Claims
- 1. A fusion weldable alloy consisting essentially of:ElementRange (wt. %)Al + Ti1-9B0-0.01C0-0.15Co0-25Cr5-30Fe0-10Hf + Y + Sc0-0.009Mo + W1-15Nb + Ta0-8Ni40-68Pd4-32Re + Rh0-10V0-5Zr0-0.015wherein the wt % of Al is 1≦Al<4 and the total amount of Pd+Ni lies is the range of 55-72 wt. %.
- 2. A fusion weldable alloy consisting essentially of:ElementRange (wt. %)Al + Ti1-9B0-0.01C0-0.15Co0-25Cr5-30Fe0-10Hf + Y + Sc0-0.009Mo + W1-15Nb + Ta0-8Ni40-68Pd4-32Re + Rh0-10V0-5Zr0-0.015wherein the wt % of Al is between 1 and 3 and the amount of Ta is ≦5 wt % and the total amount of Pd+Ni lies is the range of 55-72 wt %.
Parent Case Info
This application is also a continuation-in-part of Ser. No. 08/630,812 filed Apr. 10, 1996 now abandoned.
PRIORITY AND GOVERNMENT SPONSORSHIP
This invention was made with Government support under Contract Number N00039-92-C-0100 awarded by the United States Department of the Navy. The Government has certain rights in this invention.
US Referenced Citations (4)
Number |
Name |
Date |
Kind |
4061495 |
Selman et al. |
Dec 1977 |
|
4261742 |
Coupland et al. |
Apr 1981 |
|
4447503 |
Dardi et al. |
May 1984 |
|
4719080 |
Duhl et al. |
Jan 1988 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
08/630812 |
Apr 1996 |
US |
Child |
09/075102 |
|
US |