The present application claims priority of China Patent application No. 201710008242.9 filed on Jan. 5, 2017, the content of which is incorporated in its entirety as portion of the present application by reference herein.
At least one embodiment of the present disclosure relates to a touch panel, a manufacturing method thereof, and a display device.
Currently, touch panel technology generally has the following types: capacitive type, resistive type, optical type, electromagnetic type, ultrasonic type and so on. In general, a capacitive touch panel includes a self-capacitive touch panel and a mutual-capacitive touch panel. The self-capacitive touch panel includes a touch electrode array made of a transparent conductive material on a base substrate, these touch electrodes respectively form the capacitance with the ground. Upon a finger touching the self-capacitive touch panel, the capacitance of the finger will be superimposed on a corresponding touch electrode. A touch detection chip can determine a touch position by detecting the change of a capacitance value of each of the touch electrodes in a touch time period. The mutual-capacitive touch panel includes a horizontal electrode and a vertical electrode which are insulated from each other and made of a transparent conductive material on a base substrate, and a capacitance is formed on a position where the two electrodes intersect with each other. Upon a finger touching the touch panel, a coupling between the two electrodes near a touch point is affected, thereby changing a capacitance value between the two electrodes. A touch detection chip can determine the touch position by detecting the change of the capacitance value in a touch time period.
In general, the touch display device can be divided into two types, such as an on-cell type and an in-cell type, according to a relationship between the touch structure and a display panel. A typical one glass solution (OGS) touch panel belongs to an on-cell type touch panel, and is a technology that directly forming an indium tin oxide (ITO) conductive film and a sensor on a protective glass, wherein one glass simultaneously plays a dual role of protecting the glass and the sensor.
At least one embodiment of the present disclosure provides a touch panel and a manufacturing method thereof, and a display device. In the touch panel, the longest lead in a plurality of leads adopts a transparent conductive layer lead, which can reduce the influence of particles on the leads, and decrease the probability of the electrical test failure caused by particles without increasing the number of processes, thereby saving costs and improving yield.
At least one embodiment of the present disclosure provides a touch panel, which includes a base substrate, the base substrate includes a touch area and a lead end area; the touch area is provided with a plurality of first electrodes and a plurality of second electrodes, and the second electrodes are intersected and insulated with the first electrodes; a plurality of leads, electrically connected with the plurality of first electrodes and the plurality of second electrodes respectively, and connected to the lead end area, and the plurality of leads include a transparent conductive layer lead.
At least one embodiment of the present disclosure provides a display device, which includes the abovementioned touch panel.
At least one embodiment of the present disclosure provides a manufacturing method a touch panel, which including: forming a touch area and a lead end area on a base substrate; forming a plurality of first electrodes in the touch area; forming a plurality of second electrodes in the touch area, and the plurality of second electrodes are intersected and insulated with the plurality of first electrodes; forming a plurality of leads on an edge of the touch area, the plurality of leads are electrically connected with the plurality of first electrodes and the plurality of second electrodes respectively, and connected to the lead end area, and the plurality of leads include a transparent conductive layer lead.
In order to clearly illustrate the technical solution of embodiments of the present disclosure, the drawings of the embodiments or related technical description will be briefly described in the following, it is obvious that the drawings in the description are only related to some embodiments of the present disclosure and not limited to the present disclosure.
10—base substrate; 11—touch area; 12—lead end area; 20—first electrode; 30—second electrode; 40—lead; 60—black matrix; 70—transparent conductive bridge; 80—insulating layer; 100—base substrate; 110—touch area; 120—lead end area; 200—first electrode; 210—first sub-electrode; 300—second electrode; 310—second sub-electrode; 320—connection portion; 400—lead; 410—transparent conductive layer lead; 420—metal lead; 421—first metal lead; 422—second metal lead; 430—first lead; 431—first transparent conductive layer lead; 440—second lead; 441—second transparent conductive layer lead; 500—first insulating layer; 510—lap portion; 600—black matrix; 700—transparent conductive bridge; 800—second insulating layer; 900—lap lead.
In order to make objects, technical details and advantages of the embodiments of the disclosure apparent, the technical solutions of the embodiments will be described in a clearly and fully understandable way in connection with the drawings related to the embodiments of the disclosure. Apparently, the described embodiments are just a part but not all of the embodiments of the disclosure. Based on the described embodiments herein, those skilled in the art can obtain other embodiment(s), without any inventive work, which should be within the scope of the disclosure.
Unless otherwise defined, all the technical and scientific terms used herein have the same meanings as commonly understood by one of ordinary skill in the art to which the present disclosure belongs. The terms “first,” “second,” etc., which are used in the present disclosure, are not intended to indicate any sequence, amount or importance, but distinguish various components. Also, the terms “comprise,” “comprising,” “include,” “including,” etc., are intended to specify that the elements or the objects stated before these terms encompass the elements or the objects and equivalents thereof listed after these terms, but do not preclude the other elements or objects. “On,” “under,” “left,” “right” and the like are only used to indicate relative position relationship, and when the position of the object which is described is changed, the relative position relationship may be changed accordingly.
