Certain chemical reactions, for example, thermal condensation or dehydrochlorination, may require high temperatures and involve corrosive reactants. One such reaction is the gas phase reaction of trichlorosilane (HSiCl3) with vinyl chloride (H2C═CHCl), which does not progress quickly until the temperatures exceed 500° C. This reaction liberates hydrogen chloride, HCl(g), which is corrosive to most metallurgies (e.g., even those containing high levels of Ni, Cr, and Mo for resistance). Moreover, at these temperatures, trichlorosilane reacts with nickel-containing metals to form intermetallic silicide compounds, which in turn can be etched by HCl, leading to an increased corrosion/pitting rate. Undesirable side reactions may occur, for example, the decomposition of vinyl chloride to soot when in excess of trichlorosilane. Soot can lead to operation and maintenance problems. Similarly, if trichlorosilane is fed in stoichiometric excess, the formation of 1,2-bis(trichlorosilyl)ethane and other heavy silicon-based compounds becomes prominent, resulting in waste chlorosilanes.
Accordingly, what is needed are thermal condensation reactors that avoid these problems and processes of using the same.
Described herein are thermal condensation reactors (and processes of using the same). A presently described thermal condensation reactor comprises a heat transfer chamber, wherein the heat transfer chamber is a fluidized bed having a fluidization gas flow in a first direction, and wherein the heat transfer chamber has a plurality of heating zones that may be maintained at different temperatures, and a plurality of reaction tubes disposed in the heat transfer chamber in a second direction perpendicular to the fluidization gas flow, each reaction tube having a reactant gas flow that passes through the plurality of heating zones. Also described are processes for producing vinyltrichlorosilane and other alkenyl-functional halosilanes, comprising premixing vinyl chloride and a hydrido-functional halosilane to create a reactant gas, introducing the reactant gas into a plurality of reaction tubes arranged horizontally with respect to the base in a fluidized bed, and passing the reactant gas through a plurality of heating zones in the fluidized bed, wherein the plurality of heating zones are maintained at different temperatures.
Refractory and other insulation materials may be used to reduce heat loss in the zones requiring heat input. The position of the materials may vary depending on the technology used. For example, refractory materials may be employed internal to the chamber if the heat input is driven by a pulse combustion unit, but it would be advantageous to use refractory outside of the heat transfer chamber if resistance heating elements are employed. Internal refractory materials have an additional benefit with respect to erosion, but erosion can also be managed using application of hard-faced metal overlay onto the chambers or the high velocity-oxygen fuel (HVOF)-applied ceramic coatings to the metal surface.
The thermal condensation reactor 100 includes a stationary inlet head 104. The stationary inlet head 104 is attached to the heat transfer chamber 102. Reactants enter the stationary head 104 (e.g., inlet side).
The thermal condensation reactor 100 includes a plurality of reaction tubes 106. Although a single reaction tube numbered 106 is depicted for simplicity of illustration, it is understood that a plurality of tubes is contemplated, and thus we refer to reaction tubes 106 throughout this disclosure. The plurality of reaction tubes 106 are in fluid communication with the stationary head 104 and extend through the heat transfer chamber 102. Accordingly, reactants enter the plurality of reaction tubes 106 at the stationary head 104, and are carried through the plurality of reaction tubes in the heat transfer chamber 102, experiencing the plurality of heating zones 102a-c. The reactants are sealed from the heat transfer chamber 102.
Differential thermal expansion between the tubes and the body of the heat transfer chamber and supports must be accommodated. The thermal condensation reactor 100 includes a floating head 108. The plurality of reaction tubes 106 exit the heat transfer chamber 102 into the floating head 108 (e.g., outlet side). The reaction product is thereby collected in the floating head 108. A cooling transition unit 110 surrounds the floating head 108. The cooling transition unit 110 may be used to control the temperature of the reaction products. In one embodiment, the function of the floating head could be replaced with a flexible tubesheet.
