The invention relates generally to laser hybrid welding systems, and, more particularly, to controllers for laser hybrid welding systems.
Welding is a process that has become increasingly ubiquitous in various industries and applications. A variety of welding techniques have been developed that seek to provide fast welding capabilities with adequate penetration and gap bridgeability. While laser beam welding provides speed and deep penetration benefits, such a welding process typically requires tight joint fitup for the laser beam to adequately bridge the gap between the workpieces. Arc welding processes, on the other hand, typically provide for welding more slowly than laser-beam processes, but are capable of bridging much larger gaps than laser-beams. As such, a variety of hybrid welding techniques have been developed that combine laser-beam welding with arc welding processes, such as gas metal arc welding (GMAW). This type of welding process typically aims a laser beam at a location where a weld joint is to be formed, and follows it closely, typically via the same, hybrid welding torch, with a more conventional shielded arc for additional fusion and filler metal deposition.
While hybrid welding processes provide good bridgeability at high speeds, such processes are often associated with drawbacks, such as intolerability of gaps in the joint. These drawbacks often reduce or eliminate the applicability of laser hybrid welding to a variety of applications, such as pipelines, ship building, and automotive manufacturing. Some advances, such as beam width increasing systems, have been made to improve the gap filling associated with laser hybrid welding. However, laser hybrid welding still poses challenges surrounding gap filling since penetration cannot be adequately controlled when gaps occur in the weld. Accordingly, there exists a need for systems that address these limitations of laser hybrid welding.
In an exemplary embodiment, a laser hybrid welding system includes a sensor adapted to acquire data regarding a parameter of a laser hybrid welding operation. The laser hybrid welding system also includes a controller communicatively coupled to the sensor and adapted to receive the acquired data from the sensor and to determine whether the acquired data is indicative of a welding defect. If the acquired data is indicative of a welding defect, the controller is adapted to output a control signal that directs the laser hybrid welding system to attempt to fix the welding defect.
In another embodiment, a controller for a laser hybrid welding system includes interface circuitry adapted to receive data regarding a parameter of a laser hybrid welding operation and to output one or more control signals. The controller also includes a processor communicatively coupled to the interface circuitry and adapted to receive the data from the interface circuitry and to process the received data to determine whether a weld defect has occurred. The controller also includes memory coupled to the processor and adapted to receive and store the processed data from the processor for later retrieval.
In another embodiment, a laser hybrid welding system includes a sensor adapted to acquire data regarding a parameter of a laser hybrid welding operation. The laser hybrid welding system also includes a controller communicatively coupled to the sensor and adapted to receive the acquired data from the sensor and to determine whether the acquired data is indicative of a welding defect. If the acquired data is indicative of a welding defect, the controller is further configured to alert an operator of the welding defect and to log the welding defect as an error in an associated memory.
These and other features, aspects, and advantages of the present invention will become better understood when the following detailed description is read with reference to the accompanying drawings in which like characters represent like parts throughout the drawings, wherein:
As described in detail below, embodiments are provided of a laser hybrid welding system adapted to identify and/or to fix a weld defect occurring during a laser hybrid welding process. The disclosed laser hybrid systems may be configured to detect and/or repair weld defects such as those sometimes referred to as “burn-through”, a “suck-back”, inadequate weld reinforcement, improper alignment, cracks, incomplete penetration, and incomplete fusion. To that end, the laser hybrid welding system may include one or more devices that provide feedback to a controller regarding one or more weld parameters. For instance, in one embodiment, the laser hybrid welding system may include sensors, such as a voltage sensor and/or a current sensor that measure the weld voltage and/or amperage during the welding process and transmit the acquired data to the controller for processing. Such parameters may provide an indication of a weld defect that has occurred. For further example, a leading camera and a following camera that image an area directly in front of the weld location and directly behind the weld location may be provided. The controller may compare the pre-weld and post-weld images to determine whether a weld defect has occurred. Still further, the controller may time stamp the acquired data and utilize such time stamps (e.g., in conjunction with a known or estimated rate of advance) to compute the location of the detected weld defect with respect to a reference (e.g., present) location. Additionally, one or more audio sensors may be employed to determine the presence and location of the weld defect. As such, embodiments of the presently disclosed laser hybrid welding systems may be capable of detecting and repairing weld defects during the welding process.
Turning now to the drawings,
The welding system 10 includes a welder 12 that provides supplies, such as welding wire, power, and so forth, to a welding operation 14 being performed by a robot 16. In the illustrated embodiment, the welder 12 includes a gas supply 18, a power supply 20, a laser generator 22, and a wire feeder 24 that supply gas through cable 26, power through cable 28, laser power through cable 30, and wire through cable 32, respectively, to a welding torch for use in the welding operation 14. It should be noted that the cables 26, 28, 30, and 32 may be combined into a single cable 34 that couples the welder 12 to the welding torch in some embodiments.
