to improve extreme pressure, anti-wear or oxidation inhibiting properties, of a sulfurized composition according to claim 19.
- 34. A lubricating composition comprising a major proportion of lubricating oil and a minor proportion, sufficient to improve extreme pressure, anti-wear or oxidation inhibiting properties, of a sulfurized composition according to claim 20.
- 35. A lubricating composition comprising a major proportion of lubricating oil and a minor proportion, sufficient to improve extreme pressure, anti-wear or oxidation inhibiting properties, of a sulfurized composition according to claim 21.
- 36. A lubricating composition comprising a major proportion of lubricating oil and a minor proportion, sufficient to improve extreme pressure, anti-wear or oxidation inhibiting properties, of a sulfurized composition according to claim 22.
- 37. A lubricating composition comprising a major proportion of lubricating oil and a minor proportion, sufficient to improve extreme pressure, anti-wear or oxidation inhibiting properties, of a sulfurized composition according to claim 23.
- 38. A lubricating composition comprising a major proportion of a lubricating oil and a minor proportion, sufficient to improve extreme pressure, anti-wear or oxidation inhibiting properties and comprising about 0.1-10% by weight of said lubricating composition, of a sulfurized composition according to claim 24.
- 39. A lubricating composition comprising a major proportion of a lubricating oil and a minor proportion, sufficient to improve extreme pressure, anti-wear or oxidation inhibiting properties and comprising about 0.1-10% by weight of said lubricating composition, of a sulfurized composition according to claim 25.
Parent Case Info
This application is a continuation-in-part of copending application Ser. No. 949,285, filed Oct. 6, 1978 now abandoned. Said copending application is a continuation-in-part of Ser. No. 814,583, filed July 11, 1977, now U.S. Pat. No. 4,119,550, which is a continuation-in-part of Ser. No. 666,545, filed Mar. 15, 1976, which in turn is a continuation-in-part of Ser. No. 560,676, filed Mar. 21, 1975. The latter two applications are now abandoned.
US Referenced Citations (1)
Number |
Name |
Date |
Kind |
4191659 |
Davis |
Mar 1980 |
|
Continuation in Parts (4)
|
Number |
Date |
Country |
Parent |
949285 |
Oct 1978 |
|
Parent |
814583 |
Jul 1977 |
|
Parent |
666545 |
Mar 1976 |
|
Parent |
560676 |
Mar 1975 |
|