The present invention relates to the field of testing materials and more particularly to an apparatus for in-line testing and surface analysis on a mechanical property tester. More specifically, the invention relates to an apparatus and a method for in-line surface analysis on a mechanical tester, with multiple sequential measurements of the test surface by means of a microscope, interferometer, profilometer, scatterometer, or another surface-condition analyzing tool. The invention may find use in tribology and wear and scratch testing.
During a tribology test, the engaging surfaces of two samples are brought in contact to measure friction and wear. In a reciprocating, rotary, fretting, or oscillating test, one of the samples may move while the other sample remains stationary. In some cases, the upper sample may be stationary while in other cases the upper sample may be moveable. The test requires applying a known force and studying the effects of force, speed, time, temperature, or other factors of friction, wear, life of coatings or bulk materials, lubricants, fluids, etc. In tribology, important parameters are load, stroke, speed, and environmental conditions.
A variety of methods and apparatuses can be used for measuring and analyzing the results of tribology tests. Such methods and apparatuses can be classified as mechanical, electrical, and optical. Each of these groups offers different implementation. For example, a scratch test measures the adhesion or hardness of coating or matrix materials. Typically, such a test involves moving a sharp tip for a fixed distance at a known velocity under an increasing or constant load. The final scratch marks are analyzed (during and after test) to calculate adhesion or hardness of the material. Such methods and apparatus are available in a variety of modifications, one of which is a tester coupled with an atomic force microscope.
For example, US Patent Application Publication 2015/0075264 issued in 2015 discloses an optical microscope used for pre-inspection of a subject, wherein an atomic force microscope (AFM) integrated with the optical microscope is passed over a subject and the subject surface is scanned according to the measured deflection of the AFM cantilever. A laser is directed at the cantilever, and the reflected laser light is incident on a photodiode that accordingly detects deflection of the cantilever. The AFM cantilever deflects according to one of the mechanical contact forces, van der Waals force, capillary forced, chemical bonding, electrostatic force, magnetic force, etc.
One of the advanced methods in the field of material testing is the use of confocal microscopy (see. e.g., U.S. Pat. No. 7,839,496 issued on Nov. 23, 2010 to Leonard J. Borucki). The invention relates to a sample holder for confocal microscopy of chemical mechanical polishing (CMP) pad samples cut or otherwise removed from either new or used CMP pads that maintains uniform load and pressure over the part of the sample visible to the confocal microscope.
U.S. Pat. No. 5,760,950 issued on Jun. 2, 1998 to Maly, et al, discloses a scanning confocal microscope optical system for forming an image of a subject illuminated by light from an illumination system that includes a Nipkow disk arranged perpendicular to a light propagation path and that has a surface on which a plurality of pinholes are distributed substantially symmetrically about an axis perpendicular to the surface of the disk. The system further includes components for projecting an image of a first set of pinholes onto a second set of pinholes, the image being formed of light transmitted by the first set of pinholes when the first set is illuminated by light that impinges on the first side of the disk. The system further includes a collective lens and a first objective lens for focusing light transmitted by the second set of pinholes onto the subject and for collecting light reflected by the subject. The first objective lens has a large numerical aperture. Light reflected by the subject passes through the second set of pinholes. Finally, the system may include a device for spinning the Nipkow disk about the axis.
Chinese Patent No. 102607977 B issued in 2014 describes an abrasion in-situ measuring device and a method based on digital image processing. This device comprises an attachment to a universal material tester and contains a frame attachable to the base of the tester and supporting sliders moveable in the directions of X, Y, and Z axes, one slider of which carries a digital microscope that can be used for recording the results of testing in situ and for subsequent analysis of the recorded data.
However, the device of the type described above has disadvantages such as positional inaccuracy after attachment/dismantling; nonrepeatability of measurement point position at multiple measurements of the same sample in the course of a single test cycle, a complex structure, low compactness, etc.
Also known in the art are various interferometers such as a Fabry-Pérot and Nomarsky. An interferometer suitable for tribology is the Nexview™ 3D Optical Surface Profiler of Zygo®, CT, USA. This interferometer is capable of measuring any surface—from super smooth to very rough, with subnanometer precision.
The interferometer includes an automated 200-mm Integrated Measurement Stage. In tribology this instrument is used, e.g., for 3D measurements and for inspection of surface roughness, in particular, for inspection of properties such as height of micro roughness and surface nonuniformity.
