1. Field of Invention
The invention relates generally to the processing of semiconductor wafers, and relates more particularly to an apparatus for reducing entrapment of foreign matter along a moveable shaft of a substrate support.
2. Background of the Invention
Integrated circuits have evolved into complex devices that can include millions of transistors, capacitors and resistors on a single chip. The evolution of chip designs continually requires faster circuitry and greater circuit density that demand increasingly precise fabrication techniques and processes. One fabrication process frequently used is chemical vapor deposition (CVD). Chemical vapor deposition is generally employed to deposit a thin film on a substrate or a semiconductor wafer.
Chemical vapor deposition is generally accomplished by introducing a precursor gas into a vacuum chamber. The precursor gas is typically directed through a showerhead situated near the top of the chamber. The precursor gas reacts to form a layer of material on the surface of the substrate that is positioned on a heated substrate support (e.g., a heater) typically fabricated from aluminum. In some systems, the substrate support is mounted upon a moveable (e.g., moveable longitudinally, or rotatable) shaft that is disposed within a sleeve. Purge gas is routed through holes in the support to the edge of the substrate to prevent deposition at the substrate's edge that may cause the substrate to adhere to the support. Deposition by-products produced during the reaction are pumped from the chamber through an exhaust system.
In operation, particles or loose foreign matter may be generated by the system, or inadvertently introduced thereto, and these particles can travel within the confines of the chamber. In particular, particles may travel near the shaft utilized to control the elevation of a substrate support within the processing chamber. The particles may stick to the moving shaft and accumulate in the annulus, or gap, between the shaft and the sleeve that guides the shaft through the bottom of the chamber. The accumulation of particles between the shaft and sleeve can damage both components, leading to premature wear and/or failure of the system.
Reducing the annulus between the sleeve and the shaft is one method for minimizing the area in which particles may travel and/or become trapped. Although reducing the gap is a generally effective method for reducing particle accumulation and damage, a small gap still exists that is typically large enough to trap smaller particles. Alternatively, some designs have employed o-rings (sometimes in conjunction with a lubricant) positioned to seal the gap. However, standard o-rings are subjected to abrasion by particulates disposed on the shaft, and thus may not effectively seal the gap after a period of use. Furthermore, standard o-rings tend to generate particles when subjected to processing chamber conditions, exacerbating the particle entrapment problem rather than solving it.
Therefore, there is a need for an apparatus for reducing the entrapment of particles and foreign matter along a moveable shaft of a substrate support.
In one embodiment, a guard ring for reducing particle entrapment along a moveable shaft of a substrate support is provided. In one embodiment, a substantially annular guard ring is positioned within a step formed in a sleeve that circumscribes the shaft. The guard ring is positioned to substantially seal a gap separating the shaft from the sleeve, advantageously reducing component wear due to particulate entrapment.
In another embodiment, a guard ring comprises a base portion having an inner perimeter and an outer perimeter, a first flange coupled to the inner perimeter, a second flange coupled to the outer perimeter, and a continuous channel separating the first flange from the second flange. The first flange is adapted to bias the ring against the shaft, thereby accommodating displacement and/or misalignment of the shaft relative to the processing chamber.
So that the manner in which the above recited features of the present invention may be understood in detail, a more particular description of the invention, briefly summarized above, may be had by reference to embodiments, some of which are illustrated in the appended drawings.
To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that features of one embodiment may be beneficially incorporated in other embodiments without further recitation.
It is to be noted, however, that the appended drawings illustrate only exemplary embodiments of this invention and are therefore not to be considered limiting of its scope, for the invention may admit to other equally effective embodiments.
The invention is a guard ring for preventing particle entrapment along a moveable shaft of a substrate support. The invention is illustratively described below as deployed in a chemical vapor deposition system, such as a barrier chemical vapor deposition (BCVD) system, available from Applied Materials, Inc. of Santa Clara, Calif. However, it should be understood that the invention has utility in other system configurations such as physical vapor deposition systems, ion implant systems, etch systems, chemical vapor deposition systems and any other wafer processing system in which the reduction of particle damage to a moving shaft is necessary or desirable.