In a study, the inventor(s) of the present application has found that during the deposition or photolithographic processes for manufacturing metal leads, because the line width of the leads is relatively narrow, the leads are easy to be blocked by particles, thereby causing the electrical test failure, for example, an open circuit or a short circuit phenomenon. Furthermore, the longer the length of the leads, the greater the probability of the leads being blocked by the particles, and the greater the probability of generating the electrical test failure.
At least one embodiment of the present disclosure provides a touch panel and a manufacturing method thereof, and a display device. The touch panel includes a base substrate, the base substrate includes a touch area and a lead end area; the touch area is provided with a plurality of first electrodes and a plurality of second electrodes, and the second electrodes are intersected and insulated with the first electrodes; a plurality of leads, electrically connected with the plurality of first electrodes and the plurality of second electrodes respectively, and connected to the lead end area, and the plurality of leads include a transparent conductive layer lead. In the touch panel, the longest lead in the plurality of leads adopts the transparent conductive layer lead, which can reduce the influence of particles on the leads, and decrease the probability of the electrical test failure caused by particles without increasing the number of processes, thereby saving cost and improving yield.
Hereafter, the touch panel, the manufacturing method thereof, and the display device provided by the embodiments of the present disclosure will be described with reference to the accompanying drawings.
An embodiment of the present disclosure provides a touch panel, as illustrated in
In general, the longer a length of a lead, the greater the probability of the lead being blocked by particles, and greater the probability of generating the electrical test failure. Therefore, in the present embodiment, the transparent conductive layer lead 410 can be utilized to replace a lead electrically connected with the first electrode 200 which is farthest from the lead end area 120, that is, a lead having the longest length, so as to prevent the lead having the longest length from being blocked by particles, prevent the touch panel from encountering a short circuit or an open circuit phenomenon during electrical test or actual use, and the product yield of the touch panel provided by the present embodiment can also be improved. Certainly, the embodiment of the present disclosure includes but is not limited thereto, the transparent conductive layer lead can be further electrically connected with a second electrode which is farthest from the lead end area.
For example, the touch panel provided by an example of the present embodiment, as illustrated in
For example, the transparent conductive layer lead has a width range of 0.5 cm-1.5 cm. For example, upon a material of the transparent conductive layer lead adopting indium tin oxide (ITO), the sheet resistance Rs of the general indium tin oxide is about 18±4 Ω/□, the present embodiment takes a case where the width of the transparent conductive layer lead is 1.5 cm as an example to calculate that the line resistance of the transparent conductive layer lead is approximately 12000 Ω/m; the sheet resistance of a general metal lead is about 0.3±0.05 Ω/□, a line width of the general metal lead is about 30 μm, and then it is calculated that the line resistance of the general metal lead is approximately 10000 Ω/m. Comparing the line resistance of transparent conductive layer lead and the general metal lead, it can be found that the line resistance of the two is not much different. Therefore, a case of replacing the longest metal lead with the transparent conductive layer lead cannot increase the resistance, and has little effect on the line resistance of the touch panel. Furthermore, because a size of the particles is much less than 0.5 cm-1.5 cm, the particles cannot block the transparent conductive layer lead, thereby greatly reducing or even eliminating the probability of the transparent conductive layer lead. being blocked, and then the product yield of the touch panel can be improved.
For example, as illustrated in
For example, as illustrated in
For example, as illustrated in
For example, as illustrated in
For example, as illustrated in
For example, as illustrated in
It should be noted that, as illustrated in
For example, as illustrated in
For example, a material of the transparent conductive layer lead 410 can be the same as a material of the transparent conductive bridge 700, for example, the material of the two can be indium tin oxide and so on, the present embodiment is not limited thereto. That is, the transparent conductive layer lead 410 and the transparent conductive bridge 700 can be simultaneously formed through a patterning process, so as to decrease the probability of the electrical test failure caused by particles without increasing the number of processes, thereby saving cost and improving yield.
Another embodiment of the present disclosure provides a touch panel, which is different from the abovementioned embodiment is that, the transparent conductive bridge 320 is disposed on the connection portion 320 in the present embodiment.
For example, as illustrated to
For example, the plurality of first leads 430 further include a plurality of first metal leads 421; the plurality of second leads 440 further include a plurality of second metal leads 422.
For example, the plurality of first leads 430 and the plurality of second leads 440 are connected to a touch detection chip, the touch detection chip inputs/receives a signal through the leads, and determines the touch position by analyzing received signals of each touch electrode.
