The present disclosure relates to generation of electrical power using fuel cells. More particularly, the present disclosure provides a novel way to manufacture fuel cell bipolar plates with the advantage of rapid prototyping, one piece design, hollow structures and weight savings, as well as providing an assembly procedure to reduce contact resistance.
Previous state of the art processes for manufacturing fuel cell bipolar plates include machining together molded carbon and formed metal foils. The major limitation of these past processes is that they require expensive tooling that cannot be reconfigured rapidly to incorporate new design. These processes lead to two piece bipolar plates that require an extra set of gasket seals and grooves needed to seal the fuel cell stack in the assembly steps to build a functioning fuel cell. Specifically, creating a typical bipolar plate involves welding together at least two pieces. This welded portion is then provided with gasket seals, which can leak or otherwise become damaged, in addition to forming grooves in the welded portion to accommodate the seals.
In one embodiment, a bipolar plate for a fuel cell is provided. The bipolar plate includes a main body with a first end and a second end spaced from the first end along a longitudinal axis of the main body. At least one inlet is disposed at the first end of the main body. At least one outlet corresponding to the at least one inlet is disposed at the second end of the main body. At least one continuous flow path extends from the at least one inlet to the at least one outlet. The main body comprises a single, contiguous piece.
In another embodiment, a bipolar plate for a fuel cell is provided. The bipolar plate includes a main body with a first end and a second end spaced from the first end along a longitudinal axis of the main body. At least one inlet is disposed at the first end of the main body. At least one outlet corresponding to the at least one inlet is disposed at the second end of the main body. At least one continuous flow path extends from the at least one inlet to the at least one outlet. The at least one continuous flow path has a corrugated, I-beam shape. A reactant boss seal is in fluid communication with the at least one continuous flow path. The reactant boss seal provides fluid communication between the at least one continuous flow path and the at least one inlet. The main body comprises a single, contiguous piece.
In another embodiment, a method of manufacturing a bipolar plate for a proton exchange membrane fuel cell is provided. The method includes designing a bipolar plate for a fuel cell in which the bipolar plate including at least one continuous flow path; three-dimensionally printing the bipolar plate with a direct metal laser sintering process in which the bipolar plate being printed as a single, contiguous piece; polishing the bipolar plate; and surface-coating the bipolar plate.
Proton exchange membrane fuel cells are devices used to generate electrical power from the reaction of hydrogen with oxygen. In a proton exchange fuel cell, an oxidation-reduction reaction occurs in which hydrogen gas (which serves as fuel) is dissociated to form two protons and two electrons. The protons react with one oxygen atom (provided from oxygen gas (O2) present in the air). The remaining two electrons pass through an external circuit to provide electromotive force and complete the reaction with oxygen to form water and heat. Typical bipolar plates include one or more inlets to receive the hydrogen fuel, oxygen gas, and water (which serves as a coolant for the fuel cell). Specifically, there is one inlet for the hydrogen fuel, one inlet for the air, and one inlet for the water. Each inlet interacts with a corresponding outlet. The inlets are in fluid communication with the corresponding outlets via a flow path that traverses a portion of the bipolar plate.
The objective of this disclosure is to create bipolar plates for fuel cells with the advantages of: (1) rapid prototyping; (2) one piece design; (3) hollow structures; (4) possible weight savings; and (5) providing an assembly procedure to reduce contact resistance, shown from the design of solid models of the plates. As a result, a bipolar plate can be rapidly built from a base powder material, and the final bipolar plate is manufactured as one piece. For example, the bipolar plate can be manufactured using three-dimensional (3D) printing, as described in more detail below. A direct metal laser sintering process can be used to 3D print (i.e. build) the bipolar plate. In some embodiments, the bipolar plate includes a printed reactant boss seal to provide sealing and reactant flow therethrough. The bipolar plate includes a hollow flow path that that allows for the removal of powder after the sintering process. Advantageously, once the bipolar plate is formed, it can be assembled with any standard fuel cell that is known in the art. The assembly process uses compressive cycling to minimize the contact resistance. An optimal range of surface finishes can be 1.5 to 5 Sa microns.