The lid 110 is supported by the walls 106 and can be removed to service the chamber body 102. The lid 110 is generally comprised of aluminum and may additionally contain heat transfer fluid channels for regulating the temperature of the lid 110 by flowing a heat transfer fluid therethrough.
A showerhead 118 is coupled to an interior side 120 of the lid 110. The showerhead 118 is typically fabricated from aluminum. The showerhead 118 generally includes a perimeter mounting ring 122 that surrounds a “dish-shaped” center section 124. The mounting ring 122 includes a plurality of mounting holes 126 that pass therethrough, each accepting a mounting screw 128 that threads into a mating hole 130 in the lid 110. The center section 124 includes a perforated area 132 that facilitates passage of gases therethrough.
A mixing block 134 is disposed in the lid 110. The mixing block 134 is coupled to the gas source 104, such that process and other gases may be introduced to the process volume 112 by passing through the mixing block 134 and showerhead 118. Typically, cleaning gases from a cleaning source (not shown) are also introduced through the mixing block 134 to the process volume 112. A perforated blocker plate 136 is disposed between the showerhead 118 and mixing block 134 to enhance the uniform distribution of gases passing through the showerhead 118 and into the chamber body 102. The blocker plate 136 is typically fabricated from aluminum.
A substrate support assembly 138 is disposed beneath the showerhead 118, typically centrally disposed within the chamber body 102. The support assembly 138 supports a substrate 140 during processing and includes an elevator shaft 142 coupled thereto. The support assembly 138 generally is fabricated from aluminum, ceramic or a combination of aluminum and ceramic. The support assembly 138 typically includes a vacuum port (not shown) and at least one embedded heating element (not shown). The vacuum port is used to apply a vacuum between the substrate 140 and support assembly 138, for securing the substrate to the substrate support assembly 138 during processing. The heating element, such as an electrode disposed in the support assembly 138, is coupled to a power source (not shown) for heating the support assembly 138 and substrate 140 positioned thereon to a predetermined temperature. In one embodiment, the heating element maintains the substrate 140 at a uniform temperature of about 150 to 400 degrees. Alternatively, heating lamps or other heat sources may be utilized to heat the substrate 140.
The shaft 142 is coupled between the support assembly 138 and an actuator 144. The shaft 142 provides a conduit for electrical leads, vacuum and gas supply lines between the support assembly 138 and other components of the system 100. The actuator 144 moves the support assembly 138 between an elevated position as shown for processing and a lowered position for facilitating substrate transfer. In addition, the actuator 144 may include a mechanism for rotating the shaft 142. A bellows 146 disposed between the support assembly 138 or shaft 142 and the chamber bottom 108 provides a vacuum seal between the process volume 112 and the atmosphere outside the chamber body 102 while facilitating movement of the support assembly 138.
In one embodiment, the shaft 142 is disposed substantially centrally through an aperture 152 formed in the chamber bottom 108. In another illustrated, the aperture 152 is formed in sleeve disposed in the chamber bottom 108. Alternatively, a sleeve may be formed integrally in the bottom 108 of the chamber body 102. The sleeve 150 is generally a bushing positioned in the chamber bottom 108 to prevent gauling or other wear issues as the shaft 142 moves through the aperture 152 formed in the bottom 108.
The support assembly 138 generally is grounded such that RF power supplied by a power source (not shown) to the showerhead 118 (or other electrode positioned within or near the lid assembly of the chamber) may excite the gases disposed in the process volume 112 between the support assembly 138 and the showerhead 118. The RF power, generally having a frequency of between a few Hz to 13 MHz or higher is provided in a wattage suitable for the substrate surface area. In one embodiment, the power source comprises a dual frequency source that provides a low frequency power at less than about 2 MHz (preferably about 200 to 500 kHz) and a high frequency power at greater than 13 MHz (preferably about 13.56 kHz). The frequencies may be fixed or variable. Illustratively, for a 550 mm×650 mm substrate, the low frequency power is about 0.3 to about 2 kW while the high frequency power is about 1 to 5 kW. Generally, the power requirements decrease or increase with a corresponding decrease or increase in substrate size.
