This invention relates generally to the field of materials technology, and more particularly to the field of welding of superalloy materials.
Nickel-based and cobalt-based superalloy materials are commonly used to provide high mechanical strength for very high temperature applications, such as for the blades or other components of a gas turbine engine. Such components are very expensive, and thus the repair of a damaged part is preferred over its replacement. However, known weld repair techniques for superalloy materials have met with only limited success, due primarily to the propensity of superalloy materials to develop cracks during such welding operations. In addition to hot cracking of the weld filler metal and heat affected zone, these materials exhibit strain age cracking, which results in cracks extending into the base metal of the component.
Several techniques have been proposed to improve the weldability of superalloy materials. U.S. Pat. No. 4,336,312 describes a combination of a controlled chemical modification of a cast nickel-based superalloy material along with a pre-weld thermal conditioning cycle. U.S. Pat. No. 6,364,971 describes a laser welding technique used following a pre-conditioning hot isostatic process. U.S. Pat. No. 6,333,484 describes a welding technique wherein the entire weld area is preheated to a maximum ductility temperature range, and this elevated temperature is maintained during the welding and solidification of the weld. Each of these patents is incorporated by reference herein.
The assignee of the present invention produces gas turbine engines utilizing a variety of materials, including blades formed of a directionally solidified (DS) cast nickel-based superalloy material sold by Cannon-Muskegon Corporation under the designation CM-247 LC. CM-247 LC is known to have the following nominal composition, expressed as weight percentages: carbon 0.07%; chrome 8%; cobalt 9%; molybdenum 0.5%; tungsten 10%; tantalum 3.2%; titanium 0.7%; aluminum 5.6%; boron 0.015%; zirconium 0.01%; hafnium 1.4%; and the balance nickel. Such blades are currently repaired by welding at elevated temperatures, so called hot-box welding, utilizing specially selected filler metal. Hot-box weld repairs may take eight hours or more to complete, and the requirement for working inside of the hot box to maintain the elevated temperature makes it difficult to perform such welds robotically.
A process is described herein for pre-conditioning a superalloy material so that the material may be welded successfully at ambient temperature conditions without inducing an unacceptable degree of strain age cracks in the base material. One embodiment of this process is described in detail herein for welding the known material described above and designated by Cannon-Muskegon Corporation as CM-247 LC.
The present invention includes a pre-weld conditioning regiment that heats the material from ambient temperature and holds the base material at a predetermined elevated soak temperature for a selected period, then cools the material at a controlled slow rate to a predetermined reduced but still elevated temperature, and then rapidly cools the material to close to ambient temperature. It is believed that the inventive regiment results in the growth of gamma prime to a desired volume percent, thereby providing a degree of ductility to the material that allows it to undergo a fusion welding process at ambient conditions with little or no cracking of the base material.
Some known prior art processes overage a superalloy material at the solution heat treatment temperature (the lowest temperature at which carbides in the material dissolve) prior to welding, such as the process described in U.S. Pat. No. 6,364,971. In contrast, the present invention utilizes a pre-weld conditioning soak temperature that is below the solution heat treatment temperature. For one embodiment of welding CM-247 LC material, a soak temperature of about 2,225° F. (1,218° C.) is used, which is 45° F. (25° C.) below the solution heat treatment temperature for that material of 2,270° F. In other embodiments, the soak temperature may be as much as about 65 or 70 or 75° F. (about 36 or 39 or 42° C.) below the solution heat treatment temperature, or as little as 15 or 20 or 25° F. (about 8 or 11 or 14° C.) below the solution heat treatment temperature, or within a range between any two of those temperatures. The material may be heated in a vacuum furnace with a working pressure of no more than about 2×10−3 torr in one embodiment, and holding that pressure throughout the heating, soaking and cooling steps. The material may be heated at a rate of about 28±5° F. (about 15±3° C.) per minute (i.e. increasing the temperature of the furnace at that rate), although the heat-up rate has been found not to be critical and may be a different rate so long as it is not so fast as to cause cracking or detrimental distortion of the component formed of the material. The temperature is then maintained at the soak temperature for a time period sufficiently long to allow the elevated temperature to soak the entire thickness of the component, or at least the entire thickness of the component that will be affected by subsequent fusion welding, such as about one hour per inch of thickness for the embodiment of CM-247 LC material.
