Claims
- 1. A method for modifying residual cornering force or residual self-aligning torque of a tire, said tire to be molded by a tire mold, said tire mold for forming treads on the surface of said tire, said tire mold forming tread elements on the surface of a tread of said tire, said tread elements having tread edges, said mold having a plurality of selectively removable insert portions effective to chamfer said tread edges, said method comprising the steps of:
- choosing predetermined insert portions to modify the residual cornering force or residual self-aligning torque of said tire, and;
- removing the predetermined insert portions of said mold such that selected edges of said tread elements are unchamfered partially or completely.
- 2. The method for modifying residual cornering force or residual self-aligning torque of tires of claim 1 further comprising the steps of:
- measuring residual cornering force of a first tire produced by said tire mold;
- comparing the measured residual cornering force for sa id first tire produced by said tire mold to a specification range of residual cornering force;
- removing an insert portion of said tire mold if the measured residual cornering force is outside the specification range;
- molding a second tire in said mold;
- measuring residual cornering force of said second tire produced by said tire mold;
- comparing the measured residual cornering force for said second tire produced by said tire mold to a specification range of residual cornering force; and,
- removing additional insert portions of said mold until the measured residual cornering force is within the specification range.
- 3. A method for modifying residual cornering force or residual self-aligning torque of tires, said tires to be molded by a tire mold, said tire mold comprising a plurality of recesses for forming treads on the surface of said tires, said method comprising the steps of:
- measuring residual cornering force of a first tire produced by said tire mold;
- comparing the measured residual cornering force for said first tire produced by said tire mold to a specification range of residual cornering force;
- installing a chamfering means for chamfering said treads in said tire mold if the measured residual cornering force is outside the specification range;
- molding a second tire in said mold;
- measuring residual cornering force of said second tire produced by said tire mold;
- comparing the measured residual cornering force for said second tire produced by said tire mold to a specification range of residual cornering force; and,
- adjusting said chamfering means until the measured residual cornering force is within the specification range.
Parent Case Info
This is a division, of application Ser. No. 08/588,036, filed Jan. 17, 1996.
US Referenced Citations (9)
Foreign Referenced Citations (2)
Number |
Date |
Country |
599566 |
Jun 1994 |
EPX |
3-186405 |
Aug 1991 |
JPX |
Divisions (1)
|
Number |
Date |
Country |
Parent |
588036 |
Jan 1996 |
|