The stationary head 104 includes a bonnet 112 which is attached to heat transfer chamber 102. A gasket 113 is located between the bonnet 112 and the heat transfer chamber 102. The gasket 113 seals the connection between the bonnet 112 and the heat transfer chamber 102. In some embodiments, a primary function of the gasket 113 is to keep fluidized bed media out of the bonnet 112. Accordingly, a variety of gasket designs are contemplated, including, for example, a gasket, a double gasket, or a ring joint. Certain gasket details are dependent on thermal expansion mitigation strategy for the fluidized bed media.
The bonnet 112 cooperates with other components to define one or more plenums, as will be described herein. A primary gas feed inlet 114 is disposed in the bonnet 112. Reactants enter a plenum defined by the bonnet 112 via the primary gas feed inlet 114.
An inlet feed gas manifold 116 and a reactor tubesheet face 118 are disposed inside the bonnet 112. The reactor tubesheet face 118 abuts the heat transfer chamber 102. The inlet feed gas manifold 116 and the reactor tubesheet face 118 are disposed coplanar to each other and extend to the edges of the bonnet 112. The inlet feed gas manifold 116 and the reactor tubesheet face 118 each have a plurality of ports, respectively numbered as 116a and 118a, for receiving the plurality of reaction tubes 106. Each of the ports 116a and 118a will receive a respective reaction tube 106. Any number of reaction tubes 106 are contemplated, depending on space limitations, reactor capacity, and other considerations.
As will be described in more detail with respect to
Optionally, a shroud gas port 120 is in fluid combination with the second plenum defined between the inlet feed gas manifold 116, bonnet 112, and the reactor tubesheet face 118. The shroud gas port 120 introduces a nonreactive gas (e.g., shroud gas) to the second plenum (e.g., plenum 321 of
The thermal condensation reactor 100 includes a plurality of plates 122a-e. The plurality of plates 122a-e are disposed in the heat transfer chamber 102 to support the plurality of reaction tubes 106. For example, each of the plurality of plates 122a, 122b, 122c, 122d, 122e include a plurality of apertures. Each of the plurality of apertures is configured to receive a respective reaction tube of the plurality of reaction tubes 106. The plurality of reaction tubes 106 are supported by corresponding apertures in the plurality of plates 122a, 122b, 122c, 122d, 122e. As depicted, the bonnet 112 is attached to the plate 122a, which is adjacent to the reactor tubesheet face 118.
Although five plates 122a-e are illustrated, it is understood that any number of plates are contemplated. It is noted that the placement of the plates 122b-d does not necessarily correspond to the boundaries of heating zones 102a-c, rather, the boundaries of the heating zones are dictated by the position of the external heating source(s) (not depicted).
The plates 122a-e may be affixed to the heat transfer chamber 102 in a variety of manners, for example, by mechanical fasteners (e.g., plates 122a, 122b, 122d and 122e), or by moveable supports (e.g., plates 122c with respect to roller support 210 (as will be described with respect to
A plurality of baffles 124a-b are disposed in the heat transfer chamber 102. The plurality of baffles 124a-b support operation of the heat transfer chamber 102 as a fluidized bed. Additional baffles (not depicted) may be disposed in the heat transfer chamber 102. It is understood that the heat transfer chamber 102 may include any number of baffles similar to baffles 124a-b. It is understood that the plates 122b-d will also act as baffles in the operation as will be explained.
A plurality of gas ports 126a-d are disposed in fluid communication with the heat transfer chamber 102. The plurality of gas ports 126a, 126b, 126c, and 126d are configured to introduce a nonreactive gas to the heat transfer chamber 102. It is understood that any number of gas ports are contemplated, however, it is beneficial to have at least one gas port associated with each heating zone (e.g., heating zones 102a-c), as will be explained. Although not depicted, a distributor plenum (such as, for example, a sparger, a sintered metal perforated plate gas distributor, or a porous plate) may be placed inside the heat transfer chamber 102 above the gas ports 126a-d.
