Claims
- 1. A method for preventing the gelling of a foam-forming mixture comprising water and about 8-12wt % by weight of an alkyl aromatic sulfonate having an average molecular weight of about 400 to about 600 and an alkyl group comprising 16 to 40 carbon atoms, comprising the addition of a viscosity control agent to the mixture prior to storage of the mixture, prior to transporting the mixture, after the mixture has been stored for an extended period of time or after the mixture has been exposed to low temperatures, wherein the viscosity control agent is added in an amount effective to prevent the gelling of the mixture during storage and/or transporting of the mixture and further wherein the viscosity control agent comprises alpha olefin sulfonates, alpha olefin sulfonate dimers, alkylphenolethoxylates, alkyl diphenylether disulfonates, dialkyl diphenyl ether disulfonates, alcohol ethoxysulfates, alcohol ethoxy sulfonates, or mixtures thereof.
- 2. The method of claim 1 wherein the mixtures has gelled prior to addition of the viscosity control agent which when added decreases the viscosity of the gelled mixture and prevents the gelling of the mixture.
- 3. The method of claim 1 wherein the at least one alkyl group comprises 20 to 24 carbon atoms.
- 4. The method of claim 1 wherein the alkyl aromatic sulfonate has an average molecular weight of about 450 to about 550.
- 5. The method of claim 1 wherein the alkyl aromatic sulfonate has an average molecular weight of about 475 to about 525.
- 6. The method according to claim 1 wherein the viscosity control agent is an alpha-olefin which comprises about 0.2 to about 5% by weight of the mixture.
- 7. The method of claim 6 wherein the viscosity control agent comprises about 0.4 to about 2% by weight of the mixture.
- 8. The method of claim 6 where the alpha-olefin sulfonate has 12 to 16 carbon atoms.
- 9. The method according to claim 1 wherein the viscosity control agent comprises an alpha olefin sulfonate dimer which is present in an amount of about 0.2 to about 5% by weight of the mixture.
- 10. The method according to claim 1 wherein the viscosity control agent comprises about 0.8 to about 1.6% by weight of the mixture.
- 11. The method of claim 1 wherein the sulfonate component of the alkyl aromatic sulfonate is in a water soluble salt form which comprises sodium, potassium, ammonium or an alkyl ammonium.
- 12. The method of claim 1 wherein the sulfonate component of the alkyl aromatic sulfonate is in an acid form.
- 13. The method of claim 1 wherein the alkyl aromatic sulfonate comprises about 9 to about 11% by weight of the mixture.
- 14. The method of claim 1 wherein the viscosity control agent is added prior to the storage and/or transporting of the mixture.
- 15. The method of claim 1 wherein the viscosity control agent is added after the mixture has been stored for an extended period of time and/or after exposure to the mixture to low temperatures.
Parent Case Info
This application is a division of application Ser. No. 07/409,595, filed Sep. 22, 1989 now U.S. Pat. No. 5,000,262.
US Referenced Citations (12)
Foreign Referenced Citations (1)
| Number |
Date |
Country |
| 1248340 |
Jan 1989 |
CAX |
Divisions (1)
|
Number |
Date |
Country |
| Parent |
409595 |
Sep 1989 |
|