The main body 12 can be substantially made from a base material, such as a Ti-6Al-4V alloy; however, it will be appreciated that main body can comprise another suitable alloy or combination of alloys (e.g., 316 stainless steel, commercially pure titanium (TiCP) and aluminum alloy (AlSi10Mg), austenitic steels, ferrous steels, aluminum alloys, titanium alloys, pure aluminum and pure titanium and the like). The main body 12 can have dimensions ranging from approximately 40 mm to approximately 100 mm in width, and from approximately 80 mm to approximately 120 mm in length. For example, the main body 12 can have a width of approximately 40.0 mm (inclusive), and a length of approximately 80.0 mm (inclusive). However, it will be appreciated that the main body 12 can have any suitable dimensions to allow: (1) the at least flow path 22 to be disposed within the main body; and (2) allow the bipolar plate 10 to be a component of a fuel cell (not shown). The main body 12 is sized and dimensioned such that the at least one flow path 22 extends across a portion of the width of the main body and extends across a portion of the length of the main body, depending on the selected dimensions of the main body 12. The main body 12 includes a portion over which the at least one flow path 22 does not extend across to accommodate the inlets and the outlets 18 and 20 (e.g., typical approximately 7.5 mm of the length and the width of the main body 12). For example, the at least one flow path 22 can extend across a portion of the width of the main body 12, ranging from approximately 33 mm to approximately 68 mm, and across a portion of the length of the of the main body, ranging from approximately 65 mm to approximately 105 mm. Advantageously, the main body 12 of the bipolar plate 10 can be formed as a single, contiguous piece, as described in more detail below.
Referring to
Additionally,
At 52, the bipolar plate 10 is designed for a fuel cell, such as a proton exchange membrane fuel cell. The bipolar plate 10 can be designed on a computer. This allows the bipolar plate 10 to be printed with a 3D printer that is connected to the computer. The bipolar plate 10 can be designed (as described above) to include the main body 12 with the flow path 22 that fluidly connects the inlets 18 and the outlets 20. The bipolar plate 10 can be designed to additionally and optionally include at least one of the reactant boss seal 28 and the mixing tabs 34 (each of which is described above). As such, it will be appreciated that multiple designs of the bipolar plate 10 can be generated.
At 54, the bipolar plate 10 is three-dimensionally printed with a direct metal laser sintering process (or any other suitable process, such as electron beam melting). The main body 12 of the bipolar plate 10 can be three-dimensionally printed with at least a Ti-6Al-4V alloy (or any other suitable alloy or combination of alloys). During the direct metal laser sintering process, the continuous flow path 22 is formed within the solid interior 24 of the main body 12. The continuous flow path 22 can be formed to include at least one of: (1) a corrugated, I-beam cross-sectional shape; and (2) a triple serpentine flow path that substantially extends across a length of the main body 12. Advantageously, the bipolar plate 10 can be printed as a single, contiguous piece, thereby creating a bipolar plate that does not have at least two pieces welded together and provided with gasket seals and corresponding grooves. Additionally, at 54, the at least one mixing tab 34 can be formed within the continuous flow path 22. Advantageously, the mixing tabs 34 can help remove bubbles during fluid flow through the flow path 22. Additionally, the reactant boss seal 28 can be formed within the continuous flow path 22. Advantageously, (1) the reactant boss seal 28 provides fluid communication between the flow path 22 and the inlets 20, and (2) can only be formed by 3D design and printing, since the welding of two metal pieces to form a bipolar plate would prevent the reactant boss seal from being formed in such a bipolar plate.
At 56, the bipolar plate 10 is polished. Specifically, the exterior surface 26 of the main body 12 is polished. The main body 12 can be polished with at least one of a physical polishing process, an electro-polishing process, and a mechanical-physical-catalyst process, (although any other suitable polishing process can be used). Preferably, the mechanical-physical catalyst polishing process is used. The exterior surface 26 of the main body 12 can be polished to include a surface roughness between approximately 1.5 Sa microns (inclusive) to approximately 5.0 Sa microns (inclusive).
At 58, the bipolar plate 10 is surface-coated. Specifically, the exterior surface 26 of the main body 12 is surface-coated after the exterior surface is polished. The surface-coating advantageously enhances electron conductivity and retard corrosion, thereby minimizing contact resistance through surface coatings, corrosion protection and proper surface finish. The exterior surface 26 can be surface coated with at least one of a gold-sputtering process, a coat electro-deposited coating process, a nitride coating process, and a TiO2/gold nano-dot coating process. Preferably, the TiO2/gold nano-dot coating process is used using TiO2/gold nano-dot coatings available from TREADSTONE TECHNOLOGIES, INC. (Princeton, N.J., U.S.A.). Such TiO2/gold nano-dot coatings are described in U.S. Patent Publication No. 2014/0224650, which is incorporated herein by reference in its entirety.
At 60, after three-dimensionally printing the bipolar plate 10 with a direct metal laser sintering process (54), a fluid is flowed through the continuous flow path 22. The fluid can be any suitable liquid (e.g., water) or gas (e.g., air), and is flowed through the flow path 22 to remove any debris (such as powder) that is disposed within the flow path. During formation of the bipolar plate 10 (and specifically the flow path 22), powder from the base material (e.g., the Ti-6Al-4V alloy) can collect within the flow path. The fluid is flowed through the flow path 22 to remove this powder, and any other debris disposed therein, so that air can flow uninterrupted through the flow path from the inlets 18 to the outlets 20.