Although not depicted, the heat transfer chamber 102 has a top portion for enclosing the heat transfer chamber 102. The top portion may have heating elements to control temperature. The top portion includes one or more collection plenums for collecting the nonreactive gas introduced via gas ports 126a-d. The one or more collection plenums may be in fluid communication with an exhaust (e.g., a common exhaust).
A plurality of drain ports 128a-d are disposed in fluid communication with the heat transfer chamber 102 for draining solids from the heat transfer chamber (e.g., although not depicted, the heat transfer chamber may contain solid particles, preferably a fluidized bed of solid particles (such as, for example, Geldart Group A powder forms). It is understood that any number of drain ports are contemplated.
A plurality of supports 130a-e are disposed under the heat transfer chamber 102 for structural support. It is understood that any number of supports are contemplated.
The cooling transition unit 110 has a gas port 126e, drain port 128e, and a support 130f, substantially similar in operation to those having the same reference numerals and described with respect to the heat transfer chamber 102. Although not depicted, the cooling transition unit 110 may contain solid particles, preferably a fluidized bed of solid particles (such as, for example, Geldart Group A powder forms). Fluidization of this zone reduces interferences in thermal expansion and reduces the amount of baffling required to maintain fluidization in the previous zone.
A vapor outlet 132 is disposed in the cooling transition unit 110, in fluid communication with the floating head 108. Reaction product (e.g., including optional shroud gases) from the plurality of reaction tubes 106 are collected through the vapor outlet 132.
A roller support 210 extends between the plate 122c and the heat transfer chamber 102 to attach the plate to the heat chamber while allowing, for example, thermal expansion of the plate.
The floating head 108 includes a plate 222 to support the plurality of reaction tubes 106. A sealing ring 224 is disposed between the plate 222 and the plate 122/heat transfer chamber 102 to seal the reaction products in the floating head 108 from the cooling transition unit 110 and the heat transfer chamber 102.
A roller support 226 moveably connects the floating head 108 to the heat transfer chamber 102. For example, the floating head 108 may float at a rear of the heat transfer chamber 102 such that a location of the floating head with respect to the heat transfer chamber may fluctuate in one direction (e.g., due to thermal expansion).
The reaction tube 306 includes a gas injection port 306a which extends axially from a reaction tube liner 306b. In one embodiment, the gas injection port 306a fits sufficiently loosely in the reaction tube liner 306b so as to allow gas to pass between the respective exterior and interior surfaces of their respective walls. Reactants in a first plenum 319 defined between the bonnet 312 and the inlet feed gas manifold 316 enter the gas injection port 306a. A sealing connector 334 is disposed in the inlet feed gas manifold 316 engaging the gas injection port 306a. The connector 334 can comprise multiple sealing arrangements such as a sealing gland or compression fitting. Accordingly, the first plenum 319 is sealed relative to a second plenum 321 defined between a coplanar second side of the inlet elliptical head, the bonnet 312, and the reactor tubesheet face 318. Optionally, a shroud gas is introduced into the second plenum 321.
A sealing gland (or stuffing box) 336 is disposed in the reactor tubesheet face 318, engaging the reaction tube liner 306b. The sealing gland 336 enables a gas-tight seal between the heat transfer chamber 302 and the second plenum 321. Commercially available sealing glands may be procured, inter alia, from Conax Technologies, Buffalo, N.Y., USA. A compressible sealant 336a (such as, for example, flexible graphite) engages the exterior of the reaction tube liner 306b. The second plenum 321 is sealed relative to the heat transfer chamber 302. A passage 336b extends through the sealing gland 336 to the reaction tube liner 306b. Gasses in the second plenum, for example, a shroud gas, may enter the reaction tube liner 306b via the passage 336b of the sealing gland 336.