The longest leads of the plurality of first leads 430 and the plurality of second leads 440 in the touch panel provided by the present embodiment adopt the first transparent conductive layer lead 431 and the second transparent conductive layer lead 441, which can reduce the influence of particles on the leads; on the other hand, the first transparent conductive layer lead 431 and the second transparent conductive layer lead 441 can be disposed in the same layer with the transparent conductive bridge 700, for example, they can be simultaneously formed through a patterning process, so as to decrease the probability of the electrical test failure caused by particles without increasing the number of processes, thereby saving cost and improving yield. In addition, the first transparent conductive layer lead 431 and the plurality of first metal leads 421 are disposed on different layers, and an orthogonal projection of the first metal leads 421 on the base substrate 100 falls within an orthogonal projection of the first transparent conductive layer lead 431 on the base substrate 100; the second transparent conductive layer lead 441 and the plurality of second metal leads 422 are disposed in different layers, and an orthogonal projection of the second metal leads 422 on the base substrate 100 falls within an orthogonal projection of the second transparent conductive layer lead 441 on the base substrate 100, so as to reduce the width of the leads arranged on an edge of the touch panel, thereby achieving a narrow frame design.
An embodiment of the present disclosure provides a manufacturing method of a touch panel, flow diagram and the specific steps are illustrated in
S401: forming a touch area and a lead end area on a base substrate.
For example, the base substrate can be made of one or more materials, such as glass, polyimide, polycarbonate, polyacrylates, polyetherimide, polyethersulfone, polyethylene terephthalate, and polyethylene naphthalate.
S402: forming a plurality of first electrodes in the touch area.
S403: forming a plurality of second electrodes in the touch area, and the plurality of second electrodes are intersected and insulated with the plurality of first electrodes.
S404: forming a plurality of leads on an edge of the touch area, the plurality of leads are electrically connected with the plurality of first electrodes and the plurality of second electrodes respectively, and connected to the lead end area, the plurality leads include a transparent conductive layer lead.
In the manufacturing method of the touch panel provided by the present embodiment, a width of the transparent conductive layer lead is wider than that of a general lead, so as to decrease the probability of the transparent conductive layer lead being blocked by the particles and the electrical test failure, and prevent the occurrence of a short circuit or an open circuit phenomenon, so that the product yield can be improved.
In general, the longer the length of the leads, the greater the probability of that the leads being blocked by the particles, and the greater the probability of generating the electrical test failure. Therefore, the present embodiment can make a lead electrically connected with the first electrode and/or the second electrode farthest from the lead end area, that is, a lead having the longest length, as the transparent conductive layer lead, so as to prevent the lead having the longest length from being blocked by particles, and prevent the touch panel from encountering a short circuit or an open circuit phenomenon during electrical test or actual use, and the product yield of the touch panel provided by the present embodiment can also be improved. Certainly, the embodiment of the present disclosure includes but is not limited thereto, the transparent conductive layer lead can further electrically connected with the second electrode farthest from the lead end area.
For example, in the manufacturing method of the touch panel provided by an example of the present embodiment, the plurality of leads further include metal leads, the manufacturing method further includes: forming a first insulating layer between the metal leads and the transparent conductive layer lead. Thus, the first insulating layer can insulate the metal leads and the transparent conductive layer lead from each other. And because the transparent conductive layer lead and the plurality of metal leads are disposed on different layers, an orthogonal projection of the transparent conductive layer lead on the base substrate can be overlapped with an orthogonal projection of the plurality of metal leads on the base substrate. Thus, the width of the transparent conductive layer lead can be set wider without increasing the width of the edge of the touch area, so as to not only ensure good conductivity, but also greatly decrease the probability of the leads being blocked by the particles and generating the electrical test failure.
For example, in the manufacturing method of the touch panel provided by an example of the present embodiment, each of the plurality of first electrodes includes a plurality of first sub-electrodes disposed at intervals, each of the plurality of second electrodes includes a plurality of second sub-electrodes and a connection portion disposed between two adjacent ones of the plurality of second sub-electrodes, the manufacturing method further includes: forming a transparent conductive bridge between two adjacent ones of the plurality of first sub-electrodes to electrically connect the two adjacent ones of the plurality of first sub-electrodes; the transparent conductive layer lead is formed simultaneously with the transparent conductive bridge or the connection portion through a patterning process. Thus, the manufacturing method of the touch panel does not increase a new preparation process compared with a general process; and a width of the transparent conductive layer lead is wider than that of a general lead, so as to decrease the probability of the electrical test failure caused by particles without increasing the number of processes, and prevent the occurrence of a short circuit or an open circuit phenomenon, thereby saving cost and improving the product yield.
