Barrel container for use with dry barrel polishing

Information

  • Patent Application
  • 20020013125
  • Publication Number
    20020013125
  • Date Filed
    July 24, 2001
    23 years ago
  • Date Published
    January 31, 2002
    22 years ago
Abstract
A barrel container for a dry barrel polishing machine includes a container body made of an elastic material and having an access opening through which polishing chips and workpieces are put into the container body, the container body having a wall with a through hole providing communication between an exterior and an interior of the container body, and a lid opening and closing the access opening.
Description


BACKGROUND OF THE INVENTION

[0001] 1. Field of the Invention


[0002] This invention relates generally to dry barrel treating machine grinding, polishing or cleaning workpieces, and more particularly to a barrel container used with a dry barrel polishing machines.


[0003] 2. Description of the Related Art


[0004] One of types of barrel polishing machines uses a rotational barrel container. The barrel container includes a container body having an opening and a lid closing the opening of the container body. The container body comprises a casing generally made of steel and a lining made of an elastic material and attached to an inner wall of the casing. The lining relieves collision of polishing chips and workpieces against an inner wall of the barrel container during polishing, thereby preventing the steel wall of the container from wear. The lid also includes a steel base and a lining attached to the inside of the base. One or more barrel containers are mounted on a barrel polishing machine.


[0005] The aforesaid steel casing is made by bending a steel plate 39 as shown in FIGS. 10 to 12. For example, a container body 47 as shown in FIG. 12 has a hexagonal section and includes an opening 40 formed in one of the six sides thereof. In the manufacture of the container body 47, a steel plate 39 is bent so as to have a hexagonal section. Thereafter, two hexagonal steel plates 42 are welded to both open ends of the container body respectively so that a hollow casing 41 is formed. Previously divided cores 44a and 44b are then inserted through the opening 40 into the casing 41. The divided cores 44a and 44b are connected together in the casing 41 to be assembled into an integral core 44. A bridge member 31 is mounted between flanges 45 formed along peripheral edges of the opening 40. The core 44 is then hung on the bridge member 31. A material for a lining 46, for example, molten polyurethane resin, is poured into a space between an inner wall of the casing 41 and the core 44. The molten resin is cooled to be solidified such that a barrel polishing container 47 with the polyurethane lining 46 is formed.


[0006] There are two types of barrel polishing machines, namely, dry barrel polishing machines using no water and wet barrel polishing machines using water. In view of environmental protection and economy in treating costs, the dry barrel polishing machines have recently been predominant. Japanese Patent No. 2643103 discloses a barrel container used in the dry polishing. The disclosed barrel container includes an external air intake portion or vent formed in the casing or the lid for introducing external air into the casing. The container further includes a dust exhaust portion formed in the casing or the lid for exhausting dust resulting from polishing. The barrel container is attached to a polishing machine and rotated so that polishing chips and workpieces are moved at high speeds in the barrel container. As a result, the workpieces are polished. During polishing, air is drawn through the external air intake into the barrel container by the operation of a dust collector. The drawn air is caused to flow through the polishing chips and workpieces in the barrel container to thereby cool them. Furthermore, dust resulting from polishing are exhausted through the dust exhaust portion to the dust collector side. Thus, loading of the polishing chips due to dust resulting from polishing, which is a problem peculiar to the dry polishing, can be prevented.


[0007] There are two methods of manufacturing the barrel container for dry barrel polishing machines. In one method, the steel body 41 is made in the same manner as described above and thereafter, molten polyurethane or the like is cast into the lining 46 which is attached to an inner wall of the body. Subsequently, a plurality of small holes 50 are formed so as to serve as the external air intake and the dust exhaust portion. The polishing chips and workpieces cannot pass through the holes 50. See FIG. 13A. In the other method, a large vent 51 is formed in the body 41. The lining 46 with another vent 52 slightly larger than the vent 51 is cast. Thereafter, a polyurethane piece 5 having small holes 4 is fitted with the vent 52 by bolts etc. as shown in FIG. 13B. Each hole 4 has such a diameter that the polishing chip and workpiece cannot pass therethrough.


[0008] In the former method, however, both body 41 and lining 46 need to be simultaneously drilled. It is difficult to form such a small hole as the holes 50 through which the polishing chips and workpieces cannot pass. The reason for this is that a small hole is closed upon extraction of a drill since polyurethane is an elastomer. Even if holes should be formed, end faces of the holes 50 would be deteriorated as the result of drilling. As a result, the end faces of the holes 50 would be worn such that peripheral portions of the holes are partially worn. The partial wear of the peripheral portions of the holes necessitates replacement of the overall lining, increasing the manufacturing cost.