Turning to
Turning to
In operation, the thermal condensation reactor 100 may find use as a multi-zone, fluidized bed assisted heating/cooling arrangement for thermal condensation or dehydrochlorination reactions. For example, in one embodiment, the thermal condensation reaction may be thermal condensation of a reactant gas comprising a hydrido-functional halosilane and an alkenyl halide, and the thermal condensation forms an alkenyl-functional halosilane. For example, the hydrido-functional halosilane may have formula RwHxSiX(4−w−x), where subscript subscript w is 0 to 2, subscript x is 1 to 3, and a quantity (w+x) is 1 to 3; each R is an independently selected monovalent hydrocarbon group of 1 to 18 carbon atoms that is free of aliphatic unsaturation, and each X is an independently selected halogen atom such as F, Cl, Br, or I, alternatively Cl or Br, and alternatively Cl. The monovalent hydrocarbon group for R may be alkyl (e.g., methyl, ethyl, or hexyl; alternatively methyl) or aryl (e.g., phenyl, tolyl, or xylyl; alternatively phenyl). The alkenyl halide may have formula R′Xa, where subscript a is 1 up to the valence of R′; R′ is an alkenyl functional group such as vinyl, vinylidene, allyl, or hexenyl; and X is as described above. Exemplary hydrido-functional halosilanes include monochlorosilane (H3SiCl), dimethylchlorosilane [(CH3)2HSiCl], dichlorosilane (H2SiCl2), and trichlorosilane (HSiCl3). Exemplary alkenyl halides include vinyl chloride, vinylidene chloride, allyl chloride, and hexenyl chloride . The alkenyl-functional halosilane that may be prepared in the thermal condensation reactor 100 may have formula R′uRyHzSiX(4-y-z), where subscript u is 1, 2, or 3 (alternatively 1), subscript y is 0, 1, or, 2; subscript z is 0, 1, or 2, and a quantity (u+y+z) is 1 to 3. Alkenyl-functional halosilanes that may be prepared in the thermal condensation reactor 100 include vinyl trichlorosilane, (e.g., when the hydrido-functional halosilane is HSiCl3 and the alkenyl halide is vinyl chloride), or dimethylvinylchlorosilane [(CH3)2(CH2═CH)SiCl] (e.g., when the hydrido-functional halosilane is dimethylchlorosilane and the alkenyl halide is vinyl chloride). The gas phase reaction of trichlorosilane with vinyl chloride does not progress quickly until the temperatures exceed 500° C.
The thermal condensation reactor 100 delivers the greater than 500° C. temperatures needed to operate the reaction at good conversion per pass while at the same time suppressing the consequence of exotherm associated with the process chemistry. To achieve this, a plurality of reaction tubes 106 (e.g., fit with an interior liners having chemical resistance to HCl and good thermal conductivity (such as, for example, isomolded graphite, carbon fiber/carbon composite, isomolded graphite with SiC-coating, or silicon carbide such as Saint-Gobain Hexaloy® SiC)) are used. Because the coefficient of thermal expansion of the liner is less than the reactor tube metallurgy, the liner will need to slide during growth. The sliding may be assisted through use of a flexible graphite film and/or saddle placed on the bottom of the liner. Also, the length of the interior liner should be preferably longer than the length of the tubes. The plurality of reaction tubes 106 are arranged parallel to the flow of the reactants and cross-flow (e.g., perpendicular or nearly perpendicular (e.g., plus or minus 15 degrees from perpendicular)) to the flow of fluidization gas. As illustrated, this creates a horizontal flow of the reactants and a vertical flow of fluidization gas. The horizontal configuration offers advantages in mechanically supporting the plurality of reaction tubes 106 and maintenance operations. Use of silicon carbide may offer sufficient oxidation resistance to allow an oxidative treatment of deposited soot that accumulates in the process over time. As part of a maintenance cycle, hydrogen addition at temperatures in excess of 600° C. may, e.g., may also, be employed to methanize soot-like compounds to a vapor form.