The welder 12 also includes a user interface 34 coupled to a controller 36 and interface circuitry 30. During use, an operator may input desired weld operating parameters to the welder 12 via the user interface 26. Additionally, the user interface 26 may be utilized by the welding system 10 to communicate detection of one or more weld defects to the user as the weld progresses. For example, the user interface 26 may be configured to notify the operator when a burn-through, an excess weld reinforcement or a suck-back defect has occurred. In some embodiments, such defects may be determined by the presence of a first sensor 32 and a second sensor 34 that are configured to sense one or more parameters of the weld. For example, the first sensor 32 may be adapted to measure the actual weld voltage level and the second sensor 34 may be adapted to measure the actual weld current level. The acquired measurements may then be communicated back to the interface circuitry 40 in the welder 12 via cables 46 and 48. The interface circuitry 40 then routes the acquired measurements to the controller 38 in the desired way. For example, the interface circuitry 40 may be configured to obtain measurement data from the sensors as the data is acquired, for rapid detection and repair of defects. Alternatively, they may transmit such data to the controller 38 at predetermined periods of time (e.g., once every five minutes, once every ten minutes, etc.). After receiving the measurement data, the controller 38 processes the data to determine whether a defect has occurred and, if so, where in the weld material the defect exists. For example, a processor located in the controller may convert the voltage-time data and the amperage-time data to the frequency domain via a fast Fourier transform (FFT) and analyze the converted data to determine the presence of a weld defect based upon known frequencies that should occur in normal welding, and those that can occur that are characteristics of such defects. The controller 38 may then notify the operator of the defect via the user interface 36 and/or may direct the repair of such a defect.
Furthermore, the presence of one or more weld defects may be detected via the use of a leading camera 50 positioned in front of the weld and a following camera 52 positioned behind a weld as the welding operation 14 proceeds in the direction indicated by arrow 54. That is, the leading camera 50 may be configured to record the weld from a position ahead of the weld and to transmit the recorded data to the interface circuitry 40 via cable 56. Similarly, the following camera 52 may be configured to record the weld from a position behind the weld and to transmit the recorded data to the interface circuitry 40 via cable 58. The controller 38 may then be adapted to receive the recorded information from the interface circuitry 40 and to process the inputs from both the leading camera 50 and the following camera 52. For example, the controller 38 may digitally compare the images obtained before and after the weld to identify changes that may be indicative of a defect, such as a burn-through, a suck-back, and so forth. Additionally, the controller 38 may integrate the information gained from the processing of the acquired data from the cameras 50 and 52 with the information gained from the processing of the data from the sensors 42 and 44. The controller 38 may use such information to determine the presence, location, and characteristics of a defect. As before, if a defect is detected, the controller 38 may notify the operator of the defect via the user interface 36 and/or may direct the repair of the defect.
It should be noted that a variety of modifications may be made to the welding system of
Furthermore, although the welding system of
Still further, during use, the processor 62 may be configured to communicate the identification of a defect to the operator via the user interface 36 in the welder 12. That is, after receiving and processing the one or more data inputs from the interface circuitry 64, the processor 62 may output a signal that directs the user interface 36 to communicate to the operator the presence of a weld defect and the actions taken to fix the defect. If the data inputs indicate that no weld defect has occurred, the processor 62 may be configured to output a signal to the user interface 36 directing the interface to notify the operator that the welding operation is proceeding without any errors. It should be noted that such communications may take any suitable form. For example, a visual or audible alarm may be generated that the operator can easily detect and identify as such. It is also contemplated that some operators may use specialized equipment such as helmets with operator feedback or communication (e.g., LED's visible in the helmet, head-up displays, headphones, etc.). The notification of the occurrence of a defect, and even a time or location indication, can be provided by such means.
It should be noted that the controller may be configured to process one or more acquired measurements, utilize such measurements to identify a defect, and alter one or more parameters of the welding process to ensure that future defects do not occur. For example, in one embodiment, the weld voltage and weld current may be sensed and recorded over time during the welding process. Such data may then be transferred into the frequency domain via a FFT to identify the presence of one or more defects. The presence of a defect may trigger generation of an error signal corresponding to an item in a lookup table or a neural network. The controller may use the item to direct a setting of the welder and/or the laser that will alter the correct parameter to fix the detected defect. Indeed, a variety of such procedures may be utilized by the controller to detect and fix the weld defect.
Embodiments of the presently disclosed control system are configured to process data from one or more sensors and/or cameras at the weld location regarding characteristics of the weld. In this way, such embodiments of the control system may be capable of identifying the presence, nature, and location of the weld defect 126. For example, the control system may time stamp the acquired data and integrate the time stamped data with the torch travel speed to determine the location of the defect. Additionally, if the travel speed changes over time along the length of the workpieces, the controller may be configured to integrate the varying travel speed with the time stamped data to determine the position of the weld defect 126.