[0009] In the latter method, a steel plate with vent holes 51 is bent into the steel body 41. Thereafter, when the lining is formed, dummy molds are fitted with the vents 51 and 52 respectively so that the material for the lining can be prevented from flowing into the vents 51 and so that the vents 52 are formed in the lining 46 after completion of the lining. The dummy molds are removed after the material for the lining has been solidified. The polyurethane piece 5 having small holes 4 through which the polishing chip and workpiece cannot pass is attached to the vents 52 by bolts. However, since the steel body 41 has a definite limitation of accuracy in the bending, spring back sometimes results in distortion as shown in FIG. 14 after bending. As a result, a space between the body 41 and the core 44 becomes non-uniform when the lining 46 is formed. One vent 51 is displaced such that a thickness of the lining becomes non-uniform. When the polyurethane piece 5 is fixed to the vent 52 by bolts, a difference is made between a thickness of the piece 5 and the thickness of the lining of the vent 52. The difference causes the aforesaid partial wear. A downward force is applied to the body 41 from above particularly when the lid is closed, whereupon the distortion is increased. This increases the difference between the thicknesses of the piece 5 and the lining, resulting in a gap.


[0010] Further, polishing chips and workpieces are moved at high speeds in the barrel container in the dry barrel polishing. Accordingly, the polishing chips and workpieces repeatedly collide against the lining wall. When the workpieces are soft, the collision results in marks on the workpieces. Water serves as a buffer in the conventional wet polishing, thereby preventing forming of the marks on the workpieces. Accordingly, the conventional barrel container for the wet barrel polishing has a high hardness from the viewpoint of wear resistance. However, when the container for the dry barrel polishing has the same hardness as that of the wet barrel polishing, the aforesaid marks are formed on the workpieces.



SUMMARY OF THE INVENTION

[0011] Therefore, an object of the present invention is to provide a barrel container which has an inner wall with no difference in thickness in spite of the presence of a vent and in which workpieces are hard to undergo marks due to collision against the inner wall.


[0012] The present invention provides a barrel container for a dry barrel polishing machine, comprising a container body made of an elastic material and having an access opening through which polishing chips and workpieces are put into the container body, the container body having a wall with a through hole providing communication between an exterior and an interior of the container body, and a lid opening and closing the access opening.


[0013] According to the above-described barrel container, the container body is made of the elastic material although the conventional casing body is made of steel. Accordingly, the container body has a uniform thickness in spite of the presence of the vents. There is no difference in the thickness even when a piece having the same thickness and formed with small holes is attached to the container body. Furthermore, since the container body is made of the elastic material such the polyurethane resin, it is light-weight, and a load of carrying the barrel container can be reduced. Furthermore, when the container body is made of the polyurethane resin with high wear and abrasion resistance, the barrel container can be used for a long period of time. Moreover, since the container body of the barrel container has a larger thickness than the lining of the conventional container body made of steel, the service life of the barrel container can further be improved. Additionally, shock due to the collision of workpieces against the inner wall of the container body can be reduced in the dry barrel polishing as compared with the case of the wet barrel treatment. Thus, the marks due to the collision can be reduced.


[0014] In a preferred form, the elastic material is polyurethane. In this case, the polyurethane preferably has a hardness ranging between 60 and 80 in ISO 7619 Shore A durometer hardness. Consequently, shock due to the collision of workpieces against the inner wall of the container body can be reduced in the dry barrel polishing as compared with the case of the wet barrel treatment. Thus, the marks due to the collision can be reduced.


[0015] In another preferred form, the container body has a hole formed in the wall thereof. In this case, the barrel container further comprises a piece made of an elastic material and having a number of small holes, the piece being attached to the hole of the wall of the container body. Additionally, the barrel container further comprises a plate mounted on an outer wall of the container body so as to cover the hole, the plate having air permeability. In this case, the piece is bolted to the plate at an inner wall of the container body.


[0016] In further another preferred form, the barrel container further comprises a barrel casing enclosing the container body with a space being defined in the barrel casing so as to communicate via the through hole of the container body with an interior of the container body, and a hollow shaft supporting the barrel container so that the barrel container is rotatable, the shaft having a communication passage defined therein so as to provide communication between the space of the barrel casing and a dust collector.


[0017] In still further another preferred form, the container body has a hexagonal section and includes two peripheral sides adjacent to the access opening and a bottom, said peripheral sides and bottom being formed with a plurality of the through holes respectively, the bottom communicating with the space in the barrel casing for exhaust of air, the two peripheral sides communicating via the barrel casing with an exterior of the barrel casing for intake of air.







BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Other objects, features and advantages of the present invention will become clear upon reviewing the following description of a preferred embodiment, made with reference to the accompanying drawings, in which:


[0019]
FIG. 1 is a front view of a barrel container of one embodiment in accordance with the present invention;


[0020]
FIG. 2 is a plan view of the barrel container;


[0021]
FIG. 3 is a side view of the barrel container;


[0022]
FIG. 4 is a sectional front view of the barrel container;


[0023]
FIG. 5 is a sectional side view of the barrel container;


[0024]
FIG. 6 is a sectional front view of a barrel casing enclosing the barrel container with a lid being attached to the barrel container;


[0025]
FIG. 7 is a partially sectional side view of the barrel casing enclosing the barrel container;


[0026]
FIG. 8 is a sectional side view of a plurality of the barrel containers mounted on a turret;


[0027]
FIG. 9 is a sectional view of a container body of the barrel container, showing a manufacturing stage of the container body;


[0028]
FIG. 10 is a schematic exploded perspective view of a body of a conventional barrel container;


[0029]
FIG. 11 is a sectional view of the body in which a core is set;


[0030]
FIG. 12 is a perspective view of the conventional barrel container with a lining attached thereto;


[0031]
FIGS. 13A and 13B are sectional views of a container body for the conventional barrel container; and


[0032]
FIG. 14 is a partially broken enlarged section of the container body.







DETAILED DESCRIPTION OF A PREFERRED EMBODIMENT

[0033] One embodiment of the present invention will be described with reference to FIGS. 1 to 5. Referring to FIG. 1, the barrel container 1 of the embodiment is shown. The barrel container 1 comprises a container body 2 and a lid 3. The container body 2 is made of an elastic material, for example, by molding from molten polyurethane resin. The polyurethane resin has a hardness of 70 in ISO 7619 Shore A durometer hardness. No water is used as a buffer in the dry barrel polishing. Accordingly, since workpieces violently collide against an inner wall of the container body 2, the workpieces are easy to have marks due to the collision. However, the marks due to the collision can be reduced when the hardness of the container body 2 is set at such a value as described above. When the hardness of the container body 2 is less than 60 in ISO 7619 Shore A durometer hardness, the mechanical strength of the container body 2 is too low. When the hardness of the container body 2 exceeds 80, the marks on the workpieces due to the collision tend to be increased. Thus, the hardness of the container body 2 preferably ranges between 60 and 80 in ISO 7619 Shore A durometer hardness type A. Although the container body 2 is made of the polyurethane resin in the embodiment, a thermosetting resin solidified by the molding, such as a polyester resin, maybe used instead of the polyurethane resin.


[0034] The container body 2 has a hexagonal section and accordingly includes six peripheral sides. Both ends of the container body 2 serve as thick portions 2a reinforcing the body. Two of the six peripheral sides are formed with vents 25a and 25b respectively. Each vent is dimensioned so that polishing chips and/or workpieces are allowed to pass therethrough. Two steel plates 6a and 6b are embedded during molding so as to surround the vents 25a and 25b on the outer faces of the peripheral sides of the container body 2 respectively. Each of the plates 6a and 6b has a central opening. Two polyurethane pieces 5a and 5b are fixed to the plates 6a and 6b by bolts and nuts inside the casing body 2. Each of the pieces 5a and 5b has a number of small holes 4 through which the polishing chips and workpieces are not allowed to pass. The polyurethane pieces 5a and 5b, and the small holes 4 are also formed by the molding.


[0035] The container body 2 has an access opening 2b formed in one of the peripheral sides thereof. The polishing chips and workpieces are put through the opening 2b into the container body 2. The opening 2b has a peripheral edge protruding in its entirety. The protruding edge of the opening 2b serves as a seal 2c sealing the opening when the lid 3 is closed. A rectangular reinforcing frame 7 is embedded in the container body 2 during the molding so as to be disposed around the seal 2c. The frame 7 may or may not be provided. A connecting plate 24 is screwed to the frame 7. A carrying bar 8 is mounted on the plate 24.