The liner is secured with a sealing gland 336 (as shown in
Optionally, a shroud gas is co-fed to the reactor. For the reaction of trichlorosilane with vinyl chloride, use of silicon tetrachloride (SiCl4) as the shroud gas provides benefit as a diluent that can reduce migration of carbon species near the reaction tube wall while reducing Si—H/Si—Cl rearrangement reactions leading to dichlorosilane and vinyldichlorosilane in the effluent. The shroud gas is comprised of an organohalosilane, most preferably the halogenation product of the hydrido-functional halosilane feed agent and hydrogen halide (HX). For example, for reactions involving trichlorosilane with vinyl chloride, silicon tetrachloride would be used as the shroud gas since the halogenation product of trichlorosilane (HSiCl3) and HCl is silicon tetrachloride (SiCl4). Similarly, for reactions involving dimethylchlorosilane with vinyl chloride, dimethyldichlorosilane [(CH3)2SiCl2] would be used. The shroud gas is introduced into the second plenum defined between the inlet feed gas manifold 116, bonnet 112, and the reactor tubesheet face 118 via the shroud gas port 120. Shroud gas flows around the gas injection port 306a for each reaction tube through the passage 336b, which extends through the sealing gland 336 to the reaction tube liner 306b. The passage 336b is configured with a sufficient pressure drop to encourage balanced distribution of shroud gas between all of the plurality of reaction tubes 106. Similarly, for each gas injection port 306a containing the vinyl chloride/trichlorosilane feed mixture, there will exist an orifice plate at entry to encourage uniform distribution of gas between individual reaction tubes 106.
The plurality of reaction tubes 106 extend from the bonnet 112, pass through heat transfer chamber 102, and terminate at the floating head 108. The heat transfer chamber 102 is a heated trough with a plurality of heating zones 102a-c. Inside the heat transfer chamber 102, a fluidization gas (such, as for example, nitrogen) is used to fluidize a solid medium, forming a fluidized bed. As illustrated, the fluidization gas travels perpendicular to the plurality of reaction tubes 106. The fluidization gas (such, as for example, nitrogen) is delivered to the heat transfer chamber 102 via a plurality of gas ports 126a-d, and may pass through a sparger, sintered metal perforated plate, or a gas distributor. The heat transfer chamber 102 has a top (not depicted) sealed with multiple collection plenums that may combine to a common exhaust. The non-reactive fluidization gas can be cooled (e.g., upon exit from the heat transfer chamber 102) as needed to meet requirements for a blower operation (such as, for example, to recirculate the nitrogen) and if desired, energy conservation methods such as gas-to-gas interchange with the supplying gas injection nozzle 126a can be used to reduce heat input within heating zone 102a. Prior to the blower, entrained solids may be passed through a cyclone and returned to the heat transfer chamber 102. In the preferred embodiments, the fluidization behavior in the heat transfer chamber may (e.g., should) reside in the bubbling regime (e.g., to reduce the amount of entrained solids leaving the system).
Regarding the solid medium, a Geldart Group A powder form is used, preferably a brown aluminum oxide having a Sauter (or surface-to-volume) mean particle size of 100 pm. This material has good strength and adequate abrasion resistance for the superficial gas velocity range of interest, e.g., approximately 1.2-1.5 times minimum fluidization velocity. Each heating zone 102a-c may have some baffles (e.g., to reduce cross-mixing of solids). Bed level is maintained within each heating zone so as to fully submerge the bundle of reaction tubes 106 when fluidized.
A temperature of the solids in each zone (heating zones 102a-c) may be controlled by varying the power input through the electrical heaters (see
To accommodate thermal expansion, numerous methods can be employed. Differential expansion of the reactor can be on the order of 2 inches at the highest temperatures for a large commercial scale reactor process. Roller supports (such as, for example, the roller support 210 and the roller support 226) may be employed to accommodate thermal expansion. Additional devices could may include steel/graphite slide plates or ceramic (SiC) slide bearings. Optionally, an expansion bellows (not shown) can be incorporated into the vapor outlet 132.