At 62, the bipolar plate 10 is assembled into a fuel cell (not shown). For example, at least one bipolar plate 10 is sandwiched between at least one catalyst coated membrane (not shown) and at least one gas diffusion layer (not shown). One or more gaskets (not shown) can be disposed between the bipolar plate(s) 10 and the catalyst coated membrane or gas diffusion layer. The fuel cell (including the bipolar plates 10) is then compressed together and secured with screws. However the fuel cell can be secured with any suitable attachment mechanism (e.g., magnets, buckles, hook and loop arrangements, straps, snaps, and the like.
At 64, after the bipolar plate 10 is assembled into the fuel cell, a mechanical cycling process is performed to reduce contact resistance between the bipolar plate and the remainder of the fuel cell. Multiple fuel cells can be assembled together to form a stack. Assembly of the bipolar plates into a stack of cells is common practice for those skilled in the art. After the stack is assembled it is important consider compressive strength by compressing the whole assembly to >1.0 mega-pascal (MPa) and released to <0.25 MPa and returned to >1.0 MPa. The processes are known in the art.
The results summarizing the performance of the design of the bipolar plate 10 against a bipolar plate made from a carbon baseline material are presented in
It will be appreciated that the processes 52-62 can be performed in any suitable order, except as specified above. For example, flowing the fluid through the flow path 22 (described at 60) can be performed before polishing the bipolar plate 10 (described at 56) and/or surface-coating the bipolar plate (described at 58). Additionally, forming the mixing tabs 34 and/or the reactant boss seal 28 can be optionally performed as sub-processes of the direct laser sintering process (described at 54).
This disclosure could apply to electron beam melting or any other additive manufacturing process used to form parts from electronically conductive materials. Although the preferred embodiment of this disclosure is for use in fuel cells it could be used in any other gas-electrode application.
The foregoing description of the specific embodiments will so fully reveal the general nature of the disclosure that others can, by applying knowledge within the art, readily modify and/or adapt for various applications such specific embodiments, without undue experimentation, without departing from the general concept of the present disclosure. Therefore, such adaptations and modifications are intended to be within the meaning and range of equivalents of the disclosed embodiments claimed herein and below, based on the teaching and guidance presented herein and the claims which follow:
The present application is related to, and claims the benefit of priority to, U.S. Provisional Application No. 62/057,337, entitled PROTON EXCHANGE MEMBRANE FUEL CELL WITH 3-D PRINTED BIPOLAR PLATES, filed on Sep. 30, 2014, having at least two of the same inventors Benjamin D. Gould and Joseph A. Rodgers and assigned to the same entity, i.e., the U.S. Government, as the present disclosure, and is herein incorporated by reference in its entirety.
Number | Name | Date | Kind |
---|---|---|---|
5186806 | Clark | Feb 1993 | A |
5616431 | Kusunoki et al. | Apr 1997 | A |
6261710 | Marianowski | Jul 2001 | B1 |
6838202 | Brady et al. | Jan 2005 | B2 |
6974648 | Goebel | Dec 2005 | B2 |
7306875 | Garceau | Dec 2007 | B2 |
7459227 | Rock et al. | Dec 2008 | B2 |
7781087 | Rock et al. | Aug 2010 | B2 |
7805834 | White et al. | Oct 2010 | B2 |
8158299 | Blank et al. | Apr 2012 | B2 |
8236461 | Gao | Aug 2012 | B2 |
8263259 | Kearl | Sep 2012 | B2 |
8389182 | Owejan et al. | Mar 2013 | B2 |
8450023 | Conti et al. | May 2013 | B2 |
8501364 | Owejan et al. | Aug 2013 | B2 |
8623565 | Das et al. | Jan 2014 | B2 |
8889314 | Connor et al. | Nov 2014 | B2 |
20030203260 | Lee | Oct 2003 | A1 |
20040209150 | Rock | Oct 2004 | A1 |
20050260473 | Wang | Nov 2005 | A1 |
20060134502 | Garceau | Jun 2006 | A1 |
20090092872 | Miyazawa | Apr 2009 | A1 |
20100035118 | Sato | Feb 2010 | A1 |
20110207026 | Tseng et al. | Aug 2011 | A1 |
20120183881 | Sugita | Jul 2012 | A1 |
20130089809 | Farrington | Apr 2013 | A1 |
Number | Date | Country |
---|---|---|
102013221012 | Apr 2015 | DE |
Number | Date | Country | |
---|---|---|---|
20160093898 A1 | Mar 2016 | US |
Number | Date | Country | |
---|---|---|---|
62057337 | Sep 2014 | US |