[0036] The manufacture of the container body 2 will now be described with reference to FIG. 9. A metal mold 30 has an inner face conforming to a shape of the container body 2. The mold 30 is divided into pieces 30a, 30b and 30c when the molten resin is solidified into the container body 2 to be taken out of the mold. A bridge member 31 is mounted on an upper end of the mold 30. A core 32 is hung on the bridge member 31 as shown in FIG. 9. The core 32 is also divided into pieces 32a and 32b so that the solidified container body 2 is taken out of the mold. The aforesaid plates 6a and 6b and frame 7 are fixed to the mold 30 by screws (not shown) so as to be located to correspond to the vents 25a and 25b and opening 2b respectively. Dummy molds 33a and 33b are mounted on the plates 6a and 6b further mounted on the mold 30, so as to correspond to the vents 25a and 25b, respectively. The container body 2 has a thickness equal to an addition of a thickness of the dummy mold 33a or 33b and a thickness of the plate 6a or 6b.


[0037] The molten polyurethane resin is poured into the mold 30 when the bridge member 31, core 32, plates 6a and 6b, frame 7 and dummy molds 33a and 33b have been set on the mold 30. Upon solidification of the resin, the core 32, bridge member 31, mold 3c and dummy molds 33a and 33b are disassembled in this order so that the container body 2 is obtained.


[0038] The lid 3 will now be described in detail with reference to FIGS. 1 to 5. The lid 3 includes a base 10 made of a light-weight alloy such as an aluminum alloy. A lining 9 made of the same material as of the container body 2 is formed on an inside of the lid 3 by the molding. Two handholds 11 are mounted on an outside of the base 10. The lid 3 is pressed by a clamp shaft 21 when attached to the container body 2 to be closed. The lid 3 has two friction plates 12 attached to a surface of the lid 3 against which the clamp shaft 21 abuts. A locking mechanism 26 is provided on the base 10 for rotating the clamp shaft 21 for closure of the lid 3. The locking mechanism 26 includes a rod 13 and a compression coil spring 14 disposed about the rod between insertion plates 15a and 15b upstanding on the base 10. The spring 14 usually urges the rod 13 toward an insertion plate 15c.


[0039]
FIGS. 6 and 7 illustrate a closing mechanism for the lid 3. Reference numeral 16 designates a barrel casing for accommodating the barrel container 1. The barrel casing 16 is mounted on a rotational shaft 17a and a hollow rotational shaft 17b, both of which shafts are disposed on a central axis of the barrel casing 16. A partition plate 18 is provided in the interior of the barrel casing 16 to be spaced from the bottom of the casing. The barrel container 1 is supported on the partition plate 18 with rectangular sponge rubber members 19 being interposed therebetween. The partition plate 18 has rectangular notches 18a each of which is located inside the sponge rubber member 19. A pair of side plates 20 are fixed to both upper ends of the barrel casing 16 by bolts so as to be perpendicular to the rotational shafts 17a and 17b, respectively. The clamp shaft 21 is rotatably supported between the side plates 20. The clamp shaft 21 includes a rotational shaft and an eccentric cam 22 fitted with the shaft and extending substantially an entire length of the shaft. When the clamp shaft 21 is inserted into the side plates 20 and a central shaft 21a is then held to be rotated in the direction of arrow A, a protruding end of the eccentric cam 22 presses the friction plate 12 of the lid 3, closing the lid 3 against the container body 2. In this case, the sponge rubber members 19 are compressed such that airtightness is effected between the barrel container 1 and the partition plate 18. For example, four barrel casings 16 accommodating the respective barrel containers 1 are rotatably mounted on two revolving circular turrets 23 so as to be arranged along circumferences of the turrets at regular intervals, as shown in FIG. 8.


[0040] The following describes a case where workpieces are polished using the barrel container 1. Workpieces and polishing chips are put through the opening 2b into the container body 2. The barrel container 1 is then enclosed in the barrel casing 16, and the lid 3 is placed on the opening 2b. The clamp shaft 21 is inserted into the side plates 20, and the shaft 21a is then held to be rotated in the direction of arrow A so that the barrel container 1 is fixed to the barrel casing 16. The rod 13 of the locking mechanism 26 is previously retreated against the spring 14. When the rod 13 is returned after the shaft 21a has been rotated, the shaft 21a is fixed by the rod 13, whereupon rebound of the shaft is prevented. When the turrets 23 are revolved in the direction of arrow D in FIG. 8 and the shafts 17a and 17b are rotated in the direction of arrow E in FIG. 8, the workpieces are polished in each barrel container 1 as the result of revolution of the turrets 23 and rotation of each barrel container 1.