The apparatus of the invention for in-line testing and surface analysis of a sample on a mechanical property tester contains a base that supports a column in a stationary manner and moveably supports an X-stage with a drive unit for moving the X-stage on the base in the direction of the X-axis. The X-stage, in turn, supports a tribology drive unit with a replaceable drive that may reproduce linear reciprocation of the sample in the X-axis or Y-axis direction or rotation of a sample table that supports a sample to be tested. The column moveably supports at least two units, one being an optical microscope and the other being a test unit that may function as a hardness tester, or alternatively, the column may additionally support a second test unit, e.g., a scratch or abrasive wear tester, and a microscope in combination with an interferometer for 3D measurements. In all cases, the sample holding unit moves along a line that is oriented in the X-axis direction and may be aligned with the position of the working field of the optical microscope so that after each test the sample can be repeatedly positioned in the working field of the optical microscope and/or interferometer without removal from the sample table supported by the tribology drive unit on the X-stage. The Y-axis movement of the tribology drive unit may be used for presetting the position of the sample relative to the optical instrument or interferometer before multiple and repeated movement of the X-stage in the X-axis direction. Such an arrangement makes it possible to provide compact construction, reliably positioning the sample in the same place for repeated measurements to observe the dynamics of changes on the surface of the sample and to improve repeatability and accuracy of the measurement results. Alternately, the apparatus of the invention may combine a confocal microscope with an interferometer since the confocal microscope allows observation of the sample surface, while the interferometer allows 3D measurements of the surface structural elements, such as micro roughness caused by, e.g., an abrasion test. Precise positioning of the sample at the same point during multiple, repeated observations and measurements is provided by installing the tribology drive unit on a layered piezoelectric drive package that is equipped with X,Y,Z microdrives for scanning movements of a small portion of the sample surface relative to an optical beam of the interferometer.
Based on their test results, the inventors herein showed that mechanical property test results depend on the surface morphology of test samples. Surface parameters such as surface roughness, texture, tilt, etc., may significantly affect final test data (friction, wear, hardness, adhesion, etc). The inventors herein concluded that multiple surface parameter information obtained exactly at the point of test can help tremendously to obtain correct test results.
Also, after test completion, important post-test parameters such as volume wear, roughness change, crack propagation, etc., may be needed to perform test-data analysis. Currently, samples are removed from the mechanical tester and are then taken to different surface measurement instruments for pre-test and post-test measurements.
The present invention comprises an apparatus that integrally combines a material test unit with a sample measurement and analysis system installed on and sharing a common base; and a Y-stage, X-stage, and common column for supporting at least two individual Z-stages, one for the test unit and one for the measurement unit. Such an arrangement makes it possible to provide compact construction, to reliably position a sample at the same location in case of repeated measurements for observing the dynamics of surface changes on the sample, and to improve repeatability and accuracy of measurement results.
The apparatus of the invention is designated by reference numeral 20 and is schematically shown in
The apparatus 20 comprises a base 22 that supports Y-stage 24, which is moveable in the direction of the Y-axis and perpendicular to the plane of the drawings (see
The above-described systems with two standard motorized stages moveable in X and Y directions are well known and commercially available, e.g., from GMT Global Inc. Each X-Y stage is a standard unit of CXN and CXC series with table sizes from 50×50 mm to 80×80 mm. The travel length for the stages may reach 420 mm. The drive is performed from a motor through a precise ball screw shaft of the C5 level of accuracy. The commercially available X-Y system mentioned above is given only as an example; many other similar systems can be used for the purposes of the invention. All the X-Y stages are equipped with respective stepping motors or servomotor drivers, which are controlled from a central processing unit (CPU).
The tribology drive 30 comprises an interchangeable unit that may be driven either from a reciprocating linear drive in the X-axis direction or from a rotary drive (see
Reference numeral 36a(
An example of a mechanism 45 for rotation of a sample table 34b is shown in
The sample table 34b is used for securing and holding a sample or specimen to be tested (not shown in
CPU controllable tester motions mentioned above for tribology drives 30a and 30b are exemplified by motions of lower drives on commercially available tribology testers produced by a number of manufacturers.
