Embodiments of the invention generally relate to an apparatus and a method for depositing materials. More specifically, embodiments of the invention are directed to a gas distribution plate having a focus ring to form a more uniform film in an atomic layer deposition chamber.
In the field of semiconductor processing, flat-panel display processing or other electronic device processing, vapor deposition processes have played an important role in depositing materials on substrates. As the geometries of electronic devices continue to shrink and the density of devices continues to increase, the size and aspect ratio of the features are becoming more aggressive, e.g., feature sizes of 0.07 μm and aspect ratios of 10 or greater. Accordingly, conformal deposition of materials to form these devices is becoming increasingly important.
During an atomic layer deposition (ALD) process, reactant gases are sequentially introduced into a process chamber containing a substrate. Generally, a first reactant is introduced into a process chamber and is adsorbed onto the substrate surface. A second reactant is then introduced into the process chamber and reacts with the first reactant to form a deposited material. A purge step may be carried out between the delivery of each reactant gas to ensure that the only reactions that occur are on the substrate surface. The purge step may be a continuous purge with a carrier gas or a pulse purge between the delivery of the reactant gases.
The flow of process gases across the surface of a substrate affects the uniformity of the resultant film. Gas distribution plates have been designed to uniformly distribute gases but film uniformity remains a difficulty. Therefore, there is a need in the art for apparatuses and methods to more uniformly distribute process gases across the surface of a substrate to improve film uniformity.
Embodiments of the invention are directed to gas distribution plates to distribute process gases over a substrate surface. The gas distribution plates comprise a body defining a thickness and a peripheral edge. The body comprises a front surface for facing the substrate, the front surface having a central region having a plurality of openings configured to distribute process gases over the substrate and a focus ring having a sloped region. The focus ring is concentric to the central region such that the thickness at the focus ring is greater than the thickness at the central region.
In some embodiments, the focus ring and central region are shaped so that when the plate is adjacent a substrate there is a first distance between the central region and the substrate and a second distance between the focus ring and the substrate which is less than the first distance to evenly distribute the process gases. In detailed embodiments, the first distance is in the range of about 1.5 to about 6 times greater than the second distance. In specific embodiments, the first distance is in the range of about 2 to about 4 times greater than the second distance.
In one or more embodiments, the front surface has an overall concave shape defined by the central region surrounded by the sloped region of the focus ring. In specific embodiments, the sloped region is sloped at an angle in the range of about 5 to about 45 degrees.
The central region of some embodiments is substantially flat. The sloped region of one or more embodiments, extends to the peripheral edge. In various embodiments, the sloped region of the focus ring extends to an outer peripheral front face area.
In one or more embodiments, the gas distribution plate further comprises at least one channel forming a fluid connection between a gas inlet channel on a back surface of the body and the plurality of openings in the central region. In some embodiments, the gas distribution plate further comprises a central port extending through about a central axis of the substantially circular body, the central port configured to prevent mixing of a fluid passing through the central port from the process gases passing through the plurality of openings. In detailed embodiments, the central port is in fluid communication with one or more of a vacuum system and a precursor source.
Additional embodiments of the invention are directed to processing chamber comprising the gas distribution plate described. In specific embodiments the processing chamber is an atomic layer deposition chamber.
Further embodiments of the invention are directed to methods of processing a substrate. A substrate having an edge region surrounding an inner region is disposed in a process chamber adjacent a gas distribution plate defining a reaction region between the substrate and the distribution plate. The reaction region is smaller at the edge region than at the inner region. At least a first process gas is flowed through the plurality of openings in the front face of the gas distribution plate to the substrate.
In detailed embodiments, the distribution plate comprises a body defining a thickness and a peripheral edge. The body comprises a front surface for facing the substrate, the front surface having a central region having a plurality of openings configured to distribute process gases over the substrate and a focus ring having a sloped region. The focus ring is concentric to the central region such that the thickness at the focus ring is greater than the thickness at the central region.
In some embodiments, the gas distribution plate further comprises a central port extending through about a central axis of the substantially circular central region. In detailed embodiments, the methods further comprise flowing at least a second process gas through the central port to the substrate. In specific embodiments, at least a partial vacuum is applied to a region between the substrate and the central region of the gas distribution plate through the central port. One or more embodiments of the methods further comprise alternately flowing the first process gas through the plurality of openings and the at least one second process gas through the central port.
So that the manner in which the above recited features of the invention are attained and can be understood in detail, a more particular description of the invention, briefly summarized above, may be had by reference to the embodiments thereof which are illustrated in the appended drawings. It is to be noted, however, that the appended drawings illustrate only typical embodiments of this invention and are therefore not to be considered limiting of its scope, for the invention may admit to other equally effective embodiments.
