This application claims the priority benefit of Japanese Patent Application No. 2018-151600, filed on Aug. 10, 2018. The entirety of the above-mentioned patent application is hereby incorporated by reference herein and made a part of this specification.
The present disclosure relates to a transfer method.
Conventionally, when transferring a metal foil onto a medium, for example, a method of placing a transfer sheet including a metal foil layer and an adhesive layer on a transfer target surface of the medium, and irradiating the transfer sheet with a laser light while the transfer sheet is pressed against the transfer target surface by a pressure welding sheet is known (see e.g., Internet URL: https://www.rolanddg.com/en/news/2018/180316-dgshape-launches-worlds-first-laser-foil-decorator, Non-Patent Literature 1). In this method, the pressure welding sheet or the transfer sheet generate heat by receiving the laser light, which heat causes the adhesive layer to soften and adhere to the transfer target surface. Thus, the metal foil of a part subjected to the laser light is transferred to the transfer target surface.
Non-Patent Literature 1:
Internet URL: https://www.rolanddg.com/en/news/2018/180316-dgshape-launches-worlds-first-laser-foil-decorator
In the transfer method described above, a configuration in which the pressure welding sheet is stretched across an inner peripheral side of a frame member is adopted, and the pressure welding sheet pressure welds the transfer sheet by pressing the frame member against the medium side. Thus, when transferring the metal foil to a medium having uneven transfer target surface, it is difficult to sufficiently pressure weld the pressure welding sheet to a bottom portion of a recess of the transfer target surface, and it is difficult to transfer the metal foil with high accuracy.
In light of the foregoing, the present disclosure provides a transfer method capable of transferring a transfer layer with high accuracy even to a medium having uneven transfer target surface.
A transfer method according to the present disclosure includes a disposing step of disposing a transfer sheet and a medium in an inside of a sealed space, and the sealed space is formed using a pressure welding sheet having flexibility in at least one part, and the transfer sheet and the medium are disposed so that an adhesive layer of the transfer sheet and a transfer layer of the transfer sheet are layered, and the adhesive layer has a thermally melting property, and the adhesive layer is contacted with the medium; a pressure welding step of suctioning the inside of the sealed space by a negative pressure and pressure welding the pressure welding sheet and the medium by the negative pressure to closely attach the transfer sheet and the medium; an irradiating step of softening the adhesive layer by irradiation of a light ray generated from a light source in a state the transfer sheet is closely attached to the medium by the pressure welding sheet and adhering the adhesive layer to the medium by a pressure welding force from the pressure welding sheet; and a peeling step of peeling off the transfer sheet from the medium after the irradiating step.
In this configuration, the transfer sheet can be pressure welded to the medium in a state the pressure welding sheet is deformed so as to follow an uneven portion of a transfer target surface of the medium by generating the negative pressure between the flexible pressure welding sheet and the medium. Thus, the transfer layer can be transferred with high accuracy even to the medium on which the uneven portion is formed.
In the transfer method described above, the pressure welding sheet may be formed of a member that transmits the light ray, and in the irradiating step, the light ray may be incident from a side of the transfer sheet.
Thus, the light ray generated from the light source can easily reach the transfer layer of the transfer sheet.
In the transfer method described above, the transfer layer may be formed of a metal foil layer, and in the irradiating step, the adhesive layer may be thermally melted when a heat generating layer disposed on a front side in an incident direction of the light ray in the metal foil layer generates heat by the light ray.
Thus, the heat generating layer can be provided above the metal foil layer which does not transmit light, and the heat generating layer is may be caused to generate heat by a light ray to thermally fuse the adhesive and easily transfer the metal foil layer. Therefore, for example, the metallic color can be easily formed on the medium M.
In the transfer method described above, the heat generating layer may be formed on the pressure welding sheet.
Thus, the handling property of the pressure welding sheet can be improved.
In the transfer method described above, the pressure welding step may include: accommodating the medium and the transfer sheet in an inside of a bag body formed by using the pressure welding sheet, and generating the negative pressure between the pressure welding sheet and the medium by suctioning the inside of the bag body.
