Claims
- 1. A laminate comprising
- (A.) a first layer having a thickness of from about 12 to 50 mils, being of a compounded and stabilized vinyl chloride polymer plastisol composition containing antimony trioxide and being free of a curing agent and
- (B.) a second layer on said first layer having a thickness of from about 12 to 50 mils, being of a compounded and stabilized vinyl chloride polymer plastisol composition containing titanium dioxide and being free of a curing agent, said layers having been heated at a temperature of from about 250.degree. to 400.degree. F. for from about one to five minutes to fuse said layers and to adhere said layers together to obtain a flexible vinyl chloride polymer laminate.
- 2. The laminate according to claim 1 in which each of said layers (A.) and (B.) the vinyl chloride polymer is homopolyvinyl chloride, in which in each of said layers (A.) and (B.) the amount of plasticizer is from about 50 to 80 parts by weight per 100 parts by weight total of vinyl chloride polymer, wherein said antimony trioxide is used in an amount of from about 2 to 6 parts by weight per 100 parts by weight of the total vinyl chloride polymer in (A.) and wherein said titanium dioxide is used in an amount of from about 2 to 6 parts by weight per 100 parts by weight of the total vinyl chloride polymer in (B.).
- 3. The laminate according to claim 2 wherein each layer contains effective amounts by weight of carbon black, fumed colloidal silica and calcium carbonate.
Parent Case Info
This is a divisional application of application Ser. No. 518,247, filed on July 28, 1983, now U.S. Pat. No. 4,515,744.
US Referenced Citations (4)
Foreign Referenced Citations (1)
Number |
Date |
Country |
4102365 |
Aug 1979 |
JPX |
Divisions (1)
|
Number |
Date |
Country |
Parent |
518247 |
Jul 1983 |
|