The cooling transition unit 110 may also be a fluidized bed, in a manner similar to that previously described with respect to the heat transfer chamber 102. The floating head 108 is disposed in this separate fluidization zone (e.g., cooling transition unit 110).
The following examples are for illustrative purposes only and are not intended to limit the scope of the appended claims.
To attempt a thermal condensation of trichlorosilane with vinyl chloride, a flow-through reaction tube (316/316L stainless steel) containing an interior liner made of SiC-coated isomolded graphite and an interior multi-element Type K thermocouple assembly with a protective Hexaloy® SiC sheath was assembled. Sealing gland assemblies were used to ensure a seal around the interior liner and a thermocouple sheath, isolating the reactants from the stainless steel reaction tube and a thermocouple assembly. The thermocouple assembly was placed coaxial to the reaction tube, and the reaction tube was submerged inside an electrically-heated, fluidized sand bath system.
Nitrogen was used as the fluidization gas for the sand bath, and fluctuations of feed pressure of nitrogen was monitored to ensure fluidization was uniform. The temperature of the sand bath was specified and controlled to the temperatures listed in
Vinyl chloride and trichlorosilane vapors with a fixed flow of argon were injected into the reaction tube under conditions of fixed reactor pressure and fixed sand bath temperature. Both the inlet and effluent of the reactor was monitored real time using a gas chromatograph (equipped with thermal conductivity detector) and a mass spectrometer. Collected liquids were also analyzed during campaigns of fixed composition. Chemicals detected in the reactor effluent included argon, hydrogen chloride, vinyl chloride, trichlorosilane, vinyl trichlorosilane, silicon tetrachloride, ethyl trichlorosilane, methyl trichlorosilane, vinyldichlorosilane, benzene,1,1,3-trichloro-1-silylcyclo-3-pentene, phenyl trichlorosilane, and 1,2-bis(trichlorosilyl)ethane (abundance of each species varied with temperature).
Using the apparatus described in Example 1, vinyl chloride and dimethylchlorosilane vapors with a fixed flow of argon were injected into the reaction tube under conditions of fixed reactor pressure and fixed sand bath temperature. Both the inlet and effluent of the reactor was monitored real time using a gas chromatograph (equipped with thermal conductivity detector) and a mass spectrometer. Collected liquids were also analyzed during campaigns of fixed composition. Chemicals detected in the reactor effluent include argon, hydrogen chloride, vinyl chloride, dimethylchlorosilane, dimethylvinylchlorosilane, dimethyldichlorosilane, ethyldimethylchlorosilane, methylvinyldichlorosilane, allyldimethylchlorosilane, phenyldimethylchlorosilane, and 1,2-bis(dimethylchlorosilyl)ethane (abundance of each species varied with temperature).
During the experimentation, residence time was held constant (14 seconds) and the reactor pressure was held fixed at 26 psia (176.9 kPa). This reaction is slower than the reaction of trichlorosilane with vinyl chloride. TABLE 1 below shows that the yield of dimethylvinylchlorosilane goes through a maximum near 580° C. with a significant decay in yield of the desired product at 595° C.
It is understood that this disclosure is not limited to the embodiments specifically disclosed and exemplified herein. Various modifications of the invention will be apparent to those skilled in the art. Such changes and modifications may be made without departing from the scope of the appended claims. Moreover, each recited range includes all combinations and sub-combinations of ranges, as well as specific numerals contained therein.
This application claims priority to U.S. Provisional Application Ser. No. 62/908,802, filed Oct. 1, 2019, the entire contents of which are incorporated by reference herein.
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/US2020/053447 | 9/30/2020 | WO |
Number | Date | Country | |
---|---|---|---|
62908802 | Oct 2019 | US |