Claims
- 1. A building having a roof wherein the structural or insulation member of the roof contains a roofing membrane comprising a laminate of
- (A) a first layer having a thickness of from about 12 to 50 mils and comprising a compounded and stabilized vinyl chloride polymer plastisol composition containing antimony trioxide and
- (B) a second layer on said first layer having a thickness of from about 12 to 50 mils and comprising a compounded and stabilized vinyl chloride polymer plastisol composition containing titanium dioxide,
- said layers having been heated at a temperature of from about 250.degree. to 400.degree. F. for from about one to five minutes to fuse said layers and to adhere said layers together to obtain a flexible vinyl chloride polymer laminate and said layer (A) being adjacent said structural or insulation member of said roof.
- 2. A building according to claim 1 in which in each layer of said laminate the vinyl chloride polymer is homopolyvinyl chloride, in which in each layer of said laminate the amount of plasticizer is from about 50 to 80 parts by weight per 100 parts by weight total of vinyl chloride polymer, wherein said antimony trioxide is used in an amount of from about 2 to 6 parts by weight per 100 parts by weight of the total vinyl chloride polymer in (A) and wherein said titanium dioxide is used in an amount of from about 2 to 8 parts by weight per 100 parts by weight of the total vinyl chloride polymer in (B).
- 3. A building according to claim 2 wherein each layer of said laminate contains effective amounts by weight of carbon black, fumed colloidal silica and calcium carbonate.
Parent Case Info
This is a divisional application of application Ser. No. 06/518,247 filed on July 28, 1983 now U.S. Pat. No. 4,515,744, granted May 7, 1985.
US Referenced Citations (2)
Divisions (1)
|
Number |
Date |
Country |
Parent |
518247 |
Jul 1983 |
|