If the feedback parameter does not indicate a weld defect, the controller outputs a control signal that guides the continuation of the welding process (i.e., does not interrupt) with the laser and the welder (block 134). If the feedback parameter does indicate a defect, the controller records the error, assigns the error an error ID (block 136), time stamps the error, and computes the defect location (block 138). It should be noted that the controller may utilize an encoder and/or one or more wireless signals to determine and/or communicate the defect location. The controller may then notify the operator of the error (block 140), for example, through the user interface on the control panel of the welder, or via the welder's equipment (e.g., helmet). If desired, the controller may then output a control signal that directs the welder to attempt to fix the defect (block 142). For example, the controller may direct the positioner or robot to back up and re-weld the area including a gap in the weld if desired. In other embodiments, however, the controller may notify the operator that an error has occurred at the determined location without attempting to repair the weld defect. Still further, the controller may be configured to log all the detected errors throughout a welding operation and provide the operator with a list of detected errors and the locations of the errors. In some embodiments, the welding system may finish the weld and proceed to back up automatically right after the weld is completed. In other embodiments, the welding system may complete the weld and allow a preset or manually set time interval to elapse before backing up to fix the defect.
If the size of the defect does not exceed the threshold, the controller directs the laser and the welder to turn off (block 150). The positioner or robot performing the welding is then backed up to the starting location of the defect (block 152) where the laser and the arc welder are turned back on (block 154). The laser hybrid welder is then directed by the controller to run another pass over the location of the defect (block 156). That is, if the detected gap is small, the laser hybrid welding operation may be interrupted to attempt to repair the gap. After repair has been attempted, the feedback parameter is re-sensed (block 158). The controller again checks whether the re-sensed feedback parameter indicates the presence of a defect (block 132). If the feedback indicates the defect has been repaired, the laser-welder is directed to continue welding with the laser and the welder (block 134). Alternatively, if the feedback parameter indicates the presence of a defect, the controller again attempts to fix the defect by repeating blocks 150, 152, 154, 156, and 158 (block 160). After repeating such blocks, the controller again checks if the feedback parameter indicates a defect (block 132). If no defect is detected, the controller directs the welder to weld as normal (block 134). If a defect is still detected, the controller notifies the operator of an error (block 162). The controller may then either terminate the welding operation and wait for operator input or continue welding while noting the location of the defect.
It should be noted that the method illustrated in
While only certain features of the invention have been illustrated and described herein, many modifications and changes will occur to those skilled in the art. It is, therefore, to be understood that the appended claims are intended to cover all such modifications and changes as fall within the true spirit of the invention.
This application is a Continuation application of U.S. patent application Ser. No. 12/776,274, entitled “Weld Defect Detection Systems and Methods for Laser Hybrid Welding”, filed May 7, 2010, which is a Non-Provisional Patent Application of U.S. Provisional Patent Application No. 61/186,116, entitled “Gap Filling with Laser Hybrid Welding”, filed Jun. 11, 2009, both of which are herein incorporated by reference.
| Number | Name | Date | Kind |
|---|---|---|---|
| 4446354 | Kearney | May 1984 | A |
| 5121339 | Jenuwine et al. | Jun 1992 | A |
| 5651903 | Shirk | Jul 1997 | A |
| 6155475 | Ekelof et al. | Dec 2000 | A |
| 6583386 | Ivkovich | Jun 2003 | B1 |
| 6844521 | Staufer et al. | Jan 2005 | B2 |
| 6854632 | Larsson | Feb 2005 | B1 |
| 7015419 | Hackl et al. | Mar 2006 | B2 |
| 7043330 | Toyserkani et al. | May 2006 | B2 |
| 7107118 | Orozco et al. | Sep 2006 | B2 |
| 7759603 | Aigner et al. | Jul 2010 | B2 |
| 8046178 | Dai et al. | Oct 2011 | B2 |
| 8552337 | Albrecht | Oct 2013 | B2 |
| 20090095720 | Kamei | Apr 2009 | A1 |
| 20100107725 | Iizuka et al. | May 2010 | A1 |
| 20110198317 | Lin | Aug 2011 | A1 |
| 20120325786 | Tolling et al. | Dec 2012 | A1 |
| Number | Date | Country |
|---|---|---|
| 2867996 | Sep 2005 | FR |
| 2005056230 | Jun 2005 | WO |
| Entry |
|---|
| International Search Report for application No. PCT/EP2010/037997 mailed Sep. 22, 2010. |
| Number | Date | Country | |
|---|---|---|---|
| 20130341311 A1 | Dec 2013 | US |
| Number | Date | Country | |
|---|---|---|---|
| 61186116 | Jun 2009 | US |
| Number | Date | Country | |
|---|---|---|---|
| Parent | 12776274 | May 2010 | US |
| Child | 14012407 | US |