Upon completion of the heat-up and soak steps, the material is then slowly cooled by cooling the furnace temperature to grow the gamma prime to a desired volume percentage. The material may be cooled at a rate of about 1° F. (about 0.5° C.) per minute to an intermediate temperature that is reduced from the soak temperature but is still above a minimum gamma prime growth temperature of the material. The intermediate temperature may be about 1,625±25° F. (885±14° C.) for the embodiment of CM-247 LC material. The purpose of the slow cool down step is to grow gamma prime to a desired volume percent, such as to about 55%, or at least 40% or 50% or in the range of 40-55% or in the range of 50-55%. The cool down rate may be in the range of 1±0.5° F. (0.5±0.28° C.). The material is then cooled rapidly to a temperature that is below the minimum gamma prime growth temperature of the material, such as by gas fan quench cooling to a temperature of no more than about 300° F. (about 149° C.) or as low as about 125° F. (about 52° C.).
The process described above will produce a material having the desired volume percentage of gamma prime, and will produce a material that can be fusion welded with matching filler material without producing cracking of the base material. This result is unexpected because the described heat treatments do no coincide with any phase diagram reference points or previously used heat treatments. For the embodiment of CM-247 LC material, about two dozen service-run gas turbine engine blades have been successfully repair welded with filler material (Mar-M247) matching the chemistry of the base material at ambient temperature with no cracking, or in a few cases, with only a low degree of cracking of the weld but not the base metal that was not detrimental to the continued use of the component, using the above described process. Conventional pre-process cleaning and post welding solution heat treatment/quench processes are used. Overage heat treatments beyond the ranges specified above have failed to prevent or minimize base metal cracking during blade repair at both elevated temperatures and at ambient temperature. Thus, the inventive process described herein satisfies the long-felt need for a process for successfully weld repairing superalloy material, and in particular for welding such materials at ambient temperatures. Turbine blades have successfully been returned to service in gas turbine engines following a weld repair at ambient temperatures using the process of the present invention; whereas heretofore, repair welds had only been successfully performed at high temperatures.
While various embodiments of the present invention have been shown and described herein, it will be obvious that such embodiments are provided by way of example only. Numerous variations, changes and substitutions may be made without departing from the invention herein. Accordingly, it is intended that the invention be limited only by the spirit and scope of the appended claims.
| Number | Name | Date | Kind |
|---|---|---|---|
| 4336312 | Clark et al. | Jun 1982 | A |
| 4582548 | Harris et al. | Apr 1986 | A |
| 4804815 | Everett | Feb 1989 | A |
| 4965095 | Baldi | Oct 1990 | A |
| 5040718 | Lee et al. | Aug 1991 | A |
| 5106010 | Stueber et al. | Apr 1992 | A |
| 5142778 | Smolinski et al. | Sep 1992 | A |
| 5374319 | Stueber et al. | Dec 1994 | A |
| 5509980 | Lim | Apr 1996 | A |
| 5554837 | Goodwater et al. | Sep 1996 | A |
| 5571345 | Ganesh et al. | Nov 1996 | A |
| 5732467 | White et al. | Mar 1998 | A |
| 5785775 | Smashey et al. | Jul 1998 | A |
| 5897801 | Smashey et al. | Apr 1999 | A |
| 6084196 | Flowers et al. | Jul 2000 | A |
| 6120624 | Vogt et al. | Sep 2000 | A |
| 6191379 | Offer et al. | Feb 2001 | B1 |
| 6333484 | Foster et al. | Dec 2001 | B1 |
| 6376801 | Farrell et al. | Apr 2002 | B1 |
| 6394971 | Peterson, Jr. et al. | May 2002 | B1 |
| 6489584 | Kelly | Dec 2002 | B1 |
| 6491207 | Smashey et al. | Dec 2002 | B1 |
| 6495793 | Tewari | Dec 2002 | B2 |
| 6659332 | Smashey et al. | Dec 2003 | B2 |
| 6872912 | Wos et al | Mar 2005 | B1 |
| 6902617 | Betz | Jun 2005 | B2 |
| 6908288 | Jackson et al. | Jun 2005 | B2 |
| 6972390 | Hu et al. | Dec 2005 | B2 |
| 20030116242 | Harrison et al. | Jun 2003 | A1 |
| 20050263220 | Malley et al. | Dec 2005 | A1 |
| 20060042729 | Kottilingam et al. | Mar 2006 | A1 |
| 20070283560 | Malley | Dec 2007 | A1 |
| Number | Date | Country | |
|---|---|---|---|
| 20090320966 A1 | Dec 2009 | US |