Accordingly, the negative pressure is generated between the pressure welding sheet and the medium without requiring a complicated operation.
In the transfer method described above, the transfer method may further include: a mounting step of mounting the medium on a mounting portion of a jig formed with the mounting portion for mounting the medium. In the pressure welding step, the inside of the sealed space may be suctioned by the negative pressure, and the pressure welding sheet and the jig may be pressure welded by the negative pressure to closely attach the transfer sheet and the medium.
Thus, the deformation of the medium can be suppressed when generating the negative pressure between the pressure welding sheet and the medium.
In the transfer method, in the disposing step, the transfer sheet and the medium may be accommodated inside a cup-shaped container from an opening portion of the cup-shaped container having the opening portion in which an upper surface side is opened, and the sealed space may be formed by closing the opening portion of the cup-shaped container with a closing member in which at least one part is made of the pressure welding sheet.
Accordingly, automation of each step of the pressure welding step and the irradiating step is facilitated.
According to the aspect of the present disclosure, the transfer layer can be transferred with high accuracy even to a medium in which the transfer target surface is uneven.
Hereinafter, embodiments of a transfer method according to the present disclosure will be described based on the drawings. The present disclosure is not limited by the embodiments. Furthermore, the configuring elements in the following embodiments include those that can be replaced by a person skilled in the art and those that are easy or substantially the same.
In the transfer method according to the present embodiment, a metal foil is transferred as a transfer layer to a transfer target surface Ma on which uneven portion Mb are formed in a medium M. As such medium M, for example, a small three-dimensional object such as a case of an electronic device including a smartphone and a tablet or a key chain may be used, or a large three-dimensional object such as a door or a window glass may be used.
As shown in
After the mounting step S10, as shown in
The mold release protective layer 13 is disposed between the heat generating layer 12 and the metal foil layer 14. The mold release protective layer 13 is adhered to the metal foil layer 14, and holds the metal foil layer 14 on the heat generating layer 12 side. The mold release protective layer 13 can be melted, for example, by heat. The metal foil layer 14 is formed to a thin film shape, for example, with a metal such as aluminum. The adhesive layer 15 is formed using, for example, a thermoplastic material, and can be adhered to a target object by being melted by heat. In the transfer sheet S1, the mold release protective layer 13 may not be provided, and may be separated into the layers of the base layer 11 and the heat generating layer 12 and the layers of the metal foil layer 14 and the adhesive layer 15.
After the disposing step S20, the transfer sheet S is pressure welded to the medium M by a negative pressure (pressure welding step S30). In the pressure welding step S30, first, as shown in
In this state, as shown in
Thus, by generating a negative pressure between the pressure welding sheet F having flexibility and the medium M, even when the uneven portion Mb are formed on the transfer target surface Ma of the medium M, the pressure welding sheet F is adsorbed to the transfer target surface Ma so as to follow the shape of the uneven portion Mb. Therefore, the transfer sheet S disposed between the pressure welding sheet F and the medium M closely attaches along the transfer target surface Ma of the medium M. In a state in which the pressure welding sheet F is pressure welded to the medium M, atmospheric pressure acts on the entire surface of the pressure welding sheet F, so that the transfer sheet S is in pressure weld with the medium M at a uniform pressure.
In the pressure welding step S30, the pressure welding sheet F may have a configuration corresponding to the type of transfer sheet S.
After the pressure welding step S30, the transfer sheet S is irradiated with a laser light (irradiating step S40). In the irradiating step S40, as shown in
When the transfer sheet S1 is used, the heat generated in the heat generating layer 12 melts the mold release protective layer 13 and softens the adhesive layer 15. When the transfer sheet S2 is used, the heat generated in the heat generating layer 42 melts the mold release protective layer 22 and softens the adhesive layer 24. In the present embodiment, since the transfer sheet S is pressure welded to the medium M by the pressure welding sheet F, a softened part G of the adhesive layer 15 or the adhesive layer 24 softened by heat is pressed against the medium M, and adheres to the transfer target surface Ma. The softened part G also adheres to the metal foil layer 14, 23 side.