For example, American Electric Power Technology (USA) offers the tribology tester UT-3000 with various, easily interchangeable lower drives such as rotary, fast reciprocating, block on ring, linear drive, etc., to replicate any motion. Choice of the drive is dictated by the test required, such as scratch test that uses a linear drive, fretting test that uses a fast reciprocating drive, or a pin on disk test that uses a rotary drive, and so on. All of these drives are independently programmable, and their interrelationships will be described later with reference to
Bruker Company offers a Universal Mechanical Tester (UMT) that offers a wide range of interchangeable drives and fixtures for testing samples under multiple different wear patterns on a single test platform. The UMT offers users infinite combinations of synchronized motion control for both upper and lower samples. The upper sample can be translated along any axis or rotated. Motion can occur either unidirectionally or in a programmed combination of axes and speeds. The lower sample has a wide range of available motion control. Linear translation is available in X and Y axes, as well as fast reciprocating linear motion for fretting and wear tests. Changeover from reciprocating to rotary motion takes just a few minutes, and the lower sample can be rotated along the vertical axis (pin-on-disk) or horizontal axis (block-on-ring).
A unique feature of the apparatus 20 of the invention for in-line test and surface analysis is a combination of a Z-axis test unit, or at least two Z-axis test units, which are installed on a common vertical column, with a measurement unit, e.g., a microscope, and/or interferometer, wherein the microscope and/or interferometer and the Z-axis test unit or units are arranged on the same line oriented in the X-axis direction, secured on the common column with possibility of adjustable positioning in the Z-axis direction, and located exactly above the trajectory of movement of the sample carried by the X-stage in the X-axis direction so that after each test the sample can be repeatedly placed into the same position for optical analysis without removal from the sample table. Such an arrangement makes it possible to provide compact construction, to reliably position the sample at the same place in case of repeated measurements for observing dynamics of changes on the surface of the sample, and to improve repeatability and accuracy of measurement results.
More specifically, as shown in
An example of a hardness tester 38 that can be installed on the column 26 is the EZ-X Series Tabletop Electromechanical Universal Tester of Simadzu Co., Japan. This tester has a capacity up to 500 N. It is equipped with high-performance load cells with accuracy of ±0.5% or ±1% of the indicated force value. The EZ-X series can be connected with the CPU of the testing machine 20 and provides objective numerical test results that can supplement analysis data. The hardness tester 38 makes it possible to test hardness by various methods such as Brinell, Vickers, Rockwell, etc.
The test probe 42, which is shown as a Brinell hardness spherical probe, is intended to interact with a sample (not shown), which is installed on the sample table 34a (
Installed on the same column 26 in its own guides 40 is a microscope 44, which is intended for observation and optically recording results of the sample tests. These results are transmitted to the CPU (
After the sample testing operation on the tribology drive 30 is over, the test unit 38 is lifted, and the entire X-stage 28 is moved by the X-stage drive, such as a lead screw and nut mechanism (27a, 27b) to the position aligned with the objective lens 44a of the microscope 44 where observation and recording of the observation analysis can be performed in accordance with conventional practice. The position of the apparatus units is shown in
It is understood that the Brinell tester with the spherical indenter 42 is shown only as an example, and the indenter may have a pyramid shape for measuring hardness on a Vickers scale, or the like.
A great variety of microscopes is available for the purposes of the invention. Most suitable is an optical digital microscope with a bright field for microscopy associated with digital imaging, a wide range of working distances, and possibilities for adjusting positions and incidence angles of light beams, etc. Reference numeral 43 (
If necessary, the column 26 may support a second Z-stage test unit 46, the position of which can be adjusted in its own vertical guides 48. The test unit 46 is provided with a tool/specimen holder 50 in which an upper stationary member 52 (
It is understood that the second Z-stage test unit 46 is equipped with a force measurement cell (not shown) that is connected to the CPU for processing the results of the tests obtained on this unit and for combining the obtained data with the data from other units in the final analysis of the sample characteristics. Such devices are known in the art.
Operation of the apparatus 20 of the invention for in-line testing and surface analysis is described below with reference to
a, and 6b illustrate another modification of the apparatus, wherein
In
As shown in the above-named drawings, the apparatus of the invention combines the laser scanning reflective confocal microscope 70 with the interferometer 72.