[0041] The barrel container 1 has two vents 25a and 25b. The vent 25b confronts the partition plate 18, and the partition plate 18 has the notches 18a. Accordingly, the interior of the barrel container 1 communicates via the space at the underside of the partition plate 18 with the hollow interior of the shaft 17b. A distal end of the shaft 17b is connected to a dust collector (not shown), which is driven during polishing so that air is drawn from the barrel container 1. As a result, shavings due to the polishing and dust are discharged through the small holes 4 of the polyurethane piece 5a attached to the vent 25b. The air is further fed through the exhaust passages B and C into the dust collector. In this case, since the sponge rubber members 19 are compressed such that airtightness is effected between the barrel container 1 and the partition plate 18, the air smoothly flows through the passages B and C. On the other hand, air is introduced through the small holes 4 of the polyurethane piece 5a of the vent 25a into the barrel container 1, so that an atmosphere in the barrel container 1 is cooled. Thus, the loading of the polishing chips can be prevented as the result of the above-described discharge of dust due to polishing and cooling the atmosphere in the barrel container 1. Furthermore, the workpieces can desirably be polished without adherence of soil thereto.


[0042] The polyurethane pieces 5a and 5b are fixed by bolts to the plates 6a and 6b respectively in the foregoing embodiment. However, the plates 6a and 6b may or may not be provided, and the polyurethane pieces 5a and 5b may be mounted directly on the casing body 2. Further, the barrel container 1 is mounted on the machine both revolving and rotating it in the foregoing embodiment. However, the barrel container 1 may be mounted on a rotary barrel polishing machine only rotating it. Additionally, the number of the vents may be one, two or more than two only if air can be introduced into the barrel container and dust due to polishing is discharged out of the barrel container.


[0043] According to the above-described embodiment, the container body of the barrel container is made by the molding without using the conventional steel casing body. Accordingly, the thickness of the container body is uniform although the container body is formed with the vents. There is no difference in the thickness even when a piece having the same thickness and formed with small holes is subsequently attached to the container body. Furthermore, since the container body is made of the elastic material such the polyurethane resin, it is light-weight, and a load of carrying the barrel container can be reduced. Furthermore, when made of the polyurethane resin with high wear and abrasion resistance, the barrel container can be used for a long period of time. Moreover, since the container body of the barrel container 1 has a larger thickness than the lining of the conventional container body made of steel, the service life of the barrel container can further be improved. Additionally, the polyurethane has a hardness ranging between 60 and 80 in ISO 7619 Shore A durometer hardness. Consequently, shock due to the collision of workpieces against the inner wall of the container body can be reduced in the dry barrel polishing as compared with the case of the wet barrel treatment. Thus, the marks due to the collision can be reduced.


[0044] The foregoing description and drawings are merely illustrative of the principles of the present invention and are not to be construed in a limiting sense. Various changes and modifications will become apparent to those of ordinary skill in the art. All such changes and modifications are seen to fall within the scope of the invention as defined by the appended claims.


Claims
  • 1. A barrel container for a dry barrel polishing machine, comprising: a container body made of an elastic material and having an access opening through which polishing chips and workpieces are put into the container body, the container body having a wall with a through hole providing communication between an exterior and an interior of the container body; and a lid opening and closing the access opening.
  • 2. A barrel container according to claim 1, wherein the elastic material is polyurethane.
  • 3. A barrel container according to claim 2, wherein the polyurethane has a hardness ranging between 60 and 80 in ISO 7619 Shore A durometer hardness.
  • 4. A barrel container according to claim 1, wherein the container body has a hole formed in the wall thereof, and which further comprises a piece made of an elastic material and having a number of small holes, the piece being attached to the hole o f the wall of the container body.
  • 5. A barrel container according to claim 4, further comprising a plate mounted on an outside of the container body so as to cover the hole, the plate having air permeability, wherein the piece is bolted to the plate at an inside of the container body.
  • 6. A barrel container according to claim 1, further comprising a barrel casing enclosing the container body with a space being defined in the barrel casing so as to communicate via the through hole of the container body with an interior of the container body, and a hollow shaft supporting the barrel container so that the barrel container is rotatable, the shaft having a communication passage defined therein so as to provide communication between the space of the barrel casing and a dust collector.
  • 7. A barrel container according to claim 6, wherein the container body has a hexagonal section and includes two peripheral sides adjacent to the access opening and a bottom, said peripheral sides and bottom being formed with a plurality of the through holes respectively, the bottom communicating with the space in the barrel casing for exhaust of air, the two peripheral sides communicating via the barrel casing with an exterior of the barrel casing for intake of air.
  • 8. A barrel container according to claim 1, wherein the container body is molded from the molten elastic material.
Priority Claims (1)
Number Date Country Kind
2000-225779 Jul 2000 JP