The present invention relates to an article comprising a plastic or glass substrate and an atmospheric gas penetration barrier fabricated by atomic layer deposition. The article may be a component of an electrical or electronic device such as an organic light emitting diode. The article may also be used as a container for applications where gas permeation is important.
Featherby and Dehaven (WO 2001067504) disclose a hermetically coated device. Formation of such a device includes the steps of providing an integrated semiconductor circuit die, applying a first layer comprising an inorganic material which envelopes the circuit die, and applying a second layer enveloping the circuit die.
Aintila (WO 9715070 A2) discloses contact bump formation on metallic contact pad areas on the surface of a substrate comprising using atomic layer epitaxy to form an oxide layer on the substrate which is opened at required points in the subsequent process step.
Aftergut and Ackerman (U.S. Pat. No. 5,641,984) disclose a hermetically packaged radiation imager including a moisture barrier. A dielectric material layer is deposited in an atomic layer expitaxy technique as part of the sealing structure.
Aftergut and Ackerman (U.S. Pat. No. 5,707,880) disclose a hermetically packaged radiation imager including a moisture barrier comprising a dielectric material layer deposited by atomic layer expitaxy.
None of the references disclosed a permeation barrier comprising a polymer or glass substrate.
This invention describes an article comprising:
The present invention is further an article comprising:
The invention further describes an embodiment that is an enclosed container.
Another embodiment of the present invention is an electrical or electronic device.
Yet another embodiment of the present invention is a light-emitting polymer device.
Yet another embodiment of the present invention is liquid crystalline polymer device.
The invention further describes an organic light emitting diode.
Another embodiment of the present invention is a transistor.
Yet another embodiment of the present invention is a circuit comprising a light emitting polymer device.
A still further article is an organic photovoltaic cell.
A second article taught herein comprises a plurality of layers, each layer comprising one article, as described above, wherein the articles are in contact with each other. In one embodiment of this second article of the articles above are in contact with each other by lamination means.
The permeation of O2 and H2O vapor through polymer films is facile. To reduce permeability for packaging applications, polymers are coated with a thin inorganic film. Al-coated polyester is common. Optically transparent barriers, predominantly SiOx or AlOy, made either by physical vapor deposition (PVD) or chemical vapor deposition (CVD), are also used in packaging. The latter films are commercially available and are known in the industry as “glass-coated” barrier films. They provide an improvement for atmospheric gas permeation of about 10×, reducing transmission rates to about 1.0 cc O2/m2/day and 1.0 ml H2O/m2/day through polyester film (M. Izu, B. Dotter, and S. R. Ovshinsky, J. Photopolymer Science and Technology., vol. 8 1995 pp 195-204). While this modest improvement is a reasonable compromise between performance and cost for many high-volume packaging applications, this performance falls far short of packaging requirements in electronics. Electronic packaging usually requires at least an order of magnitude longer desired lifetime than, for example, beverage containing. As an example, flexible displays based on organic light emitting polymers (OLEDs), fabricated on flexible polyester substrates need an estimated barrier improvement of 105-106× for exclusion of atmospheric gases since gases can seriously degrade both the light-emitting polymer and the water-sensitive metal cathode which can frequently be Ca or Ba.
Because of their inherent free volume fraction, the intrinsic permeability of polymers is, in general, too high by a factor 104-106 to achieve the level of protection needed in electronic applications, such as flexible OLED displays. Only inorganic materials, with essentially zero permeability, can provide adequate barrier protection. Ideally, a defect-free, continuous thin-film coating of an inorganic should be impermeable to atmospheric gases. However, the practical reality is that thin films have defects, such as pinholes, either from the coating process or from substrate imperfections which compromise barrier properties. Even grain boundaries in films can present a pathway for facile permeation. For the best barrier properties, films should be deposited in a clean environment on clean, defect-free substrates. The film structure should be amorphous. The deposition process should be non-directional, (i.e. CVD is preferred over PVD) and the growth mechanism to achieve a featureless microstructure would ideally be layer-by-layer to avoid columnar growth with granular microstructure.
Atomic layer deposition (ALD) is a film growth method that satisfies many of these criteria for low permeation. A description of the atomic layer deposition process can be found in “Atomic Layer Epitaxy,” by Tuomo Suntola in Thin Solid Films, vol. 216 (1992) pp. 84-89. As its name implies, films grown by ALD form by a layer by layer process. In general, a vapor of film precursor is absorbed on a substrate in a vacuum chamber. The vapor is then pumped from the chamber, leaving a thin layer of absorbed precursor, usually essentially a monolayer, on the substrate. A reactant is then introduced into the chamber under thermal conditions, which promote reaction with the absorbed precursor to form a layer of the desired material. The reaction products are pumped from the chamber. Subsequent layers of material can be formed by again exposing the substrate to the precursor vapor and repeating the deposition process. ALD is in contrast to growth by common CVD and PVD methods where growth is initiated and proceeds at finite numbers of nucleation sites on the substrate surface. The latter technique can lead to a columnar microstructures with boundaries between columns along which gas permeation can be facile. ALD can produce very thin films with extremely low gas permeability, making such films attractive as barrier layers for packaging sensitive electronic devices and components built on plastic substrates.