Such microscopes are commercially available on the market. An example is LT-9000 series Surface Scanning Laser Confocal Displacement Meter that can be purchased from Keyence, Il, USA. This device provides two-directional scanning for accuracy and stability. It combines a tuning fork and oscillating unit for using a surface-scanning laser. This allows advanced displacement and profile measurements that are unaffected by target color or angle. The microscope of LT-9000 type produces Z-axis scanning by combining a tuning fork with the confocal principle. X-axis scanning is provided by installing the tribology drive unit 74a (for linear movements) or 74b (for rotary movements) on a layered piezoelectric drive package 76 that is equipped with X,Y,Z microdrivers which are sandwiched into a layered structure for performing scanning micro displacements relative to the beam emitted from the laser scanning reflective confocal microscope 70 (
The Z-axis microdriver 77c consists of three subunits 77c-1, 77c-2 and 77c-3 on which the tribology drive unit 74a (in case of linearly tested sample) or the tribology drive unit 74b (in case of rotary tested sample) rests.
As a result, the beam may scan a small portion of the surface of the sample (not shown) supported by the sample table 80a (or 80b) installed on the tribology drive unit 74a (or 74b) in X, Y, or Z directions.
The layered piezoelectric drive package 76 with X, Y microdrives is commercially available, e.g., from ThorLabs, NJ, USA. Such units comprise Amplified Piezoelectric Actuators, 220 μm to 420 μm travel and are made in the form of 75-V Low Voltage Piezo Stacks, which develop displacement force up to 100 N with the stroke length of 220 μm or 420 μm.
Each Z-axis direction microdriver 77c-1, 77c-2, and 77c-3 is known and commercially available, e.g., from Physik Instrumente, Germany. For example, each Z-axis microdrive comprises a P-601 Motion-Amplified Piezo Flexure Z-Actuator which is a Flexure Guidance for Frictionless, Ultra-Straight Motion. This actuator has a travel ranges to 480 μm and resolution to 0.2 nm.
By coordinating the results of precise 3D measurements of the elements of surface topology made by an interferometer with the results of measurements obtained from a confocal reflective laser microscope, it becomes possible to install the selected portion of the sample surface at the same point during multiple, repeated measurements performed during the test without removing the sample from the sample table. Such periodic measurements on the same sample and in the same place of the sample surface are needed for observing and recording the dynamics of surface changes, e.g., under the effect of scratching or abrasion. Such results are possible only when a microscope and interferometer provided with a surface microscanning function are used as an indispensable combination. Another unique feature is that the aforementioned micro displacements are performed by the sample table installed on a tribology table moveable with scanning motions relative to the stationary measuring optical beam.
Although the invention is shown and described with reference to specific embodiments, it is understood that these embodiments should not be construed as limiting the areas of application of the invention and that any changes and modifications are possible, provided these changes and modifications do not depart from the scope of the attached patent claims. For example, test units other than the hardness tester, scratch tester, or abrasive wear tester can be installed on the column 26. Drives different from the screw-and-nut type can be used for moving the X-stage. The test units may be located on the left side of the column, and the microscope may be installed on the right side of the column.
Number | Name | Date | Kind |
---|---|---|---|
3147017 | Dunham | Sep 1964 | A |
4451197 | Lange | May 1984 | A |
5852232 | Samsavar | Dec 1998 | A |
6015174 | Raes et al. | Jan 2000 | A |
6057547 | Park | May 2000 | A |
6272907 | Neukermans | Aug 2001 | B1 |
7489407 | Hill | Feb 2009 | B2 |
7978346 | Riza | Jul 2011 | B1 |
8353060 | Watanabe | Jan 2013 | B2 |
8742344 | Hatakeyama | Jun 2014 | B2 |
8902431 | Liesener | Dec 2014 | B2 |
20030052495 | Casarotti et al. | Mar 2003 | A1 |
20040075288 | Baker | Apr 2004 | A1 |
20060157998 | Gershenzon et al. | Jul 2006 | A1 |
20060163480 | Koyama | Jul 2006 | A1 |
20130056635 | Kimba | Mar 2013 | A1 |
20130147939 | Nawata | Jun 2013 | A1 |
20140158885 | Noji | Jun 2014 | A1 |
20140312227 | Yoshikawa | Oct 2014 | A1 |
20150097116 | Hatakeyama | Apr 2015 | A1 |
20150206704 | Momoi | Jul 2015 | A1 |
20150287570 | Hayashi | Oct 2015 | A1 |
20170067735 | Khosla | Mar 2017 | A1 |
Number | Date | Country |
---|---|---|
WO1997045862 | Dec 1997 | WO |
Number | Date | Country | |
---|---|---|---|
20180024035 A1 | Jan 2018 | US |