After the irradiating step S40, the pump P is stopped to release the negative pressure state in the inside of the bag body B, and the medium M, the jig H and the transfer sheet S are taken out from the inside of the bag body B as shown in
After the releasing step S50, as shown in
After the peeling step S60, as shown in
As described above, the transfer method according to the present embodiment includes a disposing step of disposing the transfer sheet S and the medium M by layering the adhesive layer 15 of the transfer sheet S, in which the adhesive layer 15 and the metal foil layer 14 which is the transfer layer are layered in an inside of a sealed space formed using the pressure welding sheet F having flexibility in at least one part, so as to make contact with the medium; a pressure welding step of suctioning the inside of the sealed space by negative pressure and pressure welding the pressure welding sheet F and the medium M by the negative pressure to closely attach the transfer sheet S and the medium M; an irradiating step of softening the adhesive layer 15 by irradiation of a light ray generated from the irradiation device I which is a light source in a state the transfer sheet S is closely attached to the medium M by the pressure welding sheet F and adhering the adhesive layer 15 to the medium M by a pressure welding force from the pressure welding sheet F, and a peeling step of peeling off the transfer sheet S from the medium M after the irradiating step.
In this configuration, the transfer sheet S can be pressure welded to the medium M in a state the pressure welding sheet F is deformed so as to follow the uneven portion Mb of the transfer target surface Ma of the medium M by generating the negative pressure between the flexible pressure welding sheet F and the medium M. Thus, the metal foil which is the transfer layer can be transferred with high accuracy even to the medium M in which the uneven portion Mb is formed.
In the transfer method according to the present embodiment, the pressure welding sheet F is formed of a member that transmits a light ray, and in the irradiating step, the light ray is incident from the transfer sheet F side. The light ray generated from the irradiation device I thus can easily reach the metal foil layer 14 of the transfer sheet F.
In the transfer method according to the present embodiment, the transfer layer is formed of the metal foil layer 14, and in the irradiating step, the heat generating layer 12 disposed on the front side in the incident direction of the light ray in the metal foil layer 14 generates heat by the light ray thus thermally melting the adhesive layer 15. Thus, the heat generating layer 12 is provided above the metal foil layer 14 which does not transmit light, and the heat generating layer 12 is caused to generate heat by a light ray to thermally fuse the adhesive layer 15 and easily transfer the metal foil layer 14. Therefore, for example, the metallic color can be easily formed on the medium M.
In the transfer method according to the present embodiment, the heat generating layer 15 is formed on the pressure welding sheet F. Thus, the handling property of the pressure welding sheet F can be improved.
In the transfer method according to the present embodiment, the pressure welding step includes accommodating the medium M and the transfer sheet S in the bag body B formed using the pressure welding sheet F, and suctioning the inside of the bag body B to generate a negative pressure between the pressure welding sheet F and the medium M. Accordingly, the negative pressure is generated between the pressure welding sheet F and the medium M without requiring a complicated operation. In addition, the metal foil can be easily transferred with high accuracy even to a large medium M such as a door or a window glass.
The transfer method according to the present embodiment further includes a mounting step of mounting the medium M on the mounting portion Ha of the jig H, in which the mounting portion Ha for mounting the medium M is formed, where the pressure welding step includes suctioning the inside of the sealed space with negative pressure and pressure welding the pressure welding sheet F and the jig H by the negative pressure to closely attach the transfer sheet S and the medium M. Thus, the deformation of the medium M can be suppressed when generating the negative pressure between the pressure welding sheet F and the medium M.
Next, a second embodiment will be described.