Embodiments of the invention are directed to gas distribution plates, also referred to as showerheads, which provide improved film uniformity by improving gas flow distribution. Specific embodiments of the invention are directed to atomic layer deposition apparatuses (also called cyclical deposition) incorporating a gas distribution plate having a shape configured to improve the gas flow distribution.
As used in this specification and the appended claims, the term “gas distribution plate” and “showerhead” are used interchangeably. A “gas distribution plate” is a component of the gas distribution system and is commonly referred to as a “showerhead” due to the fact that it has a hole pattern which is often reminiscent of a shower head.
In one or more embodiments, two precursors can flow into a process chamber through two individual gas supply passages. One of these precursors will be distributed uniformly (e.g., HfCl4) and the other can be supplied through a single point of entry (usually oxidizers like water or ozone).
A showerhead with focus ring can be used for the HfCl4 distribution. A focus ring provides better edge coverage by reducing the process gap between the showerhead and the heater surface. In some embodiments, a blocker plate and baffle could also be included to further improve gas flow uniformity. An oxidizer could be introduced through a single or multiple jets directed toward the wafer or across it. A single inject could be positioned in the center of the chamber or any other location as desired.
A showerhead with variable spacing could be used for ALD applications. The variable spacing will affect the precursor residence time, effectiveness of purging of the byproducts and the reactants and used for thickness tuning. An additional central vacuum port can be positioned in the center of the showerhead. This port provides effective pumping f the central spot of the water, which is a stagnation zone for an existing peripheral axi-symmetric pumping. The central vacuum port could be used for injection of a precursor in case when pumping step does not coincide with a precursor pulse. A co-axial configuration of the central pumping port and central inject could be utilized by providing pumping tube inside of the central inject or vice versa.
The gas distribution system 130 generally comprises a mounting plate 133, a showerhead 170, and a blocker plate 160 and provides at least two separate paths for gaseous compounds into a reaction region 128 between the showerhead 170 and the substrate support 112. In the depicted embodiment, the gas distribution system 130 also serves as a lid of the process chamber 100. However, in other embodiments, the gas distribution system 130 may be a portion of a lid assembly of the chamber 100. The mounting plate 133 comprises a channel 137 and a channel 143, as well as a plurality of channels 146 that are formed to control the temperature of the gaseous compounds (e.g., by providing either a cooling or heating fluid into the channels). Such control is used to prevent decomposing or condensation of the compounds. Each of the channels 137, 143 provides a separate path for a gaseous compound within the gas distribution system 130.
Referring again to
In some embodiments, the blocker plate 160 and the showerhead 170 are electrically isolated from one another, the mounting plate 133, and chamber body 102 using insulators (not shown) formed of, for example, quartz, ceramic, and the like. The insulators are generally disposed between the contacting surfaces in annular peripheral regions thereof to facilitate electrical biasing of these components and, as such, enable plasma enhanced cyclical deposition techniques, e.g., plasma enhanced ALD (PEALD) processing.
In one exemplary embodiment, a power source may be coupled, e.g., through a matching network (both not shown), to the blocker plate 160 when the showerhead 170 and chamber body 102 are coupled to a ground terminal. The power source may be one or more of a radio-frequency (RF) or direct current (DC) power source that energizes the gaseous compound in the plenum 129 to form a plasma. Alternatively, the power source may be coupled to the showerhead 170 when the substrate support 112 and chamber body 102 are coupled to the ground terminal. In this embodiment, the gaseous compounds may be energized to form a plasma in the reaction region 128. As such, the plasma may be selectively formed either between the blocker plate 160 and showerhead 170, or between the showerhead 170 and substrate support 112.
In detailed embodiments, the focus ring 165 and central region 164 are shaped so that when the gas distribution plate (showerhead 170) is adjacent a substrate 110 there is a first distance D1 between the central region 164 and the substrate 110 and a second distance D2 between the focus ring 165 and the substrate 110 which is less than the first distance D1 to evenly distribute the process gases. The first distance D1 is in the range of about 1.5 to about 6 times greater than the second distance. In specific embodiments, the first distance D1 is in the range of about 2 to about 4 times greater than the second distance D2.
As can be seen in
In detailed embodiments the central region 164 is substantially flat. As used in this specification and the appended claims, the term “substantially flat” means that the surface has deviations from flatness that is less than about 100 μm, or that when the central region is placed an operable distance from a substrate, there is less than about a 10% deviation, or less than about a 5% deviation, in the distance to the substrate surface. In specific embodiments, the central region 164 is slightly concave.
The size of the central region 164 of the showerhead 170, and the showerhead 170 itself, can vary depending on the size of the substrate 110. For example, as shown in
Referring again to
In specific embodiments, the plurality of openings 174 are located in the central region 164 of the front surface 176. In these embodiments, the gas flowing from the plurality of openings 174 is directed generally perpendicular to the surface of the substrate 110. It is also contemplated that the plurality of openings 174 in the front surface 176 may extend along the sloped region 166 of the focus ring and even potentially to a peripheral front face 167 area. Showerheads 170 with openings 174 on the focus ring 165 present a more complicated gas flow pattern which, depending on various factors including flow rate and pressure, may provide a more even distribution of gases across the surface of the substrate 110.
