Claims
- 1. A corrosion-resistant alloy suitable for hot-dip coating steels, consisting essentially of
- aluminum: about 70% by weight
- silicon: 0.05 to 0.5% by weight
- magnesium: 0.01 to 0.5% by weight,
- balance essentially zinc.
- 2. Steel products coated with an alloy as in claim 1.
- 3. An alloy as claimed in claim 1 in which the silicon and magnesium are each about 0.20% by weight.
Priority Claims (1)
Number |
Date |
Country |
Kind |
48263 A/86 |
Jul 1986 |
ITX |
|
Parent Case Info
This application is a continuation of application Ser. No. 07/324,542, filed Mar. 16, 1989, which is a continuation of application Ser. No. 07/066,935, filed June 26, 1987, both now abandoned.
US Referenced Citations (2)
Number |
Name |
Date |
Kind |
3343930 |
Borzillo et al. |
Sep 1967 |
|
4610936 |
Isobe et al. |
Sep 1986 |
|
Continuations (2)
|
Number |
Date |
Country |
Parent |
324542 |
Mar 1989 |
|
Parent |
66935 |
Jun 1987 |
|