First, as shown in
After the mounting step, the jig H on which the medium M is mounted is mounted on a mounting stand 52 of a pressure welding device 50. The pressure welding device 50 includes a cup-shaped member 51, the mounting stand 52, a height adjustment unit 53, an O-ring 54, and a closing member 55. The cup-shaped member 51 has an opening portion in which the upper surface side is opened. The cup-shaped member 51 accommodates the medium M mounted on the jig H and the transfer sheet S. The tube member T is connected to the cup-shaped member 51, and the pump P is mounted to the tube member T. The inside of the cup-shaped member 51 can be suctioned by operating the pump P. The mounting stand 52 is disposed in the cup-shaped member 51, and the jig H is mounted thereon. When the jig H is not used, the medium M is directly mounted on the mounting stand 52. The height adjustment unit 53 adjusts the height of the mounting stand 52. The O-ring 54 is provided at the edge of the cup-shaped member 51. The closing member 55 has a frame-shape, has a shape along the edge of the cup-shaped member 51 in plan view, and has the pressure welding sheet F is disposed on the inner side. The closing member 55 is removable from the cup-shaped member 51.
After mounting the jig H on the mounting stand 52, the transfer sheet S is disposed on the transfer target surface Ma of the medium M held by the jig H (disposing step). The transfer sheet S may be either the transfer sheet S1 or the transfer sheet S2 described in the above embodiment.
After the disposing step, the closing member 55 is mounted to the cup-shaped member 51, as shown in
After mounting the closing member 55, as shown in
After the pressure welding step, the transfer sheet S is irradiated with a laser light (irradiating step). In the irradiating step, as shown in
After the irradiating step, as shown in
Thus, according to the transfer method according to the present embodiment, in the disposing step, the transfer sheet S and the medium M are accommodated in the inside of the cup-shaped container 51 from the opening portion of the cup-shaped container 51 having the opening portion in which the upper surface side is opened, and the opening portion of the cup-shaped container 51 is closed by the closing member 55 in which at least one part is formed of the pressure welding sheet F to form a sealed space. Accordingly, automation of each step of the pressure welding step and the irradiating step is facilitated.
The technical scope of the present disclosure is not limited to the above embodiments, and appropriate modifications can be made without departing from the scope of the present disclosure. For example, a case of transferring the metal foil to the medium M has been described by way of example in each of the embodiments described above, but the above embodiments can be applied even in the case of transferring a hologram or the like.
Furthermore, a case where the metal foil is transferred to the medium M in the state in which nothing is formed in the transfer target surface Ma has been described by way of example in the embodiments described above, but this is not the sole case. For example, the transfer method described above can be applied even to a case where the metal foil is transferred to the medium M in a state where color ink is formed on the transfer target surface Ma by an inkjet printer or the like. This enables color metallic printing on the medium M.
In the embodiments described above, the case where the heat generating layer 12 and 42 is provided on the transfer sheet S or the pressure welding sheet F, and the adhesive layer 15, 24 is melted by irradiating the heat generating layer 12, 42 with the laser light L as a light ray has been described by way of example, but this is not the sole case. For example, when irradiating a transparent adhesive layer with an ultraviolet laser light as a light ray, the adhesive layer can generate heat without providing a heat generating layer. Furthermore, in a case where a laser light using light having a wavelength longer than that of the infrared light as a light ray is used, a substance having a high polarizability such as water can be vibrated and heated. Therefore, in such a case, the heat generating layer 12 and 24 may not be provided.
Moreover, in the embodiments described above, the case where the metal foil layer 14, 23 is transferred as a transfer layer has been described by way of example, but this is not the sole case. The transfer layer may be a layer other than a metal foil, such as, for example, a layer of an image formed by usual step colors.
Number | Date | Country | Kind |
---|---|---|---|
JP2018-151600 | Aug 2018 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
20020047225 | Bruning | Apr 2002 | A1 |
20110059284 | Butzloff | Mar 2011 | A1 |
20140227527 | Brors | Aug 2014 | A1 |
20160189985 | Kasai | Jun 2016 | A1 |
20170284096 | Abe | Oct 2017 | A1 |
Entry |
---|
Hamamatsu, “DGSHAPE Launches World's First Laser Foil Decorator”, Mar. 16, 2008, Available at: https://www.rolanddg.com/en/news/2018/180316-dgshape-launches-worlds-first-laser-foil-decorator. |
Number | Date | Country | |
---|---|---|---|