The embodiment shown in
The central port 136 or the plurality of openings 174 can also be used to inject a remotely generated plasma into the reaction region 128. In embodiments of this sort, either of the first precursor source 144 or second precursor source 138 could generate a plasma outside of the reaction region 128 and then introduce the plasma through the showerhead 170.
A channel 137 is connected to the central port 136 through a gas inlet channel 135. The channel 137 and gas inlet channel 135 are shown with different diameters but it should be understood that these sizes of these channels can be the same or different depending on the specific system configuration. The channel 137 can be connected to at least one precursor source 138 or vacuum source 139. In the embodiment shown in
The showerhead 170 may be formed from a variety of materials including a metal or another electrically conductive material. In detailed embodiments, the showerhead 170 is formed from quartz or a metal, such as aluminum, steel, stainless steel, iron, nickel, chromium, aluminum nitride, an alloy thereof or combinations thereof.
The plurality of openings 174 in showerhead 300 may be arranged in various configurations and can have differing sizes and numbers. In detailed embodiments, each of the plurality of openings 174 have a diameter within the range from about 0.10 mm to about 1.00 mm. In specific embodiments, each of the plurality of openings 174 has a diameter in the range of about 0.20 mm to about 0.80 mm. In more specific embodiments, each of the plurality of openings has a diameter in the range of about 0.40 mm to about 0.60 mm. The showerhead 170 of detailed embodiments has at least about 100 holes. In specific embodiments, the showerhead 170 has at least about 1000 openings 174 or at least about 1,500 openings 174. The showerhead 170 of some embodiments may have as many as 6,000 openings or 10,000 openings depending on size, distribution pattern of the openings 310, size of the substrate 110 to be processed and the desired exposure rate. The openings 174 may have a varying or consistent geometry from hole to hole. In a specific embodiment, the showerhead 170 is constructed from metal (e.g., aluminum or stainless steel) and has about 1,500 holes that are formed with a diameter of about 0.50 mm.
Additional embodiments of the invention are directed to process chambers 100 comprising the gas distribution plate (showerhead 170) described. In some embodiments, the process chamber 100 is a chemical vapor deposition chamber. The process chamber 100 of specific embodiments is an atomic layer deposition chamber.
Further embodiments of the invention are directed to methods of processing a substrate. A substrate 110 having an edge region 114 surrounding an inner region 115 is disposed in a process chamber 100 adjacent a gas distribution plate (showerhead 170). A reaction region 128 is defined as the region between the substrate 110 and the gas distribution plate (showerhead 170). The reaction region 128 is smaller a the edge region 114 than at the inner region 115. Stated differently, the size of the gap between the edge region 114 of the substrate and the showerhead 170 is smaller than the size of the gap between the inner region 115 and the showerhead 170. At least a first process gas from a first precursor source 144 is flowed through the plurality of openings 174 in the front surface 176 of the gas distribution plate (showerhead 170) to the substrate 110.
Some embodiments further comprise flowing at least a second process gas from a second precursor source 138 through the central port 136 in the showerhead 170 to the substrate 110. One or more embodiments further comprise applying at least a partial vacuum from a vacuum source 139 to the reaction region 128 between the substrate 110 and the central region 164 of the gas distribution plate (showerhead 170) through the central port 136 in the showerhead 170.
In detailed embodiments, a first process gas from a first precursor source 144 is flowed through a plurality of openings 174 in the showerhead 170 to the substrate 110. After the first process gas has reacted with the substrate 110, a purge gas or vacuum can be employed to remove any unreacted first process gas or reaction byproducts. A second process gas is then flowed from a second precursor source 138 through the central port 136 to the substrate 110. Each of these process gas reactions can be repeated before flowing the other process gas to the substrate and the entire process can be repeated multiple times. A third process gas (not shown) can be flowed through the showerhead 170 through the same channels 145 and openings 174 or through a different channel and openings which are segregated from the first set. This allows for multiple atomic layer deposition reactions to be performed in the same chamber with the same showerhead 170. Additionally, the third process gas can be connected to the metering/switching device 140 and allowed to flow through the central port 136 to the substrate 110.
Although the invention herein has been described with reference to particular embodiments, it is to be understood that these embodiments are merely illustrative of the principles and applications of the present invention. It will be apparent to those skilled in the art that various modifications and variations can be made to the method and apparatus of the present invention without departing from the spirit and scope of the invention. Thus, it is intended that the present invention include modifications and variations that are within the scope of the appended claims and their equivalents.