For example, the manufacturing method of the touch panel provided by an example of the present embodiment further includes: forming a second insulating layer between the connection portion and the transparent conductive bridge, the first insulating layer and the second insulating layer are simultaneously formed through a patterning process. Thus, the manufacturing method of the touch panel does not increase a new preparation process compared with a general process, so as to save the cost.
As illustrated in
For example, a base material of the black matrix 600 can be chromium and so on, and can also be acrylic resin mixed with black pigment (mainly carbon), for example, a black resin containing carbon, titanium, nickel and other raw materials can be incorporated in the photoresist. It should be noted that, a second view of
As illustrated in
As illustrated in
As illustrated in
As illustrated in
As illustrated in
As illustrated in
For example, each of the first electrodes 200 includes a plurality of first sub-electrodes 210 disposed at interval. For example, the plurality of first sub-electrodes 210 disposed at interval are arranged in an array, adjacent ones of the plurality of first sub-electrodes 210 arranged in the X direction are electrically connected with each other through the transparent conductive bridge 700, therefore, a column of the plurality of first sub-electrodes 210 arranged in the X direction constitutes one first electrode 200, the present embodiment is not limited thereto.
For example, each of the second electrodes includes a plurality of second sub-electrodes 310 and a connection portion 320 disposed between adjacent ones of the plurality of second sub-electrodes. For example, adjacent ones of the plurality of second sub-electrodes 310 arranged in the Y direction are electrically connected with each other through the connection portion 320, therefore, a row of the plurality of second sub-electrodes 310 arranged in the Y direction and the plurality of connection portion 320 constitute one second electrode 300, the present embodiment is not limited thereto.
For example, the plurality of first electrodes 200 and the plurality of second electrodes 300 can be transparent conductive layers. For example, a selected material of the two includes transparent conductive oxide, for example, the transparent conductive oxide can include a combination or at least one selected from the group consisting of indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO) indium oxide (In2O3), indium gallium oxide (IGO), and aluminum zinc oxide (AZO), the embodiment of the present disclosure is not limited thereto. Certainly, the plurality of first electrodes 200 and the plurality of second electrodes can also be thin transparent metal layers, for example, a thickness of the transparent metal layers has a range of 10 nm-20 nm.
As illustrated in
As illustrated in
For example, in the manufacturing method of the touch panel provided by an example of the present embodiment, after forming the plurality of leads, the method further includes forming a protective layer (which is not illustrated in figures) on the touch panel. For example, a material of the protective layer can be photoresist and so on, the present embodiment is not limited thereto.
It should be noted that, the abovementioned preparation steps are only schematic steps, the present embodiment is not limited thereto, the steps can further include a step of forming two transparent conductive layer leads, and the corresponding steps will also be slightly different, which is not repeated herein.
An embodiment of the present disclosure provides a display device. The display device includes the touch panel in any of the abovementioned embodiments. The longest lead among the plurality of leads in the touch panel of the display device adopts the transparent conductive layer lead, which can reduce the influence of particles on the leads, and decrease the probability of the electrical test failure caused by particles without increasing the number of processes, thereby saving cost and improving yield. In addition, the transparent conductive layer lead and the plurality of metal leads are disposed on different layers, and an orthogonal projection of the metal leads on the base substrate falls within an orthogonal projection of the transparent conductive layer lead on the base substrate, so as to reduce the width of the leads arranged on an edge of the touch panel, thereby achieving a narrow frame, design.
For example, the display panel includes a liquid crystal display panel or a light emitting diode display device.
For example, the display device can be a display device such as a liquid display device, an electronic paper, a light emitting diode display device, etc., and any product or component having a display function such as a television, a digital camera, a mobile phone, a watch, a tablet computer, a notebook computer, a navigator, or the like including these display devices.
The following points should to be explained:
(1) Unless otherwise defined, in the embodiments and accompanying drawings in the present disclosure, the same reference numeral represents the same meaning.
(2) The accompanying drawings involve only the structure(s) in connection with the embodiment(s) of the present disclosure, and other structure(s) can be referred to common design(s).
(3) For the purpose of clarity, in accompanying drawings for illustrating the embodiment(s) of the present disclosure, layer(s) or area(s) may be enlarged. However, it should understood that, the case in which a component or element such as a layer, film, area, substrate or the like is referred to be “on” or “under” another component or element, it may be directly on or under the another component or element or a component or element is interposed therebetween.
The foregoing is only the embodiments of the present invention and not intended to limit the scope of protection of the present invention, alternations or replacements which can be easily envisaged by any skilled person being familiar with the present technical field shall fall into the protection scope of the present disclosure. Thus, the protection scope of the present disclosure should be based on the protection scope of the claims.
Number | Date | Country | Kind |
---|---|---|---|
201710008242.9 | Jan 2017 | CN | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/CN2017/107358 | 10/23/2017 | WO | 00 |