This invention describes barrier layers formed by ALD on plastic substrates and useful for preventing the passage of atmospheric gases. The substrates of this invention include the general class of polymeric materials, such as described by but not limited to those in Polymer Materials, (Wiley, New York, 1989) by Christopher Hall or Polymer Permeability, (Elsevier, London, 1985) by J. Comyn. Common examples include polyethylene terephthalate (PET) and polyethylene naphthalate (PEN), which are commercially available as film base by the roll. The materials formed by ALD, suitable for barriers, include oxides and nitrides of Groups IVB, VB, VIB, IIIA, and IVA of the Periodic Table and combinations thereof. Of particular interest in this group are SiO2, Al2O3, and Si3N4. One advantage of the oxides in this group is optical transparency which is attractive for electronic displays and photovoltaic cells where visible light must either exit or enter the device. The nitrides of Si and Al are also transparent in the visible spectrum.
The precursors used in the ALD process to form these barrier materials can be selected from precursors known to those skilled in the art and tabulated in published references such as M. Leskela and M. Ritala, “ALD precursor chemistry: Evolution and future challenges,” in Journal de Physique IV, vol. 9, pp 837-852 (1999) and references therein.
The preferred range of substrate temperature for synthesizing these barrier coatings by ALD is 50° C.-250° C. Too high temperature (>250° C.) is incompatible with processing of temperature-sensitive plastic substrates, either because of chemical degradation of the plastic substrate or disruption of the ALD coating because of large dimensional changes of the substrate.
The preferred thickness range for barrier films is 2 nm-100 nm. A more preferred range is 2-50 nm. Thinner layers will be more tolerant to flexing without causing the film to crack. This is extremely important for polymer substrates where flexibility is a desired property. Film cracking will compromise barrier properties. Thin barrier films also increase transparency in the cases of electronic devices where input or output of light is important. There may be a minimum thickness corresponding to continuous film coverage, for which all of the imperfections of the substrate are covered by the barrier film. For a nearly defect-free substrate, the threshold thickness for good barrier properties was estimated to be at least 2 nm, but may be as thick as 10 nm.
Some oxide and nitride barrier layers coated by ALD may require a “starting” or “adhesion layer” to promote adhesion to the plastic substrate or the article requiring protection. The preferred thickness of the adhesion layer is in the range of 1 nm-100 nm. The choice of the materials for the adhesion layer will be from the same group of barrier materials. Aluminum oxide and silicon oxide are preferred for the adhesion layer, which may also be deposited by ALD, although other methods such as chemical and physical vapor deposition or other deposition methods known in the art may also be suitable.
The basic building block of the barrier structure is either: (A) a single barrier layer with or without an adhesion layer, coated by ALD on a plastic or glass substrate, or (B) a barrier layer with or without an adhesion layer, coated by ALD on each side of a plastic substrate. This basic structure can then be combined in any number of combinations by laminating this building block to itself to form multiple, independent barrier layers. It is known in the art of barrier coatings that multiple layers, physically separate, can improve the overall barrier properties by much more than a simple multiplicative factor, corresponding the number of layers. This is demonstrated, for example, in J. Phys. Chem. B 1997, vol. 101, pp 2259-2266, “Activated rate theory treatment of oxygen and water transport through silicon oxide/poly(ethylene terephthalate) composite barrier structures,” by Y. G. Tropsha and N. G. Harvey. This follows because the path for diffusing gas molecules is tortuous through multiple barrier layers that are separated. The effective diffusion path is much larger than the sum of the thickness of the individual layers.
Another barrier configuration involves directly coating the electronic or electro-optical device, requiring protection. In this regard, ALD is particularly attractive because it forms a highly conformal coating. Therefore devices with complex topographies can be fully coated and protected.
Another version of a packaging scheme is shown in
In
A substrate film of polyethylene terephthalate (PEN), 0.002 inches thick, was coated by atomic layer deposition at 120° C. with Al2O3 about 25 nm thick on one side of the PEN substrate. Prior to evaluating its permeability properties the coated PEN substrate was flexed at least once to a radius of at least 1.5 inches to remove the coated Al2O3-coated PEN substrate from the rigid silicon carrier wafer, to which it was attached with Kapton® tape during ALD deposition. The oxygen transport rate with 50% relative humidity was measured with a commercial instrument (MOCON Ox-Tran 2/20) through the film with Al2O3 deposited by ALD. After 80 hours of measurement time, within the measurement sensitivity (0.005 cc-O2/m2/day), no oxygen transport (<0.005 cc/m2/day) through the barrier film was detected, in spite of the severe prior flexing. For comparison, we measured oxygen transport of about 10 cc-O2/m2/day through an uncoated PEN substrate.
Number | Date | Country | |
---|---|---|---|
60471020 | May 2003 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 10846749 | May 2004 | US |
Child | 12055560 | US |