As illustrated in
In operation, the semiconductor substrate 140 is secured to the support assembly 138 by providing a vacuum therebetween. The temperature of the substrate 140 is elevated to a pre-determined process temperature by regulating thermal transfer to the support assembly by the heating element. During the deposition process, the substrate is heated to a steady temperature, typically between 300° C. and 550° C.
Gaseous components, which in one embodiment may include silane and tungsten hexafluoride, are supplied from a gas panel to the process chamber through the mixing block 134 and showerhead 118 to form a gaseous mixture. The gaseous mixture reacts to form a layer of tungsten on the substrate 140. To prevent deposition at the substrate's edge and possible adherence of the substrate 140 to the support assembly 138, purge gases flow from a conduit in the support assembly 138 around the perimeter of the substrate 140.
Returning to
Returning to
In one embodiment, the shaft 142 is positioned substantially concentrically within the sleeve 150, and the lip 240 is substantially continuous around the circumference of the shaft 142. However, if the shaft 142 shifts so that the shaft 142 becomes positioned eccentrically within the sleeve 150, the distance from the shaft 142 to the sleeve 150 will vary around the diameter of the shaft 152. Thus in one embodiment, the guard ring 162 is formed of a resilient material, and the sealing lip 240 has a diameter that is smaller than the diameter of the shaft 142 so that contact is maintained around the shaft's diameter even when there is eccentricity between the shaft 142 and sleeve 150.
The guard ring 162 is positioned to substantially prevent the entrapment of particles and loose foreign matter between the shaft 142 and the sleeve 150. Referring back to
In an embodiment illustrated in a top view of a guard ring 400 in
In another embodiment illustrated in
In another embodiment illustrated in
Referring simultaneously to
The guard ring 604 illustrated in
Thus, the present invention represents a significant advancement in the fabrication and processing of integrated circuits. A guard ring and assembly are provided that substantially prevent the entrapment of particles and foreign matter between a sleeve and a substrate support having a moveable shaft. Therefore, the occurrence of premature wear and/or failure of a processing system due to particle entrapment is substantially reduced.
Although the teachings of the present invention that have been shown and described in detail in a plasma enhanced chemical vapor deposition chamber, those skilled in the art can readily devise other varied embodiments in other processing chambers that incorporate the use of lift pins to separate a substrate from a support surface that still incorporate the teachings and do not depart from the scope and spirit of the invention.
This application is a divisional of U.S. patent application Ser. No. 10/775,769 filed Feb. 5, 2004 now U.S. Pat. No. 7,279,049, which is incorporated by reference in its entirety.
Number | Name | Date | Kind |
---|---|---|---|
3830508 | Endicott | Aug 1974 | A |
3951478 | Olsen et al. | Apr 1976 | A |
5273588 | Foster et al. | Dec 1993 | A |
5508519 | Bennett et al. | Apr 1996 | A |
5873177 | Honda et al. | Feb 1999 | A |
5938343 | Grantz et al. | Aug 1999 | A |
6221221 | Al-Shaikh et al. | Apr 2001 | B1 |
6506257 | Horiguchi et al. | Jan 2003 | B2 |
6932885 | Oka | Aug 2005 | B1 |
20030141673 | Olgado et al. | Jul 2003 | A1 |
Number | Date | Country |
---|---|---|
10-163155 | Jun 1998 | JP |
11-108196 | Apr 1999 | JP |
11-135469 | May 1999 | JP |
Number | Date | Country | |
---|---|---|---|
20080017115 A1 | Jan 2008 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 10775769 | Feb 2004 | US |
Child | 11866505 | US |